GB/T 14976 07Cr19Ni10 Seamless Stainless Steel Pipe
What is GB/T 14976 07Cr19Ni10 Seamless Stainless Steel Pipe
Fluid-transport packages written to Chinese product standards look to GB/T 14976-2025 rather than inventing a mill grade from AISI shorthand alone. 07Cr19Ni10 is the Table 2/3 Chinese grade name for this austenitic chemistry (S30409). GB/T 14976 07Cr19Ni10 exists so buyers stop pretending ordinary 06Cr19Ni10 meets a written elevated-temperature carbon floor on Chinese fluid specs.
Mill path for 07Cr19Ni10: manufacture symbol W-C/W-H, Table 1 heat treatment, Table 2 cast chemistry, Table 3 tensile floors, hydrostatic or NDT per 7.3. SHH STEEL can make and supply the grade to that stack. Typical use: high-temperature process steam headers, heat-recovery fluid loops, reformer transfer at moderate pressure, and hot utility lines written to 304H-class chemistry.
Body text may mention 304H / UNS S30409 (unified S30409) for cross-reference, but the H1 and order line stay on 07Cr19Ni10. Silent alias swaps are how wrong carbon ceilings and wrong tensile tables enter the MTC. Keep this caution in view: the 0.04–0.10% carbon window is intentional — do not dual-file as 022Cr19Ni10; clause 7.5 exempts this mark from mandatory IGC, so corrosive as-welded aqueous duty still prefers an L or stabilised sister.
Order the standard the drawing and regulatory file actually require. Inside this 14976 series, compare 06Cr19Ni10, 07Cr17Ni12Mo2, 07Cr19Ni11Ti, 07Cr18Ni11Nb before stretching surface finish or wall alone. Duty thread: controlled-carbon 18-8 austenitic seamless pipe aimed at elevated-temperature fluid lines that need a carbon floor. Document the medium, design temperature, and weld map beside the 07Cr19Ni10 line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Weld-shop note tied to 07Cr19Ni10: 308H-class fillers when matching hot strength; do not treat the joint like a low-carbon L weld without procedure review.
Inside this GB/T 14976 series, compare 06Cr19Ni10, 07Cr17Ni12Mo2, 07Cr19Ni11Ti, 07Cr18Ni11Nb. Hub: GB/T 14976. ASTM/ASME related product pages (not interchangeable by default): A312 TP304H.
Chemical Composition of GB/T 14976 07Cr19Ni10
Table 2 sets the melt limits for 07Cr19Ni10. Highlight band: C 0.04–0.10, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.030, Ni 8.00–11.00, Cr 18.00–20.00. Product analysis, when ordered, applies GB/T 222 stainless product tolerances on top of Table 2. Alias note: 304H / UNS S30409. Every ladle analysis for 07Cr19Ni10 is checked against those windows before the heat is released to piercing or drawing, and the same numbers reappear on the inspection document. Weld-shop note tied to 07Cr19Ni10: 308H-class fillers when matching hot strength; do not treat the joint like a low-carbon L weld without procedure review.
The composition table below is the cast window SHH STEEL quotes against for 07Cr19Ni10. Edition framing is GB/T 14976-2025. Use thread: high-temperature process steam headers, heat-recovery fluid loops, reformer transfer at moderate pressure, and hot utility lines written to 304H-class chemistry. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 2, SHH STEEL will confirm melt feasibility for 07Cr19Ni10 before the order is acknowledged. Weld-shop note tied to 07Cr19Ni10: 308H-class fillers when matching hot strength; do not treat the joint like a low-carbon L weld without procedure review.
| Grade | C | Si | Mn | P | S | Ni | Cr |
|---|---|---|---|---|---|---|---|
| 07Cr19Ni10 | 0.04–0.10 | ≤1.00 | ≤2.00 | ≤0.035 | ≤0.030 | 8.00–11.00 | 18.00–20.00 |
Mechanical Properties of GB/T 14976 07Cr19Ni10
Table 3 mechanical acceptance for 07Cr19Ni10: Rm min 520 MPa, Rp0.2 min 205 MPa, elongation longitudinal min 35% / transverse min 30%. Delivery framing: solution annealed. Sampling follows chapter 8/10 rules for the batch of 07Cr19Ni10. Tensile sampling follows the batch rules for the ordered test unit of 07Cr19Ni10, and retests follow GB/T 2102 when a result sits under the Table 3 floor. Keep the 07Cr19Ni10 caution visible here: the 0.04–0.10% carbon window is intentional — do not dual-file as 022Cr19Ni10; clause 7.5 exempts this mark from mandatory IGC, so corrosive as-welded aqueous duty still prefers an L or stabilised sister.
| Grade | Rm min (MPa) | Rp0.2 min (MPa) | A long. min (%) | A trans. min (%) |
|---|---|---|---|---|
| 07Cr19Ni10 | 520 | 205 | 35 | 30 |
Ambient values from GB/T 14976-2025 Table 3 for 07Cr19Ni10. Heat treatment (Table 1): 1010–1150 °C, water or rapid cool. Density 7.93 kg/dm³. Delivery: solution annealed.
Seamless Pipe Manufacture of GB/T 14976 07Cr19Ni10
SHH STEEL can produce 07Cr19Ni10 as cold-finished seamless (W-C) or hot-finished seamless (W-H), then apply Table 1 heat treatment and pickle (or bright anneal) as ordered. Bevel ends are available by agreement; square-cut plain ends are the default when the PO is silent. Seamless W-C and W-H options remain available for 07Cr19Ni10; the acknowledgement repeats the manufacture symbol so production cannot silently change route after the PO is firm. This paragraph is locked to 07Cr19Ni10 duty: controlled-carbon 18-8 austenitic seamless pipe aimed at elevated-temperature fluid lines that need a carbon floor.
After forming, 07Cr19Ni10 receives Table 1 treatment — 1010–1150 °C, water or rapid cool. Austenitic heats take solution annealing with water or other rapid cool per Table 1; hot-rolled austenitic pipe may count in-line rapid cool inside the Table 1 temperature band as meeting heat treatment (6.3.2) unless the purchaser forbids it. Use thread: high-temperature process steam headers, heat-recovery fluid loops, reformer transfer at moderate pressure, and hot utility lines written to 304H-class chemistry.
Marking carries the grade 07Cr19Ni10, manufacture cues, manufacturer ID, and GB/T 2102 items. Size hint: hot-finished W-H common for heavier hot-service walls; cold-drawn W-C for thinner precision OD. Weld thread for fabricator joints: 308H-class fillers when matching hot strength; do not treat the joint like a low-carbon L weld without procedure review.
Dimensions and Tolerances for GB/T 14976 07Cr19Ni10
Dimensional order lines for 07Cr19Ni10 should state OD × wall (or ID × wall), length type, end finish, and PA or PC tolerance class. Use: high-temperature process steam headers, heat-recovery fluid loops, reformer transfer at moderate pressure, and hot utility lines written to 304H-class chemistry. Tolerance class (PA/PC) follows the precision ordered for 07Cr19Ni10, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Application context for 07Cr19Ni10 stays high-temperature process steam headers, heat-recovery fluid loops, reformer transfer at moderate pressure, and hot utility lines written to 304H-class chemistry.
OD and wall tolerances differ for hot-finished W-H versus cold-finished W-C and for PA versus PC — quote the manufacture symbol with the size. Caution: the 0.04–0.10% carbon window is intentional — do not dual-file as 022Cr19Ni10; clause 7.5 exempts this mark from mandatory IGC, so corrosive as-welded aqueous duty still prefers an L or stabilised sister.
Equivalent Grades for GB/T 14976 07Cr19Ni10
Do not treat 304H / UNS S30409 as interchangeable paperwork for GB/T 14976 07Cr19Ni10. Chemistry kinship is not acceptance kinship under this product standard. Hydrostatic, NDT, and heat-treatment text diverge across systems even when the cast analysis looks familiar. Keep the governing standard symbol on the acknowledgement so mechanical tables cannot drift under a trade name (07Cr19Ni10).
| System | Designation | Notes |
|---|---|---|
| GB/T 14976 | 07Cr19Ni10 | Governing pipe grade for this page |
| Commercial / UNS (body only) | 304H / UNS S30409 | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A312 related | Related chemistry family (no identical grade asserted) | Related chemistry — different product standard; not interchangeable by default |
| EN / other | No one-to-one asserted | Starting point for comparison only against local product specs |
When the service outgrows 07Cr19Ni10, move to a sister rather than stretching the alias: 06Cr19Ni10, 07Cr17Ni12Mo2, 07Cr19Ni11Ti, 07Cr18Ni11Nb. Apps context: high-temperature process steam headers, heat-recovery fluid loops, reformer transfer at moderate pressure, and hot utility lines written to 304H-class chemistry. Full list under GB/T 14976. Keep the governing standard symbol on the acknowledgement so mechanical tables cannot drift under a trade name (07Cr19Ni10).
Heat Treatment and Delivery Condition for GB/T 14976 07Cr19Ni10
Mill heat treatment for 07Cr19Ni10: 1010–1150 °C, water or rapid cool. Bright annealing or overall machining may omit pickling when the surface is scale-free. Delivery label: solution annealed. Recorded furnace charts for 07Cr19Ni10 should support the Table 1 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. This paragraph is locked to 07Cr19Ni10 duty: controlled-carbon 18-8 austenitic seamless pipe aimed at elevated-temperature fluid lines that need a carbon floor.
Certificate wording for 07Cr19Ni10 should show the heat-treatment condition actually performed, not a generic “annealed” stamp that hides temperature. Use: high-temperature process steam headers, heat-recovery fluid loops, reformer transfer at moderate pressure, and hot utility lines written to 304H-class chemistry. Field heat treatment of 07Cr19Ni10 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. This paragraph is locked to 07Cr19Ni10 duty: controlled-carbon 18-8 austenitic seamless pipe aimed at elevated-temperature fluid lines that need a carbon floor.
Corrosion Resistance of GB/T 14976 07Cr19Ni10
oxidation resistance is adequate for many hot utility duties, but aqueous chloride pitting remains similar to standard 06Cr19Ni10 Special Annex A cryogenic or Annex B oxygen extras are not a blanket corrosion warranty. Family filing: austenitic. Clause 7.5 exempts 07Cr19Ni10 from mandatory IGC — do not assume a Strauss coupon will appear unless the PO adds it.
Do not market invented PREN digits. Bring medium chemistry and SHH STEEL will map 07Cr19Ni10 honestly against 06Cr19Ni10, 07Cr17Ni12Mo2, 07Cr19Ni11Ti, 07Cr18Ni11Nb. Role: controlled-carbon 18-8 austenitic seamless pipe aimed at elevated-temperature fluid lines that need a carbon floor. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 07Cr19Ni10 rather than relying on wall thickness alone. This paragraph is locked to 07Cr19Ni10 duty: controlled-carbon 18-8 austenitic seamless pipe aimed at elevated-temperature fluid lines that need a carbon floor.
Applications of GB/T 14976 07Cr19Ni10 Seamless Pipe
Typical BOM language pairs GB/T 14976 07Cr19Ni10 with OD × wall, W-C or W-H, PA/PC, and heat-treatment condition. Primary sketch: high-temperature process steam headers, heat-recovery fluid loops, reformer transfer at moderate pressure, and hot utility lines written to 304H-class chemistry. Spool fabricators should copy 07Cr19Ni10 onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Corrosion framing beside 07Cr19Ni10: oxidation resistance is adequate for many hot utility duties, but aqueous chloride pitting remains similar to standard 06Cr19Ni10.
Spell 07Cr19Ni10 on isometrics, spool sheets and valve specs alike. Sister options when the medium hardens: 06Cr19Ni10, 07Cr17Ni12Mo2, 07Cr19Ni11Ti, 07Cr18Ni11Nb. Commissioning teams benefit when the as-built dossier repeats 07Cr19Ni10 beside heat numbers, linking isometric revisions to the same mill certificates. Weld-shop note tied to 07Cr19Ni10: 308H-class fillers when matching hot strength; do not treat the joint like a low-carbon L weld without procedure review.
Weldability of GB/T 14976 07Cr19Ni10
Weldability of 07Cr19Ni10 follows austenitic practice. Filler/shop note: 308H-class fillers when matching hot strength; do not treat the joint like a low-carbon L weld without procedure review. Caution: the 0.04–0.10% carbon window is intentional — do not dual-file as 022Cr19Ni10; clause 7.5 exempts this mark from mandatory IGC, so corrosive as-welded aqueous duty still prefers an L or stabilised sister.
For corrosive as-welded duty on 07Cr19Ni10, confirm low-carbon, stabilisation, or anneal practice as applicable. Shop note: 308H-class fillers when matching hot strength; do not treat the joint like a low-carbon L weld without procedure review. Consumable lot control and shielding-gas notes for 07Cr19Ni10 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Weld-shop note tied to 07Cr19Ni10: 308H-class fillers when matching hot strength; do not treat the joint like a low-carbon L weld without procedure review.
Surface Finishes for GB/T 14976 07Cr19Ni10
Iron-free handling after pickle matters for 07Cr19Ni10 — carbon-steel strapping stains show up later as rust blooms on finished pipe. Standard route is solution annealed and pickled when HT is specified; polish scope must name the surface. Apps: high-temperature process steam headers, heat-recovery fluid loops, reformer transfer at moderate pressure, and hot utility lines written to 304H-class chemistry.
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard pipe mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
OD stencil ink on 07Cr19Ni10 should be chloride-lean and removable where coatings follow. Passivation will not repair a cast that missed chemistry windows. Close bundles only after free-iron and burn marks are cleared. Free-iron control continues through storage and shipment, because late carbon-steel contact can stain an otherwise clean pickle (07Cr19Ni10).
Inspection and Testing for GB/T 14976 07Cr19Ni10
SHH STEEL reports the tests actually performed for 07Cr19Ni10 — no surrogate NDT lines. Hydrostatic vs eddy-current/ultrasonic choice belongs on the PO when replacement is allowed. Caution: the 0.04–0.10% carbon window is intentional — do not dual-file as 022Cr19Ni10; clause 7.5 exempts this mark from mandatory IGC, so corrosive as-welded aqueous duty still prefers an L or stabilised sister.
NDT acceptance defaults to GB/T 5777 U3 or GB/T 7735 E4H/E4 when UT/ET replace hydro; Annex A/B may tighten to U2.5. Size context: hot-finished W-H common for heavier hot-service walls; cold-drawn W-C for thinner precision OD. Non-conforming 07Cr19Ni10 lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Size practice for 07Cr19Ni10 remains hot-finished W-H common for heavier hot-service walls; cold-drawn W-C for thinner precision OD.
Packaging and Shipping for GB/T 14976 07Cr19Ni10
Export packing for GB/T 14976 07Cr19Ni10 is built around rust prevention and transit abrasion control. Bundle tickets repeat the grade symbol and heat number. Duty: controlled-carbon 18-8 austenitic seamless pipe aimed at elevated-temperature fluid lines that need a carbon floor. Bundle tickets for 07Cr19Ni10 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Application context for 07Cr19Ni10 stays high-temperature process steam headers, heat-recovery fluid loops, reformer transfer at moderate pressure, and hot utility lines written to 304H-class chemistry.
Marking paint and ink stickers stay chloride-lean. Heat numbers on tags match the MTC for 07Cr19Ni10. Desiccant and wrap choices for 07Cr19Ni10 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Size practice for 07Cr19Ni10 remains hot-finished W-H common for heavier hot-service walls; cold-drawn W-C for thinner precision OD.
Photographic packing records are available on request for project QA files on 07Cr19Ni10. Claims handling for 07Cr19Ni10 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Corrosion framing beside 07Cr19Ni10: oxidation resistance is adequate for many hot utility duties, but aqueous chloride pitting remains similar to standard 06Cr19Ni10.
Why Choose SHH STEEL
SHH STEEL can produce and supply GB/T 14976 07Cr19Ni10. Buyers choose SHH STEEL for 07Cr19Ni10 because the paperwork matches the stencil: Table 2 chemistry, Table 3 tensile, Table 1 heat treatment, and honest seamless marking. Application fit: high-temperature process steam headers, heat-recovery fluid loops, reformer transfer at moderate pressure, and hot utility lines written to 304H-class chemistry.
SHH STEEL will not invent PREN posters or warehouse tonnages. Bring OD × wall, medium notes, and test scope — we will quote 07Cr19Ni10 cleanly. Ask for a written acknowledgement that names 07Cr19Ni10, W-C or W-H, and the Table 1 heat-treatment condition before melt. SHH STEEL can make 07Cr19Ni10 to that written scope.
Supply Capability
Supply capability for 07Cr19Ni10 covers seamless manufacture symbols, Table 1 heat treatment, and Table 3 mechanical acceptance. SHH STEEL can make the sizes on your list when the mill slot fits. Role: controlled-carbon 18-8 austenitic seamless pipe aimed at elevated-temperature fluid lines that need a carbon floor. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for 07Cr19Ni10 when the mill schedule allows.
| Item | Capability |
|---|---|
| Standard | GB/T 14976-2025 seamless stainless steel pipes for fluid transport |
| Grade | 07Cr19Ni10 (S30409) |
| Product form | Seamless pipe only — cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H) |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered) |
| Typical size practice | OD × wall per GB/T 17395; PA ordinary or PC higher precision; usual length 4000–12000 mm |
| Wall / ordering | Nominal OD×wall, OD×min wall, or ID×wall by agreement |
Stock / Available sizes
Stock / Available sizes for 07Cr19Ni10: common OD×wall combinations as the project uses. Seamless W-C versus W-H availability varies by diameter — confirm route with the RFQ. Hint: hot-finished W-H common for heavier hot-service walls; cold-drawn W-C for thinner precision OD. SHH STEEL can supply alternate walls and precision classes for 07Cr19Ni10 once the design pressure and corrosion allowance are clear.
Mill certificates, packing photos, and third-party witness can be bundled into the 07Cr19Ni10 supply scope when the PO says so. Use: high-temperature process steam headers, heat-recovery fluid loops, reformer transfer at moderate pressure, and hot utility lines written to 304H-class chemistry. SHH STEEL can produce trial lengths of 07Cr19Ni10 for procedure qualification before the bulk release when the project calendar needs it.
FAQ
-
What is GB/T 14976 07Cr19Ni10 seamless stainless steel pipe used for?
- GB/T 14976 07Cr19Ni10 is seamless stainless pipe for fluid transport — high-temperature process steam headers, heat-recovery fluid loops, reformer transfer at moderate pressure, and hot utility lines written to 304H-class chemistry. Role summary: controlled-carbon 18-8 austenitic seamless pipe aimed at elevated-temperature fluid lines that need a carbon floor. It is a Chinese product standard grade (S30409), not an automatic ASTM A312 certificate.
-
Is GB/T 14976 07Cr19Ni10 seamless only, or does it cover welded pipe?
- Seamless only. Clause 6.2 limits manufacture to cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 07Cr19Ni10 when the mill can meet the ordered size and tests. Welded pipe belongs under other standards, not 14976.
-
What heat treatment applies to 07Cr19Ni10?
- 07Cr19Ni10 is delivered solution annealed under GB/T 14976. Table 1 reference: 1010–1150 °C, water or rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Keep the purchase order locked to GB/T 14976 and 07Cr19Ni10 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
-
How does 07Cr19Ni10 compare with sister grades 06Cr19Ni10, 07Cr17Ni12Mo2, 07Cr19Ni11Ti?
- 07Cr19Ni10 is filed as austenitic. Typical sisters on the same RFQ are 06Cr19Ni10, 07Cr17Ni12Mo2, 07Cr19Ni11Ti. Design caution: the 0.04–0.10% carbon window is intentional — do not dual-file as 022Cr19Ni10; clause 7.5 exempts this mark from mandatory IGC, so corrosive as-welded aqueous duty still prefers an L or stabilised sister Pick the sister when the medium or strength floor outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 07Cr19Ni10?
- Expect cast analysis (Table 2), room-temperature tensile results (Table 3), dimensions, hydrostatic test (or replacing UT/ET), appearance, and every special annex or IGC test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
-
Is 304H / UNS S30409 the same as ordering 07Cr19Ni10?
- No. 304H / UNS S30409 is a commercial / UNS cross-walk for body text (unified S30409). The purchase order should lock GB/T 14976 and 07Cr19Ni10 so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GB/T 14976 07Cr19Ni10?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 07Cr19Ni10 within GB/T 17395 practice, with PA or PC precision and measured or min-wall options by agreement. Size context: hot-finished W-H common for heavier hot-service walls; cold-drawn W-C for thinner precision OD. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
How should 07Cr19Ni10 be welded on site?
- Shop guidance: 308H-class fillers when matching hot strength; do not treat the joint like a low-carbon L weld without procedure review. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: the 0.04–0.10% carbon window is intentional — do not dual-file as 022Cr19Ni10; clause 7.5 exempts this mark from mandatory IGC, so corrosive as-welded aqueous duty still prefers an L or stabilised sister
-
When should I choose a higher-Mo or superaustenitic grade instead of 07Cr19Ni10?
- Move when chloride pitting, crevice attack, or reducing-acid risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: the 0.04–0.10% carbon window is intentional — do not dual-file as 022Cr19Ni10; clause 7.5 exempts this mark from mandatory IGC, so corrosive as-welded aqueous duty still prefers an L or stabilised sister Sister pointers: 06Cr19Ni10, 07Cr17Ni12Mo2, 07Cr19Ni11Ti. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GB/T 14976 07Cr19Ni10 with ASTM A312?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 14976 07Cr19Ni10 does not clear ASTM acceptance by default. State both standards, sizes, and test scopes before melt. Keep the purchase order locked to GB/T 14976 and 07Cr19Ni10 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
-
What surface finishes are available for 07Cr19Ni10?
- Pickled after heat treatment is the usual fluid-transport supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 07Cr19Ni10 when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
GB/T 14976 07Cr19Ni10 is seamless stainless steel pipe for fluid transport — controlled-carbon 18-8 austenitic seamless pipe aimed at elevated-temperature fluid lines that need a carbon floor. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 06Cr19Ni10, 07Cr17Ni12Mo2, 07Cr19Ni11Ti. Related ASTM pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.