GB/T 14976 06Cr17Ni12Mo2Ti Seamless Stainless Steel Pipe | GB/T 14976 Stainless Steel Pipe - SHH STEEL

GB/T 14976 06Cr17Ni12Mo2Ti Seamless Stainless Steel Pipe

GB/T 14976 06Cr17Ni12Mo2Ti seamless stainless steel pipe (316Ti / UNS S31668, S31668), austenitic, Table 2 cast analysis, Rm min 530 MPa / Rp0.2 min 205 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
Grade
06Cr17Ni12Mo2Ti (S31668 / 316Ti / UNS S31668 — body alias)
Standard
GB/T 14976-2025
Product form
Seamless stainless steel pipe (W-C / W-H), delivery solution annealed
Size
OD × wall per GB/T 17395; PA/PC precision; usual length 4000–12000 mm; other by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Pipe Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GB/T 14976 06Cr17Ni12Mo2Ti Seamless Stainless Steel Pipe

When the approved vendor list and isometric notes say GB/T 14976, the grade mark has to be the Chinese designation. 06Cr17Ni12Mo2Ti is the full product grade for this austenitic seamless pipe. GB/T 14976 06Cr17Ni12Mo2Ti exists so buyers stop pretending a titanium sticker on 06Cr17Ni12Mo2 paperwork is the same as ordering the stabilised mark.

SHH STEEL can supply 06Cr17Ni12Mo2Ti seamless pipe in cold-finished or hot-finished routes, with plain or bevelled ends, random or cut lengths, and GB/T 2102 / EN 10204 3.1 style inspection documents when specified. Role on the line: Ti-stabilised Mo austenitic seamless pipe for chloride fluid systems welded without post-weld anneal. Size and test clarity on the RFQ lets SHH STEEL lock the correct W-C or W-H symbol for 06Cr17Ni12Mo2Ti before production starts. Weld-shop note tied to 06Cr17Ni12Mo2Ti: 316L or Ti-bearing fillers per WPS; limit heat input that can dissolve stabilisation carbides.

Equivalence talk to 316Ti / UNS S31668 belongs in engineering notes, not as a substitute for the Chinese grade. Lock GB/T 14976 06Cr17Ni12Mo2Ti, OD × wall, manufacture route, and any Annex A/B extras before melt. Watch-out: Ti window is 5(C+N)–0.70 — do not dual-file as plain 06Cr17Ni12Mo2; confirm Ti on the MTC line.

Related ASTM pipe pages share chemistry families but not Chinese acceptance text — confirm before dual-cert claims. Sisters on this hub: 022Cr17Ni12Mo2, 06Cr17Ni12Mo2, 06Cr18Ni11Ti, 06Cr18Ni11Nb. Use thread: chemical transfer with dense field welds, heat-exchange fluid loops, and process lines that want 316Ti-class stabilisation plus molybdenum. Document the medium, design temperature, and weld map beside the 06Cr17Ni12Mo2Ti line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Weld-shop note tied to 06Cr17Ni12Mo2Ti: 316L or Ti-bearing fillers per WPS; limit heat input that can dissolve stabilisation carbides.

Inside this GB/T 14976 series, compare GB/T 14976 022Cr17Ni12Mo2, GB/T 14976 06Cr17Ni12Mo2, GB/T 14976 06Cr18Ni11Ti, GB/T 14976 06Cr18Ni11Nb. Hub: GB/T 14976. ASTM/ASME related product pages (not interchangeable by default): ASTM A312 TP316Ti.

Buyers comparing 06Cr17Ni12Mo2Ti tubulars with sheet/plate can link Stainless Steel Pipes and Tubes, Stainless Steel Sheets and Plates, and GB/T 4237 06Cr17Ni12Mo2Ti so purchasing does not treat one product form as the other. Flat Chinese grades in-family are indexed at GB/T 4237. Do not stretch a 06Cr17Ni12Mo2Ti pipe certificate onto plate.

Chemical Composition of GB/T 14976 06Cr17Ni12Mo2Ti

Chemistry control on 06Cr17Ni12Mo2Ti starts at the ladle. Expect C ≤0.08, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.030, Ni 10.00–14.00, Cr 16.00–18.00, Mo 2.00–3.00 within Table 2, reported on the inspection document against the heat. Body alias 316Ti / UNS S31668 does not widen those windows. Every ladle analysis for 06Cr17Ni12Mo2Ti is checked against those windows before the heat is released to piercing or drawing, and the same numbers reappear on the inspection document. Size practice for 06Cr17Ni12Mo2Ti remains W-C common for welded spool programmes; heat treatment 1000–1100 °C per Table 1.

Read the table with the family in mind — austenitic — and with caution Ti window is 5(C+N)–0.70 — do not dual-file as plain 06Cr17Ni12Mo2; confirm Ti on the MTC line. Numbers without the matching Table 1 heat-treatment row are incomplete purchase data. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 2, SHH STEEL will confirm melt feasibility for 06Cr17Ni12Mo2Ti before the order is acknowledged. Application context for 06Cr17Ni12Mo2Ti stays chemical transfer with dense field welds, heat-exchange fluid loops, and process lines that want 316Ti-class stabilisation plus molybdenum.

Grade C Si Mn P S Ni Cr Mo N Ti
06Cr17Ni12Mo2Ti ≤0.08 ≤1.00 ≤2.00 ≤0.035 ≤0.030 10.00–14.00 16.00–18.00 2.00–3.00 ≤0.10 5(C+N)–0.70

Mechanical Properties of GB/T 14976 06Cr17Ni12Mo2Ti

Proof stress and tensile minima for 06Cr17Ni12Mo2Ti sit at Rm min 530 MPa, Rp0.2 min 205 MPa, elongation longitudinal min 35% / transverse min 30%. Flattening or bend testing backs ductility when ordered. Watch-out: Ti window is 5(C+N)–0.70 — do not dual-file as plain 06Cr17Ni12Mo2; confirm Ti on the MTC line. Tensile sampling follows the batch rules for the ordered test unit of 06Cr17Ni12Mo2Ti, and retests follow GB/T 2102 when a result sits under the Table 3 floor. Size practice for 06Cr17Ni12Mo2Ti remains W-C common for welded spool programmes; heat treatment 1000–1100 °C per Table 1.

Grade Rm min (MPa) Rp0.2 min (MPa) A long. min (%) A trans. min (%)
06Cr17Ni12Mo2Ti 530 205 35 30

Ambient values from GB/T 14976-2025 Table 3 for 06Cr17Ni12Mo2Ti. Heat treatment (Table 1): 1000–1100 °C, water or rapid cool. Density 7.98 kg/dm³. Delivery: solution annealed.

Seamless Pipe Manufacture of GB/T 14976 06Cr17Ni12Mo2Ti

SHH STEEL can produce 06Cr17Ni12Mo2Ti as cold-finished seamless (W-C) or hot-finished seamless (W-H), then apply Table 1 heat treatment and pickle (or bright anneal) as ordered. Bevel ends are available by agreement; square-cut plain ends are the default when the PO is silent. Seamless W-C and W-H options remain available for 06Cr17Ni12Mo2Ti; the acknowledgement repeats the manufacture symbol so production cannot silently change route after the PO is firm. Application context for 06Cr17Ni12Mo2Ti stays chemical transfer with dense field welds, heat-exchange fluid loops, and process lines that want 316Ti-class stabilisation plus molybdenum.

Process control for 06Cr17Ni12Mo2Ti ends with verified heat treatment (1000–1100 °C, water or rapid cool) and surface conditioning. Austenitic heats take solution annealing with water or other rapid cool per Table 1; hot-rolled austenitic pipe may count in-line rapid cool inside the Table 1 temperature band as meeting heat treatment (6.3.2) unless the purchaser forbids it.

Bevel geometry is by agreement when ordered without a drawing. Size practice: W-C common for welded spool programmes; heat treatment 1000–1100 °C per Table 1. Density for theoretical weight of 06Cr17Ni12Mo2Ti: 7.98 kg/dm³ per Table 1. Hydrostatic pressure or NDT class for 06Cr17Ni12Mo2Ti is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Application context for 06Cr17Ni12Mo2Ti stays chemical transfer with dense field welds, heat-exchange fluid loops, and process lines that want 316Ti-class stabilisation plus molybdenum.

Dimensions and Tolerances for GB/T 14976 06Cr17Ni12Mo2Ti

Usual length for GB/T 14976 pipe is 4000–12000 mm; fixed and multiple lengths sit inside that band with stated plus tolerances. For 06Cr17Ni12Mo2Ti, confirm whether your project uses OD or ID ordering. Context: W-C common for welded spool programmes; heat treatment 1000–1100 °C per Table 1. Tolerance class (PA/PC) follows the precision ordered for 06Cr17Ni12Mo2Ti, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Size practice for 06Cr17Ni12Mo2Ti remains W-C common for welded spool programmes; heat treatment 1000–1100 °C per Table 1.

Full-length bend ≤0.15% of length; per-metre bend ≤1.5 mm (S≤15 mm) or ≤2.0 mm (S>15 mm). 06Cr17Ni12Mo2Ti must meet those geometry floors unless a written waiver exists. Fixed lengths and multiple cut lengths for 06Cr17Ni12Mo2Ti are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. This paragraph is locked to 06Cr17Ni12Mo2Ti duty: Ti-stabilised Mo austenitic seamless pipe for chloride fluid systems welded without post-weld anneal.

Equivalent Grades for GB/T 14976 06Cr17Ni12Mo2Ti

The table below maps GB/T 14976 06Cr17Ni12Mo2Ti to commercial aliases and related systems without inventing false one-to-one substitutes. Alias 316Ti / UNS S31668 stays body-only. Pack caution: Ti window is 5(C+N)–0. Sister grades in the same series each carry their own chemistry row and must be ordered by their own designation (06Cr17Ni12Mo2Ti).

System Designation Notes
GB/T 14976 06Cr17Ni12Mo2Ti Governing pipe grade for this page
Commercial / UNS (body only) 316Ti / UNS S31668 Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A312 related Related chemistry family (no identical grade asserted) Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

Order discipline for 06Cr17Ni12Mo2Ti still points at GB/T 14976, not the brochure alias. Neighbours GB/T 14976 022Cr17Ni12Mo2, GB/T 14976 06Cr17Ni12Mo2, GB/T 14976 06Cr18Ni11Ti, GB/T 14976 06Cr18Ni11Nb each carry their own mechanical table. Category hub: GB/T 14976. Wall basis, tensile floors, and NDT clauses rarely map one-for-one even when the cast analysis looks familiar to a commercial alias (06Cr17Ni12Mo2Ti).

Heat Treatment and Delivery Condition for GB/T 14976 06Cr17Ni12Mo2Ti

Other heat-treatment schedules are allowed only by written agreement (6.3.4) — silence means Table 1 defaults. For 06Cr17Ni12Mo2Ti: 1000–1100 °C, water or rapid cool. Recorded furnace charts for 06Cr17Ni12Mo2Ti should support the Table 1 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Weld-shop note tied to 06Cr17Ni12Mo2Ti: 316L or Ti-bearing fillers per WPS; limit heat input that can dissolve stabilisation carbides.

After local hot work in the field, restore solution annealed practice when the corrosion file demands it. Caution: Ti window is 5(C+N)–0.70 — do not dual-file as plain 06Cr17Ni12Mo2; confirm Ti on the MTC line. Field heat treatment of 06Cr17Ni12Mo2Ti after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Weld-shop note tied to 06Cr17Ni12Mo2Ti: 316L or Ti-bearing fillers per WPS; limit heat input that can dissolve stabilisation carbides.

Corrosion Resistance of GB/T 14976 06Cr17Ni12Mo2Ti

Pick tests that match how 06Cr17Ni12Mo2Ti is filed — austenitic. Corrosion thread: stabilisation plus Mo improves weld-decay resistance in many chloride process media versus unstabilised standard-carbon 316. Caution: Ti window is 5(C+N)–0.70 — do not dual-file as plain 06Cr17Ni12Mo2; confirm Ti on the MTC line. Coupon orientation, weld condition, and surface finish for 06Cr17Ni12Mo2Ti belong in the corrosion test order so annex results can be compared to the installed spool honestly. Keep the 06Cr17Ni12Mo2Ti caution visible here: Ti window is 5(C+N)–0.70 — do not dual-file as plain 06Cr17Ni12Mo2; confirm Ti on the MTC line.

Oxygen-line Annex B and cryogenic Annex A add impact, UT, and cleanliness rules — they do not change the alloy selection logic. Use thread: chemical transfer with dense field welds, heat-exchange fluid loops, and process lines that want 316Ti-class stabilisation plus molybdenum. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 06Cr17Ni12Mo2Ti rather than relying on wall thickness alone. This paragraph is locked to 06Cr17Ni12Mo2Ti duty: Ti-stabilised Mo austenitic seamless pipe for chloride fluid systems welded without post-weld anneal.

Applications of GB/T 14976 06Cr17Ni12Mo2Ti Seamless Pipe

Project types that repeatedly call 06Cr17Ni12Mo2Ti: chemical transfer with dense field welds, heat-exchange fluid loops, and process lines that want 316Ti-class stabilisation plus molybdenum. Duty: Ti-stabilised Mo austenitic seamless pipe for chloride fluid systems welded without post-weld anneal. Caution still applies: Ti window is 5(C+N)–0.70 — do not dual-file as plain 06Cr17Ni12Mo2; confirm Ti on the MTC line.

Cryogenic, oxygen, and corrosive process lines all appear in 14976’s scope options — alloy choice still follows the medium. For this mark: Ti-stabilised Mo austenitic seamless pipe for chloride fluid systems welded without post-weld anneal. Commissioning teams benefit when the as-built dossier repeats 06Cr17Ni12Mo2Ti beside heat numbers, linking isometric revisions to the same mill certificates. Application context for 06Cr17Ni12Mo2Ti stays chemical transfer with dense field welds, heat-exchange fluid loops, and process lines that want 316Ti-class stabilisation plus molybdenum.

Weldability of GB/T 14976 06Cr17Ni12Mo2Ti

Even seamless W-C/W-H pipe of 06Cr17Ni12Mo2Ti will see field welds. Use: 316L or Ti-bearing fillers per WPS; limit heat input that can dissolve stabilisation carbides. Restore heat treatment when the WPS and corrosion file require it. Procedure qualification for 06Cr17Ni12Mo2Ti should use the same product form and wall class as production, including the seamless finish that will ship. Weld-shop note tied to 06Cr17Ni12Mo2Ti: 316L or Ti-bearing fillers per WPS; limit heat input that can dissolve stabilisation carbides.

Dissimilar welds to carbon steel need buttering and dilution control — especially on Mo and high-Ni grades. Role context: Ti-stabilised Mo austenitic seamless pipe for chloride fluid systems welded without post-weld anneal. Consumable lot control and shielding-gas notes for 06Cr17Ni12Mo2Ti stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. This paragraph is locked to 06Cr17Ni12Mo2Ti duty: Ti-stabilised Mo austenitic seamless pipe for chloride fluid systems welded without post-weld anneal.

Surface Finishes for GB/T 14976 06Cr17Ni12Mo2Ti

Welded or heavily formed 06Cr17Ni12Mo2Ti may need bead dressing or ID attention for flow and inspection — call that out rather than assuming mill habit. Size/finish context stays tied to GB/T 14976 seamless stainless fluid-transport pipe. Caution: Ti window is 5(C+N)–0. Chloride-lean stencil ink and iron-free packing materials are part of the finish package, not optional warehouse habits (06Cr17Ni12Mo2Ti).

Finish Typical supply Order note
Solution annealed and pickled Standard pipe mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

For 06Cr17Ni12Mo2Ti, passivation is an add-on film treatment when the end-user file asks for it — never a fix for missed anneal. Final visual standards reject embedded free iron, grinding burns, and unrepaired weld undercut. Use chloride-lean stencil practice and iron-free packing on this pipe. Passivation and polish are sequenced only after heat-treatment evidence is already on the certificate for 06Cr17Ni12Mo2Ti.

Inspection and Testing for GB/T 14976 06Cr17Ni12Mo2Ti

Batching rules limit pieces per heat/size/heat-treat lot. For 06Cr17Ni12Mo2Ti, keep the heat identity unbroken from melt to bundle tag. Duty: Ti-stabilised Mo austenitic seamless pipe for chloride fluid systems welded without post-weld anneal. Sampling plans for 06Cr17Ni12Mo2Ti keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. This paragraph is locked to 06Cr17Ni12Mo2Ti duty: Ti-stabilised Mo austenitic seamless pipe for chloride fluid systems welded without post-weld anneal.

Intergranular corrosion testing is mandatory for most austenitics — see the IGC note for 06Cr17Ni12Mo2Ti. Order extras (grain size, inclusions, elevated tensile) under 7.8.3 when needed. Non-conforming 06Cr17Ni12Mo2Ti lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Size practice for 06Cr17Ni12Mo2Ti remains W-C common for welded spool programmes; heat treatment 1000–1100 °C per Table 1.

Packaging and Shipping for GB/T 14976 06Cr17Ni12Mo2Ti

Small-OD 06Cr17Ni12Mo2Ti often ships in crates; large-OD in strapped bundles with OD pads. Confirm destination handling limits on the RFQ. Use: chemical transfer with dense field welds, heat-exchange fluid loops, and process lines that want 316Ti-class stabilisation plus molybdenum. Bundle tickets for 06Cr17Ni12Mo2Ti repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Application context for 06Cr17Ni12Mo2Ti stays chemical transfer with dense field welds, heat-exchange fluid loops, and process lines that want 316Ti-class stabilisation plus molybdenum.

Bevelled ends get protectors so landing edges survive trucking. Size hint: W-C common for welded spool programmes; heat treatment 1000–1100 °C per Table 1. Desiccant and wrap choices for 06Cr17Ni12Mo2Ti follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. This paragraph is locked to 06Cr17Ni12Mo2Ti duty: Ti-stabilised Mo austenitic seamless pipe for chloride fluid systems welded without post-weld anneal.

Storage advice on arrival: keep bundles dry and off carbon-steel floors. Use thread: chemical transfer with dense field welds, heat-exchange fluid loops, and process lines that want 316Ti-class stabilisation plus molybdenum. Claims handling for 06Cr17Ni12Mo2Ti starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Keep the 06Cr17Ni12Mo2Ti caution visible here: Ti window is 5(C+N)–0.70 — do not dual-file as plain 06Cr17Ni12Mo2; confirm Ti on the MTC line.

Why Choose SHH STEEL

Project teams working to Chinese fluid-transport specs need a supplier that reads Chinese grade names correctly. SHH STEEL can make 06Cr17Ni12Mo2Ti to that discipline. Caution we keep visible: Ti window is 5(C+N)–0.70 — do not dual-file as plain 06Cr17Ni12Mo2; confirm Ti on the MTC line. SHH STEEL can produce and supply 06Cr17Ni12Mo2Ti against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade.

Dual-cert discussions (GB/T + ASTM) are handled with two acceptance regimes in view, not one certificate stretched by hope. Sisters: 022Cr17Ni12Mo2, 06Cr17Ni12Mo2, 06Cr18Ni11Ti, 06Cr18Ni11Nb. Ask for a written acknowledgement that names 06Cr17Ni12Mo2Ti, W-C or W-H, and the Table 1 heat-treatment condition before melt. SHH STEEL can make 06Cr17Ni12Mo2Ti to that written scope.

Supply Capability

Whether you need prototype spools or project tonnage of 06Cr17Ni12Mo2Ti, SHH STEEL can supply against a clear OD × wall and test matrix. Duty: chemical transfer with dense field welds, heat-exchange fluid loops, and process lines that want 316Ti-class stabilisation plus molybdenum. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for 06Cr17Ni12Mo2Ti when the mill schedule allows.

Item Capability
Standard GB/T 14976-2025 seamless stainless steel pipes for fluid transport
Grade 06Cr17Ni12Mo2Ti (S31668)
Product form Seamless pipe only — cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H)
Delivery condition solution annealed
Documents Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered)
Typical size practice OD × wall per GB/T 17395; PA ordinary or PC higher precision; usual length 4000–12000 mm
Wall / ordering Nominal OD×wall, OD×min wall, or ID×wall by agreement

Stock / Available sizes

Stock / Available sizes: SHH STEEL quotes piercing/drawing slots for 06Cr17Ni12Mo2Ti rather than promising anonymous warehouse tons. Typical conversation starts around W-C common for welded spool programmes; heat treatment 1000–1100 °C per Table 1. SHH STEEL can supply alternate walls and precision classes for 06Cr17Ni12Mo2Ti once the design pressure and corrosion allowance are clear.

If the project needs dual GB/T 14976 + ASTM documentation, say so before melt. Caution: Ti window is 5(C+N)–0.70 — do not dual-file as plain 06Cr17Ni12Mo2; confirm Ti on the MTC line. SHH STEEL can produce trial lengths of 06Cr17Ni12Mo2Ti for procedure qualification before the bulk release when the project calendar needs it.

FAQ

What is GB/T 14976 06Cr17Ni12Mo2Ti seamless stainless steel pipe used for?
GB/T 14976 06Cr17Ni12Mo2Ti is seamless stainless pipe for fluid transport — chemical transfer with dense field welds, heat-exchange fluid loops, and process lines that want 316Ti-class stabilisation plus molybdenum. Role summary: Ti-stabilised Mo austenitic seamless pipe for chloride fluid systems welded without post-weld anneal. It is a Chinese product standard grade (S31668), not an automatic ASTM A312 certificate.
Is GB/T 14976 06Cr17Ni12Mo2Ti seamless only, or does it cover welded pipe?
Seamless only. Clause 6.2 limits manufacture to cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 06Cr17Ni12Mo2Ti when the mill can meet the ordered size and tests. Welded pipe belongs under other standards, not 14976.
What heat treatment applies to 06Cr17Ni12Mo2Ti?
06Cr17Ni12Mo2Ti is delivered solution annealed under GB/T 14976. Table 1 reference: 1000–1100 °C, water or rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Keep the purchase order locked to GB/T 14976 and 06Cr17Ni12Mo2Ti so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
How does 06Cr17Ni12Mo2Ti compare with sister grades 022Cr17Ni12Mo2, 06Cr17Ni12Mo2, 06Cr18Ni11Ti?
06Cr17Ni12Mo2Ti is filed as austenitic. Typical sisters on the same RFQ are 022Cr17Ni12Mo2, 06Cr17Ni12Mo2, 06Cr18Ni11Ti. Design caution: Ti window is 5(C+N)–0.70 — do not dual-file as plain 06Cr17Ni12Mo2; confirm Ti on the MTC line Pick the sister when the medium or strength floor outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 06Cr17Ni12Mo2Ti?
Expect cast analysis (Table 2), room-temperature tensile results (Table 3), dimensions, hydrostatic test (or replacing UT/ET), appearance, and every special annex or IGC test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
Is 316Ti / UNS S31668 the same as ordering 06Cr17Ni12Mo2Ti?
No. 316Ti / UNS S31668 is a commercial / UNS cross-walk for body text (unified S31668). The purchase order should lock GB/T 14976 and 06Cr17Ni12Mo2Ti so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GB/T 14976 06Cr17Ni12Mo2Ti?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 06Cr17Ni12Mo2Ti within GB/T 17395 practice, with PA or PC precision and measured or min-wall options by agreement. Size context: W-C common for welded spool programmes; heat treatment 1000–1100 °C per Table 1. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should 06Cr17Ni12Mo2Ti be welded on site?
Shop guidance: 316L or Ti-bearing fillers per WPS; limit heat input that can dissolve stabilisation carbides. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: Ti window is 5(C+N)–0.70 — do not dual-file as plain 06Cr17Ni12Mo2; confirm Ti on the MTC line
When should I choose a higher-Mo or superaustenitic grade instead of 06Cr17Ni12Mo2Ti?
Move when chloride pitting, crevice attack, or reducing-acid risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: Ti window is 5(C+N)–0.70 — do not dual-file as plain 06Cr17Ni12Mo2; confirm Ti on the MTC line Sister pointers: 022Cr17Ni12Mo2, 06Cr17Ni12Mo2, 06Cr18Ni11Ti. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GB/T 14976 06Cr17Ni12Mo2Ti with ASTM A312?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 14976 06Cr17Ni12Mo2Ti does not clear ASTM acceptance by default. State both standards, sizes, and test scopes before melt. Keep the purchase order locked to GB/T 14976 and 06Cr17Ni12Mo2Ti so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
What surface finishes are available for 06Cr17Ni12Mo2Ti?
Pickled after heat treatment is the usual fluid-transport supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 06Cr17Ni12Mo2Ti when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

GB/T 14976 06Cr17Ni12Mo2Ti is seamless stainless steel pipe for fluid transport — Ti-stabilised Mo austenitic seamless pipe for chloride fluid systems welded without post-weld anneal. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 022Cr17Ni12Mo2, 06Cr17Ni12Mo2, 06Cr18Ni11Ti. Related ASTM pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X