GB/T 14976 07Cr17Ni12Mo2 Seamless Stainless Steel Pipe | GB/T 14976 Stainless Steel Pipe - SHH STEEL

GB/T 14976 07Cr17Ni12Mo2 Seamless Stainless Steel Pipe

GB/T 14976 07Cr17Ni12Mo2 seamless stainless steel pipe (316H / UNS S31609, S31609), austenitic, Table 2 cast analysis, Rm min 515 MPa / Rp0.2 min 205 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
Grade
07Cr17Ni12Mo2 (S31609 / 316H / UNS S31609 — body alias)
Standard
GB/T 14976-2025
Product form
Seamless stainless steel pipe (W-C / W-H), delivery solution annealed
Size
OD × wall per GB/T 17395; PA/PC precision; usual length 4000–12000 mm; other by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Pipe Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GB/T 14976 07Cr17Ni12Mo2 Seamless Stainless Steel Pipe

GB/T 14976 covers seamless stainless pipe for fluid service — cold-drawn or hot-finished — with hydrostatic proof and optional Annex A cryogenic or Annex B oxygen extras. Inside that standard, 07Cr17Ni12Mo2 is filed as austenitic. GB/T 14976 07Cr17Ni12Mo2 stops the habit of calling every Mo pipe “316” when the design actually needs a carbon floor.

From pierce/extrude/draw through marking and bundle protection, SHH STEEL can produce GB/T 14976 07Cr17Ni12Mo2 for the sizes and tests on your RFQ. Application sketch: hot process fluid headers, high-temperature chloride-lean chemical lines, and heat-recovery loops written to 316H-class chemistry. Size and test clarity on the RFQ lets SHH STEEL lock the correct W-C or W-H symbol for 07Cr17Ni12Mo2 before production starts. Keep the 07Cr17Ni12Mo2 caution visible here: clause 7.5 exempts this mark from mandatory IGC — corrosive as-welded aqueous duty still prefers 022Cr17Ni12Mo2 or stabilised Ti grades.

On the floor people shorten marks; in QA they must not. 07Cr17Ni12Mo2 under GB/T 14976 carries specific Table 2 windows and Table 3 floors that a loose “316H” note will not enforce. Caution: clause 7.5 exempts this mark from mandatory IGC — corrosive as-welded aqueous duty still prefers 022Cr17Ni12Mo2 or stabilised Ti grades.

Cryogenic Annex A and oxygen Annex B sit in 14976’s special-requirements clause; still match the alloy to the medium. For 07Cr17Ni12Mo2, that means: controlled-carbon Mo austenitic seamless pipe for elevated-temperature fluid lines that need hot strength plus molybdenum. Nearby marks: 06Cr17Ni12Mo2, 07Cr19Ni10, 07Cr19Ni11Ti, 06Cr17Ni12Mo2N. Document the medium, design temperature, and weld map beside the 07Cr17Ni12Mo2 line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Keep the 07Cr17Ni12Mo2 caution visible here: clause 7.5 exempts this mark from mandatory IGC — corrosive as-welded aqueous duty still prefers 022Cr17Ni12Mo2 or stabilised Ti grades.

Inside this GB/T 14976 series, compare GB/T 14976 06Cr17Ni12Mo2, GB/T 14976 07Cr19Ni10, GB/T 14976 07Cr19Ni11Ti, GB/T 14976 06Cr17Ni12Mo2N. Hub: GB/T 14976. ASTM/ASME related product pages (not interchangeable by default): ASTM A312 TP316H.

Buyers comparing 07Cr17Ni12Mo2 tubulars with sheet/plate can link Stainless Steel Pipes and Tubes, Stainless Steel Sheets and Plates, and GB/T 4237 07Cr17Ni12Mo2 so purchasing does not treat one product form as the other. Flat Chinese grades in-family are indexed at GB/T 4237. Quote 07Cr17Ni12Mo2 pipe and plate under separate line items.

Chemical Composition of GB/T 14976 07Cr17Ni12Mo2

For 07Cr17Ni12Mo2, the melt ticket has to show Table 2 compliance — C 0.04–0.10, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.030, Ni 10.00–14.00, Cr 16.00–18.00, Mo 2.00–3.00. Optional alloying footnotes in the standard still forbid blurring grade identity. Corrosion framing: Mo helps aqueous chlorides relative to 18-8; hot oxidation is secondary to the carbon-floor mission.

Where Mo, Cu, Ti, Nb, Al or N appear, they are intentional levers for 07Cr17Ni12Mo2, not optional marketing. Confirm them on the MTC line-by-line. Role: controlled-carbon Mo austenitic seamless pipe for elevated-temperature fluid lines that need hot strength plus molybdenum. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 2, SHH STEEL will confirm melt feasibility for 07Cr17Ni12Mo2 before the order is acknowledged. Size practice for 07Cr17Ni12Mo2 remains W-H for heavier hot-service walls; confirm ≥1040 °C solution practice on the certificate.

Grade C Si Mn P S Ni Cr Mo
07Cr17Ni12Mo2 0.04–0.10 ≤1.00 ≤2.00 ≤0.035 ≤0.030 10.00–14.00 16.00–18.00 2.00–3.00

Mechanical Properties of GB/T 14976 07Cr17Ni12Mo2

Do not confuse Table 3 pipe tensile floors with plate or tube standards that share the 316H / UNS S31609 alias. For 07Cr17Ni12Mo2 under 14976 expect Rm min 515 MPa, Rp0.2 min 205 MPa, elongation longitudinal min 35% / transverse min 30%, verified per heat/lot rules. Tensile sampling follows the batch rules for the ordered test unit of 07Cr17Ni12Mo2, and retests follow GB/T 2102 when a result sits under the Table 3 floor. Corrosion framing beside 07Cr17Ni12Mo2: Mo helps aqueous chlorides relative to 18-8; hot oxidation is secondary to the carbon-floor mission.

Grade Rm min (MPa) Rp0.2 min (MPa) A long. min (%) A trans. min (%)
07Cr17Ni12Mo2 515 205 35 30

Ambient values from GB/T 14976-2025 Table 3 for 07Cr17Ni12Mo2. Heat treatment (Table 1): ≥1040 °C, water or rapid cool. Density 7.98 kg/dm³. Delivery: solution annealed.

Seamless Pipe Manufacture of GB/T 14976 07Cr17Ni12Mo2

GB/T 14976 manufactures 07Cr17Ni12Mo2 as seamless pipe only — cold-rolled or cold-drawn (symbol W-C) or hot-rolled, extruded, forged or expanded (symbol W-H). SHH STEEL confirms the manufacture symbol on the acknowledgement before piercing or drawing starts; welded pipe is outside this standard. Seamless W-C and W-H options remain available for 07Cr17Ni12Mo2; the acknowledgement repeats the manufacture symbol so production cannot silently change route after the PO is firm. Corrosion framing beside 07Cr17Ni12Mo2: Mo helps aqueous chlorides relative to 18-8; hot oxidation is secondary to the carbon-floor mission.

Cold-drawn austenitic 07Cr17Ni12Mo2 may ship cold-worked only by written agreement (6.3.3) with negotiated bend and tensile rules — silence means heat-treated delivery. Heat treatment: ≥1040 °C, water or rapid cool. Austenitic heats take solution annealing with water or other rapid cool per Table 1; hot-rolled austenitic pipe may count in-line rapid cool inside the Table 1 temperature band as meeting heat treatment (6.3.2) unless the purchaser forbids it.

Hydrostatic testing is mandatory; ultrasonic or eddy-current may replace hydro per 7.3.3 when agreed. Manufacture stays seamless-only. Size: W-H for heavier hot-service walls; confirm ≥1040 °C solution practice on the certificate. Hydrostatic pressure or NDT class for 07Cr17Ni12Mo2 is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Keep the 07Cr17Ni12Mo2 caution visible here: clause 7.5 exempts this mark from mandatory IGC — corrosive as-welded aqueous duty still prefers 022Cr17Ni12Mo2 or stabilised Ti grades.

Dimensions and Tolerances for GB/T 14976 07Cr17Ni12Mo2

Out-of-table OD×wall combinations are by agreement — still under the same grade symbol 07Cr17Ni12Mo2. Duty: controlled-carbon Mo austenitic seamless pipe for elevated-temperature fluid lines that need hot strength plus molybdenum. Tolerance class (PA/PC) follows the precision ordered for 07Cr17Ni12Mo2, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Corrosion framing beside 07Cr17Ni12Mo2: Mo helps aqueous chlorides relative to 18-8; hot oxidation is secondary to the carbon-floor mission.

Ovality and wall unevenness, when ordered, stay within 80% of the respective OD and wall tolerances. Size reminder: W-H for heavier hot-service walls; confirm ≥1040 °C solution practice on the certificate. Fixed lengths and multiple cut lengths for 07Cr17Ni12Mo2 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Corrosion framing beside 07Cr17Ni12Mo2: Mo helps aqueous chlorides relative to 18-8; hot oxidation is secondary to the carbon-floor mission.

Equivalent Grades for GB/T 14976 07Cr17Ni12Mo2

Buyers searching under 316H / UNS S31609 still need the GB/T 14976 07Cr17Ni12Mo2 row locked on the acknowledgement. Inside austenitic practice the mechanical table and inspection clauses of GB/T 14976 control acceptance, not a brochure equivalent. Duty context: controlled-carbon Mo austenitic seamless pipe for elevated-temperature fluid lines that need hot strength plus molybdenum.

System Designation Notes
GB/T 14976 07Cr17Ni12Mo2 Governing pipe grade for this page
Commercial / UNS (body only) 316H / UNS S31609 Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A312 related Related chemistry family (no identical grade asserted) Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

Order discipline for 07Cr17Ni12Mo2 still points at GB/T 14976, not the brochure alias. Neighbours GB/T 14976 06Cr17Ni12Mo2, GB/T 14976 07Cr19Ni10, GB/T 14976 07Cr19Ni11Ti, GB/T 14976 06Cr17Ni12Mo2N each carry their own mechanical table. Category hub: GB/T 14976. Keep the governing standard symbol on the acknowledgement so mechanical tables cannot drift under a trade name (07Cr17Ni12Mo2).

Heat Treatment and Delivery Condition for GB/T 14976 07Cr17Ni12Mo2

Hot-finished austenitic seamless may use in-line rapid cool inside the Table 1 band under 6.3.2 unless the purchaser forbids it. Confirm for 07Cr17Ni12Mo2. Band: ≥1040 °C, water or rapid cool. Recorded furnace charts for 07Cr17Ni12Mo2 should support the Table 1 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Application context for 07Cr17Ni12Mo2 stays hot process fluid headers, high-temperature chloride-lean chemical lines, and heat-recovery loops written to 316H-class chemistry.

Grain-size or inclusion testing under 7.8.3 applies only when ordered — state any extra metallographic demand on the PO for 07Cr17Ni12Mo2. Field heat treatment of 07Cr17Ni12Mo2 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Size practice for 07Cr17Ni12Mo2 remains W-H for heavier hot-service walls; confirm ≥1040 °C solution practice on the certificate.

Corrosion Resistance of GB/T 14976 07Cr17Ni12Mo2

Medium, temperature, crevice geometry and weld condition decide whether 07Cr17Ni12Mo2 is enough. Summary: Mo helps aqueous chlorides relative to 18-8; hot oxidation is secondary to the carbon-floor mission. Escalate via sisters 06Cr17Ni12Mo2, 07Cr19Ni10, 07Cr19Ni11Ti, 06Cr17Ni12Mo2N when coupons fail. Coupon orientation, weld condition, and surface finish for 07Cr17Ni12Mo2 belong in the corrosion test order so annex results can be compared to the installed spool honestly. Application context for 07Cr17Ni12Mo2 stays hot process fluid headers, high-temperature chloride-lean chemical lines, and heat-recovery loops written to 316H-class chemistry.

Surface finish and iron contamination control often matter as much as bulk chemistry on sanitary-lean duties for 07Cr17Ni12Mo2. Corrosion framing: Mo helps aqueous chlorides relative to 18-8; hot oxidation is secondary to the carbon-floor mission. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 07Cr17Ni12Mo2 rather than relying on wall thickness alone. Keep the 07Cr17Ni12Mo2 caution visible here: clause 7.5 exempts this mark from mandatory IGC — corrosive as-welded aqueous duty still prefers 022Cr17Ni12Mo2 or stabilised Ti grades.

Applications of GB/T 14976 07Cr17Ni12Mo2 Seamless Pipe

From utility rooms to process racks, 07Cr17Ni12Mo2 shows up wherever Chinese fluid specs want austenitic seamless behaviour. Use list: hot process fluid headers, high-temperature chloride-lean chemical lines, and heat-recovery loops written to 316H-class chemistry. Spool fabricators should copy 07Cr17Ni12Mo2 onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Corrosion framing beside 07Cr17Ni12Mo2: Mo helps aqueous chlorides relative to 18-8; hot oxidation is secondary to the carbon-floor mission.

If the only reason for 07Cr17Ni12Mo2 is “we always used this alias,” reopen the corrosion file before repeating the order. Caution: clause 7.5 exempts this mark from mandatory IGC — corrosive as-welded aqueous duty still prefers 022Cr17Ni12Mo2 or stabilised Ti grades. Commissioning teams benefit when the as-built dossier repeats 07Cr17Ni12Mo2 beside heat numbers, linking isometric revisions to the same mill certificates. This paragraph is locked to 07Cr17Ni12Mo2 duty: controlled-carbon Mo austenitic seamless pipe for elevated-temperature fluid lines that need hot strength plus molybdenum.

Weldability of GB/T 14976 07Cr17Ni12Mo2

Automatic mill welding is outside GB/T 14976; manual and automatic field welds must still respect 07Cr17Ni12Mo2 chemistry. Guidance: 316H-class fillers when matching hot strength; do not default to L procedures without review. Procedure qualification for 07Cr17Ni12Mo2 should use the same product form and wall class as production, including the seamless finish that will ship. Size practice for 07Cr17Ni12Mo2 remains W-H for heavier hot-service walls; confirm ≥1040 °C solution practice on the certificate.

Ferrite control on high-Ni austenitics and hydrogen management on martensitic 07Cr17Ni12Mo2 are procedure items, not afterthoughts. Guidance: 316H-class fillers when matching hot strength; do not default to L procedures without review. Consumable lot control and shielding-gas notes for 07Cr17Ni12Mo2 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Keep the 07Cr17Ni12Mo2 caution visible here: clause 7.5 exempts this mark from mandatory IGC — corrosive as-welded aqueous duty still prefers 022Cr17Ni12Mo2 or stabilised Ti grades.

Surface Finishes for GB/T 14976 07Cr17Ni12Mo2

On 07Cr17Ni12Mo2, cosmetics never outrank correct heat treatment. Passivation and polish are sequenced after the anneal that qualifies the pipe. Duty locked here: controlled-carbon Mo austenitic seamless pipe for elevated-temperature fluid lines that need hot strength plus molybdenum. Name which surface carries each finish callout. Free-iron control continues through storage and shipment, because late carbon-steel contact can stain an otherwise clean pickle (07Cr17Ni12Mo2).

Finish Typical supply Order note
Solution annealed and pickled Standard pipe mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

Reject grinding burns, embedded free iron, and unrepaired undercut on 07Cr17Ni12Mo2 before bundles close. Passivation analogues (A967-style) are optional extras — the governing step remains correct heat treatment under GB/T 14976 for this austenitic mark. Passivation and polish are sequenced only after heat-treatment evidence is already on the certificate for 07Cr17Ni12Mo2.

Inspection and Testing for GB/T 14976 07Cr17Ni12Mo2

Third-party witness (SGS/TUV-style) is available when the project mandate requires it. Base acceptance still tracks GB/T 14976 for 07Cr17Ni12Mo2. Sampling plans for 07Cr17Ni12Mo2 keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. This paragraph is locked to 07Cr17Ni12Mo2 duty: controlled-carbon Mo austenitic seamless pipe for elevated-temperature fluid lines that need hot strength plus molybdenum.

Dimensional inspection against Table 4/5 tolerances closes the lot. Failures retest per GB/T 2102 — they are not silently shipped. Role: controlled-carbon Mo austenitic seamless pipe for elevated-temperature fluid lines that need hot strength plus molybdenum. Non-conforming 07Cr17Ni12Mo2 lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Weld-shop note tied to 07Cr17Ni12Mo2: 316H-class fillers when matching hot strength; do not default to L procedures without review.

Packaging and Shipping for GB/T 14976 07Cr17Ni12Mo2

Seaworthy packing is available for ocean legs — desiccant, VCI, and wrap specs by agreement. Grade mark 07Cr17Ni12Mo2 stays visible on outer tags. Oxygen Annex B adds oil-free packing language when invoked. Bundle tickets for 07Cr17Ni12Mo2 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Size practice for 07Cr17Ni12Mo2 remains W-H for heavier hot-service walls; confirm ≥1040 °C solution practice on the certificate.

Container loading plans should keep heavy walls from crushing thin-wall 07Cr17Ni12Mo2 layers. Desiccant and wrap choices for 07Cr17Ni12Mo2 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Weld-shop note tied to 07Cr17Ni12Mo2: 316H-class fillers when matching hot strength; do not default to L procedures without review.

Shortages or transit damage claims need photos against the packing list before installation starts — tag identity must still read 07Cr17Ni12Mo2. Claims handling for 07Cr17Ni12Mo2 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Weld-shop note tied to 07Cr17Ni12Mo2: 316H-class fillers when matching hot strength; do not default to L procedures without review.

Why Choose SHH STEEL

From RFQ clarification through MTC release, SHH STEEL treats 07Cr17Ni12Mo2 as a governed product grade, not a marketing synonym for 316H / UNS S31609. Role: controlled-carbon Mo austenitic seamless pipe for elevated-temperature fluid lines that need hot strength plus molybdenum. SHH STEEL can produce and supply 07Cr17Ni12Mo2 against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade.

Response time stays short because common 07Cr17Ni12Mo2 enquiry sizes and document packs are already exercised on prior Chinese-spec orders. Use: hot process fluid headers, high-temperature chloride-lean chemical lines, and heat-recovery loops written to 316H-class chemistry. Ask for a written acknowledgement that names 07Cr17Ni12Mo2, W-C or W-H, and the Table 1 heat-treatment condition before melt. SHH STEEL can make 07Cr17Ni12Mo2 to that written scope.

Supply Capability

Capability framing for 07Cr17Ni12Mo2: Chinese-spec seamless fluid pipe, W-C/W-H manufacture, documented heats. Caution remains: clause 7.5 exempts this mark from mandatory IGC — corrosive as-welded aqueous duty still prefers 022Cr17Ni12Mo2 or stabilised Ti grades. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for 07Cr17Ni12Mo2 when the mill schedule allows.

Item Capability
Standard GB/T 14976-2025 seamless stainless steel pipes for fluid transport
Grade 07Cr17Ni12Mo2 (S31609)
Product form Seamless pipe only — cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H)
Delivery condition solution annealed
Documents Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered)
Typical size practice OD × wall per GB/T 17395; PA ordinary or PC higher precision; usual length 4000–12000 mm
Wall / ordering Nominal OD×wall, OD×min wall, or ID×wall by agreement

Stock / Available sizes

Stock / Available sizes — treat published ranges as capability envelopes. Actual ex-stock pieces of 07Cr17Ni12Mo2 change weekly; the reliable path is an OD × wall matrix on the enquiry. Duty: controlled-carbon Mo austenitic seamless pipe for elevated-temperature fluid lines that need hot strength plus molybdenum. SHH STEEL can supply alternate walls and precision classes for 07Cr17Ni12Mo2 once the design pressure and corrosion allowance are clear.

Repeat orders for 07Cr17Ni12Mo2 go faster when prior heat records and accepted WPS numbers are referenced on the new RFQ. Role: controlled-carbon Mo austenitic seamless pipe for elevated-temperature fluid lines that need hot strength plus molybdenum. SHH STEEL can produce trial lengths of 07Cr17Ni12Mo2 for procedure qualification before the bulk release when the project calendar needs it.

FAQ

What is GB/T 14976 07Cr17Ni12Mo2 seamless stainless steel pipe used for?
GB/T 14976 07Cr17Ni12Mo2 is seamless stainless pipe for fluid transport — hot process fluid headers, high-temperature chloride-lean chemical lines, and heat-recovery loops written to 316H-class chemistry. Role summary: controlled-carbon Mo austenitic seamless pipe for elevated-temperature fluid lines that need hot strength plus molybdenum. It is a Chinese product standard grade (S31609), not an automatic ASTM A312 certificate.
Is GB/T 14976 07Cr17Ni12Mo2 seamless only, or does it cover welded pipe?
Seamless only. Clause 6.2 limits manufacture to cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 07Cr17Ni12Mo2 when the mill can meet the ordered size and tests. Welded pipe belongs under other standards, not 14976.
What heat treatment applies to 07Cr17Ni12Mo2?
07Cr17Ni12Mo2 is delivered solution annealed under GB/T 14976. Table 1 reference: ≥1040 °C, water or rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Keep the purchase order locked to GB/T 14976 and 07Cr17Ni12Mo2 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
How does 07Cr17Ni12Mo2 compare with sister grades 06Cr17Ni12Mo2, 07Cr19Ni10, 07Cr19Ni11Ti?
07Cr17Ni12Mo2 is filed as austenitic. Typical sisters on the same RFQ are 06Cr17Ni12Mo2, 07Cr19Ni10, 07Cr19Ni11Ti. Design caution: clause 7.5 exempts this mark from mandatory IGC — corrosive as-welded aqueous duty still prefers 022Cr17Ni12Mo2 or stabilised Ti grades Pick the sister when the medium or strength floor outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 07Cr17Ni12Mo2?
Expect cast analysis (Table 2), room-temperature tensile results (Table 3), dimensions, hydrostatic test (or replacing UT/ET), appearance, and every special annex or IGC test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
Is 316H / UNS S31609 the same as ordering 07Cr17Ni12Mo2?
No. 316H / UNS S31609 is a commercial / UNS cross-walk for body text (unified S31609). The purchase order should lock GB/T 14976 and 07Cr17Ni12Mo2 so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GB/T 14976 07Cr17Ni12Mo2?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 07Cr17Ni12Mo2 within GB/T 17395 practice, with PA or PC precision and measured or min-wall options by agreement. Size context: W-H for heavier hot-service walls; confirm ≥1040 °C solution practice on the certificate. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should 07Cr17Ni12Mo2 be welded on site?
Shop guidance: 316H-class fillers when matching hot strength; do not default to L procedures without review. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: clause 7.5 exempts this mark from mandatory IGC — corrosive as-welded aqueous duty still prefers 022Cr17Ni12Mo2 or stabilised Ti grades
When should I choose a higher-Mo or superaustenitic grade instead of 07Cr17Ni12Mo2?
Move when chloride pitting, crevice attack, or reducing-acid risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: clause 7.5 exempts this mark from mandatory IGC — corrosive as-welded aqueous duty still prefers 022Cr17Ni12Mo2 or stabilised Ti grades Sister pointers: 06Cr17Ni12Mo2, 07Cr19Ni10, 07Cr19Ni11Ti. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GB/T 14976 07Cr17Ni12Mo2 with ASTM A312?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 14976 07Cr17Ni12Mo2 does not clear ASTM acceptance by default. State both standards, sizes, and test scopes before melt. Keep the purchase order locked to GB/T 14976 and 07Cr17Ni12Mo2 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
What surface finishes are available for 07Cr17Ni12Mo2?
Pickled after heat treatment is the usual fluid-transport supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 07Cr17Ni12Mo2 when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

GB/T 14976 07Cr17Ni12Mo2 is seamless stainless steel pipe for fluid transport — controlled-carbon Mo austenitic seamless pipe for elevated-temperature fluid lines that need hot strength plus molybdenum. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 06Cr17Ni12Mo2, 07Cr19Ni10, 07Cr19Ni11Ti. Related ASTM pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X