GB/T 14976 015Cr21Ni26Mo5Cu2 Seamless Stainless Steel Pipe | GB/T 14976 Stainless Steel Pipe - SHH STEEL

GB/T 14976 015Cr21Ni26Mo5Cu2 Seamless Stainless Steel Pipe

GB/T 14976 015Cr21Ni26Mo5Cu2 seamless stainless steel pipe (904L-class / UNS N08904-related, S39042), austenitic, Table 2 cast analysis, Rm min 490 MPa / Rp0.2 min 220 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
Grade
015Cr21Ni26Mo5Cu2 (S39042 / 904L-class / UNS N08904-related — body alias)
Standard
GB/T 14976-2025
Product form
Seamless stainless steel pipe (W-C / W-H), delivery solution annealed
Size
OD × wall per GB/T 17395; PA/PC precision; usual length 4000–12000 mm; other by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Pipe Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GB/T 14976 015Cr21Ni26Mo5Cu2 Seamless Stainless Steel Pipe

When the approved vendor list and isometric notes say GB/T 14976, the grade mark has to be the Chinese designation. 015Cr21Ni26Mo5Cu2 is the full product grade for this austenitic seamless pipe. GB/T 14976 015Cr21Ni26Mo5Cu2 is the Chinese high-alloy seamless fluid mark in the 904L conversation — governed by Table 2/3, not a warehouse nickname.

SHH STEEL can supply 015Cr21Ni26Mo5Cu2 seamless pipe in cold-finished or hot-finished routes, with plain or bevelled ends, random or cut lengths, and GB/T 2102 / EN 10204 3.1 style inspection documents when specified. Role on the line: high-Ni Mo-Cu austenitic seamless pipe for severe reducing-acid and chloride fluid service (904L-class family). Size and test clarity on the RFQ lets SHH STEEL lock the correct W-C or W-H symbol for 015Cr21Ni26Mo5Cu2 before production starts. This paragraph is locked to 015Cr21Ni26Mo5Cu2 duty: high-Ni Mo-Cu austenitic seamless pipe for severe reducing-acid and chloride fluid service (904L-class family).

Equivalence talk to 904L-class / UNS N08904-related belongs in engineering notes, not as a substitute for the Chinese grade. Lock GB/T 14976 015Cr21Ni26Mo5Cu2, OD × wall, manufacture route, and any Annex A/B extras before melt. Watch-out: Ni 23–28% / Mo 4–5% / Cu 1–2% — not interchangeable with 015Cr20Ni18Mo6CuN without corrosion review.

Related ASTM pipe pages share chemistry families but not Chinese acceptance text — confirm before dual-cert claims. Sisters on this hub: 015Cr20Ni18Mo6CuN, 022Cr19Ni13Mo3, 022Cr18Ni14Mo2Cu2, 06Cr19Ni13Mo3. Use thread: sulphuric and mixed-acid transfer, seawater-lean process lines, scrubber fluid piping, and aggressive chemical headers on Chinese specs. Document the medium, design temperature, and weld map beside the 015Cr21Ni26Mo5Cu2 line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Size practice for 015Cr21Ni26Mo5Cu2 remains cold-drawn W-C preferred; heat treatment 1065–1150 °C; density 8.05.

Inside this GB/T 14976 series, compare GB/T 14976 015Cr20Ni18Mo6CuN, GB/T 14976 022Cr19Ni13Mo3, GB/T 14976 022Cr18Ni14Mo2Cu2, GB/T 14976 06Cr19Ni13Mo3. Hub: GB/T 14976.

Chemical Composition of GB/T 14976 015Cr21Ni26Mo5Cu2

Chemistry control on 015Cr21Ni26Mo5Cu2 starts at the ladle. Expect C ≤0.020, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.030, Ni 23.00–28.00, Cr 19.00–23.00, Mo 4.00–5.00 within Table 2, reported on the inspection document against the heat. Body alias 904L-class / UNS N08904-related does not widen those windows. Every ladle analysis for 015Cr21Ni26Mo5Cu2 is checked against those windows before the heat is released to piercing or drawing, and the same numbers reappear on the inspection document. Application context for 015Cr21Ni26Mo5Cu2 stays sulphuric and mixed-acid transfer, seawater-lean process lines, scrubber fluid piping, and aggressive chemical headers on Chinese specs.

Read the table with the family in mind — austenitic — and with caution Ni 23–28% / Mo 4–5% / Cu 1–2% — not interchangeable with 015Cr20Ni18Mo6CuN without corrosion review. Numbers without the matching Table 1 heat-treatment row are incomplete purchase data. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 2, SHH STEEL will confirm melt feasibility for 015Cr21Ni26Mo5Cu2 before the order is acknowledged. Keep the 015Cr21Ni26Mo5Cu2 caution visible here: Ni 23–28% / Mo 4–5% / Cu 1–2% — not interchangeable with 015Cr20Ni18Mo6CuN without corrosion review.

Grade C Si Mn P S Ni Cr Mo Cu N
015Cr21Ni26Mo5Cu2 ≤0.020 ≤1.00 ≤2.00 ≤0.035 ≤0.030 23.00–28.00 19.00–23.00 4.00–5.00 1.00–2.00 ≤0.10

Mechanical Properties of GB/T 14976 015Cr21Ni26Mo5Cu2

Proof stress and tensile minima for 015Cr21Ni26Mo5Cu2 sit at Rm min 490 MPa, Rp0.2 min 220 MPa, elongation longitudinal min 35% / transverse min 30%. Flattening or bend testing backs ductility when ordered. Watch-out: Ni 23–28% / Mo 4–5% / Cu 1–2% — not interchangeable with 015Cr20Ni18Mo6CuN without corrosion review. Tensile sampling follows the batch rules for the ordered test unit of 015Cr21Ni26Mo5Cu2, and retests follow GB/T 2102 when a result sits under the Table 3 floor. Keep the 015Cr21Ni26Mo5Cu2 caution visible here: Ni 23–28% / Mo 4–5% / Cu 1–2% — not interchangeable with 015Cr20Ni18Mo6CuN without corrosion review.

Grade Rm min (MPa) Rp0.2 min (MPa) A long. min (%) A trans. min (%)
015Cr21Ni26Mo5Cu2 490 220 35 30

Ambient values from GB/T 14976-2025 Table 3 for 015Cr21Ni26Mo5Cu2. Heat treatment (Table 1): 1065–1150 °C, water or rapid cool. Density 8.05 kg/dm³. Delivery: solution annealed.

Seamless Pipe Manufacture of GB/T 14976 015Cr21Ni26Mo5Cu2

GB/T 14976 manufactures 015Cr21Ni26Mo5Cu2 as seamless pipe only — cold-rolled or cold-drawn (symbol W-C) or hot-rolled, extruded, forged or expanded (symbol W-H). SHH STEEL confirms the manufacture symbol on the acknowledgement before piercing or drawing starts; welded pipe is outside this standard. Seamless W-C and W-H options remain available for 015Cr21Ni26Mo5Cu2; the acknowledgement repeats the manufacture symbol so production cannot silently change route after the PO is firm. Size practice for 015Cr21Ni26Mo5Cu2 remains cold-drawn W-C preferred; heat treatment 1065–1150 °C; density 8.05.

Process control for 015Cr21Ni26Mo5Cu2 ends with verified heat treatment (1065–1150 °C, water or rapid cool) and surface conditioning. Austenitic heats take solution annealing with water or other rapid cool per Table 1; hot-rolled austenitic pipe may count in-line rapid cool inside the Table 1 temperature band as meeting heat treatment (6.3.2) unless the purchaser forbids it.

Bevel geometry is by agreement when ordered without a drawing. Size practice: cold-drawn W-C preferred; heat treatment 1065–1150 °C; density 8.05. Density for theoretical weight of 015Cr21Ni26Mo5Cu2: 8.05 kg/dm³ per Table 1. Hydrostatic pressure or NDT class for 015Cr21Ni26Mo5Cu2 is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Keep the 015Cr21Ni26Mo5Cu2 caution visible here: Ni 23–28% / Mo 4–5% / Cu 1–2% — not interchangeable with 015Cr20Ni18Mo6CuN without corrosion review.

Dimensions and Tolerances for GB/T 14976 015Cr21Ni26Mo5Cu2

Usual length for GB/T 14976 pipe is 4000–12000 mm; fixed and multiple lengths sit inside that band with stated plus tolerances. For 015Cr21Ni26Mo5Cu2, confirm whether your project uses OD or ID ordering. Context: cold-drawn W-C preferred; heat treatment 1065–1150 °C; density 8.05. Tolerance class (PA/PC) follows the precision ordered for 015Cr21Ni26Mo5Cu2, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Keep the 015Cr21Ni26Mo5Cu2 caution visible here: Ni 23–28% / Mo 4–5% / Cu 1–2% — not interchangeable with 015Cr20Ni18Mo6CuN without corrosion review.

Full-length bend ≤0.15% of length; per-metre bend ≤1.5 mm (S≤15 mm) or ≤2.0 mm (S>15 mm). 015Cr21Ni26Mo5Cu2 must meet those geometry floors unless a written waiver exists. Fixed lengths and multiple cut lengths for 015Cr21Ni26Mo5Cu2 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. This paragraph is locked to 015Cr21Ni26Mo5Cu2 duty: high-Ni Mo-Cu austenitic seamless pipe for severe reducing-acid and chloride fluid service (904L-class family).

Equivalent Grades for GB/T 14976 015Cr21Ni26Mo5Cu2

European and ASTM marks may sit near 904L-class / UNS N08904-related, yet GB/T 14976 hydrostatic and heat-treatment text for 015Cr21Ni26Mo5Cu2 still diverge. Keep 015Cr21Ni26Mo5Cu2 as the governing symbol. Caution retained from pack notes: Ni 23–28% / Mo 4–5% / Cu 1–2% — not interchangeable with 015Cr20Ni18Mo6CuN without corrosion review.

System Designation Notes
GB/T 14976 015Cr21Ni26Mo5Cu2 Governing pipe grade for this page
Commercial / UNS (body only) 904L-class / UNS N08904-related (unified S39042) Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A312 related 904L-family related marks Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

Sister pages worth reading beside 015Cr21Ni26Mo5Cu2: GB/T 14976 015Cr20Ni18Mo6CuN, GB/T 14976 022Cr19Ni13Mo3, GB/T 14976 022Cr18Ni14Mo2Cu2, GB/T 14976 06Cr19Ni13Mo3. Duty locked here: high-Ni Mo-Cu austenitic seamless pipe for severe reducing-acid and chloride fluid service (904L-class family). Any EN or ASTM designation above is a starting point for comparison, not a substitute grade on the GB/T 14976 certificate. Series hub: GB/T 14976.

Buyers comparing 015Cr21Ni26Mo5Cu2 tubulars with sheet/plate can the parent hubs are Stainless Steel Pipes and Tubes and Stainless Steel Sheets and Plates; related plate chemistry is published as GB/T 4237 015Cr21Ni26Mo5Cu2. See also the GB/T 4237 hub for related plate designations. Keep 015Cr21Ni26Mo5Cu2 acceptance text on the governing pipe/tube standard.

Heat Treatment and Delivery Condition for GB/T 14976 015Cr21Ni26Mo5Cu2

Other heat-treatment schedules are allowed only by written agreement (6.3.4) — silence means Table 1 defaults. For 015Cr21Ni26Mo5Cu2: 1065–1150 °C, water or rapid cool. Recorded furnace charts for 015Cr21Ni26Mo5Cu2 should support the Table 1 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Corrosion framing beside 015Cr21Ni26Mo5Cu2: high alloy content targets reducing acids and strong chlorides; still confirm coupons rather than inventing PREN posters.

After local hot work in the field, restore solution annealed practice when the corrosion file demands it. Caution: Ni 23–28% / Mo 4–5% / Cu 1–2% — not interchangeable with 015Cr20Ni18Mo6CuN without corrosion review. Field heat treatment of 015Cr21Ni26Mo5Cu2 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Corrosion framing beside 015Cr21Ni26Mo5Cu2: high alloy content targets reducing acids and strong chlorides; still confirm coupons rather than inventing PREN posters.

Corrosion Resistance of GB/T 14976 015Cr21Ni26Mo5Cu2

Pick tests that match how 015Cr21Ni26Mo5Cu2 is filed — austenitic. Corrosion thread: high alloy content targets reducing acids and strong chlorides; still confirm coupons rather than inventing PREN posters. Caution: Ni 23–28% / Mo 4–5% / Cu 1–2% — not interchangeable with 015Cr20Ni18Mo6CuN without corrosion review. Coupon orientation, weld condition, and surface finish for 015Cr21Ni26Mo5Cu2 belong in the corrosion test order so annex results can be compared to the installed spool honestly. Weld-shop note tied to 015Cr21Ni26Mo5Cu2: over-alloyed Ni-Cr-Mo-Cu fillers; strict heat-input control and solution anneal when required.

Oxygen-line Annex B and cryogenic Annex A add impact, UT, and cleanliness rules — they do not change the alloy selection logic. Use thread: sulphuric and mixed-acid transfer, seawater-lean process lines, scrubber fluid piping, and aggressive chemical headers on Chinese specs. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 015Cr21Ni26Mo5Cu2 rather than relying on wall thickness alone. This paragraph is locked to 015Cr21Ni26Mo5Cu2 duty: high-Ni Mo-Cu austenitic seamless pipe for severe reducing-acid and chloride fluid service (904L-class family).

Applications of GB/T 14976 015Cr21Ni26Mo5Cu2 Seamless Pipe

Project types that repeatedly call 015Cr21Ni26Mo5Cu2: sulphuric and mixed-acid transfer, seawater-lean process lines, scrubber fluid piping, and aggressive chemical headers on Chinese specs. Duty: high-Ni Mo-Cu austenitic seamless pipe for severe reducing-acid and chloride fluid service (904L-class family). Caution still applies: Ni 23–28% / Mo 4–5% / Cu 1–2% — not interchangeable with 015Cr20Ni18Mo6CuN without corrosion review.

Cryogenic, oxygen, and corrosive process lines all appear in 14976’s scope options — alloy choice still follows the medium. For this mark: high-Ni Mo-Cu austenitic seamless pipe for severe reducing-acid and chloride fluid service (904L-class family). Commissioning teams benefit when the as-built dossier repeats 015Cr21Ni26Mo5Cu2 beside heat numbers, linking isometric revisions to the same mill certificates. Size practice for 015Cr21Ni26Mo5Cu2 remains cold-drawn W-C preferred; heat treatment 1065–1150 °C; density 8.05.

Weldability of GB/T 14976 015Cr21Ni26Mo5Cu2

Even seamless W-C/W-H pipe of 015Cr21Ni26Mo5Cu2 will see field welds. Use: over-alloyed Ni-Cr-Mo-Cu fillers; strict heat-input control and solution anneal when required. Restore heat treatment when the WPS and corrosion file require it. Procedure qualification for 015Cr21Ni26Mo5Cu2 should use the same product form and wall class as production, including the seamless finish that will ship. Application context for 015Cr21Ni26Mo5Cu2 stays sulphuric and mixed-acid transfer, seawater-lean process lines, scrubber fluid piping, and aggressive chemical headers on Chinese specs.

Dissimilar welds to carbon steel need buttering and dilution control — especially on Mo and high-Ni grades. Role context: high-Ni Mo-Cu austenitic seamless pipe for severe reducing-acid and chloride fluid service (904L-class family). Consumable lot control and shielding-gas notes for 015Cr21Ni26Mo5Cu2 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Keep the 015Cr21Ni26Mo5Cu2 caution visible here: Ni 23–28% / Mo 4–5% / Cu 1–2% — not interchangeable with 015Cr20Ni18Mo6CuN without corrosion review.

Surface Finishes for GB/T 14976 015Cr21Ni26Mo5Cu2

Finish options for 015Cr21Ni26Mo5Cu2 follow the ordered heat-treatment route under GB/T 14976. Descaled/pickled stock is the workhorse; bright annealed or polished surfaces are quoted when the datasheet owner writes a measurable Ra or appearance line. Delivery crib note: solution annealed. Chloride-lean stencil ink and iron-free packing materials are part of the finish package, not optional warehouse habits (015Cr21Ni26Mo5Cu2).

Finish Typical supply Order note
Solution annealed and pickled Standard pipe mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

Passivation restores the chromium-rich film after pickling or light fabrication on 015Cr21Ni26Mo5Cu2; it does not replace the heat treatment that sets mechanical properties under GB/T 14976. Keep carbon-steel tooling and strapping off finished bundles so free-iron stains do not bloom in service. Reject grinding burns and unrepaired defects before packing closes.

Inspection and Testing for GB/T 14976 015Cr21Ni26Mo5Cu2

Batching rules limit pieces per heat/size/heat-treat lot. For 015Cr21Ni26Mo5Cu2, keep the heat identity unbroken from melt to bundle tag. Duty: high-Ni Mo-Cu austenitic seamless pipe for severe reducing-acid and chloride fluid service (904L-class family). Sampling plans for 015Cr21Ni26Mo5Cu2 keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Corrosion framing beside 015Cr21Ni26Mo5Cu2: high alloy content targets reducing acids and strong chlorides; still confirm coupons rather than inventing PREN posters.

Intergranular corrosion testing is mandatory for most austenitics — see the IGC note for 015Cr21Ni26Mo5Cu2. Order extras (grain size, inclusions, elevated tensile) under 7.8.3 when needed. Non-conforming 015Cr21Ni26Mo5Cu2 lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Size practice for 015Cr21Ni26Mo5Cu2 remains cold-drawn W-C preferred; heat treatment 1065–1150 °C; density 8.05.

Packaging and Shipping for GB/T 14976 015Cr21Ni26Mo5Cu2

Small-OD 015Cr21Ni26Mo5Cu2 often ships in crates; large-OD in strapped bundles with OD pads. Confirm destination handling limits on the RFQ. Use: sulphuric and mixed-acid transfer, seawater-lean process lines, scrubber fluid piping, and aggressive chemical headers on Chinese specs. Bundle tickets for 015Cr21Ni26Mo5Cu2 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Corrosion framing beside 015Cr21Ni26Mo5Cu2: high alloy content targets reducing acids and strong chlorides; still confirm coupons rather than inventing PREN posters.

Bevelled ends get protectors so landing edges survive trucking. Size hint: cold-drawn W-C preferred; heat treatment 1065–1150 °C; density 8.05. Desiccant and wrap choices for 015Cr21Ni26Mo5Cu2 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Weld-shop note tied to 015Cr21Ni26Mo5Cu2: over-alloyed Ni-Cr-Mo-Cu fillers; strict heat-input control and solution anneal when required.

Storage advice on arrival: keep bundles dry and off carbon-steel floors. Use thread: sulphuric and mixed-acid transfer, seawater-lean process lines, scrubber fluid piping, and aggressive chemical headers on Chinese specs. Claims handling for 015Cr21Ni26Mo5Cu2 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Application context for 015Cr21Ni26Mo5Cu2 stays sulphuric and mixed-acid transfer, seawater-lean process lines, scrubber fluid piping, and aggressive chemical headers on Chinese specs.

Why Choose SHH STEEL

Project teams working to Chinese fluid-transport specs need a supplier that reads Chinese grade names correctly. SHH STEEL can make 015Cr21Ni26Mo5Cu2 to that discipline. Caution we keep visible: Ni 23–28% / Mo 4–5% / Cu 1–2% — not interchangeable with 015Cr20Ni18Mo6CuN without corrosion review. SHH STEEL can produce and supply 015Cr21Ni26Mo5Cu2 against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade.

Dual-cert discussions (GB/T + ASTM) are handled with two acceptance regimes in view, not one certificate stretched by hope. Sisters: 015Cr20Ni18Mo6CuN, 022Cr19Ni13Mo3, 022Cr18Ni14Mo2Cu2, 06Cr19Ni13Mo3. Ask for a written acknowledgement that names 015Cr21Ni26Mo5Cu2, W-C or W-H, and the Table 1 heat-treatment condition before melt. SHH STEEL can make 015Cr21Ni26Mo5Cu2 to that written scope.

Supply Capability

Whether you need prototype spools or project tonnage of 015Cr21Ni26Mo5Cu2, SHH STEEL can supply against a clear OD × wall and test matrix. Duty: sulphuric and mixed-acid transfer, seawater-lean process lines, scrubber fluid piping, and aggressive chemical headers on Chinese specs. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for 015Cr21Ni26Mo5Cu2 when the mill schedule allows.

Item Capability
Standard GB/T 14976-2025 seamless stainless steel pipes for fluid transport
Grade 015Cr21Ni26Mo5Cu2 (S39042)
Product form Seamless pipe only — cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H)
Delivery condition solution annealed
Documents Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered)
Typical size practice OD × wall per GB/T 17395; PA ordinary or PC higher precision; usual length 4000–12000 mm
Wall / ordering Nominal OD×wall, OD×min wall, or ID×wall by agreement

Stock / Available sizes

Stock / Available sizes: SHH STEEL quotes piercing/drawing slots for 015Cr21Ni26Mo5Cu2 rather than promising anonymous warehouse tons. Typical conversation starts around cold-drawn W-C preferred; heat treatment 1065–1150 °C; density 8.05. SHH STEEL can supply alternate walls and precision classes for 015Cr21Ni26Mo5Cu2 once the design pressure and corrosion allowance are clear. SHH STEEL can supply alternate walls and PA/PC classes for 015Cr21Ni26Mo5Cu2 once design pressure and corrosion allowance are clear. Corrosion framing beside 015Cr21Ni26Mo5Cu2: high alloy content targets reducing acids and strong chlorides; still confirm coupons rather than inventing PREN posters.

If the project needs dual GB/T 14976 + ASTM documentation, say so before melt. Caution: Ni 23–28% / Mo 4–5% / Cu 1–2% — not interchangeable with 015Cr20Ni18Mo6CuN without corrosion review. SHH STEEL can produce trial lengths of 015Cr21Ni26Mo5Cu2 for procedure qualification before the bulk release when the project calendar needs it.

FAQ

What is GB/T 14976 015Cr21Ni26Mo5Cu2 seamless stainless steel pipe used for?
GB/T 14976 015Cr21Ni26Mo5Cu2 is seamless stainless pipe for fluid transport — sulphuric and mixed-acid transfer, seawater-lean process lines, scrubber fluid piping, and aggressive chemical headers on Chinese specs. Role summary: high-Ni Mo-Cu austenitic seamless pipe for severe reducing-acid and chloride fluid service (904L-class family). It is a Chinese product standard grade (S39042), not an automatic ASTM A312 certificate.
Is GB/T 14976 015Cr21Ni26Mo5Cu2 seamless only, or does it cover welded pipe?
Seamless only. Clause 6.2 limits manufacture to cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 015Cr21Ni26Mo5Cu2 when the mill can meet the ordered size and tests. Welded pipe belongs under other standards, not 14976.
What heat treatment applies to 015Cr21Ni26Mo5Cu2?
015Cr21Ni26Mo5Cu2 is delivered solution annealed under GB/T 14976. Table 1 reference: 1065–1150 °C, water or rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Keep the purchase order locked to GB/T 14976 and 015Cr21Ni26Mo5Cu2 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
How does 015Cr21Ni26Mo5Cu2 compare with sister grades 015Cr20Ni18Mo6CuN, 022Cr19Ni13Mo3, 022Cr18Ni14Mo2Cu2?
015Cr21Ni26Mo5Cu2 is filed as austenitic. Typical sisters on the same RFQ are 015Cr20Ni18Mo6CuN, 022Cr19Ni13Mo3, 022Cr18Ni14Mo2Cu2. Design caution: Ni 23–28% / Mo 4–5% / Cu 1–2% — not interchangeable with 015Cr20Ni18Mo6CuN without corrosion review Pick the sister when the medium or strength floor outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 015Cr21Ni26Mo5Cu2?
Expect cast analysis (Table 2), room-temperature tensile results (Table 3), dimensions, hydrostatic test (or replacing UT/ET), appearance, and every special annex or IGC test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
Is 904L-class / UNS N08904-related the same as ordering 015Cr21Ni26Mo5Cu2?
No. 904L-class / UNS N08904-related is a commercial / UNS cross-walk for body text (unified S39042). The purchase order should lock GB/T 14976 and 015Cr21Ni26Mo5Cu2 so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GB/T 14976 015Cr21Ni26Mo5Cu2?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 015Cr21Ni26Mo5Cu2 within GB/T 17395 practice, with PA or PC precision and measured or min-wall options by agreement. Size context: cold-drawn W-C preferred; heat treatment 1065–1150 °C; density 8.05. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should 015Cr21Ni26Mo5Cu2 be welded on site?
Shop guidance: over-alloyed Ni-Cr-Mo-Cu fillers; strict heat-input control and solution anneal when required. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: Ni 23–28% / Mo 4–5% / Cu 1–2% — not interchangeable with 015Cr20Ni18Mo6CuN without corrosion review
When should I choose a higher-Mo or superaustenitic grade instead of 015Cr21Ni26Mo5Cu2?
Move when chloride pitting, crevice attack, or reducing-acid risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: Ni 23–28% / Mo 4–5% / Cu 1–2% — not interchangeable with 015Cr20Ni18Mo6CuN without corrosion review Sister pointers: 015Cr20Ni18Mo6CuN, 022Cr19Ni13Mo3, 022Cr18Ni14Mo2Cu2. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GB/T 14976 015Cr21Ni26Mo5Cu2 with ASTM A312?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 14976 015Cr21Ni26Mo5Cu2 does not clear ASTM acceptance by default. State both standards, sizes, and test scopes before melt. Keep the purchase order locked to GB/T 14976 and 015Cr21Ni26Mo5Cu2 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
What surface finishes are available for 015Cr21Ni26Mo5Cu2?
Pickled after heat treatment is the usual fluid-transport supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 015Cr21Ni26Mo5Cu2 when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

GB/T 14976 015Cr21Ni26Mo5Cu2 is seamless stainless steel pipe for fluid transport — high-Ni Mo-Cu austenitic seamless pipe for severe reducing-acid and chloride fluid service (904L-class family). SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 015Cr20Ni18Mo6CuN, 022Cr19Ni13Mo3, 022Cr18Ni14Mo2Cu2. Related ASTM pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X