GB/T 14976 022Cr19Ni10 Seamless Stainless Steel Pipe
What is GB/T 14976 022Cr19Ni10 Seamless Stainless Steel Pipe
GB/T 14976 covers seamless stainless pipe for fluid service — cold-drawn or hot-finished — with hydrostatic proof and optional Annex A cryogenic or Annex B oxygen extras. Inside that standard, 022Cr19Ni10 is filed as austenitic. If the isometrics are full of field welds and the medium is aqueous, GB/T 14976 022Cr19Ni10 is usually the honest Chinese 304L answer — not a hope that 06Cr19Ni10 “will be fine”.
From pierce/extrude/draw through marking and bundle protection, SHH STEEL can produce GB/T 14976 022Cr19Ni10 for the sizes and tests on your RFQ. Application sketch: chemical transfer, food and beverage CIP, pharmaceutical utilities, LNG-lean cold lines under Annex A when ordered, and welded spool work on Chinese fluid specs. Size and test clarity on the RFQ lets SHH STEEL lock the correct W-C or W-H symbol for 022Cr19Ni10 before production starts. Size practice for 022Cr19Ni10 remains cold-drawn W-C dominates sanitary and precision OD; hot-finished W-H for thicker pressure walls.
On the floor people shorten marks; in QA they must not. 022Cr19Ni10 under GB/T 14976 carries specific Table 2 windows and Table 3 floors that a loose “304L” note will not enforce. Caution: Rm and proof floors sit below 06Cr19Ni10 — do not substitute L stock into a drawing that needs the higher Table 3 tensile without engineer sign-off.
Cryogenic Annex A and oxygen Annex B sit in 14976’s special-requirements clause; still match the alloy to the medium. For 022Cr19Ni10, that means: low-carbon 18-8 austenitic seamless pipe for welded fluid systems that cannot rely on post-weld anneal. Nearby marks: 06Cr19Ni10, 022Cr17Ni12Mo2, 06Cr18Ni11Ti, 022Cr19Ni10N. Document the medium, design temperature, and weld map beside the 022Cr19Ni10 line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Corrosion framing beside 022Cr19Ni10: low carbon sharply cuts weld-zone sensitisation versus standard 06Cr19Ni10; chloride pitting still tracks Mo-free 18-8.
Inside this GB/T 14976 series, compare 06Cr19Ni10, 022Cr17Ni12Mo2, 06Cr18Ni11Ti, 022Cr19Ni10N. Hub: GB/T 14976. ASTM/ASME related product pages (not interchangeable by default): A312 TP304L.
Chemical Composition of GB/T 14976 022Cr19Ni10
For 022Cr19Ni10, the melt ticket has to show Table 2 compliance — C ≤0.030, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.030, Ni 8.00–12.00, Cr 18.00–20.00. Optional alloying footnotes in the standard still forbid blurring grade identity. Corrosion framing: low carbon sharply cuts weld-zone sensitisation versus standard 06Cr19Ni10; chloride pitting still tracks Mo-free 18-8.
Where Mo, Cu, Ti, Nb, Al or N appear, they are intentional levers for 022Cr19Ni10, not optional marketing. Confirm them on the MTC line-by-line. Role: low-carbon 18-8 austenitic seamless pipe for welded fluid systems that cannot rely on post-weld anneal. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 2, SHH STEEL will confirm melt feasibility for 022Cr19Ni10 before the order is acknowledged. Weld-shop note tied to 022Cr19Ni10: 308L fillers; keep interpass moderate and avoid carbon-steel contamination on pickled OD.
| Grade | C | Si | Mn | P | S | Ni | Cr |
|---|---|---|---|---|---|---|---|
| 022Cr19Ni10 | ≤0.030 | ≤1.00 | ≤2.00 | ≤0.035 | ≤0.030 | 8.00–12.00 | 18.00–20.00 |
Mechanical Properties of GB/T 14976 022Cr19Ni10
Do not confuse Table 3 pipe tensile floors with plate or tube standards that share the 304L / UNS S30403 alias. For 022Cr19Ni10 under 14976 expect Rm min 480 MPa, Rp0.2 min 175 MPa, elongation longitudinal min 40% / transverse min 35%, verified per heat/lot rules. Tensile sampling follows the batch rules for the ordered test unit of 022Cr19Ni10, and retests follow GB/T 2102 when a result sits under the Table 3 floor. Weld-shop note tied to 022Cr19Ni10: 308L fillers; keep interpass moderate and avoid carbon-steel contamination on pickled OD.
| Grade | Rm min (MPa) | Rp0.2 min (MPa) | A long. min (%) | A trans. min (%) |
|---|---|---|---|---|
| 022Cr19Ni10 | 480 | 175 | 40 | 35 |
Ambient values from GB/T 14976-2025 Table 3 for 022Cr19Ni10. Heat treatment (Table 1): 1010–1150 °C, water or rapid cool. Density 7.93 kg/dm³. Delivery: solution annealed.
Seamless Pipe Manufacture of GB/T 14976 022Cr19Ni10
Seamless is not optional wording for 022Cr19Ni10: clause 6.2 limits manufacture to W-C or W-H seamless routes. Pick W-C when OD precision and surface finish dominate; pick W-H when wall and tonnage favour hot working. SHH STEEL will not quietly substitute a welded route under a 14976 line item. Seamless W-C and W-H options remain available for 022Cr19Ni10; the acknowledgement repeats the manufacture symbol so production cannot silently change route after the PO is firm. Size practice for 022Cr19Ni10 remains cold-drawn W-C dominates sanitary and precision OD; hot-finished W-H for thicker pressure walls.
Cold-drawn austenitic 022Cr19Ni10 may ship cold-worked only by written agreement (6.3.3) with negotiated bend and tensile rules — silence means heat-treated delivery. Heat treatment: 1010–1150 °C, water or rapid cool. Austenitic heats take solution annealing with water or other rapid cool per Table 1; hot-rolled austenitic pipe may count in-line rapid cool inside the Table 1 temperature band as meeting heat treatment (6.3.2) unless the purchaser forbids it.
Hydrostatic testing is mandatory; ultrasonic or eddy-current may replace hydro per 7.3.3 when agreed. Manufacture stays seamless-only. Size: cold-drawn W-C dominates sanitary and precision OD; hot-finished W-H for thicker pressure walls. Hydrostatic pressure or NDT class for 022Cr19Ni10 is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Application context for 022Cr19Ni10 stays chemical transfer, food and beverage CIP, pharmaceutical utilities, LNG-lean cold lines under Annex A when ordered, and welded spool work on Chinese fluid specs.
Dimensions and Tolerances for GB/T 14976 022Cr19Ni10
Out-of-table OD×wall combinations are by agreement — still under the same grade symbol 022Cr19Ni10. Duty: low-carbon 18-8 austenitic seamless pipe for welded fluid systems that cannot rely on post-weld anneal. Tolerance class (PA/PC) follows the precision ordered for 022Cr19Ni10, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. This paragraph is locked to 022Cr19Ni10 duty: low-carbon 18-8 austenitic seamless pipe for welded fluid systems that cannot rely on post-weld anneal.
Ovality and wall unevenness, when ordered, stay within 80% of the respective OD and wall tolerances. Size reminder: cold-drawn W-C dominates sanitary and precision OD; hot-finished W-H for thicker pressure walls. Fixed lengths and multiple cut lengths for 022Cr19Ni10 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. This paragraph is locked to 022Cr19Ni10 duty: low-carbon 18-8 austenitic seamless pipe for welded fluid systems that cannot rely on post-weld anneal.
Equivalent Grades for GB/T 14976 022Cr19Ni10
Identity first: GB/T 14976 022Cr19Ni10 is the HX/pipe grade for this page. 304L / UNS S30403 helps buyers who think in AISI/UNS labels. Role: low-carbon 18-8 austenitic seamless pipe for welded fluid systems that cannot rely on post-weld anneal. Foreign product standards remain separate documents. Treat any brochure “equivalent” claim as an engineering comparison against both product standards, not as permission to swap certificates on the mill floor (022Cr19Ni10).
| System | Designation | Notes |
|---|---|---|
| GB/T 14976 | 022Cr19Ni10 | Governing pipe grade for this page |
| Commercial / UNS (body only) | 304L / UNS S30403 | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A312 related | 304L chemistry family | Related chemistry — different product standard; not interchangeable by default |
| EN / other | No one-to-one asserted | Starting point for comparison only against local product specs |
Inside this series compare 06Cr19Ni10, 022Cr17Ni12Mo2, 06Cr18Ni11Ti, 022Cr19Ni10N before swapping marks for medium or temperature. Keep this caution visible for 022Cr19Ni10: Rm and proof floors sit below 06Cr19Ni10 — do not substitute L stock into a drawing that needs the higher Table 3 tensile without engineer sign-off. Hub: GB/T 14976.
Heat Treatment and Delivery Condition for GB/T 14976 022Cr19Ni10
Hot-finished austenitic seamless may use in-line rapid cool inside the Table 1 band under 6.3.2 unless the purchaser forbids it. Confirm for 022Cr19Ni10. Band: 1010–1150 °C, water or rapid cool. Recorded furnace charts for 022Cr19Ni10 should support the Table 1 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. This paragraph is locked to 022Cr19Ni10 duty: low-carbon 18-8 austenitic seamless pipe for welded fluid systems that cannot rely on post-weld anneal.
Grain-size or inclusion testing under 7.8.3 applies only when ordered — state any extra metallographic demand on the PO for 022Cr19Ni10. Field heat treatment of 022Cr19Ni10 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Corrosion framing beside 022Cr19Ni10: low carbon sharply cuts weld-zone sensitisation versus standard 06Cr19Ni10; chloride pitting still tracks Mo-free 18-8.
Corrosion Resistance of GB/T 14976 022Cr19Ni10
Medium, temperature, crevice geometry and weld condition decide whether 022Cr19Ni10 is enough. Summary: low carbon sharply cuts weld-zone sensitisation versus standard 06Cr19Ni10; chloride pitting still tracks Mo-free 18-8. Escalate via sisters 06Cr19Ni10, 022Cr17Ni12Mo2, 06Cr18Ni11Ti, 022Cr19Ni10N when coupons fail. Coupon orientation, weld condition, and surface finish for 022Cr19Ni10 belong in the corrosion test order so annex results can be compared to the installed spool honestly. Keep the 022Cr19Ni10 caution visible here: Rm and proof floors sit below 06Cr19Ni10 — do not substitute L stock into a drawing that needs the higher Table 3 tensile without engineer sign-off.
Surface finish and iron contamination control often matter as much as bulk chemistry on sanitary-lean duties for 022Cr19Ni10. Corrosion framing: low carbon sharply cuts weld-zone sensitisation versus standard 06Cr19Ni10; chloride pitting still tracks Mo-free 18-8. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 022Cr19Ni10 rather than relying on wall thickness alone. Weld-shop note tied to 022Cr19Ni10: 308L fillers; keep interpass moderate and avoid carbon-steel contamination on pickled OD.
Applications of GB/T 14976 022Cr19Ni10 Seamless Pipe
From utility rooms to process racks, 022Cr19Ni10 shows up wherever Chinese fluid specs want austenitic seamless behaviour. Use list: chemical transfer, food and beverage CIP, pharmaceutical utilities, LNG-lean cold lines under Annex A when ordered, and welded spool work on Chinese fluid specs. Spool fabricators should copy 022Cr19Ni10 onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Size practice for 022Cr19Ni10 remains cold-drawn W-C dominates sanitary and precision OD; hot-finished W-H for thicker pressure walls.
If the only reason for 022Cr19Ni10 is “we always used this alias,” reopen the corrosion file before repeating the order. Caution: Rm and proof floors sit below 06Cr19Ni10 — do not substitute L stock into a drawing that needs the higher Table 3 tensile without engineer sign-off. Commissioning teams benefit when the as-built dossier repeats 022Cr19Ni10 beside heat numbers, linking isometric revisions to the same mill certificates. Size practice for 022Cr19Ni10 remains cold-drawn W-C dominates sanitary and precision OD; hot-finished W-H for thicker pressure walls.
Weldability of GB/T 14976 022Cr19Ni10
Automatic mill welding is outside GB/T 14976; manual and automatic field welds must still respect 022Cr19Ni10 chemistry. Guidance: 308L fillers; keep interpass moderate and avoid carbon-steel contamination on pickled OD. Procedure qualification for 022Cr19Ni10 should use the same product form and wall class as production, including the seamless finish that will ship. Size practice for 022Cr19Ni10 remains cold-drawn W-C dominates sanitary and precision OD; hot-finished W-H for thicker pressure walls.
Ferrite control on high-Ni austenitics and hydrogen management on martensitic 022Cr19Ni10 are procedure items, not afterthoughts. Guidance: 308L fillers; keep interpass moderate and avoid carbon-steel contamination on pickled OD. Consumable lot control and shielding-gas notes for 022Cr19Ni10 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. This paragraph is locked to 022Cr19Ni10 duty: low-carbon 18-8 austenitic seamless pipe for welded fluid systems that cannot rely on post-weld anneal.
Surface Finishes for GB/T 14976 022Cr19Ni10
Welded or heavily formed 022Cr19Ni10 may need bead dressing or ID attention for flow and inspection — call that out rather than assuming mill habit. Size/finish context stays tied to GB/T 14976 seamless stainless fluid-transport pipe. Caution: Rm and proof floors sit below 06Cr19Ni10 — do not substitute L stock into a drawing that needs the higher Table 3 tensile without engineer sign-off.
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard pipe mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
Passivation restores the chromium-rich film after pickling or light fabrication on 022Cr19Ni10; it does not replace the heat treatment that sets mechanical properties under GB/T 14976. Keep carbon-steel tooling and strapping off finished bundles so free-iron stains do not bloom in service. Reject grinding burns and unrepaired defects before packing closes.
Inspection and Testing for GB/T 14976 022Cr19Ni10
Third-party witness (SGS/TUV-style) is available when the project mandate requires it. Base acceptance still tracks GB/T 14976 for 022Cr19Ni10. Sampling plans for 022Cr19Ni10 keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Keep the 022Cr19Ni10 caution visible here: Rm and proof floors sit below 06Cr19Ni10 — do not substitute L stock into a drawing that needs the higher Table 3 tensile without engineer sign-off.
Dimensional inspection against Table 4/5 tolerances closes the lot. Failures retest per GB/T 2102 — they are not silently shipped. Role: low-carbon 18-8 austenitic seamless pipe for welded fluid systems that cannot rely on post-weld anneal. Non-conforming 022Cr19Ni10 lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Application context for 022Cr19Ni10 stays chemical transfer, food and beverage CIP, pharmaceutical utilities, LNG-lean cold lines under Annex A when ordered, and welded spool work on Chinese fluid specs.
Packaging and Shipping for GB/T 14976 022Cr19Ni10
Seaworthy packing is available for ocean legs — desiccant, VCI, and wrap specs by agreement. Grade mark 022Cr19Ni10 stays visible on outer tags. Oxygen Annex B adds oil-free packing language when invoked. Bundle tickets for 022Cr19Ni10 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Corrosion framing beside 022Cr19Ni10: low carbon sharply cuts weld-zone sensitisation versus standard 06Cr19Ni10; chloride pitting still tracks Mo-free 18-8.
Container loading plans should keep heavy walls from crushing thin-wall 022Cr19Ni10 layers. Desiccant and wrap choices for 022Cr19Ni10 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Weld-shop note tied to 022Cr19Ni10: 308L fillers; keep interpass moderate and avoid carbon-steel contamination on pickled OD.
Shortages or transit damage claims need photos against the packing list before installation starts — tag identity must still read 022Cr19Ni10. Claims handling for 022Cr19Ni10 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Application context for 022Cr19Ni10 stays chemical transfer, food and beverage CIP, pharmaceutical utilities, LNG-lean cold lines under Annex A when ordered, and welded spool work on Chinese fluid specs.
Why Choose SHH STEEL
From RFQ clarification through MTC release, SHH STEEL treats 022Cr19Ni10 as a governed product grade, not a marketing synonym for 304L / UNS S30403. Role: low-carbon 18-8 austenitic seamless pipe for welded fluid systems that cannot rely on post-weld anneal. SHH STEEL can produce and supply 022Cr19Ni10 against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade.
Response time stays short because common 022Cr19Ni10 enquiry sizes and document packs are already exercised on prior Chinese-spec orders. Use: chemical transfer, food and beverage CIP, pharmaceutical utilities, LNG-lean cold lines under Annex A when ordered, and welded spool work on Chinese fluid specs. Ask for a written acknowledgement that names 022Cr19Ni10, W-C or W-H, and the Table 1 heat-treatment condition before melt. SHH STEEL can make 022Cr19Ni10 to that written scope.
Supply Capability
Capability framing for 022Cr19Ni10: Chinese-spec seamless fluid pipe, W-C/W-H manufacture, documented heats. Caution remains: Rm and proof floors sit below 06Cr19Ni10 — do not substitute L stock into a drawing that needs the higher Table 3 tensile without engineer sign-off. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for 022Cr19Ni10 when the mill schedule allows.
| Item | Capability |
|---|---|
| Standard | GB/T 14976-2025 seamless stainless steel pipes for fluid transport |
| Grade | 022Cr19Ni10 (S30403) |
| Product form | Seamless pipe only — cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H) |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered) |
| Typical size practice | OD × wall per GB/T 17395; PA ordinary or PC higher precision; usual length 4000–12000 mm |
| Wall / ordering | Nominal OD×wall, OD×min wall, or ID×wall by agreement |
Stock / Available sizes
Stock / Available sizes — treat published ranges as capability envelopes. Actual ex-stock pieces of 022Cr19Ni10 change weekly; the reliable path is an OD × wall matrix on the enquiry. Duty: low-carbon 18-8 austenitic seamless pipe for welded fluid systems that cannot rely on post-weld anneal. SHH STEEL can supply alternate walls and precision classes for 022Cr19Ni10 once the design pressure and corrosion allowance are clear.
Repeat orders for 022Cr19Ni10 go faster when prior heat records and accepted WPS numbers are referenced on the new RFQ. Role: low-carbon 18-8 austenitic seamless pipe for welded fluid systems that cannot rely on post-weld anneal. SHH STEEL can produce trial lengths of 022Cr19Ni10 for procedure qualification before the bulk release when the project calendar needs it.
FAQ
-
What is GB/T 14976 022Cr19Ni10 seamless stainless steel pipe used for?
- GB/T 14976 022Cr19Ni10 is seamless stainless pipe for fluid transport — chemical transfer, food and beverage CIP, pharmaceutical utilities, LNG-lean cold lines under Annex A when ordered, and welded spool work on Chinese fluid specs. Role summary: low-carbon 18-8 austenitic seamless pipe for welded fluid systems that cannot rely on post-weld anneal. It is a Chinese product standard grade (S30403), not an automatic ASTM A312 certificate.
-
Is GB/T 14976 022Cr19Ni10 seamless only, or does it cover welded pipe?
- Seamless only. Clause 6.2 limits manufacture to cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 022Cr19Ni10 when the mill can meet the ordered size and tests. Welded pipe belongs under other standards, not 14976.
-
What heat treatment applies to 022Cr19Ni10?
- 022Cr19Ni10 is delivered solution annealed under GB/T 14976. Table 1 reference: 1010–1150 °C, water or rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Keep the purchase order locked to GB/T 14976 and 022Cr19Ni10 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
-
How does 022Cr19Ni10 compare with sister grades 06Cr19Ni10, 022Cr17Ni12Mo2, 06Cr18Ni11Ti?
- 022Cr19Ni10 is filed as austenitic. Typical sisters on the same RFQ are 06Cr19Ni10, 022Cr17Ni12Mo2, 06Cr18Ni11Ti. Design caution: Rm and proof floors sit below 06Cr19Ni10 — do not substitute L stock into a drawing that needs the higher Table 3 tensile without engineer sign-off Pick the sister when the medium or strength floor outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 022Cr19Ni10?
- Expect cast analysis (Table 2), room-temperature tensile results (Table 3), dimensions, hydrostatic test (or replacing UT/ET), appearance, and every special annex or IGC test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
-
Is 304L / UNS S30403 the same as ordering 022Cr19Ni10?
- No. 304L / UNS S30403 is a commercial / UNS cross-walk for body text (unified S30403). The purchase order should lock GB/T 14976 and 022Cr19Ni10 so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GB/T 14976 022Cr19Ni10?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 022Cr19Ni10 within GB/T 17395 practice, with PA or PC precision and measured or min-wall options by agreement. Size context: cold-drawn W-C dominates sanitary and precision OD; hot-finished W-H for thicker pressure walls. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
How should 022Cr19Ni10 be welded on site?
- Shop guidance: 308L fillers; keep interpass moderate and avoid carbon-steel contamination on pickled OD. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: Rm and proof floors sit below 06Cr19Ni10 — do not substitute L stock into a drawing that needs the higher Table 3 tensile without engineer sign-off
-
When should I choose a higher-Mo or superaustenitic grade instead of 022Cr19Ni10?
- Move when chloride pitting, crevice attack, or reducing-acid risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: Rm and proof floors sit below 06Cr19Ni10 — do not substitute L stock into a drawing that needs the higher Table 3 tensile without engineer sign-off Sister pointers: 06Cr19Ni10, 022Cr17Ni12Mo2, 06Cr18Ni11Ti. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GB/T 14976 022Cr19Ni10 with ASTM A312?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 14976 022Cr19Ni10 does not clear ASTM acceptance by default. State both standards, sizes, and test scopes before melt. Keep the purchase order locked to GB/T 14976 and 022Cr19Ni10 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
-
What surface finishes are available for 022Cr19Ni10?
- Pickled after heat treatment is the usual fluid-transport supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 022Cr19Ni10 when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
GB/T 14976 022Cr19Ni10 is seamless stainless steel pipe for fluid transport — low-carbon 18-8 austenitic seamless pipe for welded fluid systems that cannot rely on post-weld anneal. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 06Cr19Ni10, 022Cr17Ni12Mo2, 06Cr18Ni11Ti. Related ASTM pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.