GB/T 14976 06Cr18Ni11Ti Seamless Stainless Steel Pipe

GB/T 14976 06Cr18Ni11Ti seamless stainless steel pipe (321 / UNS S32168, S32168), austenitic, Table 2 cast analysis, Rm min 520 (S≤9.5 mm) / 485 (S>9.5 mm) MPa / Rp0.2 min 205 (S≤9.5) / 170 (S>9.5) MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
Grade
06Cr18Ni11Ti (S32168 / 321 / UNS S32168 — body alias)
Standard
GB/T 14976-2025
Product form
Seamless stainless steel pipe (W-C / W-H), delivery solution annealed
Size
OD × wall per GB/T 17395; PA/PC precision; usual length 4000–12000 mm; other by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Pipe Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GB/T 14976 06Cr18Ni11Ti Seamless Stainless Steel Pipe

GB/T 14976 covers seamless stainless pipe for fluid service — cold-drawn or hot-finished — with hydrostatic proof and optional Annex A cryogenic or Annex B oxygen extras. Inside that standard, 06Cr18Ni11Ti is filed as austenitic. GB/T 14976 06Cr18Ni11Ti is the Chinese 321 seamless fluid mark — stabilisation is on the melt ticket, not a sticker after the fact.

From pierce/extrude/draw through marking and bundle protection, SHH STEEL can produce GB/T 14976 06Cr18Ni11Ti for the sizes and tests on your RFQ. Application sketch: chemical transfer with dense field welds, heat-exchange fluid loops, and process lines that want 321-class stabilisation on Chinese specs. Size and test clarity on the RFQ lets SHH STEEL lock the correct W-C or W-H symbol for 06Cr18Ni11Ti before production starts. Corrosion framing beside 06Cr18Ni11Ti: Ti stabilisation cuts weld decay risk versus standard-carbon 06Cr19Ni10; chloride pitting still tracks Mo-free 18-8.

On the floor people shorten marks; in QA they must not. 06Cr18Ni11Ti under GB/T 14976 carries specific Table 2 windows and Table 3 floors that a loose “321” note will not enforce. Caution: Rm/Rp0.2 are wall-dependent (S≤9.5 vs S>9.5) — quote the ordered wall against Table 3 footnotes. Keep isometric notes, valve specs, and the mill acknowledgement aligned on 06Cr18Ni11Ti so informal alias language cannot reopen the carbon or molybdenum window after melt. Keep the 06Cr18Ni11Ti caution visible here: Rm/Rp0.2 are wall-dependent (S≤9.5 vs S>9.5) — quote the ordered wall against Table 3 footnotes.

Cryogenic Annex A and oxygen Annex B sit in 14976’s special-requirements clause; still match the alloy to the medium. For 06Cr18Ni11Ti, that means: Ti-stabilised 18-8 austenitic seamless pipe for fluid systems welded without post-weld solution anneal. Nearby marks: 07Cr19Ni11Ti, 06Cr18Ni11Nb, 022Cr19Ni10, 06Cr17Ni12Mo2Ti. Document the medium, design temperature, and weld map beside the 06Cr18Ni11Ti line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Corrosion framing beside 06Cr18Ni11Ti: Ti stabilisation cuts weld decay risk versus standard-carbon 06Cr19Ni10; chloride pitting still tracks Mo-free 18-8.

Inside this GB/T 14976 series, compare GB/T 14976 07Cr19Ni11Ti, GB/T 14976 06Cr18Ni11Nb, GB/T 14976 022Cr19Ni10, GB/T 14976 06Cr17Ni12Mo2Ti. Hub: GB/T 14976. ASTM/ASME related product pages (not interchangeable by default): ASTM A312 TP321.

Chemical Composition of GB/T 14976 06Cr18Ni11Ti

For 06Cr18Ni11Ti, the melt ticket has to show Table 2 compliance — C ≤0.08, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.030, Ni 9.00–12.00, Cr 17.00–19.00, Ti 5(C+N)–0.70. Optional alloying footnotes in the standard still forbid blurring grade identity. Corrosion framing: Ti stabilisation cuts weld decay risk versus standard-carbon 06Cr19Ni10; chloride pitting still tracks Mo-free 18-8.

Where Mo, Cu, Ti, Nb, Al or N appear, they are intentional levers for 06Cr18Ni11Ti, not optional marketing. Confirm them on the MTC line-by-line. Role: Ti-stabilised 18-8 austenitic seamless pipe for fluid systems welded without post-weld solution anneal. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 2, SHH STEEL will confirm melt feasibility for 06Cr18Ni11Ti before the order is acknowledged. Application context for 06Cr18Ni11Ti stays chemical transfer with dense field welds, heat-exchange fluid loops, and process lines that want 321-class stabilisation on Chinese specs.

Grade C Si Mn P S Ni Cr Ti
06Cr18Ni11Ti ≤0.08 ≤1.00 ≤2.00 ≤0.035 ≤0.030 9.00–12.00 17.00–19.00 5(C+N)–0.70

Mechanical Properties of GB/T 14976 06Cr18Ni11Ti

Do not confuse Table 3 pipe tensile floors with plate or tube standards that share the 321 / UNS S32168 alias. For 06Cr18Ni11Ti under 14976 expect Rm min 520 (S≤9.5 mm) / 485 (S>9.5 mm) MPa, Rp0.2 min 205 (S≤9.5) / 170 (S>9.5) MPa, elongation longitudinal min 35% / transverse min 30%, verified per heat/lot rules. Note: Rm/Rp0.2 depend on wall: S≤9.5 mm → 520/205; S>9.5 mm → 485/170.

Grade Rm min (MPa) Rp0.2 min (MPa) A long. min (%) A trans. min (%)
06Cr18Ni11Ti 520 (S≤9.5 mm) / 485 (S>9.5 mm) 205 (S≤9.5) / 170 (S>9.5) 35 30

Ambient values from GB/T 14976-2025 Table 3 for 06Cr18Ni11Ti. Heat treatment (Table 1): 920–1150 °C, water or rapid cool. Rm/Rp0.2 depend on wall: S≤9.5 mm → 520/205; S>9.5 mm → 485/170. Density 7.93 kg/dm³. Delivery: solution annealed.

Seamless Pipe Manufacture of GB/T 14976 06Cr18Ni11Ti

GB/T 14976 manufactures 06Cr18Ni11Ti as seamless pipe only — cold-rolled or cold-drawn (symbol W-C) or hot-rolled, extruded, forged or expanded (symbol W-H). SHH STEEL confirms the manufacture symbol on the acknowledgement before piercing or drawing starts; welded pipe is outside this standard. Seamless W-C and W-H options remain available for 06Cr18Ni11Ti; the acknowledgement repeats the manufacture symbol so production cannot silently change route after the PO is firm. Weld-shop note tied to 06Cr18Ni11Ti: 321/308L fillers per WPS; avoid excessive heat that re-dissolves Ti carbides.

Cold-drawn austenitic 06Cr18Ni11Ti may ship cold-worked only by written agreement (6.3.3) with negotiated bend and tensile rules — silence means heat-treated delivery. Heat treatment: 920–1150 °C, water or rapid cool. Austenitic heats take solution annealing with water or other rapid cool per Table 1; hot-rolled austenitic pipe may count in-line rapid cool inside the Table 1 temperature band as meeting heat treatment (6.3.2) unless the purchaser forbids it.

Hydrostatic testing is mandatory; ultrasonic or eddy-current may replace hydro per 7.3.3 when agreed. Manufacture stays seamless-only. Size: W-C common; heat treatment 920–1150 °C; watch wall footnote on tensile. Hydrostatic pressure or NDT class for 06Cr18Ni11Ti is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Keep the 06Cr18Ni11Ti caution visible here: Rm/Rp0.2 are wall-dependent (S≤9.5 vs S>9.5) — quote the ordered wall against Table 3 footnotes.

Dimensions and Tolerances for GB/T 14976 06Cr18Ni11Ti

Out-of-table OD×wall combinations are by agreement — still under the same grade symbol 06Cr18Ni11Ti. Duty: Ti-stabilised 18-8 austenitic seamless pipe for fluid systems welded without post-weld solution anneal. Tolerance class (PA/PC) follows the precision ordered for 06Cr18Ni11Ti, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Weld-shop note tied to 06Cr18Ni11Ti: 321/308L fillers per WPS; avoid excessive heat that re-dissolves Ti carbides.

Ovality and wall unevenness, when ordered, stay within 80% of the respective OD and wall tolerances. Size reminder: W-C common; heat treatment 920–1150 °C; watch wall footnote on tensile. Fixed lengths and multiple cut lengths for 06Cr18Ni11Ti are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. This paragraph is locked to 06Cr18Ni11Ti duty: Ti-stabilised 18-8 austenitic seamless pipe for fluid systems welded without post-weld solution anneal.

Equivalent Grades for GB/T 14976 06Cr18Ni11Ti

Lock 06Cr18Ni11Ti on the PO when the datasheet owner wants GB/T 14976 seamless stainless fluid-transport pipe. Commercial talk as 321 / UNS S32168 is fine in emails; mill paperwork must still show GB/T 14976 06Cr18Ni11Ti. Application framing: chemical transfer with dense field welds, heat-exchange fluid loops, and process lines that want 321-class stabilisation on Chinese specs.

System Designation Notes
GB/T 14976 06Cr18Ni11Ti Governing pipe grade for this page
Commercial / UNS (body only) 321 / UNS S32168 Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A312 related 321 chemistry family Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

Order discipline for 06Cr18Ni11Ti still points at GB/T 14976, not the brochure alias. Neighbours GB/T 14976 07Cr19Ni11Ti, GB/T 14976 06Cr18Ni11Nb, GB/T 14976 022Cr19Ni10, GB/T 14976 06Cr17Ni12Mo2Ti each carry their own mechanical table. Category hub: GB/T 14976. Treat any brochure “equivalent” claim as an engineering comparison against both product standards, not as permission to swap certificates on the mill floor (06Cr18Ni11Ti).

Project teams specifying 06Cr18Ni11Ti should the parent hubs are Stainless Steel Pipes and Tubes and Stainless Steel Sheets and Plates; related plate chemistry is published as GB/T 3280 06Cr18Ni11Ti. See also the GB/T 4237 hub for related plate designations. Confirm 06Cr18Ni11Ti OD × wall and plate thickness on separate drawings.

Heat Treatment and Delivery Condition for GB/T 14976 06Cr18Ni11Ti

Hot-finished austenitic seamless may use in-line rapid cool inside the Table 1 band under 6.3.2 unless the purchaser forbids it. Confirm for 06Cr18Ni11Ti. Band: 920–1150 °C, water or rapid cool. Recorded furnace charts for 06Cr18Ni11Ti should support the Table 1 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Keep the 06Cr18Ni11Ti caution visible here: Rm/Rp0.2 are wall-dependent (S≤9.5 vs S>9.5) — quote the ordered wall against Table 3 footnotes.

Grain-size or inclusion testing under 7.8.3 applies only when ordered — state any extra metallographic demand on the PO for 06Cr18Ni11Ti. Field heat treatment of 06Cr18Ni11Ti after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Keep the 06Cr18Ni11Ti caution visible here: Rm/Rp0.2 are wall-dependent (S≤9.5 vs S>9.5) — quote the ordered wall against Table 3 footnotes.

Corrosion Resistance of GB/T 14976 06Cr18Ni11Ti

Medium, temperature, crevice geometry and weld condition decide whether 06Cr18Ni11Ti is enough. Summary: Ti stabilisation cuts weld decay risk versus standard-carbon 06Cr19Ni10; chloride pitting still tracks Mo-free 18-8. Escalate via sisters 07Cr19Ni11Ti, 06Cr18Ni11Nb, 022Cr19Ni10, 06Cr17Ni12Mo2Ti when coupons fail. Coupon orientation, weld condition, and surface finish for 06Cr18Ni11Ti belong in the corrosion test order so annex results can be compared to the installed spool honestly. Weld-shop note tied to 06Cr18Ni11Ti: 321/308L fillers per WPS; avoid excessive heat that re-dissolves Ti carbides.

Surface finish and iron contamination control often matter as much as bulk chemistry on sanitary-lean duties for 06Cr18Ni11Ti. Corrosion framing: Ti stabilisation cuts weld decay risk versus standard-carbon 06Cr19Ni10; chloride pitting still tracks Mo-free 18-8. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 06Cr18Ni11Ti rather than relying on wall thickness alone. Keep the 06Cr18Ni11Ti caution visible here: Rm/Rp0.2 are wall-dependent (S≤9.5 vs S>9.5) — quote the ordered wall against Table 3 footnotes.

Applications of GB/T 14976 06Cr18Ni11Ti Seamless Pipe

From utility rooms to process racks, 06Cr18Ni11Ti shows up wherever Chinese fluid specs want austenitic seamless behaviour. Use list: chemical transfer with dense field welds, heat-exchange fluid loops, and process lines that want 321-class stabilisation on Chinese specs. Spool fabricators should copy 06Cr18Ni11Ti onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Size practice for 06Cr18Ni11Ti remains W-C common; heat treatment 920–1150 °C; watch wall footnote on tensile.

If the only reason for 06Cr18Ni11Ti is “we always used this alias,” reopen the corrosion file before repeating the order. Caution: Rm/Rp0.2 are wall-dependent (S≤9.5 vs S>9.5) — quote the ordered wall against Table 3 footnotes. Commissioning teams benefit when the as-built dossier repeats 06Cr18Ni11Ti beside heat numbers, linking isometric revisions to the same mill certificates. Size practice for 06Cr18Ni11Ti remains W-C common; heat treatment 920–1150 °C; watch wall footnote on tensile.

Weldability of GB/T 14976 06Cr18Ni11Ti

Automatic mill welding is outside GB/T 14976; manual and automatic field welds must still respect 06Cr18Ni11Ti chemistry. Guidance: 321/308L fillers per WPS; avoid excessive heat that re-dissolves Ti carbides. Procedure qualification for 06Cr18Ni11Ti should use the same product form and wall class as production, including the seamless finish that will ship. Size practice for 06Cr18Ni11Ti remains W-C common; heat treatment 920–1150 °C; watch wall footnote on tensile.

Ferrite control on high-Ni austenitics and hydrogen management on martensitic 06Cr18Ni11Ti are procedure items, not afterthoughts. Guidance: 321/308L fillers per WPS; avoid excessive heat that re-dissolves Ti carbides. Consumable lot control and shielding-gas notes for 06Cr18Ni11Ti stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. This paragraph is locked to 06Cr18Ni11Ti duty: Ti-stabilised 18-8 austenitic seamless pipe for fluid systems welded without post-weld solution anneal.

Surface Finishes for GB/T 14976 06Cr18Ni11Ti

Welded or heavily formed 06Cr18Ni11Ti may need bead dressing or ID attention for flow and inspection — call that out rather than assuming mill habit. Size/finish context stays tied to GB/T 14976 seamless stainless fluid-transport pipe. State OD/ID scope for 06Cr18Ni11Ti before booking grind or polish.

Finish Typical supply Order note
Solution annealed and pickled Standard pipe mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

Do not polish over unresolved defects on 06Cr18Ni11Ti; inspection comes before cosmetics. Passivation after pickle or shop welding is good practice in chloride-lean service, but GB/T 14976 acceptance still rests on correct heat treatment. Pack away from carbon-steel contact. Chloride-lean stencil ink and iron-free packing materials are part of the finish package, not optional warehouse habits (06Cr18Ni11Ti).

Inspection and Testing for GB/T 14976 06Cr18Ni11Ti

Third-party witness (SGS/TUV-style) is available when the project mandate requires it. Base acceptance still tracks GB/T 14976 for 06Cr18Ni11Ti. Sampling plans for 06Cr18Ni11Ti keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. This paragraph is locked to 06Cr18Ni11Ti duty: Ti-stabilised 18-8 austenitic seamless pipe for fluid systems welded without post-weld solution anneal.

Dimensional inspection against Table 4/5 tolerances closes the lot. Failures retest per GB/T 2102 — they are not silently shipped. Role: Ti-stabilised 18-8 austenitic seamless pipe for fluid systems welded without post-weld solution anneal. Non-conforming 06Cr18Ni11Ti lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Weld-shop note tied to 06Cr18Ni11Ti: 321/308L fillers per WPS; avoid excessive heat that re-dissolves Ti carbides.

Packaging and Shipping for GB/T 14976 06Cr18Ni11Ti

Seaworthy packing is available for ocean legs — desiccant, VCI, and wrap specs by agreement. Grade mark 06Cr18Ni11Ti stays visible on outer tags. Oxygen Annex B adds oil-free packing language when invoked. Bundle tickets for 06Cr18Ni11Ti repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Weld-shop note tied to 06Cr18Ni11Ti: 321/308L fillers per WPS; avoid excessive heat that re-dissolves Ti carbides.

Container loading plans should keep heavy walls from crushing thin-wall 06Cr18Ni11Ti layers. Desiccant and wrap choices for 06Cr18Ni11Ti follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Keep the 06Cr18Ni11Ti caution visible here: Rm/Rp0.2 are wall-dependent (S≤9.5 vs S>9.5) — quote the ordered wall against Table 3 footnotes.

Shortages or transit damage claims need photos against the packing list before installation starts — tag identity must still read 06Cr18Ni11Ti. Claims handling for 06Cr18Ni11Ti starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Weld-shop note tied to 06Cr18Ni11Ti: 321/308L fillers per WPS; avoid excessive heat that re-dissolves Ti carbides.

Why Choose SHH STEEL

From RFQ clarification through MTC release, SHH STEEL treats 06Cr18Ni11Ti as a governed product grade, not a marketing synonym for 321 / UNS S32168. Role: Ti-stabilised 18-8 austenitic seamless pipe for fluid systems welded without post-weld solution anneal. SHH STEEL can produce and supply 06Cr18Ni11Ti against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade.

Response time stays short because common 06Cr18Ni11Ti enquiry sizes and document packs are already exercised on prior Chinese-spec orders. Use: chemical transfer with dense field welds, heat-exchange fluid loops, and process lines that want 321-class stabilisation on Chinese specs. Ask for a written acknowledgement that names 06Cr18Ni11Ti, W-C or W-H, and the Table 1 heat-treatment condition before melt. SHH STEEL can make 06Cr18Ni11Ti to that written scope.

Supply Capability

Capability framing for 06Cr18Ni11Ti: Chinese-spec seamless fluid pipe, W-C/W-H manufacture, documented heats. Caution remains: Rm/Rp0.2 are wall-dependent (S≤9.5 vs S>9.5) — quote the ordered wall against Table 3 footnotes. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for 06Cr18Ni11Ti when the mill schedule allows. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for 06Cr18Ni11Ti when the mill schedule allows. This paragraph is locked to 06Cr18Ni11Ti duty: Ti-stabilised 18-8 austenitic seamless pipe for fluid systems welded without post-weld solution anneal.

Item Capability
Standard GB/T 14976-2025 seamless stainless steel pipes for fluid transport
Grade 06Cr18Ni11Ti (S32168)
Product form Seamless pipe only — cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H)
Delivery condition solution annealed
Documents Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered)
Typical size practice OD × wall per GB/T 17395; PA ordinary or PC higher precision; usual length 4000–12000 mm
Wall / ordering Nominal OD×wall, OD×min wall, or ID×wall by agreement

Stock / Available sizes

Stock / Available sizes — treat published ranges as capability envelopes. Actual ex-stock pieces of 06Cr18Ni11Ti change weekly; the reliable path is an OD × wall matrix on the enquiry. Duty: Ti-stabilised 18-8 austenitic seamless pipe for fluid systems welded without post-weld solution anneal. SHH STEEL can supply alternate walls and precision classes for 06Cr18Ni11Ti once the design pressure and corrosion allowance are clear.

Repeat orders for 06Cr18Ni11Ti go faster when prior heat records and accepted WPS numbers are referenced on the new RFQ. Role: Ti-stabilised 18-8 austenitic seamless pipe for fluid systems welded without post-weld solution anneal. SHH STEEL can produce trial lengths of 06Cr18Ni11Ti for procedure qualification before the bulk release when the project calendar needs it.

FAQ

What is GB/T 14976 06Cr18Ni11Ti seamless stainless steel pipe used for?
GB/T 14976 06Cr18Ni11Ti is seamless stainless pipe for fluid transport — chemical transfer with dense field welds, heat-exchange fluid loops, and process lines that want 321-class stabilisation on Chinese specs. Role summary: Ti-stabilised 18-8 austenitic seamless pipe for fluid systems welded without post-weld solution anneal. It is a Chinese product standard grade (S32168), not an automatic ASTM A312 certificate.
Is GB/T 14976 06Cr18Ni11Ti seamless only, or does it cover welded pipe?
Seamless only. Clause 6.2 limits manufacture to cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 06Cr18Ni11Ti when the mill can meet the ordered size and tests. Welded pipe belongs under other standards, not 14976.
What heat treatment applies to 06Cr18Ni11Ti?
06Cr18Ni11Ti is delivered solution annealed under GB/T 14976. Table 1 reference: 920–1150 °C, water or rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Keep the purchase order locked to GB/T 14976 and 06Cr18Ni11Ti so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
How does 06Cr18Ni11Ti compare with sister grades 07Cr19Ni11Ti, 06Cr18Ni11Nb, 022Cr19Ni10?
06Cr18Ni11Ti is filed as austenitic. Typical sisters on the same RFQ are 07Cr19Ni11Ti, 06Cr18Ni11Nb, 022Cr19Ni10. Design caution: Rm/Rp0.2 are wall-dependent (S≤9.5 vs S>9.5) — quote the ordered wall against Table 3 footnotes Pick the sister when the medium or strength floor outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 06Cr18Ni11Ti?
Expect cast analysis (Table 2), room-temperature tensile results (Table 3), dimensions, hydrostatic test (or replacing UT/ET), appearance, and every special annex or IGC test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
Is 321 / UNS S32168 the same as ordering 06Cr18Ni11Ti?
No. 321 / UNS S32168 is a commercial / UNS cross-walk for body text (unified S32168). The purchase order should lock GB/T 14976 and 06Cr18Ni11Ti so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GB/T 14976 06Cr18Ni11Ti?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 06Cr18Ni11Ti within GB/T 17395 practice, with PA or PC precision and measured or min-wall options by agreement. Size context: W-C common; heat treatment 920–1150 °C; watch wall footnote on tensile. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should 06Cr18Ni11Ti be welded on site?
Shop guidance: 321/308L fillers per WPS; avoid excessive heat that re-dissolves Ti carbides. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: Rm/Rp0.2 are wall-dependent (S≤9.5 vs S>9.5) — quote the ordered wall against Table 3 footnotes
When should I choose a higher-Mo or superaustenitic grade instead of 06Cr18Ni11Ti?
Move when chloride pitting, crevice attack, or reducing-acid risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: Rm/Rp0.2 are wall-dependent (S≤9.5 vs S>9.5) — quote the ordered wall against Table 3 footnotes Sister pointers: 07Cr19Ni11Ti, 06Cr18Ni11Nb, 022Cr19Ni10. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GB/T 14976 06Cr18Ni11Ti with ASTM A312?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 14976 06Cr18Ni11Ti does not clear ASTM acceptance by default. State both standards, sizes, and test scopes before melt. Keep the purchase order locked to GB/T 14976 and 06Cr18Ni11Ti so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
What surface finishes are available for 06Cr18Ni11Ti?
Pickled after heat treatment is the usual fluid-transport supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 06Cr18Ni11Ti when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

GB/T 14976 06Cr18Ni11Ti is seamless stainless steel pipe for fluid transport — Ti-stabilised 18-8 austenitic seamless pipe for fluid systems welded without post-weld solution anneal. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 07Cr19Ni11Ti, 06Cr18Ni11Nb, 022Cr19Ni10. Related ASTM pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *