GB/T 14976 015Cr20Ni18Mo6CuN Seamless Stainless Steel Pipe | GB/T 14976 Stainless Steel Pipe - SHH STEEL

GB/T 14976 015Cr20Ni18Mo6CuN Seamless Stainless Steel Pipe

GB/T 14976 015Cr20Ni18Mo6CuN seamless stainless steel pipe (6%Mo superaustenitic / UNS S31252, S31252), austenitic, Table 2 cast analysis, Rm min 675 (S≤5 mm) / 655 (S>5 mm) MPa / Rp0.2 min 310 MPa, solution annealed. SHH STEEL can produce and supply W-C or W-H seamless routes with mill certificates.
Grade
015Cr20Ni18Mo6CuN (S31252 / 6%Mo superaustenitic / UNS S31252 — body alias)
Standard
GB/T 14976-2025
Product form
Seamless stainless steel pipe (W-C / W-H), delivery solution annealed
Size
OD × wall per GB/T 17395; PA/PC precision; usual length 4000–12000 mm; other by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Pipe Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is GB/T 14976 015Cr20Ni18Mo6CuN Seamless Stainless Steel Pipe

Fluid-transport packages written to Chinese product standards look to GB/T 14976-2025 rather than inventing a mill grade from AISI shorthand alone. 015Cr20Ni18Mo6CuN is the Table 2/3 Chinese grade name for this austenitic chemistry (S31252). When 06Cr19Ni13Mo3 is no longer enough chloride defence, GB/T 14976 015Cr20Ni18Mo6CuN is the governed Chinese 6Mo seamless mark — not a warehouse “904L” sticker.

Mill path for 015Cr20Ni18Mo6CuN: manufacture symbol W-C/W-H, Table 1 heat treatment, Table 2 cast chemistry, Table 3 tensile floors, hydrostatic or NDT per 7.3. SHH STEEL can make and supply the grade to that stack. Typical use: seawater injection lean lines, bleach and chlorinated chemical transfer, flue-gas scrubber fluid piping, and aggressive process media that outgrew 317L.

Body text may mention 6%Mo superaustenitic / UNS S31252 (unified S31252) for cross-reference, but the H1 and order line stay on 015Cr20Ni18Mo6CuN. Silent alias swaps are how wrong carbon ceilings and wrong tensile tables enter the MTC. Keep this caution in view: Rm is wall-dependent (675 MPa S≤5 mm / 655 MPa S>5 mm) — quote the ordered wall against Table 3, not a single poster number.

Order the standard the drawing and regulatory file actually require. Inside this 14976 series, compare 015Cr21Ni26Mo5Cu2, 022Cr19Ni13Mo3, 022Cr17Ni12Mo2, 06Cr19Ni13Mo3 before stretching surface finish or wall alone. Duty thread: 6% Mo superaustenitic seamless pipe for severe chloride and reducing-acid fluid service. Document the medium, design temperature, and weld map beside the 015Cr20Ni18Mo6CuN line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Corrosion framing beside 015Cr20Ni18Mo6CuN: high Mo + N + Cu deliver strong pitting and crevice resistance; still confirm medium chemistry rather than inventing PREN warranties.

Inside this GB/T 14976 series, compare GB/T 14976 015Cr21Ni26Mo5Cu2, GB/T 14976 022Cr19Ni13Mo3, GB/T 14976 022Cr17Ni12Mo2, GB/T 14976 06Cr19Ni13Mo3. Hub: GB/T 14976.

Chemical Composition of GB/T 14976 015Cr20Ni18Mo6CuN

Table 2 sets the melt limits for 015Cr20Ni18Mo6CuN. Highlight band: C ≤0.020, Si ≤0.80, Mn ≤1.00, P ≤0.030, S ≤0.010, Ni 17.50–18.50, Cr 19.50–20.50, Mo 6.00–6.50. Product analysis, when ordered, applies GB/T 222 stainless product tolerances on top of Table 2. Alias note: 6%Mo superaustenitic / UNS S31252. Every ladle analysis for 015Cr20Ni18Mo6CuN is checked against those windows before the heat is released to piercing or drawing, and the same numbers reappear on the inspection document. Keep the 015Cr20Ni18Mo6CuN caution visible here: Rm is wall-dependent (675 MPa S≤5 mm / 655 MPa S>5 mm) — quote the ordered wall against Table 3, not a single poster number.

The composition table below is the cast window SHH STEEL quotes against for 015Cr20Ni18Mo6CuN. Edition framing is GB/T 14976-2025. Use thread: seawater injection lean lines, bleach and chlorinated chemical transfer, flue-gas scrubber fluid piping, and aggressive process media that outgrew 317L. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 2, SHH STEEL will confirm melt feasibility for 015Cr20Ni18Mo6CuN before the order is acknowledged. Corrosion framing beside 015Cr20Ni18Mo6CuN: high Mo + N + Cu deliver strong pitting and crevice resistance; still confirm medium chemistry rather than inventing PREN warranties.

Grade C Si Mn P S Ni Cr Mo Cu N
015Cr20Ni18Mo6CuN ≤0.020 ≤0.80 ≤1.00 ≤0.030 ≤0.010 17.50–18.50 19.50–20.50 6.00–6.50 0.50–1.00 0.18–0.22

Mechanical Properties of GB/T 14976 015Cr20Ni18Mo6CuN

Table 3 mechanical acceptance for 015Cr20Ni18Mo6CuN: Rm min 675 (S≤5 mm) / 655 (S>5 mm) MPa, Rp0.2 min 310 MPa, elongation longitudinal min 35% / transverse min 30%. Note: Rm depends on wall: 675 MPa when S≤5 mm; 655 MPa when S>5 mm. Delivery framing: solution annealed. Sampling follows chapter 8/10 rules for the batch of 015Cr20Ni18Mo6CuN.

Grade Rm min (MPa) Rp0.2 min (MPa) A long. min (%) A trans. min (%)
015Cr20Ni18Mo6CuN 675 (S≤5 mm) / 655 (S>5 mm) 310 35 30

Ambient values from GB/T 14976-2025 Table 3 for 015Cr20Ni18Mo6CuN. Heat treatment (Table 1): ≥1150 °C, water or rapid cool. Rm depends on wall: 675 MPa when S≤5 mm; 655 MPa when S>5 mm. Density 8.1 kg/dm³. Delivery: solution annealed.

Seamless Pipe Manufacture of GB/T 14976 015Cr20Ni18Mo6CuN

Seamless is not optional wording for 015Cr20Ni18Mo6CuN: clause 6.2 limits manufacture to W-C or W-H seamless routes. Pick W-C when OD precision and surface finish dominate; pick W-H when wall and tonnage favour hot working. SHH STEEL will not quietly substitute a welded route under a 14976 line item. Seamless W-C and W-H options remain available for 015Cr20Ni18Mo6CuN; the acknowledgement repeats the manufacture symbol so production cannot silently change route after the PO is firm. Keep the 015Cr20Ni18Mo6CuN caution visible here: Rm is wall-dependent (675 MPa S≤5 mm / 655 MPa S>5 mm) — quote the ordered wall against Table 3, not a single poster number.

After forming, 015Cr20Ni18Mo6CuN receives Table 1 treatment — ≥1150 °C, water or rapid cool. Austenitic heats take solution annealing with water or other rapid cool per Table 1; hot-rolled austenitic pipe may count in-line rapid cool inside the Table 1 temperature band as meeting heat treatment (6.3.2) unless the purchaser forbids it. Use thread: seawater injection lean lines, bleach and chlorinated chemical transfer, flue-gas scrubber fluid piping, and aggressive process media that outgrew 317L.

Marking carries the grade 015Cr20Ni18Mo6CuN, manufacture cues, manufacturer ID, and GB/T 2102 items. Size hint: cold-drawn W-C preferred for corrosion-critical surfaces; wall callouts must match the dual Rm rows. Weld thread for fabricator joints: over-alloyed Ni-Cr-Mo fillers; strict heat-input and interpass control; solution anneal when the corrosion file demands it. Hydrostatic pressure or NDT class for 015Cr20Ni18Mo6CuN is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Application context for 015Cr20Ni18Mo6CuN stays seawater injection lean lines, bleach and chlorinated chemical transfer, flue-gas scrubber fluid piping, and aggressive process media that outgrew 317L.

Dimensions and Tolerances for GB/T 14976 015Cr20Ni18Mo6CuN

Dimensional order lines for 015Cr20Ni18Mo6CuN should state OD × wall (or ID × wall), length type, end finish, and PA or PC tolerance class. Use: seawater injection lean lines, bleach and chlorinated chemical transfer, flue-gas scrubber fluid piping, and aggressive process media that outgrew 317L. Tolerance class (PA/PC) follows the precision ordered for 015Cr20Ni18Mo6CuN, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Weld-shop note tied to 015Cr20Ni18Mo6CuN: over-alloyed Ni-Cr-Mo fillers; strict heat-input and interpass control; solution anneal when the corrosion file demands it.

OD and wall tolerances differ for hot-finished W-H versus cold-finished W-C and for PA versus PC — quote the manufacture symbol with the size. Caution: Rm is wall-dependent (675 MPa S≤5 mm / 655 MPa S>5 mm) — quote the ordered wall against Table 3, not a single poster number. Fixed lengths and multiple cut lengths for 015Cr20Ni18Mo6CuN are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Corrosion framing beside 015Cr20Ni18Mo6CuN: high Mo + N + Cu deliver strong pitting and crevice resistance; still confirm medium chemistry rather than inventing PREN warranties.

Equivalent Grades for GB/T 14976 015Cr20Ni18Mo6CuN

Equivalence language around 015Cr20Ni18Mo6CuN is often looser than a pipe purchase order can afford. GB/T 14976 015Cr20Ni18Mo6CuN governs this article; 6%Mo superaustenitic / UNS S31252 is body-only framing for catalogues and dual-cert talk, not a substitute mark on the MTC. Keep the GB/T 14976 symbol unless a written dual-cert plan lists both standards with separate test scopes.

System Designation Notes
GB/T 14976 015Cr20Ni18Mo6CuN Governing pipe grade for this page
Commercial / UNS (body only) 6%Mo superaustenitic / UNS S31252 Useful in dual-cert talk; not a substitute on the PO/MTC
ASTM A312 related 6Mo / superaustenitic family talk (no identical TP asserted) Related chemistry — different product standard; not interchangeable by default
EN / other No one-to-one asserted Starting point for comparison only against local product specs

Order discipline for 015Cr20Ni18Mo6CuN still points at GB/T 14976, not the brochure alias. Neighbours GB/T 14976 015Cr21Ni26Mo5Cu2, GB/T 14976 022Cr19Ni13Mo3, GB/T 14976 022Cr17Ni12Mo2, GB/T 14976 06Cr19Ni13Mo3 each carry their own mechanical table. Category hub: GB/T 14976. Dual marking is a purchase-order option that still requires every limit that matters for 015Cr20Ni18Mo6CuN to be verified on the heat.

On 015Cr20Ni18Mo6CuN packages that also list flats, keep tubular RFQs under Stainless Steel Pipes and Tubes, flat RFQs under Stainless Steel Sheets and Plates, and pin the plate twin with GB/T 4237 015Cr20Ni18Mo6CuN. Flat Chinese grades in-family are indexed at GB/T 4237. Quote 015Cr20Ni18Mo6CuN pipe and plate under separate line items.

Heat Treatment and Delivery Condition for GB/T 14976 015Cr20Ni18Mo6CuN

Mill heat treatment for 015Cr20Ni18Mo6CuN: ≥1150 °C, water or rapid cool. Bright annealing or overall machining may omit pickling when the surface is scale-free. Delivery label: solution annealed. Recorded furnace charts for 015Cr20Ni18Mo6CuN should support the Table 1 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Application context for 015Cr20Ni18Mo6CuN stays seawater injection lean lines, bleach and chlorinated chemical transfer, flue-gas scrubber fluid piping, and aggressive process media that outgrew 317L.

Certificate wording for 015Cr20Ni18Mo6CuN should show the heat-treatment condition actually performed, not a generic “annealed” stamp that hides temperature. Use: seawater injection lean lines, bleach and chlorinated chemical transfer, flue-gas scrubber fluid piping, and aggressive process media that outgrew 317L. Field heat treatment of 015Cr20Ni18Mo6CuN after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Corrosion framing beside 015Cr20Ni18Mo6CuN: high Mo + N + Cu deliver strong pitting and crevice resistance; still confirm medium chemistry rather than inventing PREN warranties.

Corrosion Resistance of GB/T 14976 015Cr20Ni18Mo6CuN

high Mo + N + Cu deliver strong pitting and crevice resistance; still confirm medium chemistry rather than inventing PREN warranties Special Annex A cryogenic or Annex B oxygen extras are not a blanket corrosion warranty. Family filing: austenitic. Clause 7.5 requires intergranular corrosion testing (GB/T 4334 method E) for austenitic 015Cr20Ni18Mo6CuN unless the mark is one of the four carbon-floor exemptions.

Do not market invented PREN digits. Bring medium chemistry and SHH STEEL will map 015Cr20Ni18Mo6CuN honestly against 015Cr21Ni26Mo5Cu2, 022Cr19Ni13Mo3, 022Cr17Ni12Mo2, 06Cr19Ni13Mo3. Role: 6% Mo superaustenitic seamless pipe for severe chloride and reducing-acid fluid service. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 015Cr20Ni18Mo6CuN rather than relying on wall thickness alone. Keep the 015Cr20Ni18Mo6CuN caution visible here: Rm is wall-dependent (675 MPa S≤5 mm / 655 MPa S>5 mm) — quote the ordered wall against Table 3, not a single poster number.

Applications of GB/T 14976 015Cr20Ni18Mo6CuN Seamless Pipe

Typical BOM language pairs GB/T 14976 015Cr20Ni18Mo6CuN with OD × wall, W-C or W-H, PA/PC, and heat-treatment condition. Primary sketch: seawater injection lean lines, bleach and chlorinated chemical transfer, flue-gas scrubber fluid piping, and aggressive process media that outgrew 317L. Spool fabricators should copy 015Cr20Ni18Mo6CuN onto cut lists and WPS bases so warehouse substitutions cannot quietly introduce a different carbon or molybdenum window. Keep the 015Cr20Ni18Mo6CuN caution visible here: Rm is wall-dependent (675 MPa S≤5 mm / 655 MPa S>5 mm) — quote the ordered wall against Table 3, not a single poster number.

Spell 015Cr20Ni18Mo6CuN on isometrics, spool sheets and valve specs alike. Sister options when the medium hardens: 015Cr21Ni26Mo5Cu2, 022Cr19Ni13Mo3, 022Cr17Ni12Mo2, 06Cr19Ni13Mo3. Commissioning teams benefit when the as-built dossier repeats 015Cr20Ni18Mo6CuN beside heat numbers, linking isometric revisions to the same mill certificates. This paragraph is locked to 015Cr20Ni18Mo6CuN duty: 6% Mo superaustenitic seamless pipe for severe chloride and reducing-acid fluid service.

Weldability of GB/T 14976 015Cr20Ni18Mo6CuN

Weldability of 015Cr20Ni18Mo6CuN follows austenitic practice. Filler/shop note: over-alloyed Ni-Cr-Mo fillers; strict heat-input and interpass control; solution anneal when the corrosion file demands it. Caution: Rm is wall-dependent (675 MPa S≤5 mm / 655 MPa S>5 mm) — quote the ordered wall against Table 3, not a single poster number. Procedure qualification for 015Cr20Ni18Mo6CuN should use the same product form and wall class as production, including the seamless finish that will ship. Corrosion framing beside 015Cr20Ni18Mo6CuN: high Mo + N + Cu deliver strong pitting and crevice resistance; still confirm medium chemistry rather than inventing PREN warranties.

For corrosive as-welded duty on 015Cr20Ni18Mo6CuN, confirm low-carbon, stabilisation, or anneal practice as applicable. Shop note: over-alloyed Ni-Cr-Mo fillers; strict heat-input and interpass control; solution anneal when the corrosion file demands it. Consumable lot control and shielding-gas notes for 015Cr20Ni18Mo6CuN stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. Size practice for 015Cr20Ni18Mo6CuN remains cold-drawn W-C preferred for corrosion-critical surfaces; wall callouts must match the dual Rm rows.

Surface Finishes for GB/T 14976 015Cr20Ni18Mo6CuN

Surface supply for 015Cr20Ni18Mo6CuN should be stated on the purchase order rather than left to mill default. Embedded free iron, residual scale, and chloride-bearing residues are where corrosion starts on stainless pipe, so finish is part of performance, not only appearance. Application framing: seawater injection lean lines, bleach and chlorinated chemical transfer, flue-gas scrubber fluid piping, and aggressive process media that outgrew 317L. Ambiguous “bright pipe” language is clarified before finishing slots are booked.

Finish Typical supply Order note
Solution annealed and pickled Standard pipe mill finish after solution anneal Matte, scale-free after pickling
Bright annealed When scale-free OD/ID appearance is ordered State OD, ID, or both
Ground / polished By agreement for roughness callouts Name Ra/grit and which surface; no invented default grit
Passivated When end-user spec requires (e.g. A967 analogue) Not a substitute for correct heat treatment

OD stencil ink on 015Cr20Ni18Mo6CuN should be chloride-lean and removable where coatings follow. Passivation will not repair a cast that missed chemistry windows: Rm is wall-dependent (675 MPa S≤5 mm / 655 MPa S>5 mm) — quote the ordered wall against Table 3, not a single poster number. Close bundles only after free-iron and burn marks are cleared.

Inspection and Testing for GB/T 14976 015Cr20Ni18Mo6CuN

SHH STEEL reports the tests actually performed for 015Cr20Ni18Mo6CuN — no surrogate NDT lines. Hydrostatic vs eddy-current/ultrasonic choice belongs on the PO when replacement is allowed. Caution: Rm is wall-dependent (675 MPa S≤5 mm / 655 MPa S>5 mm) — quote the ordered wall against Table 3, not a single poster number.

NDT acceptance defaults to GB/T 5777 U3 or GB/T 7735 E4H/E4 when UT/ET replace hydro; Annex A/B may tighten to U2.5. Size context: cold-drawn W-C preferred for corrosion-critical surfaces; wall callouts must match the dual Rm rows. Non-conforming 015Cr20Ni18Mo6CuN lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. Corrosion framing beside 015Cr20Ni18Mo6CuN: high Mo + N + Cu deliver strong pitting and crevice resistance; still confirm medium chemistry rather than inventing PREN warranties.

Packaging and Shipping for GB/T 14976 015Cr20Ni18Mo6CuN

Export packing for GB/T 14976 015Cr20Ni18Mo6CuN is built around rust prevention and transit abrasion control. Bundle tickets repeat the grade symbol and heat number. Duty: 6% Mo superaustenitic seamless pipe for severe chloride and reducing-acid fluid service. Bundle tickets for 015Cr20Ni18Mo6CuN repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Weld-shop note tied to 015Cr20Ni18Mo6CuN: over-alloyed Ni-Cr-Mo fillers; strict heat-input and interpass control; solution anneal when the corrosion file demands it.

Marking paint and ink stickers stay chloride-lean. Heat numbers on tags match the MTC for 015Cr20Ni18Mo6CuN. Desiccant and wrap choices for 015Cr20Ni18Mo6CuN follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Application context for 015Cr20Ni18Mo6CuN stays seawater injection lean lines, bleach and chlorinated chemical transfer, flue-gas scrubber fluid piping, and aggressive process media that outgrew 317L.

Photographic packing records are available on request for project QA files on 015Cr20Ni18Mo6CuN. Claims handling for 015Cr20Ni18Mo6CuN starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Weld-shop note tied to 015Cr20Ni18Mo6CuN: over-alloyed Ni-Cr-Mo fillers; strict heat-input and interpass control; solution anneal when the corrosion file demands it.

Why Choose SHH STEEL

SHH STEEL can produce and supply GB/T 14976 015Cr20Ni18Mo6CuN. Buyers choose SHH STEEL for 015Cr20Ni18Mo6CuN because the paperwork matches the stencil: Table 2 chemistry, Table 3 tensile, Table 1 heat treatment, and honest seamless marking. Application fit: seawater injection lean lines, bleach and chlorinated chemical transfer, flue-gas scrubber fluid piping, and aggressive process media that outgrew 317L.

SHH STEEL will not invent PREN posters or warehouse tonnages. Bring OD × wall, medium notes, and test scope — we will quote 015Cr20Ni18Mo6CuN cleanly. Ask for a written acknowledgement that names 015Cr20Ni18Mo6CuN, W-C or W-H, and the Table 1 heat-treatment condition before melt. SHH STEEL can make 015Cr20Ni18Mo6CuN to that written scope.

Supply Capability

Supply capability for 015Cr20Ni18Mo6CuN covers seamless manufacture symbols, Table 1 heat treatment, and Table 3 mechanical acceptance. SHH STEEL can make the sizes on your list when the mill slot fits. Role: 6% Mo superaustenitic seamless pipe for severe chloride and reducing-acid fluid service. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for 015Cr20Ni18Mo6CuN when the mill schedule allows.

Item Capability
Standard GB/T 14976-2025 seamless stainless steel pipes for fluid transport
Grade 015Cr20Ni18Mo6CuN (S31252)
Product form Seamless pipe only — cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H)
Delivery condition solution annealed
Documents Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered)
Typical size practice OD × wall per GB/T 17395; PA ordinary or PC higher precision; usual length 4000–12000 mm
Wall / ordering Nominal OD×wall, OD×min wall, or ID×wall by agreement

Stock / Available sizes

Stock / Available sizes for 015Cr20Ni18Mo6CuN: common OD×wall combinations as the project uses. Seamless W-C versus W-H availability varies by diameter — confirm route with the RFQ. Hint: cold-drawn W-C preferred for corrosion-critical surfaces; wall callouts must match the dual Rm rows. SHH STEEL can supply alternate walls and precision classes for 015Cr20Ni18Mo6CuN once the design pressure and corrosion allowance are clear.

Mill certificates, packing photos, and third-party witness can be bundled into the 015Cr20Ni18Mo6CuN supply scope when the PO says so. Use: seawater injection lean lines, bleach and chlorinated chemical transfer, flue-gas scrubber fluid piping, and aggressive process media that outgrew 317L. SHH STEEL can produce trial lengths of 015Cr20Ni18Mo6CuN for procedure qualification before the bulk release when the project calendar needs it.

FAQ

What is GB/T 14976 015Cr20Ni18Mo6CuN seamless stainless steel pipe used for?
GB/T 14976 015Cr20Ni18Mo6CuN is seamless stainless pipe for fluid transport — seawater injection lean lines, bleach and chlorinated chemical transfer, flue-gas scrubber fluid piping, and aggressive process media that outgrew 317L. Role summary: 6% Mo superaustenitic seamless pipe for severe chloride and reducing-acid fluid service. It is a Chinese product standard grade (S31252), not an automatic ASTM A312 certificate.
Is GB/T 14976 015Cr20Ni18Mo6CuN seamless only, or does it cover welded pipe?
Seamless only. Clause 6.2 limits manufacture to cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 015Cr20Ni18Mo6CuN when the mill can meet the ordered size and tests. Welded pipe belongs under other standards, not 14976.
What heat treatment applies to 015Cr20Ni18Mo6CuN?
015Cr20Ni18Mo6CuN is delivered solution annealed under GB/T 14976. Table 1 reference: ≥1150 °C, water or rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Keep the purchase order locked to GB/T 14976 and 015Cr20Ni18Mo6CuN so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
How does 015Cr20Ni18Mo6CuN compare with sister grades 015Cr21Ni26Mo5Cu2, 022Cr19Ni13Mo3, 022Cr17Ni12Mo2?
015Cr20Ni18Mo6CuN is filed as austenitic. Typical sisters on the same RFQ are 015Cr21Ni26Mo5Cu2, 022Cr19Ni13Mo3, 022Cr17Ni12Mo2. Design caution: Rm is wall-dependent (675 MPa S≤5 mm / 655 MPa S>5 mm) — quote the ordered wall against Table 3, not a single poster number Pick the sister when the medium or strength floor outgrows this grade rather than stretching wall alone.
What tests appear on the mill certificate for 015Cr20Ni18Mo6CuN?
Expect cast analysis (Table 2), room-temperature tensile results (Table 3), dimensions, hydrostatic test (or replacing UT/ET), appearance, and every special annex or IGC test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
Is 6%Mo superaustenitic / UNS S31252 the same as ordering 015Cr20Ni18Mo6CuN?
No. 6%Mo superaustenitic / UNS S31252 is a commercial / UNS cross-walk for body text (unified S31252). The purchase order should lock GB/T 14976 and 015Cr20Ni18Mo6CuN so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
What size range can SHH STEEL quote for GB/T 14976 015Cr20Ni18Mo6CuN?
SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 015Cr20Ni18Mo6CuN within GB/T 17395 practice, with PA or PC precision and measured or min-wall options by agreement. Size context: cold-drawn W-C preferred for corrosion-critical surfaces; wall callouts must match the dual Rm rows. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
How should 015Cr20Ni18Mo6CuN be welded on site?
Shop guidance: over-alloyed Ni-Cr-Mo fillers; strict heat-input and interpass control; solution anneal when the corrosion file demands it. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: Rm is wall-dependent (675 MPa S≤5 mm / 655 MPa S>5 mm) — quote the ordered wall against Table 3, not a single poster number
When should I choose a higher-Mo or superaustenitic grade instead of 015Cr20Ni18Mo6CuN?
Move when chloride pitting, crevice attack, or reducing-acid risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: Rm is wall-dependent (675 MPa S≤5 mm / 655 MPa S>5 mm) — quote the ordered wall against Table 3, not a single poster number Sister pointers: 015Cr21Ni26Mo5Cu2, 022Cr19Ni13Mo3, 022Cr17Ni12Mo2. SHH STEEL will not invent PREN marketing digits — bring the medium data.
Can SHH STEEL dual-certify GB/T 14976 015Cr20Ni18Mo6CuN with ASTM A312?
Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 14976 015Cr20Ni18Mo6CuN does not clear ASTM acceptance by default. State both standards, sizes, and test scopes before melt. Keep the purchase order locked to GB/T 14976 and 015Cr20Ni18Mo6CuN so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
What surface finishes are available for 015Cr20Ni18Mo6CuN?
Pickled after heat treatment is the usual fluid-transport supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 015Cr20Ni18Mo6CuN when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.

Conclusion

GB/T 14976 015Cr20Ni18Mo6CuN is seamless stainless steel pipe for fluid transport — 6% Mo superaustenitic seamless pipe for severe chloride and reducing-acid fluid service. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 015Cr21Ni26Mo5Cu2, 022Cr19Ni13Mo3, 022Cr17Ni12Mo2. Related ASTM pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X