GB/T 14976 06Cr17Ni12Mo2 Seamless Stainless Steel Pipe
What is GB/T 14976 06Cr17Ni12Mo2 Seamless Stainless Steel Pipe
When the approved vendor list and isometric notes say GB/T 14976, the grade mark has to be the Chinese designation. 06Cr17Ni12Mo2 is the full product grade for this austenitic seamless pipe. GB/T 14976 06Cr17Ni12Mo2 is the everyday Chinese 316 seamless fluid mark — still not a free pass to skip low-carbon thinking on welded corrosive joints.
SHH STEEL can supply 06Cr17Ni12Mo2 seamless pipe in cold-finished or hot-finished routes, with plain or bevelled ends, random or cut lengths, and GB/T 2102 / EN 10204 3.1 style inspection documents when specified. Role on the line: standard Mo austenitic seamless pipe for general chloride-resistant fluid transport on Chinese projects. Size and test clarity on the RFQ lets SHH STEEL lock the correct W-C or W-H symbol for 06Cr17Ni12Mo2 before production starts. Corrosion framing beside 06Cr17Ni12Mo2: Mo-bearing passive film handles many chloride process media; crevice and hot chloride SCC still need design review.
Equivalence talk to 316 / UNS S31608 belongs in engineering notes, not as a substitute for the Chinese grade. Lock GB/T 14976 06Cr17Ni12Mo2, OD × wall, manufacture route, and any Annex A/B extras before melt. Watch-out: 0.08% carbon ceiling — prefer 022Cr17Ni12Mo2 or Ti-stabilised 06Cr17Ni12Mo2Ti when corrosive field welds cannot be annealed.
Related ASTM pipe pages share chemistry families but not Chinese acceptance text — confirm before dual-cert claims. Sisters on this hub: 022Cr17Ni12Mo2, 06Cr19Ni13Mo3, 06Cr17Ni12Mo2Ti, 07Cr17Ni12Mo2. Use thread: chemical transfer, marine-adjacent utilities, heat-exchange fluid loops, and process lines that still say “316 seamless”. Document the medium, design temperature, and weld map beside the 06Cr17Ni12Mo2 line item so sister-grade swaps are engineering decisions rather than purchasing shortcuts. Application context for 06Cr17Ni12Mo2 stays chemical transfer, marine-adjacent utilities, heat-exchange fluid loops, and process lines that still say “316 seamless”.
Inside this GB/T 14976 series, compare GB/T 14976 022Cr17Ni12Mo2, GB/T 14976 06Cr19Ni13Mo3, GB/T 14976 06Cr17Ni12Mo2Ti, GB/T 14976 07Cr17Ni12Mo2. Hub: GB/T 14976. ASTM/ASME related product pages (not interchangeable by default): ASTM A312 TP316.
Beside this 06Cr17Ni12Mo2 page, tubular scope points to Stainless Steel Pipes and Tubes; flat scope points to Stainless Steel Sheets and Plates; chemistry-matched plate is GB/T 3280 06Cr17Ni12Mo2. Do not stretch a 06Cr17Ni12Mo2 pipe certificate onto plate.
Chemical Composition of GB/T 14976 06Cr17Ni12Mo2
Chemistry control on 06Cr17Ni12Mo2 starts at the ladle. Expect C ≤0.08, Si ≤1.00, Mn ≤2.00, P ≤0.035, S ≤0.030, Ni 10.00–14.00, Cr 16.00–18.00, Mo 2.00–3.00 within Table 2, reported on the inspection document against the heat. Body alias 316 / UNS S31608 does not widen those windows. Every ladle analysis for 06Cr17Ni12Mo2 is checked against those windows before the heat is released to piercing or drawing, and the same numbers reappear on the inspection document. Corrosion framing beside 06Cr17Ni12Mo2: Mo-bearing passive film handles many chloride process media; crevice and hot chloride SCC still need design review.
Read the table with the family in mind — austenitic — and with caution 0.08% carbon ceiling — prefer 022Cr17Ni12Mo2 or Ti-stabilised 06Cr17Ni12Mo2Ti when corrosive field welds cannot be annealed. Numbers without the matching Table 1 heat-treatment row are incomplete purchase data. If a purchaser specification tightens phosphorus, sulphur, or residual elements beyond Table 2, SHH STEEL will confirm melt feasibility for 06Cr17Ni12Mo2 before the order is acknowledged. Application context for 06Cr17Ni12Mo2 stays chemical transfer, marine-adjacent utilities, heat-exchange fluid loops, and process lines that still say “316 seamless”.
| Grade | C | Si | Mn | P | S | Ni | Cr | Mo |
|---|---|---|---|---|---|---|---|---|
| 06Cr17Ni12Mo2 | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.035 | ≤0.030 | 10.00–14.00 | 16.00–18.00 | 2.00–3.00 |
Mechanical Properties of GB/T 14976 06Cr17Ni12Mo2
Proof stress and tensile minima for 06Cr17Ni12Mo2 sit at Rm min 520 MPa, Rp0.2 min 205 MPa, elongation longitudinal min 35% / transverse min 30%. Flattening or bend testing backs ductility when ordered. Watch-out: 0.08% carbon ceiling — prefer 022Cr17Ni12Mo2 or Ti-stabilised 06Cr17Ni12Mo2Ti when corrosive field welds cannot be annealed. Tensile sampling follows the batch rules for the ordered test unit of 06Cr17Ni12Mo2, and retests follow GB/T 2102 when a result sits under the Table 3 floor. Application context for 06Cr17Ni12Mo2 stays chemical transfer, marine-adjacent utilities, heat-exchange fluid loops, and process lines that still say “316 seamless”.
| Grade | Rm min (MPa) | Rp0.2 min (MPa) | A long. min (%) | A trans. min (%) |
|---|---|---|---|---|
| 06Cr17Ni12Mo2 | 520 | 205 | 35 | 30 |
Ambient values from GB/T 14976-2025 Table 3 for 06Cr17Ni12Mo2. Heat treatment (Table 1): 1010–1150 °C, water or rapid cool. Density 7.98 kg/dm³. Delivery: solution annealed.
Seamless Pipe Manufacture of GB/T 14976 06Cr17Ni12Mo2
SHH STEEL can produce 06Cr17Ni12Mo2 as cold-finished seamless (W-C) or hot-finished seamless (W-H), then apply Table 1 heat treatment and pickle (or bright anneal) as ordered. Bevel ends are available by agreement; square-cut plain ends are the default when the PO is silent. Seamless W-C and W-H options remain available for 06Cr17Ni12Mo2; the acknowledgement repeats the manufacture symbol so production cannot silently change route after the PO is firm. Application context for 06Cr17Ni12Mo2 stays chemical transfer, marine-adjacent utilities, heat-exchange fluid loops, and process lines that still say “316 seamless”.
Process control for 06Cr17Ni12Mo2 ends with verified heat treatment (1010–1150 °C, water or rapid cool) and surface conditioning. Austenitic heats take solution annealing with water or other rapid cool per Table 1; hot-rolled austenitic pipe may count in-line rapid cool inside the Table 1 temperature band as meeting heat treatment (6.3.2) unless the purchaser forbids it.
Bevel geometry is by agreement when ordered without a drawing. Size practice: broad OD×wall under GB/T 17395; W-C and W-H both common — name the route on the PO. Density for theoretical weight of 06Cr17Ni12Mo2: 7.98 kg/dm³ per Table 1. Hydrostatic pressure or NDT class for 06Cr17Ni12Mo2 is frozen with the size list so quality planners can book the correct benches before the pipe is cut to length. Application context for 06Cr17Ni12Mo2 stays chemical transfer, marine-adjacent utilities, heat-exchange fluid loops, and process lines that still say “316 seamless”.
Dimensions and Tolerances for GB/T 14976 06Cr17Ni12Mo2
Usual length for GB/T 14976 pipe is 4000–12000 mm; fixed and multiple lengths sit inside that band with stated plus tolerances. For 06Cr17Ni12Mo2, confirm whether your project uses OD or ID ordering. Context: broad OD×wall under GB/T 17395; W-C and W-H both common — name the route on the PO. Tolerance class (PA/PC) follows the precision ordered for 06Cr17Ni12Mo2, and out-of-table diameters are accepted only with a written dimensional agreement on the same acknowledgement. Weld-shop note tied to 06Cr17Ni12Mo2: 316/316L fillers; heat-input control on non-L heats in corrosive service.
Full-length bend ≤0.15% of length; per-metre bend ≤1.5 mm (S≤15 mm) or ≤2.0 mm (S>15 mm). 06Cr17Ni12Mo2 must meet those geometry floors unless a written waiver exists. Fixed lengths and multiple cut lengths for 06Cr17Ni12Mo2 are protected at the ends so bevel geometry and ID cleanliness survive inland and ocean transit. Application context for 06Cr17Ni12Mo2 stays chemical transfer, marine-adjacent utilities, heat-exchange fluid loops, and process lines that still say “316 seamless”.
Equivalent Grades for GB/T 14976 06Cr17Ni12Mo2
06Cr17Ni12Mo2 is the GB/T 14976 designation for this seamless stainless fluid-transport pipe. Alias 316 / UNS S31608 appears only as a cross-walk. When a dual-cert path is required, list both GB/T 14976 06Cr17Ni12Mo2 and the foreign mark with separate scopes instead of assuming one chemistry line clears both files.
| System | Designation | Notes |
|---|---|---|
| GB/T 14976 | 06Cr17Ni12Mo2 | Governing pipe grade for this page |
| Commercial / UNS (body only) | 316 / UNS S31608 | Useful in dual-cert talk; not a substitute on the PO/MTC |
| ASTM A312 related | 316 chemistry family | Related chemistry — different product standard; not interchangeable by default |
| EN / other | No one-to-one asserted | Starting point for comparison only against local product specs |
Order discipline for 06Cr17Ni12Mo2 still points at GB/T 14976, not the brochure alias. Neighbours GB/T 14976 022Cr17Ni12Mo2, GB/T 14976 06Cr19Ni13Mo3, GB/T 14976 06Cr17Ni12Mo2Ti, GB/T 14976 07Cr17Ni12Mo2 each carry their own mechanical table. Category hub: GB/T 14976. Wall basis, tensile floors, and NDT clauses rarely map one-for-one even when the cast analysis looks familiar to a commercial alias (06Cr17Ni12Mo2).
Heat Treatment and Delivery Condition for GB/T 14976 06Cr17Ni12Mo2
Other heat-treatment schedules are allowed only by written agreement (6.3.4) — silence means Table 1 defaults. For 06Cr17Ni12Mo2: 1010–1150 °C, water or rapid cool. Recorded furnace charts for 06Cr17Ni12Mo2 should support the Table 1 temperature claim on the certificate, including quench or cool method where the family requires rapid cooling. Keep the 06Cr17Ni12Mo2 caution visible here: 0.08% carbon ceiling — prefer 022Cr17Ni12Mo2 or Ti-stabilised 06Cr17Ni12Mo2Ti when corrosive field welds cannot be annealed.
After local hot work in the field, restore solution annealed practice when the corrosion file demands it. Caution: 0.08% carbon ceiling — prefer 022Cr17Ni12Mo2 or Ti-stabilised 06Cr17Ni12Mo2Ti when corrosive field welds cannot be annealed. Field heat treatment of 06Cr17Ni12Mo2 after hot bending must chase the same family practice, or the corrosion file should formally accept the as-bent condition. Size practice for 06Cr17Ni12Mo2 remains broad OD×wall under GB/T 17395; W-C and W-H both common — name the route on the PO.
Corrosion Resistance of GB/T 14976 06Cr17Ni12Mo2
Pick tests that match how 06Cr17Ni12Mo2 is filed — austenitic. Corrosion thread: Mo-bearing passive film handles many chloride process media; crevice and hot chloride SCC still need design review. Caution: 0.08% carbon ceiling — prefer 022Cr17Ni12Mo2 or Ti-stabilised 06Cr17Ni12Mo2Ti when corrosive field welds cannot be annealed. Coupon orientation, weld condition, and surface finish for 06Cr17Ni12Mo2 belong in the corrosion test order so annex results can be compared to the installed spool honestly. Application context for 06Cr17Ni12Mo2 stays chemical transfer, marine-adjacent utilities, heat-exchange fluid loops, and process lines that still say “316 seamless”.
Oxygen-line Annex B and cryogenic Annex A add impact, UT, and cleanliness rules — they do not change the alloy selection logic. Use thread: chemical transfer, marine-adjacent utilities, heat-exchange fluid loops, and process lines that still say “316 seamless”. If operating chlorides, temperature, or crevice geometry change after award, reopen the alloy choice for 06Cr17Ni12Mo2 rather than relying on wall thickness alone. This paragraph is locked to 06Cr17Ni12Mo2 duty: standard Mo austenitic seamless pipe for general chloride-resistant fluid transport on Chinese projects.
Applications of GB/T 14976 06Cr17Ni12Mo2 Seamless Pipe
Project types that repeatedly call 06Cr17Ni12Mo2: chemical transfer, marine-adjacent utilities, heat-exchange fluid loops, and process lines that still say “316 seamless”. Duty: standard Mo austenitic seamless pipe for general chloride-resistant fluid transport on Chinese projects. Caution still applies: 0.08% carbon ceiling — prefer 022Cr17Ni12Mo2 or Ti-stabilised 06Cr17Ni12Mo2Ti when corrosive field welds cannot be annealed.
Cryogenic, oxygen, and corrosive process lines all appear in 14976’s scope options — alloy choice still follows the medium. For this mark: standard Mo austenitic seamless pipe for general chloride-resistant fluid transport on Chinese projects. Commissioning teams benefit when the as-built dossier repeats 06Cr17Ni12Mo2 beside heat numbers, linking isometric revisions to the same mill certificates. Application context for 06Cr17Ni12Mo2 stays chemical transfer, marine-adjacent utilities, heat-exchange fluid loops, and process lines that still say “316 seamless”.
Weldability of GB/T 14976 06Cr17Ni12Mo2
Even seamless W-C/W-H pipe of 06Cr17Ni12Mo2 will see field welds. Use: 316/316L fillers; heat-input control on non-L heats in corrosive service. Restore heat treatment when the WPS and corrosion file require it. Procedure qualification for 06Cr17Ni12Mo2 should use the same product form and wall class as production, including the seamless finish that will ship. Keep the 06Cr17Ni12Mo2 caution visible here: 0.08% carbon ceiling — prefer 022Cr17Ni12Mo2 or Ti-stabilised 06Cr17Ni12Mo2Ti when corrosive field welds cannot be annealed.
Dissimilar welds to carbon steel need buttering and dilution control — especially on Mo and high-Ni grades. Role context: standard Mo austenitic seamless pipe for general chloride-resistant fluid transport on Chinese projects. Consumable lot control and shielding-gas notes for 06Cr17Ni12Mo2 stay with the WPS package so site crews cannot improvise fillers that under-alloy the joint. This paragraph is locked to 06Cr17Ni12Mo2 duty: standard Mo austenitic seamless pipe for general chloride-resistant fluid transport on Chinese projects.
Surface Finishes for GB/T 14976 06Cr17Ni12Mo2
Welded or heavily formed 06Cr17Ni12Mo2 may need bead dressing or ID attention for flow and inspection — call that out rather than assuming mill habit. Size/finish context stays tied to GB/T 14976 seamless stainless fluid-transport pipe. State OD/ID scope for 06Cr17Ni12Mo2 before booking grind or polish.
| Finish | Typical supply | Order note |
|---|---|---|
| Solution annealed and pickled | Standard pipe mill finish after solution anneal | Matte, scale-free after pickling |
| Bright annealed | When scale-free OD/ID appearance is ordered | State OD, ID, or both |
| Ground / polished | By agreement for roughness callouts | Name Ra/grit and which surface; no invented default grit |
| Passivated | When end-user spec requires (e.g. A967 analogue) | Not a substitute for correct heat treatment |
SHH STEEL sequences pickle, optional passivation, and any agreed polish for 06Cr17Ni12Mo2 after the heat-treatment evidence is on the certificate. Free-iron control and packing discipline matter as much as Ra numbers for long pipe life in the field. Passivation and polish are sequenced only after heat-treatment evidence is already on the certificate for 06Cr17Ni12Mo2.
Inspection and Testing for GB/T 14976 06Cr17Ni12Mo2
Batching rules limit pieces per heat/size/heat-treat lot. For 06Cr17Ni12Mo2, keep the heat identity unbroken from melt to bundle tag. Duty: standard Mo austenitic seamless pipe for general chloride-resistant fluid transport on Chinese projects. Sampling plans for 06Cr17Ni12Mo2 keep heat identity unbroken from melt through bundle tags, including any third-party hold points written into the purchase order. Keep the 06Cr17Ni12Mo2 caution visible here: 0.08% carbon ceiling — prefer 022Cr17Ni12Mo2 or Ti-stabilised 06Cr17Ni12Mo2Ti when corrosive field welds cannot be annealed.
Intergranular corrosion testing is mandatory for most austenitics — see the IGC note for 06Cr17Ni12Mo2. Order extras (grain size, inclusions, elevated tensile) under 7.8.3 when needed. Non-conforming 06Cr17Ni12Mo2 lengths are segregated and retested or rejected under GB/T 2102 rather than reworked into unmarked stock. This paragraph is locked to 06Cr17Ni12Mo2 duty: standard Mo austenitic seamless pipe for general chloride-resistant fluid transport on Chinese projects.
Packaging and Shipping for GB/T 14976 06Cr17Ni12Mo2
Small-OD 06Cr17Ni12Mo2 often ships in crates; large-OD in strapped bundles with OD pads. Confirm destination handling limits on the RFQ. Use: chemical transfer, marine-adjacent utilities, heat-exchange fluid loops, and process lines that still say “316 seamless”. Bundle tickets for 06Cr17Ni12Mo2 repeat grade, heat, size, and quantity so receiving inspectors can match crates to the packing list without opening every wrap. Corrosion framing beside 06Cr17Ni12Mo2: Mo-bearing passive film handles many chloride process media; crevice and hot chloride SCC still need design review.
Bevelled ends get protectors so landing edges survive trucking. Size hint: broad OD×wall under GB/T 17395; W-C and W-H both common — name the route on the PO. Desiccant and wrap choices for 06Cr17Ni12Mo2 follow the voyage length and storage climate stated on the shipping order, not a one-size export habit. Size practice for 06Cr17Ni12Mo2 remains broad OD×wall under GB/T 17395; W-C and W-H both common — name the route on the PO.
Storage advice on arrival: keep bundles dry and off carbon-steel floors. Use thread: chemical transfer, marine-adjacent utilities, heat-exchange fluid loops, and process lines that still say “316 seamless”. Claims handling for 06Cr17Ni12Mo2 starts with tagged photos against the packing list so heat identity remains usable if replacement lengths are required. Keep the 06Cr17Ni12Mo2 caution visible here: 0.08% carbon ceiling — prefer 022Cr17Ni12Mo2 or Ti-stabilised 06Cr17Ni12Mo2Ti when corrosive field welds cannot be annealed.
Why Choose SHH STEEL
Project teams working to Chinese fluid-transport specs need a supplier that reads Chinese grade names correctly. SHH STEEL can make 06Cr17Ni12Mo2 to that discipline. Caution we keep visible: 0.08% carbon ceiling — prefer 022Cr17Ni12Mo2 or Ti-stabilised 06Cr17Ni12Mo2Ti when corrosive field welds cannot be annealed. SHH STEEL can produce and supply 06Cr17Ni12Mo2 against the OD × wall, seamless route, and test scope on your RFQ without swapping in an unstated sister grade.
Dual-cert discussions (GB/T + ASTM) are handled with two acceptance regimes in view, not one certificate stretched by hope. Sisters: 022Cr17Ni12Mo2, 06Cr19Ni13Mo3, 06Cr17Ni12Mo2Ti, 07Cr17Ni12Mo2. Ask for a written acknowledgement that names 06Cr17Ni12Mo2, W-C or W-H, and the Table 1 heat-treatment condition before melt. SHH STEEL can make 06Cr17Ni12Mo2 to that written scope.
Supply Capability
Whether you need prototype spools or project tonnage of 06Cr17Ni12Mo2, SHH STEEL can supply against a clear OD × wall and test matrix. Duty: chemical transfer, marine-adjacent utilities, heat-exchange fluid loops, and process lines that still say “316 seamless”. SHH STEEL can produce and supply cut lengths, bevels, and ordered annex tests for 06Cr17Ni12Mo2 when the mill schedule allows.
| Item | Capability |
|---|---|
| Standard | GB/T 14976-2025 seamless stainless steel pipes for fluid transport |
| Grade | 06Cr17Ni12Mo2 (S31608) |
| Product form | Seamless pipe only — cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H) |
| Delivery condition | solution annealed |
| Documents | Mill test certificate (GB/T 2102 / EN 10204 3.1 style as ordered) |
| Typical size practice | OD × wall per GB/T 17395; PA ordinary or PC higher precision; usual length 4000–12000 mm |
| Wall / ordering | Nominal OD×wall, OD×min wall, or ID×wall by agreement |
Stock / Available sizes
Stock / Available sizes: SHH STEEL quotes piercing/drawing slots for 06Cr17Ni12Mo2 rather than promising anonymous warehouse tons. Typical conversation starts around broad OD×wall under GB/T 17395; W-C and W-H both common — name the route on the PO. SHH STEEL can supply alternate walls and precision classes for 06Cr17Ni12Mo2 once the design pressure and corrosion allowance are clear.
If the project needs dual GB/T 14976 + ASTM documentation, say so before melt. Caution: 0.08% carbon ceiling — prefer 022Cr17Ni12Mo2 or Ti-stabilised 06Cr17Ni12Mo2Ti when corrosive field welds cannot be annealed. SHH STEEL can produce trial lengths of 06Cr17Ni12Mo2 for procedure qualification before the bulk release when the project calendar needs it.
FAQ
-
What is GB/T 14976 06Cr17Ni12Mo2 seamless stainless steel pipe used for?
- GB/T 14976 06Cr17Ni12Mo2 is seamless stainless pipe for fluid transport — chemical transfer, marine-adjacent utilities, heat-exchange fluid loops, and process lines that still say “316 seamless”. Role summary: standard Mo austenitic seamless pipe for general chloride-resistant fluid transport on Chinese projects. It is a Chinese product standard grade (S31608), not an automatic ASTM A312 certificate.
-
Is GB/T 14976 06Cr17Ni12Mo2 seamless only, or does it cover welded pipe?
- Seamless only. Clause 6.2 limits manufacture to cold-rolled/drawn (W-C) or hot-rolled/extruded/forged/expanded (W-H) seamless routes. SHH STEEL can produce and supply either seamless route for 06Cr17Ni12Mo2 when the mill can meet the ordered size and tests. Welded pipe belongs under other standards, not 14976.
-
What heat treatment applies to 06Cr17Ni12Mo2?
- 06Cr17Ni12Mo2 is delivered solution annealed under GB/T 14976. Table 1 reference: 1010–1150 °C, water or rapid cool. Other schedules need written agreement. Certificate wording should match the treatment actually performed. Keep the purchase order locked to GB/T 14976 and 06Cr17Ni12Mo2 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
-
How does 06Cr17Ni12Mo2 compare with sister grades 022Cr17Ni12Mo2, 06Cr19Ni13Mo3, 06Cr17Ni12Mo2Ti?
- 06Cr17Ni12Mo2 is filed as austenitic. Typical sisters on the same RFQ are 022Cr17Ni12Mo2, 06Cr19Ni13Mo3, 06Cr17Ni12Mo2Ti. Design caution: 0.08% carbon ceiling — prefer 022Cr17Ni12Mo2 or Ti-stabilised 06Cr17Ni12Mo2Ti when corrosive field welds cannot be annealed Pick the sister when the medium or strength floor outgrows this grade rather than stretching wall alone.
-
What tests appear on the mill certificate for 06Cr17Ni12Mo2?
- Expect cast analysis (Table 2), room-temperature tensile results (Table 3), dimensions, hydrostatic test (or replacing UT/ET), appearance, and every special annex or IGC test actually performed. SHH STEEL does not print surrogate inspection lines. Documents follow GB/T 2102 or EN 10204 3.1 style when specified.
-
Is 316 / UNS S31608 the same as ordering 06Cr17Ni12Mo2?
- No. 316 / UNS S31608 is a commercial / UNS cross-walk for body text (unified S31608). The purchase order should lock GB/T 14976 and 06Cr17Ni12Mo2 so cast limits, heat treatment, and seamless route are unambiguous. Silent alias substitution is a common root cause of wrong MTCs.
-
What size range can SHH STEEL quote for GB/T 14976 06Cr17Ni12Mo2?
- SHH STEEL can produce and supply enquiry-oriented OD × wall bands for 06Cr17Ni12Mo2 within GB/T 17395 practice, with PA or PC precision and measured or min-wall options by agreement. Size context: broad OD×wall under GB/T 17395; W-C and W-H both common — name the route on the PO. Stock / Available sizes on this page is an RFQ map, not a frozen tonnage catalogue.
-
How should 06Cr17Ni12Mo2 be welded on site?
- Shop guidance: 316/316L fillers; heat-input control on non-L heats in corrosive service. Mill heat treatment of seamless pipe does not replace a qualified WPS on fabricator joints. For corrosive as-welded duty, confirm low-carbon, stabilisation, or anneal practice as applicable. Caution: 0.08% carbon ceiling — prefer 022Cr17Ni12Mo2 or Ti-stabilised 06Cr17Ni12Mo2Ti when corrosive field welds cannot be annealed
-
When should I choose a higher-Mo or superaustenitic grade instead of 06Cr17Ni12Mo2?
- Move when chloride pitting, crevice attack, or reducing-acid risk exceeds what austenitic practice can defend for the temperature and stress state. Caution for this mark: 0.08% carbon ceiling — prefer 022Cr17Ni12Mo2 or Ti-stabilised 06Cr17Ni12Mo2Ti when corrosive field welds cannot be annealed Sister pointers: 022Cr17Ni12Mo2, 06Cr19Ni13Mo3, 06Cr17Ni12Mo2Ti. SHH STEEL will not invent PREN marketing digits — bring the medium data.
-
Can SHH STEEL dual-certify GB/T 14976 06Cr17Ni12Mo2 with ASTM A312?
- Dual documentation is possible only when chemistry and tests satisfy each standard on its own terms. An MTC that only cites GB/T 14976 06Cr17Ni12Mo2 does not clear ASTM acceptance by default. State both standards, sizes, and test scopes before melt. Keep the purchase order locked to GB/T 14976 and 06Cr17Ni12Mo2 so cast limits, heat treatment, and seamless W-C/W-H marking stay unambiguous on the mill certificate.
-
What surface finishes are available for 06Cr17Ni12Mo2?
- Pickled after heat treatment is the usual fluid-transport supply. Bright anneal, grind, or polish finishes are by agreement and must state OD/ID scope. SHH STEEL can produce and supply the ordered finish for 06Cr17Ni12Mo2 when the mill route supports it. Carbon-steel strapping never contacts the stainless OD.
Conclusion
GB/T 14976 06Cr17Ni12Mo2 is seamless stainless steel pipe for fluid transport — standard Mo austenitic seamless pipe for general chloride-resistant fluid transport on Chinese projects. SHH STEEL can produce and supply it in cold-finished or hot-finished seamless routes with the heat treatment, tests, and finishes named on your enquiry, documented on mill certificates. Sister grades often discussed alongside this mark include 022Cr17Ni12Mo2, 06Cr19Ni13Mo3, 06Cr17Ni12Mo2Ti. Related ASTM pages share chemistry families but not Chinese acceptance text. Email admin@steelspecs.com with OD × wall, W-C or W-H preference, and medium notes to start the quote.