EN 10217-7 1.4571 Welded Stainless Steel Tube | EN 10217-7 Stainless Steel - SHH STEEL

EN 10217-7 1.4571 Welded Stainless Steel Tube

EN 10217-7 1.4571 / X6CrNiMoTi17-12-2 welded stainless pressure tube (316Ti), austenitic, cast analysis per EN table, ambient Rp0.2 min 210 MPa, Rm 500–730, solution annealed 1020–1120 °C. SHH STEEL can produce and supply with EN 10204 3.1 MTCs, TC1/TC2 testing.
Grade
1.4571 / X6CrNiMoTi17-12-2 (316Ti — body alias)
Standard
EN 10217-7
Product form
Welded tube for pressure purposes (longitudinal arc/laser), solution annealed as required by delivery condition
Size
~6–219 mm OD × 0.5–12.7 mm wall within family characterisation; other sizes by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Welded Tube Manufacture
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is EN 10217-7 1.4571 Welded Stainless Steel Tube

Inside the EN 10217-7:2021 welded stainless pressure-tube list, 1.4571 / X6CrNiMoTi17-12-2 is the austenitic grade purchasers pick when the duty matches this chemistry story. The standard covers circular welded tubes for pressure and corrosion-resisting purposes; it does not accept a bare “316Ti” stamp as a substitute for steel number, delivery-condition symbol, or test category. Name EN 10217-7, 1.4571, TC1/TC2, and the options list on the purchase order so cast analysis, longitudinal weld manufacture, solution treatment where required, mechanical verification, and leak-tightness are unambiguous. Practical role: titanium-stabilised Mo-bearing austenitic welded pressure tube for as-welded chloride-adjacent chemical service at intermittent elevated temperature.

SHH STEEL can produce and supply EN 10217-7 1.4571 welded stainless steel tube — longitudinally arc- or laser-welded from strip or plate on the standard’s manufacturing routes, solution annealed where the ordered delivery condition requires it, with EN 10204 3.1 inspection documents (3.2 under Option 21) reporting cast chemistry and ambient mechanical results against the ordered edition. Typical enquiry sizes cover process and utility welded OD with W2A/WCA common on European plant specs. Browse the series hub at EN 10217-7.

If the material list still says 316Ti welded tube for a PED spool, EN 10217-7 1.4571 is the steel number that belongs on the enquiry and the stencil. Typical welded pressure duties include European chemical plant piping that historically specifies 316Ti, heat-transfer loops, and PED lines that want Mo plus stabilisation without a full fabricated anneal. Design caution: Ti stabilisation plus Mo is still not a duplex SCC answer; and Ti can affect bright polish if WP is ordered without agreement on grit Commercially the grade is often called 316Ti; keep that name on the enquiry note and in the body, never as a substitute for steel number 1.4571 / X6CrNiMoTi17-12-2 on the MTC. Sister numbers on this hub include EN 10217-7 1.4404, EN 10217-7 1.4541, EN 10217-7 1.4401, EN 10217-7 1.4435.4404, 1.4541, 1.4401, 1.4435.

Product-form discipline: order EN 10217-7 for welded 1.4571, EN 10216-5 for seamless. Dimensions lean on EN ISO 1127. Manufacture is longitudinal arc or laser from strip or plate per Table 1; spiral/helical is not invented as a listed Part 7 route in this series. Live seamless sister: EN 10216-5 1.4571. Related live ASTM/ASME anchors: A269 TP316L, A213 TP316L.

Chemical Composition of EN 10217-7 1.4571

Heat acceptance for 1.4571 starts with cast analysis to X6CrNiMoTi17-12-2. Option 6 product analysis uses the standard’s permissible deviations. SHH STEEL documents real ladle results on EN 10204 3.1 and treats private catalogue windows as non-EN unless the purchaser agrees them separately.

The following cast analysis for X6CrNiMoTi17-12-2 is taken from public BSSA EN 10217-7 data for steel number 1.4571. Maxima apply except where a range is shown. Verify against the ordered EN 10217-7:2021 text before release.

Element 1.4571 cast analysis (mass %)
Carbon (C) ≤0.08
Silicon (Si) ≤1.00
Manganese (Mn) ≤2.00
Phosphorus (P) ≤0.045
Sulfur (S) ≤0.015
Chromium (Cr) 16.5–18.5
Nickel (Ni) 10.5–13.5
Molybdenum (Mo) 2.00–2.50
Titanium (Ti) 5×C to 0.70

Public BSSA EN 10217-7 chemistry underpins the 1.4571 / X6CrNiMoTi17-12-2 table below. Cross-check is against the 2021 grade list framing. Scrap and finishing practice must still protect the austenitic property set — unlisted deliberate additions require agreement.

Mechanical Properties of EN 10217-7 1.4571

EN 10217-7 lists ambient tensile and ductility requirements for solution-annealed X6CrNiMoTi17-12-2 (steel number 1.4571) in the austenitic table, covering walls up to about 60 mm by default. Both 0.2% and 1.0% proof stresses are specified. −196 °C impact data are available as characterisation; verification is an Option-driven act.

For 1.4571, the tensile and ductility floors below are BSSA EN 10217-7 ambient figures. Solution temperatures for X6CrNiMoTi17-12-2 come from public EN stainless tables (UNCERTAIN against paid Part 7 footnotes). SHH STEEL will not inflate or swap those floors using another product standard’s numbers.

Property 1.4571 ambient (solution annealed +AT)
Rp0.2 min (MPa) 210
Rp1.0 min (MPa) 245
Rm (MPa) 500–730
A min % long / trans 35 / 30
IGC resistance (delivery) Yes (method A)
Solution annealing (public EN band) 1020–1120 °C — UNCERTAIN vs paid EN 10217-7:2021 footnote if diverges
Cooling water or air
Charpy sub-zero (transverse min J) 60 at -196 °C (Option to verify)

Mechanical source stack for 1.4571: BSSA EN 10217-7 ambient properties; public EN solution-anneal bands with UNCERTAIN paid-edition flag. Characterisation impact energies for X6CrNiMoTi17-12-2 become certificate entries only through the relevant Options.

Welded Tube Manufacture for EN 10217-7 1.4571

Part 7 production of 1.4571 / X6CrNiMoTi17-12-2 is a longitudinal weld story. Strip or plate is formed and closed by automatic arc or laser welding on a Table 1 route, with or without filler and with optional outside grind or bead work ahead of heat treatment. Everyday sizes run on strip; heavier walls use plate. Finished tubes exclude pre-forming strip-join welds. Helical manufacture is outside the listed routes — settle any non-standard seam in writing. Seamless pressure stainless is ordered under EN 10216-5, not under this welded page.

For titanium-stabilised austenitic 1.4571 (X6CrNiMoTi17-12-2), mill seams typically run without filler or with matching stabilised filler depending on wall and route; Options 3 and 4 cover inside remelt or bead working when a smoothed ID weld is wanted. Delivery symbols W0 through W2R, WCA/WCR, and WG/WP follow Table 2 — Option 5 locks them. Stabilisation is part of the chemistry story, not a licence to skip ordered heat treatment. SHH STEEL can produce and supply 1.4571 as W1A/W2A descaled or WCA/WCR cold-finished in the common band, and as WG/WP when roughness is agreed. Filler practice: stabilised Mo austenitic fillers; control heat input; avoid unstabilised dilution on corrosive joints

Without a declared TC1 or TC2, a 1.4571 order is incomplete under Part 7. Category controls tensile frequency and seam NDT intensity; leak-tightness stays per tube (Option 15 to prescribe the technique). SHH STEEL’s X6CrNiMoTi17-12-2 certificates identify the manufacturing route and delivery-condition symbol actually run.

Dimensions and Tolerances for EN 10217-7 1.4571

Buyers order 1.4571 (X6CrNiMoTi17-12-2) on outside diameter and wall thickness. EN ISO 1127 preferred sizes and stainless densities apply. EN 10217-7 tolerance classes (Option 20 → D4) govern diameter and wall; ovality and eccentricity remain inside those envelopes, and abutting-edge radial offset at the weld is limited per public text.

Exact-length Option 19 and bevel Option 18 (wall ≥ 3.2 mm) are standard extras. For 316Ti-class welded pressure tube needing tighter OD, WCA/WCR is usually discussed alongside W1A/W2A. SHH STEEL locks OD × wall, class, and symbol on the 1.4571 order prior to welding.

Route / condition Typical use Notes
W1 / W1A / W1R Hot-rolled starting flat product Descaled or bright-annealed per symbol
W2 / W2A / W2R Cold-rolled starting flat product Smoother OD than W1 family except at weld
WCA / WCR Cold finished ≥20% after weld Recrystallized weld metal; OD often ≤168.3 mm
WG / WP Ground / polished Agree ID/OD scope and grit at enquiry

Release of EN 10217-7 1.4571 includes confirmation that OD × wall sit inside the purchased class for X6CrNiMoTi17-12-2. Straightness and end condition are inspected to the standard; cold-finished routes are recommended when D4 is specified. SHH STEEL confirms OD × wall and the selected EN ISO 1127 / Part 7 tolerance class for 1.4571 / X6CrNiMoTi17-12-2 on the inspection document rather than assuming mid-tolerance catalogue values.

Equivalent Grades for EN 10217-7 1.4571

Steel number 1.4571 with name X6CrNiMoTi17-12-2 is what EN 10217-7 stamps on welded pressure tube of this analysis. Alias 316Ti is commercial language. Treat ASTM/ASME lookalikes and EN 10216-5 seamless pages as related references — verify before dual-marking or substituting.

Bill-of-materials writers sometimes list 316Ti next to EN and ASTM numbers interchangeably. For this product, steel number 1.4571 with name X6CrNiMoTi17-12-2 under EN 10217-7 is the welded acceptance path; confirm any dual mark against both mechanical tables before release to fabrication.

Reference Designation Note
EN 10217-7 1.4571 / X6CrNiMoTi17-12-2 This product standard (welded pressure tube)
EN steel name X6CrNiMoTi17-12-2 EN 10027-1 designation used in body and marking
Commercial alias (body only) 316Ti Not a substitute for the steel number on the MTC
EN 10216-5 (seamless sister) 1.4571 Related live page — different product form (seamless)
A269 TP316L A269 TP316L Related live page — different product standard
A213 TP316L A213 TP316L Related live page — different product standard

Inside this welded series, compare EN 10217-7 1.4404, EN 10217-7 1.4541, EN 10217-7 1.4401, EN 10217-7 1.4435. Hub: EN 10217-7. Seamless sister: EN 10216-5 1.4571. Live cross-standard anchors: A269 TP316L, A213 TP316L.

Heat Treatment and Delivery Condition for EN 10217-7 1.4571

Choose the Table 2 symbol for 1.4571 with heat treatment in mind. W1A/W2A, cold-finished WCA/WCR, and bright-annealed W1R/W2R all imply treated routes; mechanical acceptance for X6CrNiMoTi17-12-2 is written for solution-annealed (+AT) tube. For X6CrNiMoTi17-12-2 under steel number 1.4571, keep Option 5 in mind when the delivery-condition symbol must be contractual, and reconcile the certificate wording with the solution-annealing practice actually used on the welded tube before releasing the PED file.

Reference solution window for 1.4571: 1020–1120 °C with water or air cooling, drawn from public EN stainless tables and flagged UNCERTAIN vs paid Part 7 notes. Surface finish remains a Table 2 / Option 5 decision after heat treatment of X6CrNiMoTi17-12-2. For X6CrNiMoTi17-12-2 under steel number 1.4571, keep Option 5 in mind when the delivery-condition symbol must be contractual, and reconcile the certificate wording with the solution-annealing practice actually used on the welded tube before releasing the PED file.

Item 1.4571
Solution annealing band (public) 1020–1120 °C (UNCERTAIN vs paid Part 7 footnote)
Cooling water or air
Delivery condition symbols W0 / W1 / W1A / W1R / W2 / W2A / W2R / WCA / WCR / WG / WP (Option 5 to specify)
Inspection document EN 10204 3.1 default; 3.2 under Option 21

Delivery-condition control for 1.4571 means more than a furnace ticket: SHH STEEL records the symbol, the heat treatment implied for X6CrNiMoTi17-12-2, and cold-finished weld recrystallization status when WCA/WCR applies, then ships only material that matches that record. For X6CrNiMoTi17-12-2 under steel number 1.4571, keep Option 5 in mind when the delivery-condition symbol must be contractual, and reconcile the certificate wording with the solution-annealing practice actually used on the welded tube before releasing the PED file.

Corrosion Resistance of EN 10217-7 1.4571

Corrosion-resisting austenitic 1.4571 / X6CrNiMoTi17-12-2 is selected for welded pressure duty where the medium and temperature need Mo for pitting/crevice; Ti for as-welded IGC resistance in many chemical duties. EN 10217-7 marks intergranular-corrosion behaviour in the delivery condition against EN ISO 3651-2 methods in the mechanical tables; verification of IGC remains Option 13 even when the table says the grade resists IGC as delivered.

Do not read IGC guideline temperatures as a licence to run 1.4571 hotter without design justification. They flag sensitisation risk for X6CrNiMoTi17-12-2. Chemistry moves among EN 10217-7 1.4404, EN 10217-7 1.4541, EN 10217-7 1.4401, EN 10217-7 1.4435 are the honest upgrade path; invented PREN numbers are not EN 10217-7 acceptance text.

Applications of EN 10217-7 1.4571 Tube

EN 10217-7 1.4571 welded tube is used where PED-oriented pressure tubing must also resist corrosion and a longitudinal weld seam is accepted on the drawing. For X6CrNiMoTi17-12-2 the practical band is European chemical plant piping that historically specifies 316Ti, heat-transfer loops, and PED lines that want Mo plus stabilisation without a full fabricated anneal, supplied as welded tube in the ordered delivery condition with TC1 or TC2 testing.

It is the wrong first choice when a seamless product is mandatory (use EN 10216-5 — see EN 10216-5 1.4571), when the drawing is ASTM A269 instrumentation tubing or A312 pipe without an EN dual mark, or when the medium clearly needs a different family. SHH STEEL can produce and supply 1.4571 across the enquiry size band and will say when a sister EN number or a live ASTM/ASME page is the better fit. Related live pages: A269 TP316L, A213 TP316L.

Weldability of EN 10217-7 1.4571

1.4571 / X6CrNiMoTi17-12-2 is welded both as a mill seam under EN 10217-7 manufacturing routes and later as a fabricator joint on the PED spool. Mill seams follow the qualified longitudinal arc or laser procedures for the ordered route; shop welds use processes and fillers chosen for the EN chemistry family. For this grade: stabilised Mo austenitic fillers; control heat input; avoid unstabilised dilution on corrosive joints

Mill weldability of 1.4571 is proven on the Table 1 route; fabricator weldability is proven on the WPS. Keep those scopes apart. SHH STEEL certifies X6CrNiMoTi17-12-2 mill tube to the ordered delivery condition and inspection Options, and leaves joint design — including as-welded service limits — with the PED responsible party.

Surface Finishes for EN 10217-7 1.4571

W1A/W2A descaled, W1R/W2R/WCR bright-annealed, and WG/WP ground or polished are the finish vocabulary for 1.4571. Write roughness when WP/WG is wanted; do not assume a grit from a brochure photo of X6CrNiMoTi17-12-2. Carbon-steel banding on stainless is rejected in SHH STEEL packing rules because free-iron stains on 316Ti are expensive to remove and easy to prevent at the dock.

Anything beyond Table 2 surface language needs writing: Ra, EP, films, capped cleanliness. SHH STEEL can produce and supply finishes it can report for EN 10217-7 1.4571; unmeasured grit marketing is not offered for X6CrNiMoTi17-12-2, and commercial 316Ti habits do not override that discipline.

If the drawing shows a hygienic OD note without EN delivery language, translate it into W1R/W2R, WCR, or WP with criteria before releasing 1.4571. SHH STEEL will help map that note onto a measurable finish for X6CrNiMoTi17-12-2 instead of guessing what the last fabricator accepted on unlabeled 316Ti tube.

Inspection and Testing for EN 10217-7 1.4571

Baseline Part 7 inspection for 1.4571: cast analysis, room-temperature tensile at the ordered test-category rate, technological tests, full leak-tightness coverage, plus dimensional/visual/ID work on X6CrNiMoTi17-12-2. Hydrostatic or eddy-current leak testing may be locked with Option 15. Keep TC1/TC2, Option 13 IGC, and any impact Options visible on the 1.4571 purchase order so X6CrNiMoTi17-12-2 inspection planning matches the PED file before weld slots are locked.

TC2, Option 13 IGC, and impact Options are how purchasers thicken the 1.4571 inspection story beyond baseline leak-tightness and tensile. SHH STEEL documents chemistry, heat treatment, tensile, and NDT/leak results for X6CrNiMoTi17-12-2 and will not delete mandatory tests to chase a shorter promise date.

Technological test selection follows the diameter/wall matrix for 1.4571; do not assume flattening alone covers every size. SHH STEEL applies the matrix that matches the ordered X6CrNiMoTi17-12-2 OD × wall and cites the tests actually performed.

Packaging and Shipping for EN 10217-7 1.4571

Dispatch packing on EN 10217-7 1.4571 covers mechanical protection and stainless hygiene. Caps or plugs close the ends, bundles are size-sorted, and waterproof wrap covers long sea legs. Stabilised 316Ti finishes that were bright-annealed or polished take sleeve wrap against galling; descaled utility lengths still travel on clean timber or plastic-lined supports. Contact materials exclude bare carbon steel so X6CrNiMoTi17-12-2 OD — commercially still discussed as 316Ti — does not pick up rust blooms in transit that complicate PED receiving inspection.

Marking discipline for 1.4571: standard, steel number or X6CrNiMoTi17-12-2, size, cast, TC1/TC2, inspection marks. Delivery symbols follow manufacturer practice unless Option 5 demands them. SHH STEEL verifies the marking clause on the 316Ti order prior to shipment. SHH STEEL treats packing and marking for EN 10217-7 1.4571 / X6CrNiMoTi17-12-2 as part of product conformity, not as a warehouse afterthought, so the PED receiving inspection sees protected ends, clean contact materials, and stencil text that matches the certificate.

Ocean and road packs for 1.4571 keep heat identity visible at bundle level. Bevelled and exact-length tube is capped and segregated. SHH STEEL closes packaging only after the order’s packing and marking lines are satisfied for this 316Ti grade. SHH STEEL treats packing and marking for EN 10217-7 1.4571 / X6CrNiMoTi17-12-2 as part of product conformity, not as a warehouse afterthought, so the PED receiving inspection sees protected ends, clean contact materials, and stencil text that matches the certificate.

Why Choose SHH STEEL

SHH STEEL can produce and supply 1.4571 welded stainless pressure tube with matching heat treatment and TC1/TC2 documentation for X6CrNiMoTi17-12-2. The commercial alias 316Ti may appear in body text; it does not replace the steel number on the certificate, and sister-standard tensile floors stay off this Part 7 document.

Use LINKPLACE1.4404, LINKPLACE1.4541, LINKPLACE1.4401, LINKPLACE1.4435 as the short-list when 1.4571 is borderline. Remember: Ti stabilisation plus Mo is still not a duplex SCC answer; and Ti can affect bright polish if WP is ordered without agreement on grit The PED file needs the right steel number more than it needs a fast yes Linked sisters on this hub: EN 10217-7 1.4404, EN 10217-7 1.4541, EN 10217-7 1.4401, EN 10217-7 1.4435. Live ASTM/ASME anchors: A269 TP316L, A213 TP316L.

Supply Capability

SHH STEEL can produce and supply 1.4571 welded stainless pressure tube under EN 10217-7 with the documents and tests your enquiry lists. Capability plus Stock / Available sizes below are the sizing scratchpad for X6CrNiMoTi17-12-2. Process and utility welded od with w2a/wca common on european plant specs.

Item SHH STEEL capability for 1.4571
Standard EN 10217-7
Grade 1.4571 / X6CrNiMoTi17-12-2
Product form Welded tube for pressure purposes (longitudinal arc/laser), solution annealed as required by delivery condition
Delivery condition W0 / W1 / W1A / W1R / W2 / W2A / W2R / WCA / WCR / WG / WP (Option 5 to lock)
Typical size band ~6–219 mm OD × 0.5–12.7 mm wall within family characterisation; other sizes by agreement
Testing TC1 or TC2; leak-tightness each tube; weld-seam NDT per category / options
Documents EN 10204 3.1 (3.2 Option 21); third-party inspection on request

Stock / Available sizes

The Stock / Available sizes block for 1.4571 is a planning aid. Actual commitment waits on X6CrNiMoTi17-12-2 melt/strip position and the ordered W-symbol finishing path. Send sizes, TC1/TC2, and delivery condition to firm it up.

OD (mm) Typical walls (mm) Notes
12 / 14 / 16 / 19 / 21.3 / 25 1.0 / 1.5 / 2.0 / 2.5 Instrument / hygienic; often WCA/WCR or W2R
26.9 / 33.7 / 38 / 42.4 / 48.3 1.5 / 2.0 / 2.5 / 3.0 / 4.0 Process and utility welded pressure tube
60.3 / 76.1 / 88.9 / 114.3 2.0 / 3.0 / 4.0 / 5.0 / 6.0 Utility and process; lock W1A/W2A vs WCA
141.3 / 168.3 / 219.1 3.0 / 4.0 / 5.0 / 6.0 / 8.0 / 10 Larger welded pressure tube; watch family wall ceiling

Option-driven extras and sister comparisons (1.4404, 1.4541, 1.4401, 1.4435) belong on the enquiry. Size rows are typical, not promised stock. SHH STEEL can produce and supply EN 10217-7 1.4571 across this map when X6CrNiMoTi17-12-2 feedstock and weld capacity agree.

FAQ

What is EN 10217-7 1.4571 welded stainless steel tube used for?
EN 10217-7 1.4571 (X6CrNiMoTi17-12-2) is welded pressure tube for PED-oriented duties that need the austenitic chemistry story with a longitudinal mill seam. Typical service is European chemical plant piping that historically specifies 316Ti, heat-transfer loops, and PED lines that want Mo plus stabilisation without a full fabricated anneal. Put EN 10217-7, the steel number, and TC1/TC2 on the purchase order so chemistry, weld route, delivery condition, and tests match Part 7 — not a seamless EN 10216-5 or ASTM tubing habit.
Is EN 10217-7 1.4571 the same as 316Ti under ASTM A269 or A312?
No. Commercial alias 316Ti may point at a similar chemistry idea, but EN 10217-7 is a European welded pressure-tube standard with its own tables, test categories, and delivery-condition symbols. ASTM A269 is nominal-wall general-service tubing; A312 is pipe. Order the standard that matches the drawing. See also A269 TP316L, A213 TP316L.
Does EN 10217-7 1.4571 include seamless tube?
No. EN 10217-7 covers welded tubes only. If the line specification requires seamless product, the correct European series is EN 10216-5 for seamless pressure stainless tubes. Live seamless sister page: EN 10216-5 1.4571. Site titles for this series always say Welded Tube; the body does not pretend Part 7 can supply seamless product.
What mechanical properties does EN 10217-7 require for 1.4571?
In the solution-annealed condition, public BSSA ambient tables for EN 10217-7 list Rp0.2 min 210 MPa, Rp1.0 min 245 MPa, Rm 500–730 MPa, and elongation 35% longitudinal / 30% transverse for walls within the family’s characterisation band. Confirm against the purchased edition; do not invent creep rupture or PREN digits.
1.4571 vs sister grades — which EN 10217-7 number should I buy?
Buy 1.4571 when the enquiry names this steel number or the duty matches titanium-stabilised Mo-bearing austenitic welded pressure tube for as-welded chloride-adjacent chemical service at intermittent elevated temperature. Compare EN 10217-7 1.4404, EN 10217-7 1.4541, EN 10217-7 1.4401, EN 10217-7 1.4435 when carbon, Mo, stabilisation, nitrogen, or duplex strength points elsewhere. Design caution for this grade: Ti stabilisation plus Mo is still not a duplex SCC answer; and Ti can affect bright polish if WP is ordered without agreement on grit
What delivery conditions are available for EN 10217-7 1.4571?
Delivery-condition symbols include W0, W1, W1A, W1R, W2, W2A, W2R, WCA, WCR, WG, and WP (bead-worked “b” suffix optional). Heat treatment is part of several symbols; mechanical tables assume solution-annealed (+AT) properties. Unless Option 5 is specified, the manufacturer chooses. SHH STEEL can produce and supply the common heat-treated descaled and cold-finished routes when the order locks Option 5 and any roughness scope.
What size range can SHH STEEL supply for EN 10217-7 1.4571?
SHH STEEL can produce and supply EN 10217-7 1.4571 in a typical enquiry band covering instrumentation through process OD with walls suited to longitudinal welded routes (~6–219 mm OD × 0.5–12.7 mm wall within family characterisation; other sizes by agreement), with EN 10204 3.1 documents. Larger or heavier sizes need agreement — send the OD × wall list for a firm availability answer. Process and utility welded od with w2a/wca common on european plant specs.
TC1 or TC2 for EN 10217-7 1.4571?
Test category is mandatory order information and appears in marking. TC2 increases tensile sampling and raises the NDT / technological-test intensity on the weld seam relative to TC1. Choose TC2 when the PED file or purchaser specification demands the heavier regime. Leak-tightness applies to every tube in both categories.
Is the intergranular corrosion test mandatory for 1.4571?
No. IGC testing to EN ISO 3651-2 is Option 13. Tables mark resistance in the delivery condition for corrosion-resisting grades, but the test appears on the certificate only when ordered. Order Option 13 when the PED file or end-user specification requires a tested IGC result for 1.4571.
What documents come with SHH STEEL EN 10217-7 1.4571?
EN 10204 3.1 inspection documents report cast chemistry, delivery-condition / heat-treatment status, ambient tensile results, and leak-tightness / NDT statements. Option 21 upgrades to 3.2. Third-party inspection and PMI can be added on the order. Stencil carries EN 10217-7, 1.4571, size, cast, and test category.
How do I enquire for EN 10217-7 1.4571 with SHH STEEL?
Send EN 10217-7, steel number 1.4571 / X6CrNiMoTi17-12-2, TC1 or TC2, OD × wall list and lengths, delivery-condition symbol (or Option 5), and any Options (13 IGC, 15 leak-test method, 18 bevel, 19 exact length, 20 D4, 21 for 3.2). Add the service medium if grade selection is still open. SHH STEEL can produce and supply to that enquiry or recommend a sister number when the duty needs it.

Conclusion

EN 10217-7 1.4571 (X6CrNiMoTi17-12-2) is welded stainless pressure tube for PED-oriented service in the austenitic family — ordered by steel number, test category, and delivery-condition symbol, not by a shop alias alone. SHH STEEL can produce and supply 1.4571 with EN 10204 documentation, leak-tightness testing, and weld-seam NDT aligned to TC1 or TC2. For sizing, sister-grade advice, or a dual enquiry against seamless EN 10216-5 or live ASTM/ASME pages, contact admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X