EN 10028-2 10CrMo9-10 2.25Cr-1Mo high-temperature pressure vessel steel plate, steel number 1.7380, SHH STEEL

EN 10028-2 10CrMo9-10 Steel Plate | 10CrMo9-10 2.25Cr-1Mo Vessel Plate

EN 10028-2 10CrMo9-10 is European 2.25Cr-1Mo high-temperature vessel plate, steel number 1.7380. Yield is 310 MPa at ≤16 mm. Tensile is 480–630 MPa. SHH STEEL supplies 10CrMo9-10 as a global steel mill sourcing partner.
Keywords
EN 10028-2 10CrMo9-10, 10CrMo9-10, 10CrMo9-10 steel plate, 1.7380, 10CrMo9-10 2.25Cr-1Mo, 10CrMo9-10 equivalent, 10CrMo9-10 supplier
Equivalent Grades:
EN 1.7380 / ASTM A387 Gr 22 Cl2 / JIS SCMV4 / GB 12Cr2Mo1R — Material Specification: EN 10028-2 — Delivery: Normalized + Tempered (N+T)
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Material Comparison
Equivalent Material Grades
2.25Cr-1Mo Pressure-Vessel Service
Weldability
Heat Treatment and Delivery Condition
Dimensions
Tolerances
Supplementary Requirements
Applications
Global Delivery & Markets
Why Choose SHH STEEL
FAQ
Conclusion

What is EN 10028-2 10CrMo9-10 Steel?

10CrMo9-10 is the 2.25Cr-1Mo grade in EN 10028-2. Buyers search EN 10028-2 10CrMo9-10, 10CrMo9-10 steel plate, 1.7380, 10CrMo9-10 equivalent and 10CrMo9-10 2.25Cr-1Mo vessel plate. The numbers mean about 2.25% chromium and 1.0% molybdenum. This page is not 13CrMo4-5 and not P355GH.

Yield is 310 MPa at ≤16 mm. Tensile is 480–630 MPa. Steel number is 1.7380. Delivery is usually normalized and tempered (+NT). SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) for this grade.

Do not ship 13CrMo4-5 against a 10CrMo9-10 drawing. 13CrMo4-5 is 1.25Cr-0.5Mo. The closest ASME comparison is SA387 Grade 22 Class 1 or SA387 Grade 22 Class 2. The closest Chinese comparison is 12Cr2Mo1R steel plate. Dual marking is possible only when chemistry, tensile, impact and delivery all fit.

Company scope: China steel mill agent SHH STEEL.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Grade EN 10028-2 10CrMo9-10 Confirmed
Steel number 1.7380 Confirmed
Product specification EN 10028-2 + EN 10028-1 Applied
Steel type Alloy special steel, 2.25Cr-1Mo Confirmed
Usual delivery +NT Confirmed
Yield idea 310 MPa at ≤16 mm Confirmed
Tensile 480–630 MPa at ≤16 mm Confirmed
Supply role Global steel mill sourcing partner SHH STEEL
Markets Americas, Europe, Middle East, Africa, Asia As ordered
Certification EN 10204 3.1 or 3.2 / third-party As ordered

This plate sits in pressure vessel steel plates. Cr-Mo comparisons belong on ASME SA387. Quenched-and-tempered Cr-Mo comparisons belong on ASME SA542.

Chemical Composition

Cast analysis follows EN 10028-2 Table 1. Product analysis follows EN 10028-1 when ordered. Google queries such as 10CrMo9-10 chemical composition and 1.7380 chemistry should be answered from this table.

Cast Analysis and Product Analysis — EN 10028-2 10CrMo9-10 (1.7380)

Element Cast Analysis (%) Product Analysis, when ordered (%)
Carbon (C) 0.08 – 0.14 0.06 – 0.16
Silicon (Si), max 0.50 0.55
Manganese (Mn) 0.40 – 1.00 0.35 – 1.08
Phosphorus (P), max 0.025 0.030
Sulfur (S), max 0.010 0.013
Nitrogen (N), max 0.012 0.014
Chromium (Cr) 2.00 – 2.50 1.90 – 2.60
Copper (Cu), max 0.30 0.35
Molybdenum (Mo) 0.90 – 1.10 0.85 – 1.15
Nickel (Ni), max 0.30 0.35
Vanadium (V), max 0.20 0.22

Chromium at 2.00–2.50% plus molybdenum at 0.90–1.10% is the pair that makes 10CrMo9-10 different from 13CrMo4-5. It is not P91 9Cr plate and not carbon plate. SHH STEEL reports cast analysis on every certificate and product analysis when ordered. Density is 7.85 g/cm³.

Mechanical Properties

Buyers search 10CrMo9-10 mechanical properties, 10CrMo9-10 yield strength and 1.7380 tensile. Room-temperature values fall with thickness.

Tensile and Yield — EN 10028-2 10CrMo9-10

Thickness (mm) Yield min (MPa) Tensile (MPa)
≤ 16 310 480 – 630
16 – 40 300 480 – 630
40 – 60 290 470 – 620
60 – 100 270 460 – 610
Density 7.85 g/cm³ 7.85 g/cm³

Elongation is typically 18–20% min on thinner plate. Impact at 0 °C, 27 J, is the usual option when the order names it. Elevated-temperature proof strength is part of EN 10028-2. Ask for that table when the vessel calculation uses design temperature.

Do not quote 310 MPa yield on a 80 mm plate. Do not treat 480–630 MPa tensile as permission to stamp SA387 Grade 22 Class 2 without checking class, PWHT and impact.

Material Comparison

Grade Book What buyers search Swap?
EN 10028-2 13CrMo4-5 EN 10028-2 13CrMo4-5 steel plate No
EN 10028-2 10CrMo9-10 EN 10028-2 10CrMo9-10 steel plate This page
EN 10028-2 11CrMo9-10 EN 10028-2 11CrMo9-10 Close sister, still check
SA387 Grade 22 Class 1 SA-387 SA387 Gr.22 Cl.1 No auto swap
SA387 Grade 22 Class 2 SA-387 SA387 Gr.22 Cl.2 No auto swap
SA387 Grade 21 Class 2 SA-387 SA387 Gr.21 Cl.2 No
12Cr2Mo1R steel plate GB/T 713.2 12Cr2Mo1R No auto swap
15CrMoR steel plate GB/T 713.2 15CrMoR No
Q345R steel plate GB/T 713.2 Q345R No

Equivalent Material Grades

Search habits mix 10CrMo9-10 equivalent, 1.7380 equivalent and 10CrMo9-10 vs SA387 Grade 22. Those names help a buyer find the right page. They do not authorize substitution.

Designation Standard / region Notes
EN 10028-2 10CrMo9-10 / 1.7380 EN 10028-2 Name on this page
10CrMo910 Old DIN Historical name
SA387 Grade 22 Class 1 SA-387 Closest ASME Class 1
SA387 Grade 22 Class 2 SA-387 Higher strength class
12Cr2Mo1R steel plate GB/T 713.2 Chinese 2.25Cr-1Mo
12Cr2Mo1VR steel plate GB/T 713.2 Vanadium-bearing sister
SA387 Grade 12 Class 2 SA-387 1.25Cr-0.5Mo
SA542 Type B Class 4 SA-542 QT 2.25Cr-1Mo
SA516 Grade 70 SA-516 Carbon, no Cr-Mo

2.25Cr-1Mo Pressure-Vessel Service

Buyers pick 10CrMo9-10 for PED boilers, hydroprocessing-adjacent shells, heat-exchanger channels and high-temperature vessels that need 2.25Cr-1Mo. Search phrases such as 10CrMo9-10 boiler plate, 1.7380 steel plate and 10CrMo9-10 pressure vessel plate all point to this grade.

Do not ship SA387 Grade 12 Class 2 against 10CrMo9-10. That grade is 1.25Cr-0.5Mo. Do not ship SA387 Grade 91 Class 2 either. That grade is 9Cr. An ASME file that wants 2.25Cr-1Mo should name SA-387 Grade 22 on ASME SA387 and then write class and extras. Dual marking is possible only when both books are met.

SHH STEEL supplies this plate to fabricators in the United States, Mexico, South America, Europe, the Middle East, Africa and Asia.

Weldability

10CrMo9-10 is 2.25Cr-1Mo vessel plate. Treat welding as production welding, and as PED / ASME Code welding when the equipment is a vessel.

Qualify to the applicable code. ASME dual-name work uses ASME Section IX. Consumables must match 2.25Cr-1Mo practice. A carbon procedure written for SA516 Grade 70 is not valid. A 1.25Cr-0.5Mo procedure written for 13CrMo4-5 is the previous family. Preheat, interpass and PWHT follow thickness and hydrogen control. The fabricator owns the WPS. SHH STEEL can share mill heat data for that review.

Heat Treatment and Delivery Condition

Usual delivery from SHH STEEL is normalized and tempered EN 10028-2 10CrMo9-10 (+NT). Buyers who search 10CrMo9-10 NT or 10CrMo9-10 heat treatment are asking for this route.

If the vessel will see PWHT, say so. Test coupons then follow a simulated cycle. Extra simulation, 3.2 hold points or special NDE add time. Plan about two months when those extras are on the order.

The certificate lists EN 10028-2 10CrMo9-10; 1.7380; heat number; cast analysis; product analysis when ordered; tensile to the correct thickness column; +NT; impact when ordered; elevated-temperature values when ordered. Certificates may be EN 10204 3.1 or EN 10204 3.2.

Dimensions

Usual supply range from SHH STEEL for 10CrMo9-10 2.25Cr-1Mo vessel plate:

  • Thickness: commonly 6 mm – 150 mm, thicker by mill agreement
  • Width: 1500 mm – 4000 mm
  • Length: 3000 mm – 12000 mm

Vanadium-bearing Cr-Mo belongs on 12Cr1MoVR steel plate or 12Cr2Mo1VR steel plate. Carbon vessel plate belongs on Q345R steel plate.

Tolerances

Dimensional limits follow EN 10028-1 and EN 10029 unless the order names another tolerance table. Do not apply ASTM A36 structural tolerances to a PED vessel plate without writing them.

Supplementary Requirements

Charpy details. Temperature, energy, location and orientation. 0 °C / 27 J is common, not assumed.

Product analysis. Add this when the destination file wants finished-plate chemistry.

Elevated-temperature proof strength. Add this when the calculation uses design temperature.

Simulated PWHT. When the equipment will be stress-relieved.

NDE. EN 10160 or the named UT class.

Third-party. EN 10204 3.2 when written.

Applications

Industry Typical components
PED boilers EN 10028-2 10CrMo9-10 shells
High-temp heat exchangers 10CrMo9-10 channels
2.25Cr-1Mo vessels 10CrMo9-10 plate from SHH STEEL
Dual-certified export 10CrMo9-10 / SA387 Grade 22 Class 2 when both books fit

Global Delivery & Markets

SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply ASTM, ASME, EN, DIN, JIS and GB steel to buyers outside a single region. Origin is mill-direct, China origin.

SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.

Typical trade terms on this grade: FOB Shanghai, plus CIF to European, American, Middle East and Asian ports as the buyer names them.

Typical lead time:

  • Ex-stock: about 5–7 days
  • Mill rolling, standard +NT: about 45 days
  • Simulated PWHT, 3.2 or extra NDE: about 2 months

Why Choose SHH STEEL

SHH STEEL is a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin). On EN 10028-2 10CrMo9-10 that means mill pricing, 1.7380 chemistry reported as cast analysis and as product analysis when ordered, recorded +NT, tensile results to the correct thickness column, 3.1 as standard and 3.2 when specified.

We keep the grade on the order. 10CrMo9-10 is not 13CrMo4-5. 10CrMo9-10 is not SA387 Grade 12 Class 2. 10CrMo9-10 is not Q345R steel plate. If the drawing says Grade 91, we will not ship 10CrMo9-10 and call Cr-Mo close.

Company scope: China steel mill agent SHH STEEL.

FAQ

What is 10CrMo9-10 steel plate?
10CrMo9-10 is an EN 10028-2 2.25Cr-1Mo high-temperature pressure-vessel plate, steel number 1.7380. Yield is 310 MPa at ≤16 mm and tensile is 480–630 MPa. Delivery is usually +NT. SHH STEEL supplies this plate as a global steel mill sourcing partner.
What is the equivalent of 10CrMo9-10?
elated comparisons are old 10CrMo910, SA-387 Grade 22 and 12Cr2Mo1R. Dual marking is possible only when both books are fully met.
How is 10CrMo9-10 different from 13CrMo4-5?
13CrMo4-5 is 1.25Cr-0.5Mo. 10CrMo9-10 is 2.25Cr-1Mo.
How is 10CrMo9-10 different from X10CrMoVNb9-1?
X10CrMoVNb9-1 is 9Cr-1Mo-V (P91). 10CrMo9-10 is 2.25Cr-1Mo.

Conclusion

EN 10028-2 10CrMo9-10 Steel Plate is European 2.25Cr-1Mo high-temperature pressure-vessel plate, steel number 1.7380, at the 310 MPa yield step and 480–630 MPa tensile at ≤16 mm, usually +NT. Whether the inquiry says EN 10028-2 10CrMo9-10, 1.7380 or 10CrMo9-10 2.25Cr-1Mo Vessel Plate, SHH STEEL as a global steel mill sourcing partner and steel manufacturer & exporter (mill-direct, China origin) supplies plate with 10CrMo9-10 chemistry, heat and product analysis when ordered, recorded +NT, and EN 10204 3.1 or 3.2 certification.

SHH STEEL supplies EN 10028-2 10CrMo9-10 2.25Cr-1Mo Vessel Plate to the USA, Mexico, South America, Europe, the Middle East, Africa and Asia for work that actually names this grade.

Contact SHH STEEL for mill rolling, stock inquiry, +NT, 3.2 inspection or a quotation.

EN 10028-2 10CrMo9-10 Steel Plate, 10CrMo9-10 2.25Cr-1Mo vessel plate, 1.7380, 10CrMo9-10 supplier, global steel mill sourcing partner SHH STEEL

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X