EN 10025-2 S355J2 UPN, UPE and PFC Steel Channels

EN 10025-2 S355J2 UPN, UPE and PFC steel channels are European structural channels with 355 MPa minimum yield in the first thickness band and a 27 J impact requirement at −20 °C. This page lists verified UPN, UPE and PFC sizes, ladle chemistry, carbon equivalent, and how flange thickness governs the test location.
Keywords
EN 10025-2 S355J2 UPN, UPE and PFC Steel Channels, EN 10025-2 S355J2 Steel Channel, S355J2 UPN, S355J2 UPE, S355J0 channel
Equivalent Grades:
S355JR channel (same shape, +20 °C); S355J0 (related quality, not a separate URL); S355K2 (40 J, not its own page); S355J2 H-beam; Q355D channel — comparisons only, not automatic substitutes.
Share:
General Description
Material Specification
Available Sizes of S355J2 UPN, UPE and PFC Steel Channels
Chemical Composition of S355J2 Steel Channel
Carbon Equivalent of S355J2 Steel Channel
Mechanical Properties of S355J2 Steel Channel
Delivery Conditions, Inspection and Identification
Weldability and Surface Condition of S355J2 Steel Channels
Shape Tolerances and Theoretical Mass
Applications and Service Limits
S355J2 Steel Channel Compared with Related Grades
Near-Equivalents: Not Automatic Substitutes
Sourcing S355J2 Steel Channels from SHH STEEL
FAQ
Conclusion

What are EN 10025-2 S355J2 UPN, UPE and PFC Steel Channels?

EN 10025-2 S355J2 steel channel is a hot-rolled European structural channel whose material grade is S355J2 under EN 10025-2 and whose shape, tolerances and theoretical mass are ordered to EN 10365, with tolerances to EN 10279. S355 is the 355 MPa minimum yield class in the thinnest tabulated thickness band, and J2 is the quality grade, which carries a longitudinal Charpy V-notch requirement of 27 J at −20 °C. The steel number is 1.0577. S355J2 is a fully killed steel with nitrogen-binding elements.

This page covers the rolled channel, not plate and not an H-section. The same grade in plate form is listed separately as EN 10025-2 S355J2 steel plate. The plate page is not a substitute data sheet for channels, and neither is EN 10025-2 S355J2 H-beam.

These bars are filed under steel channel profiles in the steel structural profiles category. They may be ordered as taper-flange UPN, parallel-flange UPE, or PFC. They are not American C or MC channels, Chinese GB/T 706 channels, or Japanese channels of a similar millimetre depth, and they are not EN 10025-5 S355J2W weathering sections. The +20 °C sister is EN 10025-2 S355JR steel channel. A S355J2 angle is a different product: see EN 10025-2 S355J2 steel angle.

S355J0 is a related quality at 0 °C and is noted here rather than given its own URL. S355K2 (40 J at −20 °C) is a different quality and is not given its own page. This product is not a JR substitute and not a pressure-vessel steel.

This page covers UPN, UPE and PFC Steel Channels in EN 10025-2 S355J2. UPN and UPE follow EN 10365, with tolerances to EN 10279; PFC sizes are the parallel-flange channel series used in British and related practice. These series are not interchangeable by depth alone.

Material, Dimensions and Tolerances for S355J2 Channels

Three documents should appear, separately, on the purchase order and on the inspection certificate:

  • the material standard and edition, EN 10025-2:2019 unless the order names another edition, and the grade S355J2 (steel number 1.0577);
  • the dimensional standard, EN 10365, with tolerances to EN 10279, with the channel designation;
  • the delivery condition, inspection document type, and any agreed options such as a galvanizing chemistry or a clause 7.2.5 CEV approach.

EN 10025-2 is the material standard. It is not a size table. Size, tolerance and theoretical mass come from the dimensional standard named on the order.

S355J2 Channel Sizes: UPN, UPE and PFC Series

The tables are the verified UPN (18 sizes, UPN 50 to UPN 400), UPE (14 sizes, UPE 80 to UPE 400) and PFC (16 sizes, PFC 100×50×10 to PFC 430×100×64) series. Numeric dimensions use EN 10365:2017 as the basis, with shape tolerances to EN 10279. EN 10365:2026 is the current dimensional edition; official 2026 size tables are not used here. The edition named on the order governs. Fillet and toe radii are not specified as delivery dimensions and are omitted. Theoretical mass uses the published section area. Other EN 10365 channel families are mentioned only when they are named on the order; they are not tabulated here.

Not every mill rolls every designation in S355J2. The order should name the sections actually required.

UPN series (taper-flange): UPN 50 to UPN 400 (18 sizes)

Swipe horizontally to view all dimensions.

Designation h (mm) b (mm) tw (mm) tf (mm) A (cm²) Mass (kg/m)
UPN 50 50 38 5 7 7.1 5.6
UPN 65 65 42 5.5 7.5 9 7.1
UPN 80 80 45 6 8 11 8.6
UPN 100 100 50 6 8.5 13.5 10.6
UPN 120 120 55 7 9 17 13.4
UPN 140 140 60 7 10 20.4 16
UPN 160 160 65 7.5 10.5 24 18.8
UPN 180 180 70 8 11 28 22
UPN 200 200 75 8.5 11.5 32.2 25.3
UPN 220 220 80 9 12.5 37.4 29.4
UPN 240 240 85 9.5 13 42.3 33.2
UPN 260 260 90 10 14 48.3 37.9
UPN 280 280 95 10 15 53.3 41.8
UPN 300 300 100 10 16 58.8 46.2
UPN 320 320 100 14 17.5 75.8 59.5
UPN 350 350 100 14 16 77.3 60.6
UPN 380 380 102 13.5 16 80.4 63.1
UPN 400 400 110 14 18 91.5 71.8

UPE series (parallel-flange): UPE 80 to UPE 400 (14 sizes)

Swipe horizontally to view all dimensions.

Designation h (mm) b (mm) tw (mm) tf (mm) A (cm²) Mass (kg/m)
UPE 80 80 50 4 7 10.1 7.9
UPE 100 100 55 4.5 7.5 12.5 9.8
UPE 120 120 60 5 8 15.4 12.1
UPE 140 140 65 5 9 18.4 14.5
UPE 160 160 70 5.5 9.5 21.7 17
UPE 180 180 75 5.5 10.5 25.1 19.7
UPE 200 200 80 6 11 29 22.8
UPE 220 220 85 6.5 12 33.9 26.6
UPE 240 240 90 7 12.5 38.5 30.2
UPE 270 270 95 7.5 13.5 44.8 35.2
UPE 300 300 100 9.5 15 56.6 44.4
UPE 330 330 105 11 16 67.8 53.2
UPE 360 360 110 12 17 77.9 61.2
UPE 400 400 115 13.5 18 91.9 72.2

PFC series: PFC 100×50×10 to PFC 430×100×64 (16 sizes)

Swipe horizontally to view all dimensions.

Designation h (mm) b (mm) tw (mm) tf (mm) A (cm²) Mass (kg/m)
PFC 100×50×10 100 50 5 8.5 13 10.2
PFC 125×65×15 125 65 5.5 9.5 18.8 14.8
PFC 150×75×18 150 75 5.5 10 22.8 17.9
PFC 150×90×24 150 90 6.5 12 30.4 23.9
PFC 180×75×20 180 75 6 10.5 25.9 20.3
PFC 180×90×26 180 90 6.5 12.5 33.2 26.1
PFC 200×75×23 200 75 6 12.5 29.9 23.4
PFC 200×90×30 200 90 7 14 37.9 29.7
PFC 230×75×26 230 75 6.5 12.5 32.7 25.7
PFC 230×90×32 230 90 7.5 14 41 32.2
PFC 260×75×28 260 75 7 12 35.1 27.6
PFC 260×90×35 260 90 8 14 44.4 34.8
PFC 300×90×41 300 90 9 15.5 52.7 41.4
PFC 300×100×46 300 100 9 16.5 58 45.5
PFC 380×100×54 380 100 9.5 17.5 68.7 54
PFC 430×100×64 430 100 11 19 82.1 64.4

S355J2 Chemical Composition for Channels (EN 10025-2 Ladle Analysis)

The figures below are ladle-analysis maxima from EN 10025-2:2019 for long products in S355J2. Product analysis, where required, follows the standard’s permitted deviations; those deviations are not retabulated here.

Element Maximum, ladle analysis (mass %) Notes for S355J2 channels
C 0.20 / 0.20 / 0.22 The three columns are t ≤ 16 mm, 16 mm < t ≤ 40 mm, and t > 40 mm. For 16 mm < t ≤ 40 mm, carbon shall not exceed 0.22% when t > 30 mm. For t > 100 mm, carbon is by agreement.
Si 0.55 —
Mn 1.60 —
P 0.030 Tighter than the JR phosphorus maximum.
S 0.030 Tighter than the JR sulphur maximum.
N — No tabulated nitrogen maximum. S355J2 is a fully killed steel containing nitrogen-binding elements in amounts sufficient to bind the available nitrogen (for example at least 0.02% Al); other such elements shall be reported.
Cu 0.55 —

For these channels the nominal thickness is ordinarily the flange thickness tf, not the overall depth and not the web.

S355J2 Carbon Equivalent for Channels

EN 10025-2:2019 publishes the following ladle-analysis CEV maxima for S355J2, using the IIW formula C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15.

Nominal thickness t (mm) Maximum CEV (ladle analysis, %)
t ≤ 30 0.45
30 < t ≤ 40 0.47
40 < t ≤ 140 0.47
t > 140 Not published here; CEV is agreed, not invented.

For these channels the nominal thickness is ordinarily the flange thickness tf, not the overall depth and not the web. Clause 7.2.5 of EN 10025-2:2019 may adjust the CEV approach for S355 when that option is invoked on the order; this page does not invent alternative limits. All 48 tabulated UPN, UPE and PFC flanges in this set are 19 mm or thinner, so they sit in the first or second mechanical band and in the first CEV band when the flange is the test location. Later bands are shown because a thicker special section could be agreed.

S355J2 Channel Mechanical Properties: Yield, Tensile and −20 °C Impact

The long-product tensile table for S355J2 is as follows. Tests on long products are normally longitudinal unless otherwise ordered. For these channels the nominal thickness is ordinarily the flange thickness tf, not the overall depth and not the web. For sections with nominal thickness greater than 100 mm, the mechanical values shall be agreed. No limits beyond 150 mm are given here.

Nominal thickness t (mm) Minimum yield ReH (MPa) Tensile strength Rm (MPa) Minimum elongation A, L0 = 5.65√S0 (%)
t ≤ 16 355 470–630 22
16 < t ≤ 40 345 470–630 22
40 < t ≤ 63 335 470–630 21
63 < t ≤ 80 325 470–630 20
80 < t ≤ 100 315 470–630 20
100 < t ≤ 150 295 450–600 18

When impact testing applies, S355J2 requires 27 J at −20 °C, longitudinally unless otherwise ordered. That is not the 40 J K2 requirement, and it is not the +20 °C JR test. All 48 tabulated UPN, UPE and PFC flanges in this set are 19 mm or thinner, so they sit in the first or second mechanical band and in the first CEV band when the flange is the test location. Later bands are shown because a thicker special section could be agreed.

Delivery Conditions, Inspection and Identification

S355J2 channels are commonly delivered in the as-rolled condition of EN 10025-2, as a fully killed steel. The inspection document should identify EN 10025-2 and its edition, the grade S355J2, the dimensional designation and edition, ladle analysis and CEV, nitrogen-binding elements as required, and mechanical results including the −20 °C impact test, against the thickness at the test location, ordinarily the flange. A plate, JR, or H-beam certificate does not, by itself, identify an S355J2 channel.

Weldability and Surface Condition of S355J2 Steel Channels

S355J2 is a weldable non-alloy structural steel. Preheat and consumable choice should use the certified CEV, the actual thickness and the joint design. Surface condition for these sections commonly follows EN 10163-3 class C, subclass 1, when that is the ordered specification; this page does not reproduce those millimetre limits.

EN 10279 Shape Tolerances and Theoretical Mass

Shape, straightness, length and theoretical mass belong to the ordered editions of EN 10365 and EN 10279. The size tables use EN 10365:2017 as the numeric basis. EN 10365:2026 is the current dimensional edition; the edition named on the order governs. Mass is the published theoretical figure from the section area. Millimetre tolerance tables are not reproduced here.

Applications and Service Limits

S355J2 channels are used in frames, bracing and fabrication where a 355 MPa yield class in the first thickness band and a −20 °C impact quality are required. They are not a silent substitute for a JR or J0 order, and they are not S355K2. A UPN is not a drop-in substitute for a UPE, a PFC, or a GB/T 706 or ASTM channel of similar depth.

S355J2 Steel Channel Compared with Related Grades

The comparisons below are an orientation only; they are not automatic substitutes.

Grade / designation Standard Relationship to S355J2 channel Caution
S355JR channel EN 10025-2; same dimensional series The same yield class with a +20 °C JR impact quality. A JR certificate is not a J2 certificate. See EN 10025-2 S355JR steel channel.
S355J0 EN 10025-2, 0 °C impact quality A related quality on this page, not a separate product URL. Do not treat a J2 certificate as a silent substitute for a J0 order, or the reverse.
S355K2 EN 10025-2, 40 J at −20 °C A tougher quality at the same temperature, not given its own page here. 27 J at −20 °C is not the K2 requirement.
S355J2 H-beam EN 10025-2; dimensions EN 10365 / EN 10034 The same material grade in an IPE, HEA or HEB section. An H-section certificate does not identify a channel. See EN 10025-2 S355J2 H-beam.
Q355D channel GB/T 1591 with dimensions GB/T 706 A Chinese −20 °C comparison at the 355 MPa class, on a taper-flange shape. A GB/T 706 channel is not a UPN. See GB/T 706 Q355B steel channel for the +20 °C Chinese channel; Q355D is a different quality.

Near-Equivalents: Not Automatic Substitutes

A near-equivalent is a starting point for a discussion, not a licence to swap certificates. EN 10025-2 S355J2 steel plate uses the same grade name but a different specimen orientation. EN 10025-2 S355JR steel plate and EN 10025-2 S355JR H-beam are +20 °C products. Do not confuse this grade with EN 10025-5 S355J2W.

Sourcing S355J2 Steel Channels from SHH STEEL

SHH STEEL supplies EN 10025-2 S355J2 steel channels against a named designation list, the material edition, the −20 °C impact requirement and the inspection document type. Enquiries should state UPN, UPE or PFC designations, cut lengths or mill lengths, any processing, and whether EN 10025-2 S355JR steel channel is acceptable on part of the list.

The size tables are the verified series, not a claim that every designation is rolled in every heat. Once the list is clear, a quotation can be prepared against the stated edition and certificate.

S355J2 UPN, UPE and PFC Steel Channel FAQs

Is S355J2 the same as S355JR or S355K2?
S355J2 shares the S355 yield class with JR and K2, but JR is tested at +20 °C and K2 requires 40 J at −20 °C. S355J2 requires 27 J at −20 °C. S355J0 is a related 0 °C quality noted on this page, not a separate URL.
Which thickness is used for yield, CEV and impact?
EN 10025-2 applies the bands to the nominal thickness of the part from which the test sample is taken. For these channels that is ordinarily the flange thickness, not the overall depth. All tabulated flanges in this set are 19 mm or thinner.
Is a UPN interchangeable with a UPE or a PFC of similar depth?
No. UPN is a taper-flange series, UPE is parallel-flange, and PFC is a different designation family. They are not interchangeable by depth alone.
Which standards should appear on the inspection document?
At least EN 10025-2 and its edition, the grade S355J2, the EN 10365 designation and the EN 10279 edition used for tolerances, ladle analysis and CEV, nitrogen-binding elements as required, and mechanical results including the −20 °C impact test, against the flange thickness unless the order relocates the specimen.

Request a Quotation for EN 10025-2 S355J2 UPN, UPE and PFC Steel Channels

EN 10025-2 S355J2 UPN, UPE and PFC steel channels are European structural channels with 355 MPa minimum yield in the first thickness band and a 27 J impact requirement at −20 °C. Nominate the designation (for example UPN 200, UPE 200 or a PFC size), EN 10025-2:2019 or the edition on the order, and the inspection document type. The size tables use EN 10365:2017 as the numeric basis; EN 10365:2026 is the current dimensional edition; the ordered edition governs. Send the size list, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X