EN 10025-2 S235JR UPN, UPE and PFC Steel Channels

EN 10025-2 S235JR UPN, UPE and PFC steel channels are non-alloy structural sections (1.0038) with 235 MPa minimum yield up to 16 mm and 27 J impact at +20 °C. Dimensions follow EN 10365, with tolerances under EN 10279. The ordered edition governs. SHH STEEL reviews grade, designation, edition and certificate requirements before quoting.
Keywords
EN 10025-2 S235JR UPN, UPE and PFC Steel Channels, EN 10025-2 S235JR Steel Channel, S235JR UPN, S235JR UPE, S235JR PFC
Equivalent Grades:
Near-equivalents only, not automatic substitutes: S355JR is a higher-strength grade, not the same section; Q235B; A36; SS400; S235J0 and S235J2 have colder impact qualities.
Share:
General Description
Material Specification
Available Sizes of S235JR UPN, UPE and PFC Steel Channels
Chemical Composition
Carbon equivalent
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why Source S235JR Steel Channels from SHH STEEL
FAQ
Conclusion

What are EN 10025-2 S235JR UPN, UPE and PFC Steel Channels?

EN 10025-2 S235JR steel channel is a hot-rolled taper-flange or parallel-flange channel in non-alloy structural steel S235JR (steel number 1.0038). The material standard is EN 10025-2. Dimensions and theoretical masses for these UPN, UPE and PFC sections are those of EN 10365. Shape, dimensional and mass tolerances are those of EN 10279, not of EN 10034, which applies to I and H sections. S marks a structural steel, 235 is the minimum yield strength in MPa up to 16 mm, and JR is the impact quality, 27 J at +20 °C.

UPN is the taper-flange European channel, for example UPN 200 or UPN 400. UPE is the parallel-flange European channel, for example UPE 200 or UPE 400. A UPE 200 is not a UPN 200: the flange width, web, flange thickness and mass are those of the UPE series. PFC designations such as PFC 200×90×30 are the British parallel-flange channel series collected in the same dimensional standard; they are not a UPE of the same depth. None of these is an HEA, HEB or IPE, and none is an American C or MC or a Chinese or Japanese channel of a similar millimetre depth.

These channels are filed under EN 10025-2 steel channel profiles in the steel channel profiles category of steel structural profiles. The same grade in plate form is listed separately as EN 10025-2 S235JR steel plate. Do not use that plate page as a channel data sheet, and do not copy plate chemistry defaults onto a UPN, UPE or PFC certificate.

S235JR channels are used for building frames, bracing, stair stringers and general industrial work when the specification names this non-alloy grade in a European or British channel. The grade is not a pressure-vessel or nuclear safety material, and it is not a substitute for S355JR when a 355 MPa yield is what the order requires.

This page covers UPN, UPE and PFC Steel Channels in EN 10025-2 S235JR. UPN and UPE follow EN 10365, with tolerances to EN 10279; PFC sizes are the parallel-flange channel series used in British and related practice. These series are not interchangeable by depth alone.

Material, Dimensions and Tolerances for S235JR Channels

The order and the inspection certificate should keep material, dimensions and tolerances distinct:

  • EN 10025-2 is the material standard. This article uses ladle chemistry, carbon-equivalent and tensile values for S235JR long products from EN 10025-2:2019. The edition named on the order governs acceptance.
  • EN 10365 is the dimensional standard for these hot-rolled channels. The size tables below are reference dimensions and theoretical masses for the standard UPN, UPE and PFC series, using EN 10365:2017 as the numeric basis. EN 10365:2026 is the current edition of that standard. The edition of EN 10365 named on the order governs dimensional acceptance.
  • EN 10279 is the tolerance standard for hot-rolled taper-flange and parallel-flange channels. This article uses EN 10279:2000 as the known edition. Do not apply EN 10034 I- and H-section tolerances to a UPN, UPE or PFC. The edition of EN 10279 named on the order governs dimensional and mass tolerance acceptance.

A documented special combination — for example S235JR on an ASTM C-shape, or a UPN certified to a different material standard — is only valid if every requirement of each named standard is met. Matching a nominal 200 mm depth is not a substitution.

S235JR Channel Sizes: UPN, UPE and PFC Series

The tables list designation, depth h, flange width b, web thickness tw, flange thickness tf, theoretical area and theoretical mass for the standard taper-flange (UPN) and parallel-flange (UPE and PFC) series under EN 10365:2017. Use them to identify and estimate, not as a rolling programme for S235JR. Mid-range UPN 100 to UPN 300 and UPE 100 to UPE 300 sizes are the usual enquiry core; UPN 50 to UPN 65, UPE 80 and the PFC 430 row should be confirmed size by size. Some heavier UPN and UPE rows are commonly supplied only by agreement.

UPN 200 is 200 mm deep with a 75 mm taper flange, an 8.5 mm web, an 11.5 mm flange and a 25.3 kg/m theoretical mass. UPE 200 is also 200 mm deep, but the flange is 80 mm and parallel, the web is 6.0 mm, the flange is 11.0 mm and the mass is 22.8 kg/m. PFC 200×90×30 is a 200 mm British parallel-flange channel, 90 mm wide, 29.7 kg/m; it is not UPE 200. The thickest flange in these tables is 19 mm on PFC 430×100×64, still in the 16–40 mm yield band and well below the 100 mm agreement threshold.

Taper-flange channels (UPN series)

18 sizes, from UPN 50 to UPN 400.

Swipe horizontally to view all dimensions.

Designation h (mm) b (mm) tw (mm) tf (mm) A (cm²) Mass (kg/m)
UPN 50 50 38 5 7 7.1 5.6
UPN 65 65 42 5.5 7.5 9 7.1
UPN 80 80 45 6 8 11 8.6
UPN 100 100 50 6 8.5 13.5 10.6
UPN 120 120 55 7 9 17 13.4
UPN 140 140 60 7 10 20.4 16
UPN 160 160 65 7.5 10.5 24 18.8
UPN 180 180 70 8 11 28 22
UPN 200 200 75 8.5 11.5 32.2 25.3
UPN 220 220 80 9 12.5 37.4 29.4
UPN 240 240 85 9.5 13 42.3 33.2
UPN 260 260 90 10 14 48.3 37.9
UPN 280 280 95 10 15 53.3 41.8
UPN 300 300 100 10 16 58.8 46.2
UPN 320 320 100 14 17.5 75.8 59.5
UPN 350 350 100 14 16 77.3 60.6
UPN 380 380 102 13.5 16 80.4 63.1
UPN 400 400 110 14 18 91.5 71.8

Parallel-flange channels (UPE series)

14 sizes, from UPE 80 to UPE 400.

Swipe horizontally to view all dimensions.

Designation h (mm) b (mm) tw (mm) tf (mm) A (cm²) Mass (kg/m)
UPE 80 80 50 4 7 10.1 7.9
UPE 100 100 55 4.5 7.5 12.5 9.8
UPE 120 120 60 5 8 15.4 12.1
UPE 140 140 65 5 9 18.4 14.5
UPE 160 160 70 5.5 9.5 21.7 17
UPE 180 180 75 5.5 10.5 25.1 19.7
UPE 200 200 80 6 11 29 22.8
UPE 220 220 85 6.5 12 33.9 26.6
UPE 240 240 90 7 12.5 38.5 30.2
UPE 270 270 95 7.5 13.5 44.8 35.2
UPE 300 300 100 9.5 15 56.6 44.4
UPE 330 330 105 11 16 67.8 53.2
UPE 360 360 110 12 17 77.9 61.2
UPE 400 400 115 13.5 18 91.9 72.2

Parallel-flange channels (PFC series)

16 sizes, from PFC 100×50×10 to PFC 430×100×64.

Swipe horizontally to view all dimensions.

Designation h (mm) b (mm) tw (mm) tf (mm) A (cm²) Mass (kg/m)
PFC 100×50×10 100 50 5 8.5 13 10.2
PFC 125×65×15 125 65 5.5 9.5 18.8 14.8
PFC 150×75×18 150 75 5.5 10 22.8 17.9
PFC 150×90×24 150 90 6.5 12 30.4 23.9
PFC 180×75×20 180 75 6 10.5 25.9 20.3
PFC 180×90×26 180 90 6.5 12.5 33.2 26.1
PFC 200×75×23 200 75 6 12.5 29.9 23.4
PFC 200×90×30 200 90 7 14 37.9 29.7
PFC 230×75×26 230 75 6.5 12.5 32.7 25.7
PFC 230×90×32 230 90 7.5 14 41 32.2
PFC 260×75×28 260 75 7 12 35.1 27.6
PFC 260×90×35 260 90 8 14 44.4 34.8
PFC 300×90×41 300 90 9 15.5 52.7 41.4
PFC 300×100×46 300 100 9 16.5 58 45.5
PFC 380×100×54 380 100 9.5 17.5 68.7 54
PFC 430×100×64 430 100 11 19 82.1 64.4

Other EN 10365 channel families, such as U or CH, can be reviewed when they are named on the enquiry. Complete tables for those series are not reproduced here. American C or MC, and Chinese or Japanese channel designations, belong to their own dimensional standards, not to these UPN, UPE or PFC rows.

S235JR Chemical Composition for Channels (EN 10025-2 Ladle Analysis)

The figures below are ladle-analysis maxima for S235JR long products in EN 10025-2:2019. They are limits, not typical heat results. Do not mix them with unofficial tables that borrow plate phosphorus figures or that give S235JR a silicon maximum it does not generally have. For these channels, apply the carbon band that matches the governing nominal thickness, ordinarily the flange thickness, not the overall depth of the channel.

Element Ladle analysis, max (mass %) Notes for S235JR long products, channels
C, t ≤ 16 mm 0.17 —
C, 16 mm < t ≤ 40 mm 0.17 —
C, t > 40 mm 0.20 For nominal thickness greater than 100 mm, carbon is subject to agreement.
Si No general maximum A dash in the source table. By agreement, silicon may be set at 0.14–0.25% and phosphorus at ≤0.035% for hot-dip galvanizing category B.
Mn 1.40 —
P 0.040 See the galvanizing agreement above. Do not paste a flat-product 0.035% default onto a channel order unless that is what was agreed.
S 0.040 —
N 0.012 The nitrogen maximum does not apply if total aluminium is at least 0.020%, or if sufficient other nitrogen-binding elements are present and reported.
Cu 0.55 —
Other added elements As reported If other elements are added, they shall be mentioned on the inspection document.

S235JR Carbon Equivalent for Channels

The carbon equivalent is calculated from the ladle analysis by CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Cu + Ni)/15. The EN 10025-2:2019 maxima for S235JR long products are:

Nominal thickness (mm) Maximum CEV (ladle analysis, %)
t ≤ 30 0.35
30 < t ≤ 40 0.35
40 < t ≤ 140 0.38

The third band applies to nominal thicknesses greater than 40 mm and not more than 140 mm. For thicknesses above 140 mm, a carbon-equivalent limit is not tabulated here and must be agreed and verified on the order; no value is invented for that range. Every standard UPN, UPE and PFC flange tabulated above is 19 mm or thinner, so those rows sit in the first band (0.35%). Clause 7.2.5 of EN 10025-2:2019 addresses special conditions for S275 and S355; those conditions are not applied to S235JR on this page.

S235JR Channel Mechanical Properties: Yield, Tensile and +20 °C Impact

Tensile properties of S235JR are thickness-dependent. The values below are from EN 10025-2:2019 for long products, with elongation based on L0 = 5.65√S0. For sections with nominal thickness greater than 100 mm, the mechanical values shall be agreed and verified on the order; the 100–150 mm row is the published long-product band and is not an invented extension. No mechanical limits beyond 150 mm are invented here.

Nominal thickness t (mm) Minimum yield ReH (MPa) Tensile strength Rm (MPa) Minimum elongation A (%)
t ≤ 16 235 360–510 26
16 < t ≤ 40 225 360–510 26
40 < t ≤ 63 215 360–510 25
63 < t ≤ 80 215 360–510 24
80 < t ≤ 100 215 360–510 24
100 < t ≤ 150 195 350–500 22

Apply the band that matches the governing nominal thickness, ordinarily the flange thickness of the channel, not the 200 mm or 400 mm depth. UPN 200 has an 11.5 mm flange, so the minimum yield is 235 MPa. UPN 400 has an 18 mm flange, so the minimum yield is 225 MPa, not 235 MPa.

Quality JR requires a Charpy V-notch absorbed energy of 27 J at +20 °C. For long products the test is normally longitudinal unless the order specifies otherwise. If the project needs 27 J at 0 °C or at −20 °C, the grade to nominate is S235J0 or S235J2, not S235JR.

Delivery Conditions, Inspection and Identification

S235JR channels are commonly supplied in the as-rolled condition. The inspection document should show EN 10025-2 and its edition, the grade S235JR (1.0038), the EN 10365 designation (UPN, UPE or PFC), the EN 10279 edition used for tolerances, the delivery condition, the heat number, ladle analysis, the carbon equivalent, and the tensile and +20 °C impact results. If a galvanizing chemistry has been agreed, that agreement belongs on the document as well. An S235JR H-section certificate, or a plate certificate, does not, by itself, identify a channel.

An EN 10204 type 3.1 document, or the mill’s equivalent inspection certificate, is the usual export request; type 3.2 or nominated third-party attendance can be added when the specification requires it. Identification follows the mill’s marking practice. Length is a matter for the rolling programme and the order, often in the region of 6–15 m or 12 m.

Weldability and Surface Condition of S235JR Channels

S235JR is a weldable non-alloy structural steel when thickness, joint design and hydrogen control are taken into account. The CEV table above is the starting point; the certificate values and a procedure suited to the flange thickness are the practical controls. This page does not prescribe a procedure or a preheat chart.

The as-rolled surface is often specified to EN 10163-3:2004, class C, subclass 1, when that condition is named on the order. Blast, paint or galvanizing is an order option. Cutting, punching, forming or coating can be reviewed when that specification is sent with the enquiry. They are not assumed for every size.

EN 10279 Shape Tolerances and Theoretical Mass

Dimensional, shape and mass tolerances for these UPN, UPE and PFC sections are those of EN 10279, not of EN 10025-2 and not of EN 10034. This article uses EN 10279:2000 as the known edition and does not reproduce the millimetre tolerance tables; acceptance is against the edition named on the order.

A delivered UPN 200 will measure close to the tabulated depth, flange and thicknesses within those tolerances, not as a set of exact advertised millimetres. Out-of-square and flange tilt matter for connections, especially on a taper-flange UPN. Settlement on theoretical or weighed mass should follow the contract.

Applications and Service Limits

S235JR steel channels are used where a 235 MPa non-alloy grade and a UPN, UPE or PFC section are specified:

  • Building and industrial frames, bracing, purlins, stair stringers and general fabrications whose specification names S235JR channel rather than S355JR or a non-European channel series.
  • Export packages that compare the grade with Q235B or with A36, provided each line keeps its own material standard and shape system.

It is not specified here for pressure equipment, for nuclear safety-related components, or for members that actually require S235J0, S235J2 or S355JR. Durability comes from the coating or fire-protection system, not from the S235JR designation.

S235JR Channel Compared with S355JR, Q235B and A36

S355JR H-beams share the same material standard family at a higher yield, but they are I or H sections, not UPN, UPE or PFC channels, and they use EN 10034 rather than EN 10279 for tolerances. Q235B and A36 are useful lower-strength comparisons only if chemistry, toughness and the shape standard are also satisfied. S235JR plate is the same grade in plate form, not a channel.

Dual certification requires every requirement of each named standard to be met on the delivered piece. An S235JR H-beam or angle page in this series will be linked here once it is published; those product URLs are not pre-linked.

Near-Equivalents: Not Automatic Substitutes

The comparisons below are for orientation. They are not a licence to substitute one grade or one shape for another on a contract or an inspection certificate.

Grade / designation Standard Relationship to S235JR channel Caution
S355JR section EN 10025-2; dimensions EN 10365; tolerances EN 10279 or EN 10034 according to the shape A higher-strength grade in the same material family. S355JR has its own chemistry, CEV and 355 MPa yield table. It is not an S235JR certificate. An H-section and a UPN or UPE of similar depth are different shapes.
Q235B / A36 / SS400 GB/T 700 or ASTM A36/A36M or JIS G 3101; different shape standards Common lower-strength comparisons in export enquiries. A Chinese, American or Japanese channel follows GB/T 706, ASTM A6/A6M or JIS G 3192, not the UPN, UPE or PFC designation. A shared 235 MPa or 36 ksi discussion is not a substitution method.
S235J0 / S235J2 channel EN 10025-2 The same 235 MPa class with a colder impact quality. JR is 27 J at +20 °C. J0 is 27 J at 0 °C and J2 is 27 J at −20 °C. Those qualities are not implied by an S235JR certificate.

Sourcing S235JR Steel Channels from SHH STEEL

SHH STEEL supplies S235JR steel channels as an export trading house, coordinating mill production and project procurement. For this product the useful work is to keep UPN, UPE and PFC designations from being mixed, to keep EN 10279 from being fulfilled with an EN 10034 I-section tolerance clause, to apply the yield band to the flange thickness rather than the channel depth, and to align the EN 10365 designation, the material edition and the inspection document before a rolling programme is committed.

Sections can be sourced from mills that SHH STEEL buys from, including Masteel, Rizhao Steel, Laiwu (Shandong Steel Laiwu) and Tung Ho Steel, among others when the programme matches the order. Those mills do not each roll every UPN, UPE or PFC size in S235JR. Mid-range UPN and UPE sizes are the usual core; light UPN 50–65 rows, UPE 80 and the PFC 430 row are confirmed per line.

The same enquiry can also cover I or H sections, angles, or Chinese, Japanese or American designations, provided each line states its material standard, shape standard and size. If cutting, punching, forming or a coating system is required, include that specification for review. Export packing and container loading can be arranged to the packing list agreed for the shipment.

S235JR UPN, UPE and PFC Steel Channel FAQs

Is a UPE the same as a UPN of the same depth?
No. UPN is a taper-flange channel; UPE is a parallel-flange channel. UPE 200 is not UPN 200: the flange width, web, flange thickness and mass are different. PFC is a further parallel-flange series and is not a UPE of the same depth.
Does the 235 MPa yield apply to every S235JR channel in the tables?
No. 235 MPa is the minimum yield for nominal thickness up to 16 mm. For these channels the governing thickness is ordinarily the flange, not the overall depth. UPN 200 (tf 11.5 mm) is in the 235 MPa band; UPN 400 (tf 18 mm) is in the 225 MPa band.
Do EN 10034 tolerances apply to these channels?
No. EN 10034 covers I and H sections. Dimensional, shape and mass tolerances for UPN, UPE and PFC channels are those of EN 10279. This article uses EN 10279:2000 as the known edition; the edition named on the order governs.
Does this page use EN 10365:2026 dimensions?
The size tables use EN 10365:2017 as the numeric basis. EN 10365:2026 is the current edition of that standard. The edition named on the order governs acceptance.
Which standards should appear on the inspection document?
At least EN 10025-2 and its edition, the grade S235JR (1.0038), the UPN, UPE or PFC designation to EN 10365, the EN 10279 edition used for tolerances, the delivery condition, ladle analysis, the carbon equivalent, tensile results by thickness, and the +20 °C impact result.

Request a Quotation for EN 10025-2 S235JR UPN, UPE and PFC Steel Channels

EN 10025-2 S235JR UPN, UPE and PFC steel channels are non-alloy UPN, UPE or PFC section (1.0038) with 235 MPa minimum yield up to 16 mm. Nominate the designation to EN 10365, the tolerances to EN 10279, and the material to EN 10025-2:2019 (or the editions on the order). The tables use the EN 10365:2017 numeric basis and are reference dimensions, not a rolling list. Send the designation list, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *