EN 10025-2 S355JR UPN, UPE and PFC Steel Channels
What are EN 10025-2 S355JR UPN, UPE and PFC Steel Channels?
EN 10025-2 S355JR steel channel is a hot-rolled taper-flange or parallel-flange channel in non-alloy structural steel S355JR (steel number 1.0045). The material standard is EN 10025-2. Dimensions and theoretical masses for these UPN, UPE and PFC sections are those of EN 10365. Shape, dimensional and mass tolerances are those of EN 10279, not of EN 10034, which applies to I and H sections. S marks a structural steel, 355 is the minimum yield strength in MPa up to 16 mm, and JR is the impact quality, 27 J at +20 °C. That impact temperature is the same as for S235JR; the difference that matters on this page is the higher yield and tensile class, together with the S355JR chemistry and carbon-equivalent table.
UPN is the taper-flange European channel, for example UPN 200 or UPN 400. UPE is the parallel-flange European channel, for example UPE 200 or UPE 400. A UPE 200 is not a UPN 200: the flange width, web, flange thickness and mass are those of the UPE series. PFC designations such as PFC 200×90×30 are the British parallel-flange channel series collected in the same dimensional standard; they are not a UPE of the same depth. None of these is an HEA, HEB or IPE, and none is an American C or MC or a Chinese or Japanese channel of a similar millimetre depth.
These channels are filed under EN 10025-2 steel channel profiles in the steel channel profiles category of steel structural profiles. The same grade as a rolled I or H section is listed separately as EN 10025-2 S355JR H-beam. The same grade in plate form is listed as EN 10025-2 S355JR steel plate. Do not use either of those pages as a channel data sheet, and do not copy plate chemistry defaults, or I-section tolerances from EN 10034, onto a UPN, UPE or PFC certificate.
S355JR channels are used for building frames, bracing, stair stringers and general industrial work when the specification names this 355 MPa non-alloy grade in a European or British channel. The grade is not a pressure-vessel or nuclear safety material, and it is not a substitute for S355J0 or S355J2 when a colder impact quality is what the order requires, nor for S235JR when a 235 MPa certificate is what was specified.
This page covers UPN, UPE and PFC Steel Channels in EN 10025-2 S355JR. UPN and UPE follow EN 10365, with tolerances to EN 10279; PFC sizes are the parallel-flange channel series used in British and related practice. These series are not interchangeable by depth alone.
Material, Dimensions and Tolerances for S355JR Channels
The order and the inspection certificate should keep material, dimensions and tolerances distinct:
- EN 10025-2 is the material standard. This article uses ladle chemistry, carbon-equivalent and tensile values for S355JR long products from EN 10025-2:2019. The edition named on the order governs acceptance.
- EN 10365 is the dimensional standard for these hot-rolled channels. The size tables below are reference dimensions and theoretical masses for the standard UPN, UPE and PFC series, using EN 10365:2017 as the numeric basis. EN 10365:2026 is the current edition of that standard. The edition of EN 10365 named on the order governs dimensional acceptance.
- EN 10279 is the tolerance standard for hot-rolled taper-flange and parallel-flange channels. This article uses EN 10279:2000 as the known edition. Do not apply EN 10034 I- and H-section tolerances to a UPN, UPE or PFC. The edition of EN 10279 named on the order governs dimensional and mass tolerance acceptance.
A documented special combination — for example S355JR on an ASTM C-shape, or a UPN certified to a different material standard — is only valid if every requirement of each named standard is met. Matching a nominal 200 mm depth is not a substitution.
S355JR Channel Sizes: UPN, UPE and PFC Series
The tables list designation, depth h, flange width b, web thickness tw, flange thickness tf, theoretical area and theoretical mass for the standard taper-flange (UPN) and parallel-flange (UPE and PFC) series under EN 10365:2017. Use them to identify and estimate, not as a rolling programme for S355JR. Mid-range UPN 100 to UPN 300 and UPE 100 to UPE 300 sizes are the usual enquiry core; UPN 50 to UPN 65, UPE 80 and the PFC 430 row should be confirmed size by size. Some heavier UPN and UPE rows are commonly supplied only by agreement.
UPN 200 is 200 mm deep with a 75 mm taper flange, an 8.5 mm web, an 11.5 mm flange and a 25.3 kg/m theoretical mass, so the 355 MPa yield band applies. UPE 200 is also 200 mm deep, but the flange is 80 mm and parallel, the web is 6.0 mm, the flange is 11.0 mm and the mass is 22.8 kg/m. PFC 200×90×30 is a 200 mm British parallel-flange channel, 90 mm wide, 29.7 kg/m; it is not UPE 200. UPN 400 has an 18 mm flange, so the minimum yield is 345 MPa, not 355 MPa. The thickest flange in these tables is 19 mm on PFC 430×100×64, still in the 16–40 mm yield band and well below the 100 mm agreement threshold.
Taper-flange channels (UPN series)
18 sizes, from UPN 50 to UPN 400.
Swipe horizontally to view all dimensions.
Parallel-flange channels (UPE series)
14 sizes, from UPE 80 to UPE 400.
Swipe horizontally to view all dimensions.
Parallel-flange channels (PFC series)
16 sizes, from PFC 100×50×10 to PFC 430×100×64.
Swipe horizontally to view all dimensions.
S355JR Chemical Composition for Channels (EN 10025-2 Ladle Analysis)
The figures below are ladle-analysis maxima for S355JR long products in EN 10025-2:2019. They should not be copied from S355J0 or S355J2, which use a 0.22% carbon maximum for nominal thickness greater than 30 mm, or from a plate table that uses different phosphorus defaults. They are limits, not typical heat results. For these channels the governing thickness is ordinarily the flange thickness, not the overall depth.
S355JR Carbon Equivalent for Channels
Carbon equivalent (CEV) maxima for S355JR long products follow the table below. The third band is 40 mm < t ≤ 140 mm. A CEV limit between 140 mm and 150 mm is not published here and must be agreed, not assumed. When EN 10025-2:2019 clause 7.2.5 is invoked on the order for S355, the CEV approach may be adjusted under that option; review the clause as written rather than inventing a substitute table. All of the tabulated UPN, UPE and PFC flanges sit in the first CEV band; the later bands are shown because a thicker special section could be agreed.
S355JR Channel Mechanical Properties: Yield, Tensile and +20 °C Impact
Tensile properties of S355JR long products follow EN 10025-2:2019, with elongation based on L0 = 5.65√S0. For these channels the nominal thickness is ordinarily the flange thickness tf. UPN 200 (tf 11.5 mm) remains in the 355 MPa band; UPN 400 (tf 18 mm) and PFC 430×100×64 (tf 19 mm) are in the 345 MPa band. For sections with nominal thickness greater than 100 mm, the mechanical values shall be agreed; the 100–150 mm row is the published long-product band, not an invented extension. No mechanical limits beyond 150 mm are given here.
The JR impact requirement is 27 J at +20 °C, longitudinal unless the order states otherwise. Sharing that test temperature with S235JR does not make the two grades interchangeable on yield, tensile strength, chemistry or carbon equivalent.
Delivery Conditions, Inspection and Identification
S355JR channels are commonly supplied in the as-rolled condition. The inspection document should show EN 10025-2 and its edition, the grade S355JR (1.0045), the EN 10365 designation (UPN, UPE or PFC), the EN 10279 edition used for tolerances, the delivery condition, the heat number, ladle analysis, the carbon equivalent, and the tensile and +20 °C impact results. If a galvanizing chemistry has been agreed, or if clause 7.2.5 has been invoked, that agreement belongs on the document as well. An S355JR H-section certificate, or a plate certificate, does not, by itself, identify a channel.
An EN 10204 type 3.1 document, or the mill’s equivalent inspection certificate, is the usual export request; type 3.2 or nominated third-party attendance can be added when the specification requires it. Identification follows the mill’s marking practice. Length is a matter for the rolling programme and the order, often in the region of 6–15 m or 12 m.
Weldability and Surface Condition of S355JR Channels
S355JR is a weldable non-alloy structural steel when thickness, joint design and hydrogen control are taken into account. The CEV table above is the starting point; the certificate values and a procedure suited to the flange thickness are the practical controls. This page does not prescribe a procedure or a preheat chart.
The as-rolled surface is often specified to EN 10163-3:2004, class C, subclass 1, when that condition is named on the order. Blast, paint or galvanizing is an order option. Cutting, punching, forming or coating can be reviewed when that specification is sent with the enquiry. They are not assumed for every size.
EN 10279 Shape Tolerances and Theoretical Mass
Dimensional, shape and mass tolerances for these UPN, UPE and PFC sections are those of EN 10279, not of EN 10025-2 and not of EN 10034. This article uses EN 10279:2000 as the known edition and does not reproduce the millimetre tolerance tables; acceptance is against the edition named on the order.
A delivered UPN 200 will measure close to the tabulated depth, flange and thicknesses within those tolerances, not as a set of exact advertised millimetres. Out-of-square and flange tilt matter for connections, especially on a taper-flange UPN. Settlement on theoretical or weighed mass should follow the contract.
Applications and Service Limits
S355JR steel channels are used where a 355 MPa non-alloy grade and a UPN, UPE or PFC section are specified:
- Building and industrial frames, bracing, purlins, stair stringers and general fabrications whose specification names S355JR channel rather than S235JR or a non-European channel series.
- Export packages that compare the grade with Q355B or with A572 Grade 50 plate, provided each line keeps its own material standard and shape system.
It is not specified here for pressure equipment, for nuclear safety-related components, or for members that actually require S355J0, S355J2 or a defined lower-temperature quality. Durability comes from the coating or fire-protection system, not from the S355JR designation.
S355JR Channel Compared with S235JR, Q355B and A572 Grade 50
S355JR H-beams share the same material grade at the same yield class, but they are I or H sections, not UPN, UPE or PFC channels, and they use EN 10034 rather than EN 10279 for tolerances. Q355B H-beams and A572 Grade 50 plate are useful 345–355 MPa comparisons only if chemistry, toughness and the shape standard are also satisfied. S355JR plate is the same grade in plate form, not a channel. S235JR plate illustrates the lower-strength JR quality in this family; it is not a channel data sheet and it is not an S355JR certificate.
Dual certification requires every requirement of each named standard to be met on the delivered piece. An S355JR angle page, or an S235JR channel page, in this series will be linked here once it is published; those product URLs are not pre-linked.
Near-Equivalents: Not Automatic Substitutes
The comparisons below are for orientation. They are not a licence to substitute one grade or one shape for another on a contract or an inspection certificate.
Sourcing S355JR Steel Channels from SHH STEEL
SHH STEEL supplies S355JR steel channels as an export trading house, coordinating mill production and project procurement. For this product the useful work is to keep UPN, UPE and PFC designations from being mixed, to keep EN 10279 from being fulfilled with an EN 10034 I-section tolerance clause, to apply the yield band to the flange thickness rather than the channel depth, and to align the EN 10365 designation, the material edition and the inspection document before a rolling programme is committed.
Sections can be sourced from mills that SHH STEEL buys from, including Masteel, Rizhao Steel, Laiwu (Shandong Steel Laiwu) and Tung Ho Steel, among others when the programme matches the order. Those mills do not each roll every UPN, UPE or PFC size in S355JR. Mid-range UPN and UPE sizes are the usual core; light UPN 50–65 rows, UPE 80 and the PFC 430 row are confirmed per line.
The same enquiry can also cover I or H sections, angles, or Chinese, Japanese or American designations, provided each line states its material standard, shape standard and size. If cutting, punching, forming or a coating system is required, include that specification for review. Export packing and container loading can be arranged to the packing list agreed for the shipment.
S355JR UPN, UPE and PFC Steel Channel FAQs
-
Is a UPE the same as a UPN of the same depth?
- No. UPN is a taper-flange channel; UPE is a parallel-flange channel. UPE 200 is not UPN 200: the flange width, web, flange thickness and mass are different. PFC is a further parallel-flange series and is not a UPE of the same depth.
-
Does the 355 MPa yield apply to every S355JR channel in the tables?
- No. 355 MPa is the minimum yield for nominal thickness up to 16 mm. For these channels the governing thickness is ordinarily the flange, not the overall depth. UPN 200 (tf 11.5 mm) is in the 355 MPa band; UPN 400 (tf 18 mm) is in the 345 MPa band.
-
Do EN 10034 tolerances apply to these channels?
- No. EN 10034 covers I and H sections. Dimensional, shape and mass tolerances for UPN, UPE and PFC channels are those of EN 10279. This article uses EN 10279:2000 as the known edition; the edition named on the order governs.
-
Does this page use EN 10365:2026 dimensions?
- The size tables use EN 10365:2017 as the numeric basis. EN 10365:2026 is the current edition of that standard. The edition named on the order governs acceptance.
-
Which standards should appear on the inspection document?
- At least EN 10025-2 and its edition, the grade S355JR (1.0045), the UPN, UPE or PFC designation to EN 10365, the EN 10279 edition used for tolerances, the delivery condition, ladle analysis, the carbon equivalent, tensile results by thickness, and the +20 °C impact result.
Request a Quotation for EN 10025-2 S355JR UPN, UPE and PFC Steel Channels
EN 10025-2 S355JR UPN, UPE and PFC steel channels are non-alloy UPN, UPE or PFC section (1.0045) with 355 MPa minimum yield up to 16 mm. Nominate the designation to EN 10365, the tolerances to EN 10279, and the material to EN 10025-2:2019 (or the editions on the order). The tables use the EN 10365:2017 numeric basis and are reference dimensions, not a rolling list. Send the designation list, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.