EN 10025-2 Steel Structural Profiles
SHH STEEL supplies EN 10025-2 non-alloy structural steel channels, in grades such as S235, S275, and S355 with JR, J0, or J2 qualities as specified (for example S355JR). Dimensions typically follow EN 10365 UPN and UPE series, with tolerances to EN 10279, using designations such as UPN 160, UPN 200, UPN 300, and UPE 200. Parallel-flange channels to other practices (for example PFC) may be furnished in the same grades when specified. UPN, UPE, and ASTM C channels are not equivalent by depth alone. Sizes and certificates are confirmed per inquiry.
-
EN 10025-2 S355J2 UPN, UPE and PFC Steel Channels
EN 10025-2 S355J2 UPN, UPE and PFC steel channels are European structural channels with 355 MPa minimum yield in the first thickness band and a 27 J impact requirement at −20 °C. This page lists verified UPN, UPE and PFC sizes, ladle chemistry, carbon equivalent, and how flange thickness governs the test location.View More -
EN 10025-2 S275JR UPN, UPE and PFC Steel Channels
EN 10025-2 S275JR UPN, UPE and PFC steel channels are European structural channels with 275 MPa minimum yield in the first thickness band and a 27 J impact requirement at +20 °C. This page lists verified UPN, UPE and PFC sizes, ladle chemistry, carbon equivalent, and how flange thickness governs the test location.View More -
EN 10025-2 S355JR UPN, UPE and PFC Steel Channels
EN 10025-2 S355JR UPN, UPE and PFC steel channels are non-alloy structural sections (1.0045) with 355 MPa minimum yield up to 16 mm and 27 J impact at +20 °C. Dimensions follow EN 10365, with tolerances under EN 10279. The ordered edition governs. SHH STEEL reviews grade, designation, edition and certificate requirements before quoting.View More -
EN 10025-2 S235JR UPN, UPE and PFC Steel Channels
EN 10025-2 S235JR UPN, UPE and PFC steel channels are non-alloy structural sections (1.0038) with 235 MPa minimum yield up to 16 mm and 27 J impact at +20 °C. Dimensions follow EN 10365, with tolerances under EN 10279. The ordered edition governs. SHH STEEL reviews grade, designation, edition and certificate requirements before quoting.View More
C Channels and U Channels
SHH STEEL supplies hot-rolled steel channel profiles for frames, bracing, and equipment support. Material is specified to the project standard—for example ASTM A36, A572, or A529; ASME SA-36; EN 10025-2; GB/T 700 or GB/T 1591; JIS G 3101; ISO 630-1; or GOST 8240 practice. Dimensional series are stated separately and may include ASTM A6 C and MC channels (for example C6×8.2, C8×11.5, or C12×20.7); EN 10365 UPN and UPE (for example UPN 200 or UPE 200) with tolerances to EN 10279; GB/T 706 channels such as 16a and 20a; and JIS G 3192 channels such as 150×75 or 200×80. A grade such as ASTM A36 may be furnished as UPN or UPE when so specified and certified; C, UPN, and GB/JIS designations are not interchangeable by depth alone. Sizes and certificates are confirmed per inquiry.
Customers typically search this category as C channel, U channel, steel channel, C channel steel or U channel steel, and by series names such as MC channel, UPN, UPE, PFC (parallel flange channel) and taper flange channel. This category covers ASTM A6 C and MC channels, EN 10365 UPN and UPE, British-practice PFC, GB/T 706 channels and JIS G 3192 channels, furnished to the material standard named on the order. C, MC, UPN, UPE, PFC, GB/T 706 and JIS designations are not interchangeable by depth alone.