EN 10025-2 S355J2 H-Beam
What is EN 10025-2 S355J2 H-Beam?
EN 10025-2 S355J2 H-beam is a hot-rolled I or H section in non-alloy structural steel S355J2 (steel number 1.0577). Material is specified to EN 10025-2, dimensions to EN 10365, and tolerances to EN 10034. The yield class is the same 355 MPa used for S355JR and S355J0, but J2 is the quality that requires 27 J at −20 °C. It is also supplied as a fully killed steel, with tighter phosphorus and sulphur maxima (0.030%) than either JR or J0.
This page covers the rolled section, not plate. The same EN 10025-2 grade in plate form is listed separately as EN 10025-2 S355J2 steel plate. Long-product tests are normally longitudinal unless the order says otherwise. S355J2 is not S355K2, which keeps the −20 °C test temperature but requires 40 J rather than 27 J, and it is not the EN 10025-5 weathering grades S355J2W or S355J2WP.
These beams are filed under EN 10025-2 steel beam profiles in the steel beam profiles category of steel structural profiles. HE A, HE B and IPE are the usual series; HEM, UB or UC may be furnished when specified and certified. The published S355JR H-beam page is the +20 °C quality in this yield class, not a data sheet for J2.
S355J2 is widely specified for building and industrial frames, and for other structural work, when a 355 MPa European grade and a −20 °C impact quality are required. It is not a weathering steel, not a pressure-vessel or nuclear safety material, and not a substitute for K2 when 40 J is what the specification names.
Material, Dimensions and Tolerances for S355J2 Sections
Three documents belong on the order and on the inspection certificate, each for its own job:
- EN 10025-2 is the material standard. This article uses ladle-analysis, carbon-equivalent and tensile values for S355J2 long products from EN 10025-2:2019. The edition named on the order governs acceptance. The fully killed, nitrogen-binding requirement is part of this grade, not an optional extra.
- EN 10365 is the dimensional standard for hot-rolled I and H sections. The size tables below are reference dimensions and theoretical masses for the standard HE A, HE B and IPE series, not a mill rolling list.
- EN 10034 is the tolerance standard. Surface condition is commonly specified to EN 10163-3; the class should be confirmed when a tighter finish is required.
A special combination of this grade with a non-European shape, or of an HEA with a different material standard, is valid only when it is documented against every named requirement. A shared nominal depth is not a substitution method.
S355J2 H-Beam Sizes: HEA, HEB, IPE, UB and UC Reference Tables
The tables below give designation, depth, width, thicknesses, root radius, area and theoretical mass for the standard HE A, HE B and IPE series, consistent with EN 10365. They are for identification and estimating. Availability of S355J2 is a mill-programme question, especially for the lightest IPE rows and for HE 900–1000.
Because J2 is often specified on heavier framing as well as on ordinary beams, the thickness band matters as much as the series name. HE 160 A has a 9 mm flange and stays at 355 MPa. HE 300 B has a 19 mm flange, so the minimum yield is 345 MPa. IPE 400, at 400 × 180 × 8.6 × 13.5 mm, remains in the thinner yield band and should not be read as a 400 mm square H-section.
For a governing thickness greater than 100 mm, mechanical values shall be agreed and verified on the order. The 100–150 mm tensile row is the published long-product band; no mechanical limits beyond 150 mm are given here.
HE A (HEA) series
Wide-flange European H-sections, 24 sizes from HE 100 A to HE 1000 A.
Swipe horizontally to view all dimensions.
HE B (HEB) series
Heavier-flange European H-sections, 24 sizes from HE 100 B to HE 1000 B.
Swipe horizontally to view all dimensions.
IPE series
Parallel-flange I-beams, 18 sizes from IPE 80 to IPE 600.
Swipe horizontally to view all dimensions.
Typical mill-programme universal beams (UB) and universal columns (UC) commonly supplied in S355J2 are tabulated below. Designations follow the established EN 10365 / British universal naming (for example UB 610 × 229 × 125). The rows are a commonly supplied standard mill series, not a claim that every official EN 10365:2017 row has been reproduced or that any one mill rolls the full list in S355J2. Historic or additional depths can be reviewed on enquiry; they are not silently added to these tables. Masses are theoretical catalogue figures for identification, estimating and drawing work.
Universal beams (UB)
Swipe horizontally to view all dimensions.
Universal columns (UC)
Swipe horizontally to view all dimensions.
HEM can still be reviewed when it is named on the enquiry; a complete HEM table is not reproduced here. HW/HM/HN belong to GB/T 11263; W-shapes belong to ASTM A572 or ASTM A36 practice, not to these HEA, HEB, IPE, UB or UC rows.
S355J2 Chemical Composition (EN 10025-2 Ladle Analysis)
The figures below are ladle-analysis maxima for S355J2 long products in EN 10025-2:2019. In addition to the tighter phosphorus and sulphur, J2 is defined as a fully killed steel with nitrogen-binding elements sufficient to bind the available nitrogen. That deoxidation practice, not a tabulated nitrogen maximum, is what belongs on the inspection document.
S355J2 Carbon Equivalent
The carbon equivalent is calculated from the ladle analysis by CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Cu + Ni)/15. The EN 10025-2:2019 maxima for S355J2 long products are:
The third band applies to nominal thicknesses greater than 40 mm and not more than 140 mm. For thicknesses above 140 mm, a carbon-equivalent limit is not tabulated here and must be agreed and verified on the order; no value is invented for that range. Clause 7.2.5 of EN 10025-2:2019 addresses special conditions for S355. If that clause is to be used, it should be named on the order; this page does not invent a raised CEV figure from it.
S355J2 Mechanical Properties: Yield, Tensile and −20 °C Impact
Tensile properties of S355J2 follow the S355 long-product table in EN 10025-2:2019, with elongation based on L0 = 5.65√S0. For sections with nominal thickness greater than 100 mm, the mechanical values shall be agreed and verified on the order; the 100–150 mm row is the published long-product band and is not an invented extension. No mechanical limits beyond 150 mm are given here. Plate sampling is covered on S355J2 steel plate, not by this table.
The J2 quality requires 27 J at −20 °C. For long products the Charpy test is normally longitudinal unless the order specifies otherwise. That energy and temperature should not be confused with S355K2, which is also tested at −20 °C but at 40 J, or with S355J0 at 0 °C. A JR or J0 certificate does not demonstrate the J2 test.
HE 160 A, with a 9 mm flange, remains at 355 MPa. HE 300 B, with a 19 mm flange, is 345 MPa.
Delivery Conditions, Inspection and Identification
S355J2 sections are commonly supplied as-rolled and shall be fully killed, with the nitrogen-binding practice reported. The inspection document should show EN 10025-2 and its edition, the grade S355J2 (1.0577), the EN 10365 size designation, the EN 10034 edition used for tolerances, the delivery condition, the heat number, ladle analysis, evidence of the killed / nitrogen-binding practice (for example total aluminium), the carbon equivalent, the tensile results, and the −20 °C impact result.
An EN 10204 type 3.1 document is the usual export request; type 3.2 or nominated third-party attendance can be added when the specification requires it. Identification follows the mill’s marking practice. Length is a matter for the rolling programme and the order, often in the region of 6–15 m.
Weldability and Surface Condition of S355J2 H-Beams
S355J2 is a weldable, fully killed non-alloy structural steel when thickness, joint design and hydrogen control are taken into account. The CEV table, including the step to 0.47% above 30 mm, is the starting point. The certificate values and a procedure suited to the thickness are the practical controls. This page does not prescribe a procedure or a preheat chart.
The as-rolled surface is mill scale. Blast, paint or galvanizing is an order option. Silicon is limited to 0.55%, which still needs to be reviewed against a galvanizing specification if a coating is planned. Surface quality for sections is commonly specified to EN 10163-3.
Cutting, weld-end preparation, forming or coating can be reviewed when the specification is sent with the enquiry. They are not assumed for every size.
EN 10034 Shape Tolerances and Theoretical Mass
Dimensional and mass tolerances for these I and H sections are those of EN 10034, not of EN 10025-2. This article does not reproduce the millimetre tolerance tables; acceptance is against the edition named on the order.
A delivered HE 300 B will measure close to 300 × 300 × 11 × 19 mm within those tolerances, not as a set of exact advertised millimetres. Out-of-square and web off-centre matter for end-plate connections. Settlement on theoretical or weighed mass should follow the contract.
Applications and Service Limits
S355J2 H-beams are used where a 355 MPa European grade and a −20 °C, 27 J impact quality are specified:
- Building and industrial frames whose specification names S355J2, a common European default, rather than JR or J0.
- Members that need a −20 °C test at 27 J, but do not require the 40 J of S355K2 or a weathering grade.
- Export packages that compare the grade with Q355D or with a 50 ksi American shape, provided each line keeps its own standard and shape system.
It is not specified here for pressure equipment, for nuclear safety-related components, or for structures that actually require EN 10025-5 weathering steel or the K2 impact energy. Durability comes from the coating or fire-protection system, not from the J2 letter.
S355J2 Compared with S355JR, S355J0, S355K2 and Q355D
S355J2, S355JR and S355J0 share the 355 MPa class and the usual European I and H series, but J2 is the fully killed, −20 °C, 0.030% P and S quality. JR cannot be “used as J2” on a warmer test, and J0 stops at 0 °C. S355K2 keeps the −20 °C temperature and raises the required energy to 40 J; a J2 result of 27 J does not meet K2.
EN 10025-5 S355J2W is a weathering grade, not this product. Q355D and ASTM A572 Grade 50 are useful comparisons only when the impact test, chemistry and shape standard are also satisfied. Dual certification requires every requirement of each named standard to be met on the delivered piece.
Near-Equivalents: Not Automatic Substitutes
The comparisons below are for orientation. They are not a licence to substitute one grade for another on a contract or an inspection certificate.
Sister beam pages in this series (S235JR, S275JR, S355J0) will be linked here once they are published. Until then, use the live category and plate links above, and the published S355JR H-beam page for the +20 °C quality in this yield class.
Sourcing S355J2 H-Beams from SHH STEEL
SHH STEEL supplies S355J2 H-beams as an export trading house, coordinating mill production and project procurement. For this grade the useful work is to keep the −20 °C, 27 J test and the fully killed, 0.030% P and S chemistry from being fulfilled with a JR or J0 heat, to distinguish J2 from K2 and from EN 10025-5 weathering steels, and to align the EN 10365 designation, EN 10034 tolerances and the inspection document before a rolling programme is committed.
Sections can be sourced from mills that SHH STEEL buys from, including Masteel, Rizhao Steel, Laiwu (Shandong Steel Laiwu) and Tung Ho Steel, among others when the programme matches the order. Those mills do not each roll every HEA, HEB or IPE size in S355J2. Mid-range sizes are the usual core; heavier HE rows and uncommon IPE variants are confirmed per line.
The same enquiry can also cover Chinese, American or Japanese designations, provided each line states its material standard, shape standard and size. If cutting, weld-end preparation, forming or a coating system is required, include that specification for review. Export packing and container loading can be arranged to the packing list agreed for the shipment.
S355J2 H-Beam FAQs
-
Is S355J2 the same as S355JR or S355J0?
- No. All three are 355 MPa EN 10025-2 grades and may be rolled as the same section series, but J2 is tested at −20 °C, is fully killed, and uses 0.030% phosphorus and sulphur. JR is +20 °C with a looser chemistry table; J0 is 0 °C with 0.035% P and S. A warmer-quality certificate does not demonstrate J2.
-
Is S355J2 the same as S355K2?
- No. Both are tested at −20 °C, but K2 requires 40 J rather than 27 J. A J2 result does not meet the K2 energy requirement.
-
What does “fully killed” mean on the certificate?
- S355J2 is supplied as a fully killed steel with nitrogen-binding elements in amounts sufficient to bind the available nitrogen, for example a minimum of 0.020% total aluminium. If other nitrogen-binding elements are used, they shall be reported. There is no tabulated nitrogen maximum for this quality in the long-product table.
-
Is the minimum yield always 355 MPa?
- No. 355 MPa applies only up to 16 mm. HE 300 B has a 19 mm flange, so the minimum yield is 345 MPa. For governing thicknesses greater than 100 mm, the mechanical values shall be agreed and verified on the order.
-
Which standards should appear on the inspection document?
- At least EN 10025-2 and its edition, the grade S355J2 (1.0577), evidence of the fully killed / nitrogen-binding practice, the EN 10365 designation, the EN 10034 edition used for tolerances, the delivery condition, ladle analysis, the carbon equivalent, tensile results by thickness, and the −20 °C impact result.
Request a Quotation for EN 10025-2 S355J2 H-Beam
EN 10025-2 S355J2 H-beam is a fully killed non-alloy structural section with 355 MPa minimum yield up to 16 mm and a 27 J impact requirement at −20 °C. Nominate the HEA, HEB or IPE size to EN 10365, the tolerances to EN 10034, and the material to EN 10025-2:2019 (or the edition on the order). The tables are reference dimensions, not a rolling list. Send the size list, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.