EN 10025-2 S450J0 Steel Bearing Pile | EN 10025-2 Steel Bearing Piles - SHH STEEL

EN 10025-2 S450J0 Steel Bearing Pile

EN 10025-2 S450J0 steel bearing pile is a 450 MPa long-product quality specified in the 2004 edition for thicknesses from 3 mm to 150 mm, with a 27 J impact requirement at 0 C. The 2019 edition withdrew S450 and added S460 and S500. This page records the 2004 values and typical mill UC, HP and UBP sizes. The ordered edition governs.
Keywords
EN 10025-2 S450J0 Steel Bearing Pile, S450J0, 1.0590, universal bearing pile, HP pile
Equivalent Grades:
S460J0 (EN 10025-2:2019 family, not an automatic substitute); S355J0 / S355JR; A572 Grade 50 / Grade 65 (ASTM, different shapes). Near-equivalents only.
Share:
What is EN 10025-2 S450J0 steel bearing pile?
Ladle analysis and carbon equivalent from the 2004 edition
2004 yield, tensile, elongation and J0 impact
Typical mill UC, HP and UBP sizes
Where S450J0 bearing piles are used, and the 2019 successor discussion
Near-equivalents, not automatic substitutes
Mill sourcing and document coordination
FAQ
Conclusion

What is EN 10025-2 S450J0 Steel Bearing Pile?

EN 10025-2 S450J0 steel bearing pile is a hot-rolled structural section in non-alloy structural steel S450J0 (steel number 1.0590). S marks a structural steel, 450 is the minimum yield strength in MPa up to 16 mm, and J0 is the quality with a longitudinal Charpy V-notch requirement of 27 J at 0 °C when impact testing applies. In EN 10025-2:2004 the technical delivery conditions for this grade apply to long products with thickness from 3 mm to 150 mm. The steel is fully killed.

Edition warning. These material values are those of EN 10025-2:2004. The 2019 edition of EN 10025-2 withdrew grade S450 and added S460 and S500. S450J0 is therefore not a grade of EN 10025-2:2019. If the project names the 2019 edition, do not certify S450J0 as a 2019 grade; discuss the named 2019 grade, often a S460 quality, on the order. The ordered edition governs.

The usual pile and heavy-section shapes for this grade are universal columns (UC), H-piles (HP) and universal bearing piles (UBP). They are filed under steel beam profiles in the steel structural profiles category. They are not interlocking sheet piles, and they are not EN 10025-2 S355JR H-beam HEA or IPE rows of a similar depth.

EN 10025-2 S450J0 Chemistry (2004 Edition, Long Products)

The ladle-analysis limits below are those of EN 10025-2:2004 for S450J0. The grade is specified for long products only. For the 16–40 mm carbon column, the standard raises the carbon maximum to 0.22% when the nominal thickness exceeds 30 mm. For sections thicker than 100 mm, carbon is by agreement. For long products, phosphorus and sulphur may be 0.005% higher than the tabulated figures. The nitrogen maximum does not apply when sufficient aluminium or other nitrogen-binding elements are present, as the standard provides. The steel may contain niobium up to 0.05%, vanadium up to 0.13% and titanium up to 0.05%. Copper above 0.40% may cause hot shortness during hot forming.

Element (ladle analysis) t ≤ 16 mm 16 < t ≤ 40 mm t > 40 mm
C max (%) 0.20 0.20 (0.22 max when t > 30 mm) 0.22
Si max (%) 0.55 0.55 0.55
Mn max (%) 1.70 1.70 1.70
P max (%) 0.030 0.030 0.030
S max (%) 0.030 0.030 0.030
N max (%) 0.025 0.025 0.025
Cu max (%) 0.55 0.55 0.55

Product-analysis maxima in the same 2004 edition are C 0.23 / 0.23 (0.24% when t > 30 mm) / 0.24, Si 0.60, Mn 1.80, P 0.040, S 0.040, N 0.027 and Cu 0.60. Carbon equivalent values from the 2004 table, applicable to long products, are:

Thickness CEV max
t ≤ 16 mm 0.47
16 < t ≤ 40 mm 0.49
40 < t ≤ 63 mm 0.49
t > 63 mm Not tabulated for S450J0 in the 2004 carbon-equivalent table.

These 2004 figures must not be read as EN 10025-2:2019 limits. The 2019 edition does not list S450J0.

EN 10025-2 S450J0 Mechanical Properties (2004 Edition)

Tensile properties below are those of EN 10025-2:2004 for S450J0 long products, in the direction parallel to rolling. Thickness is that of the part from which the test sample is taken, ordinarily the flange for these sections. The 2004 scope for this grade stops at 150 mm, so no thicker yield column is given.

Nominal thickness (mm) Yield min. (MPa) Tensile (MPa) Elongation min., longitudinal (%)
3 ≤ t ≤ 16 450 550–720 17
16 < t ≤ 40 430 550–720 17
40 < t ≤ 63 410 550–720 17
63 < t ≤ 80 390 550–720 17
80 < t ≤ 100 380 550–720 17
100 < t ≤ 150 380 530–700 17

The J0 quality requires a longitudinal Charpy V-notch test at 0 °C. For sections with a nominal thickness greater than 100 mm, the impact values shall be agreed at the time of the order. Subsize specimen rules for thickness of 12 mm or less follow the general provisions of EN 10025-1 as cited in the 2004 edition.

Quality Temperature Minimum average energy
S450J0 (long products) 0 °C 27 J

EN 10025-2 S450J0 UC, HP and UBP Sizes (Typical Mill Series)

Typical mill-programme universal columns, H-piles and universal bearing piles commonly offered for this grade are tabulated below. Designations follow established European and British universal and HP naming. The rows are a commonly supplied standard mill series, not a claim that every official EN 10365:2017 row has been reproduced, and not a statement that any one mill rolls the full list in S450J0. Historic or additional sizes can be reviewed on enquiry. Masses are theoretical catalogue figures for identification, estimating and drawing work. Area is not tabulated here because it was not in the extracted mill series used for these rows.

Universal columns (UC)

Swipe horizontally to view all dimensions.

Designation Mass (kg/m) h (mm) b (mm) tw (mm) tf (mm) r (mm)
UC 356 × 406 × 1299 1299 600 476 100 140 20
UC 356 × 406 × 1202 1202 580 471 95 130 20
UC 356 × 406 × 1086 1086 569 454 78 125 20
UC 356 × 406 × 990 990 550 448 71.9 115 20
UC 356 × 406 × 900 900 531 442 65.9 106 20
UC 356 × 406 × 818 818 514 437 60.5 97 20
UC 356 × 406 × 744 744 498 432 55.6 88.9 20
UC 356 × 406 × 677 677 483 428 51.2 81.5 20
UC 356 × 406 × 634 634 474.6 424 47.6 77 20
UC 356 × 406 × 592 592 465 421 45 72.3 20
UC 356 × 406 × 551 551 455.6 418.5 42.1 67.5 20
UC 356 × 406 × 509 509 446 416 39.1 62.7 20
UC 356 × 406 × 467 467 436.6 412.2 35.8 58 20
UC 356 × 406 × 393 393 419 407 30.6 49.2 20
UC 356 × 406 × 340 340 406.4 403 26.6 42.9 20
UC 356 × 406 × 287 287 393.6 399 22.6 36.5 20
UC 356 × 406 × 235 235 381 394.8 18.4 30.2 20
UC 356 × 368 × 202 202 374.6 374.7 16.5 27 20
UC 356 × 368 × 177 177 368.2 372.6 14.4 23.8 20
UC 356 × 368 × 153 153 362 370.5 12.3 20.7 20
UC 356 × 368 × 129 129 355.6 368.6 10.4 17.5 20
UC 305 × 305 × 283 283 365.3 322.2 26.8 44.1 20
UC 305 × 305 × 240 240 352.5 318.4 23 37.7 20
UC 305 × 305 × 198 198 339.9 314.5 19.1 31.4 20
UC 305 × 305 × 158 158 327.1 311.2 15.8 25 20
UC 305 × 305 × 137 137 320.5 309.2 13.8 21.7 20
UC 305 × 305 × 118 118 314.5 307.4 12 18.7 20
UC 305 × 305 × 97 96.9 307.9 305.3 9.9 15.4 20
UC 254 × 254 × 167 167 289.1 265.2 19.2 31.7 13
UC 254 × 254 × 132 132 276.3 261.3 15.3 25.3 13
UC 254 × 254 × 107 107 266.7 258.8 12.8 20.5 13
UC 254 × 254 × 89 88.9 260.3 256.3 10.3 17.3 13
UC 254 × 254 × 73 73.1 254.1 254.6 8.6 14.2 13
UC 203 × 203 × 86 86.1 222.2 209.1 12.7 20.5 10
UC 203 × 203 × 71 71 215.8 206.4 10 17.3 10
UC 203 × 203 × 60 60 209.6 205.8 9.4 14.2 10
UC 203 × 203 × 52 52 206.2 204.3 7.9 12.5 10
UC 203 × 203 × 46 46.1 203.2 203.6 7.2 11 10
UC 152 × 152 × 51 51 170.2 157.4 11 15.7 8
UC 152 × 152 × 44 44 166 155.9 9.5 13.6 8
UC 152 × 152 × 37 37 161.8 154.4 8 11.5 8
UC 152 × 152 × 30 30 157.6 152.9 6.5 9.4 8
UC 152 × 152 × 23 23 152.4 152.2 5.8 6.8 8

H-piles (HP)

Swipe horizontally to view all dimensions.

Designation Mass (kg/m) h (mm) b (mm) tw (mm) tf (mm) r (mm)
HP 400 × 231 231 372 402 26 26 20
HP 400 × 213 213 368 400 24 24 20
HP 400 × 194 194 364 398 22 22 20
HP 400 × 176 176 360 396 20 20 20
HP 400 × 158 158 356 394 18 18 20
HP 400 × 140 140 352 392 16 16 20
HP 400 × 122 122 348 390 14 14 20
HP 360 × 180 180 362.9 378.8 21.1 21.1 20
HP 360 × 174 174 361.4 378.5 20.3 20.4 20
HP 360 × 152 152 356.4 376 17.8 17.9 20
HP 360 × 133 133 352 373.8 15.6 15.7 20
HP 360 × 109 109 346.4 371 12.8 12.9 20
HP 320 × 184 184 329 317 25 25 27
HP 320 × 147 147 319 312 20 20 27
HP 320 × 117 117 311 308 16 16 27
HP 320 × 103 103 307 306 14 14 27
HP 320 × 88 88.5 303 304 12 12 27
HP 305 × 223 223 337.9 325.7 30.3 30.4 20
HP 305 × 186 186 328.3 320.9 25.5 25.6 20
HP 305 × 180 180 326.7 319.7 24.8 24.8 20
HP 305 × 149 149 318.5 316 20.6 20.7 20
HP 305 × 126 126 312.3 312.9 17.5 17.6 20
HP 305 × 110 110 307.9 310.7 15.3 15.4 20
HP 305 × 95 94.9 303.7 308.7 13.3 13.3 20
HP 305 × 88 88.5 301.7 307.8 12.4 12.3 20
HP 305 × 79 78.9 299.3 306.4 11 11.1 20
HP 260 × 87 87.3 253 267 14 14 24
HP 260 × 75 75 249 265 12 12 24
HP 220 × 57 57.2 210 224.5 11 11 18
HP 200 × 53 53.5 204 207 11.3 11.3 10
HP 200 × 43 42.5 200 205 9 9 10

Universal bearing piles (UBP)

Swipe horizontally to view all dimensions.

Designation Mass (kg/m) h (mm) b (mm) tw (mm) tf (mm) r (mm)
UBP 356 × 368 × 174 174 361.4 378.5 20.3 20.4 20
UBP 356 × 368 × 152 152 356.4 376 17.8 17.9 20
UBP 356 × 368 × 133 133 352 373.8 15.6 15.7 20
UBP 356 × 368 × 109 109 346.4 371 12.8 12.9 20
UBP 305 × 305 × 223 223 337.9 325.7 30.3 30.4 20
UBP 305 × 305 × 186 186 328.3 320.9 25.5 25.6 20
UBP 305 × 305 × 149 149 318.5 316 20.6 20.7 20
UBP 305 × 305 × 126 126 312.3 312.9 17.5 17.6 20
UBP 305 × 305 × 110 110 307.9 310.7 15.3 15.4 20
UBP 305 × 305 × 95 94.9 303.7 308.7 13.3 13.3 20
UBP 305 × 305 × 88 88 301.7 307.8 12.4 12.3 20
UBP 305 × 305 × 79 78.9 299.3 306.4 11 11.1 20
UBP 254 × 254 × 85 85.1 254.3 260.4 14.4 14.3 13
UBP 254 × 254 × 71 71 249.7 258 12 12 13
UBP 254 × 254 × 63 63 247.1 256.6 10.6 10.7 13
UBP 203 × 203 × 54 53.9 204 207.7 11.3 11.4 10
UBP 203 × 203 × 45 44.9 200.2 205.9 9.5 9.5 10

An HP or UBP is a bearing pile, not an interlocking sheet pile, and it is not an HEA or IPE beam of similar depth. Shape tolerances for I and H sections belong to EN 10034 when that standard is named on the order. Settlement on theoretical or weighed mass should follow the contract.

EN 10025-2 S450J0 Steel Bearing Pile Applications

S450J0 UC, HP and UBP sections are used where a 2004-edition 450 MPa European section with a 0 °C impact quality is named for bearing piles or heavy columns. They are not a silent substitute for EN 10025-2 S355JR H-beam or for EN 10025-2 S355J2 H-beam. If the contract already names EN 10025-2:2019, S450J0 is not a grade of that edition; the named 2019 grade must be agreed before rolling.

Near-Equivalents for EN 10025-2 S450J0 Steel Bearing Pile

A near-equivalent is a starting point for a discussion, not a licence to swap certificates or editions.

Comparison Material / dimension system What is similar What is not interchangeable
S460J0 / S460JR EN 10025-2:2019; dimensions EN 10365 The 2019 edition added S460 (and S500) when it withdrew S450. Different edition and different grade name. Do not certify S450J0 as a 2019 grade, or the reverse, without agreement.
S355J0 / S355JR EN 10025-2; same shape families Lower-yield European sisters, including J0 at 0 °C. Yield and tensile tables are lower. See EN 10025-2 S355JR H-beam.
A572 Grade 50 / Grade 65 ASTM material; A6 HP or W shapes American structural comparisons sometimes discussed on mixed pile lists. An ASTM HP or W is not an EN UC or UBP by depth alone. See ASTM A572 Grade 50 steel beam.

Sourcing EN 10025-2 S450J0 Steel Bearing Piles from SHH STEEL

SHH STEEL supplies EN 10025-2 S450J0 bearing piles and related heavy sections against a named designation list, the edition (2004, unless a 2019 successor grade is agreed), the inspection document type and any agreed options for thickness above 100 mm. Enquiries should state the UC, HP or UBP designations, cut lengths or mill lengths, and whether a named 2019 grade is required instead.

EN 10025-2 S450J0 Steel Bearing Pile FAQs

Is S450J0 still in EN 10025-2:2019?
No. The 2019 edition withdrew S450 and added S460 and S500. The chemistry and mechanicals on this page are those of the 2004 edition. If the project names 2019, agree the named 2019 grade before rolling.
What product forms are tabulated here?
Universal columns, H-piles and universal bearing piles, which are the usual heavy-section and bearing-pile shapes for this grade. They are not interlocking sheet piles and not HEA or IPE beams.
What is the impact requirement?
J0 requires 27 J at 0 °C for long products in the 2004 edition. For sections thicker than 100 mm the impact values shall be agreed on the order.
Are the size tables the official EN 10365:2017 annex?
No. They are a commonly supplied standard mill series of UC, HP and UBP designations. Historic or additional sizes can be reviewed on enquiry and are not silently added.
Can S460J0 be shipped in place of S450J0?
Only if the purchaser agrees. The grades belong to different editions and have different names. Do not treat them as automatic substitutes.

Request a Quotation for EN 10025-2 S450J0 Steel Bearing Pile

Send the UC, HP or UBP designation list, the edition (2004, or a named 2019 successor grade), any options for thickness above 100 mm, and the inspection document type. SHH STEEL will coordinate the mill programme and the certificate against that list.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X