GB/T 11263 Steel Structural Profiles
SHH STEEL supplies GB/T 11263 hot-rolled H-beams and split T-section beams. The official GB/T 11263 series names are HW, HM, and HN, with designations such as HW 200×200, HM 300×200, and HN 400×200, plus cut T-sections taken from those H-beams. Steel grades are specified separately, commonly to GB/T 700 (for example Q235B) or GB/T 1591 (for example Q355B). HW, HM, and HN are not JIS nomenclature, and they are not equivalent to HEA, HEB, or W-shapes by nominal size. Available designations and certificates are confirmed on each inquiry.
-
GB/T 11263 Q355D H-Beam
GB/T 11263 Q355D H-beam is a Chinese as-rolled H-section in the 355 MPa yield class, listed here with Q355C and with Q355E only as an N or M quality. The page gives HW, HM and HN sizes, as-rolled chemistry, and the Table 11 impact rules, including the plate-only footnote on the as-rolled D values.View More -
GB/T 11263 Q420B H-Beam
GB/T 11263 Q420B H-beam is a Chinese as-rolled H-section with 420 MPa minimum yield in the first thickness band and a 34 J impact test at +20 °C when testing applies. The page also covers Q420C and the Q390B, C and D family, and lists the HW, HM and HN series with 2017 theoretical masses.View More -
GB/T 11263 Q355B H-Beam
GB/T 11263 Q355B H-beam is a hot-rolled Chinese H-section in as-rolled low-alloy steel Q355B (GB/T 1591-2018), with 355 MPa minimum yield up to 16 mm and 34 J longitudinal impact at +20 °C. Sizes follow the HW, HM and HN series under GB/T 11263. SHH STEEL reviews grade, condition, size series and certificate requirements before quoting.View More -
GB/T 11263 Q235B H-Beam
GB/T 11263 Q235B H-beam is a hot-rolled Chinese H-section in carbon structural steel Q235B (GB/T 700), with 235 MPa minimum yield up to 16 mm and 27 J impact at +20 °C. Sizes follow the HW, HM and HN series under GB/T 11263. SHH STEEL reviews grade, size series, standard edition and certificate requirements before quoting.View More
GB/T 11263 Steel Structural Profiles
H Beams and Wide Flange Beams
SHH STEEL supplies hot-rolled steel beam profiles for buildings, bridges, and industrial frames. Material is specified to the project standard—for example ASTM A36, A572, A992, or A709; ASME SA-36 or SA-992; EN 10025-2; GB/T 11263 with GB/T 700 or GB/T 1591 grades; JIS G 3101; ISO 630-1; or GOST practice. Dimensional series are ordered separately and may include ASTM A6 W, S, and HP shapes; EN 10365 HEA, HEB, HEM, and IPE; BS 4-1 UB and UC; GB/T 11263 HW, HM, and HN (and split T); and JIS G 3192 H-sections and I-beams, with designations such as H 300×300×10×15. HW, HM, and HN are GB/T 11263 series names, not JIS nomenclature. A grade such as ASTM A36 can be furnished in EN-series dimensions when so specified and certified; W, HEA, and metric H-sections are not equivalent by nominal depth. Available sizes and certificates are confirmed with each inquiry.
This range covers H Beams and Wide Flange Beams. Buyers also search these sections as H Beam, H-Beam, or Steel H Beams; the usual US name is Wide Flange Beam (W shape). Typical series on these pages are ASTM A6 W shapes, EN 10365 HEA, HEB and HEM, GB/T 11263 HW, HM and HN, and JIS G 3192 H-sections. I Beams are a different product family and are listed separately.