EN 10025-2 S275JR H-beam is a hot-rolled I or H section in non-alloy structural steel S275JR (steel number 1.0044). The material is specified to EN 10025-2; the section size is specified to EN 10365; and the shape and mass tolerances are specified to EN 10034. S marks a structural steel, 275 is the minimum yield strength in MPa up to 16 mm, and JR is the impact quality, 27 J at +20 °C.
In the EN 10025-2 family this grade sits between S235JR and S355JR. It is used when a 275 MPa yield class is what the design actually calls for, not as a casual stand-in for either neighbour. The rolled section, not plate, is the subject of this page. The same grade in plate form is listed separately as EN 10025-2 S275JR steel plate. Long-product tensile and impact tests are normally longitudinal unless the order says otherwise; the plate page uses a different sampling convention and is not a substitute data sheet for H-beams.
These beams are filed under EN 10025-2 steel beam profiles in the steel beam profiles category of steel structural profiles. The usual size series are HE A (HEA), HE B (HEB) and IPE. HEM, and British UB or UC sections, may be furnished when they are specified and certified. The published S355JR H-beam page is the 355 MPa JR sister, not a data sheet for S275JR.
S275JR is a general structural grade for building frames, light industrial structures and ordinary fabrication where a +20 °C impact quality is accepted. It is not a 355 MPa grade, not a weathering steel, and not a pressure-vessel or nuclear safety material. An enquiry that only says “S275 H-beam” still needs the quality letters and the dimensional standard.
Material, Dimensions and Tolerances for S275JR Sections
The purchase order and the inspection certificate should name three documents, each for its own purpose:
- EN 10025-2 is the material standard. This article uses ladle-analysis, carbon-equivalent and tensile values for S275JR long products from EN 10025-2:2019. The edition named on the order governs acceptance.
- EN 10365 is the dimensional standard for hot-rolled I and H sections, including IPE and the HE A, HE B and HE M family. The size tables below are reference dimensions and theoretical masses, not a mill rolling list.
- EN 10034 is the tolerance standard for those I and H sections. Surface condition is commonly specified to EN 10163-3; the class should be confirmed when a tighter finish is required.
A mill may certify S275JR on a non-European shape, or roll an HEA or IPE to a different material standard, if that combination is in its programme and is fully documented. Do not treat “S275JR H-beam” as if it automatically meant an HEB, and do not treat a W-shape or an HW of a similar nominal depth as the same section.
S275JR H-Beam Sizes: HEA, HEB, IPE, UB and UC Reference Tables
The following tables list the standard HE A, HE B and IPE series: designation, depth h, flange width b, web thickness tw, flange thickness tf, root radius r, area A and theoretical mass. The figures are consistent with the established EN 10365 series and are for identification and estimating. They are not a statement that every row is rolled in S275JR. Mid-range sizes are the usual enquiry core; very light IPE rows and HE 900–1000 should be confirmed line by line.
Trade shorthand HEA 240 is the same section as HE 240 A, and HEB 300 is the same as HE 300 B. Actual depth can differ from the number in the name: HE 240 A is 230 mm deep, with a 12 mm flange, so it remains in the ≤16 mm yield band for S275JR (275 MPa). HE 300 B has a 19 mm flange, so the minimum yield steps down to 265 MPa. IPE 330, by contrast, is a 330 × 160 mm I-beam, not a square H-section.
For sections with a governing thickness greater than 100 mm, mechanical values shall be agreed and verified on the order. The 100–150 mm row in the tensile table is the published long-product band, not an invented extension, and no mechanical limits beyond 150 mm are given here.
HE A (HEA) series
Wide-flange European H-sections, 24 sizes from HE 100 A to HE 1000 A.
Swipe horizontally to view all dimensions.
HE B (HEB) series
Heavier-flange European H-sections, 24 sizes from HE 100 B to HE 1000 B.
Swipe horizontally to view all dimensions.
IPE series
Parallel-flange I-beams, 18 sizes from IPE 80 to IPE 600.
Swipe horizontally to view all dimensions.
Typical mill-programme universal beams (UB) and universal columns (UC) commonly supplied in S275JR are tabulated below. Designations follow the established EN 10365 / British universal naming (for example UB 610 × 229 × 125). The rows are a commonly supplied standard mill series, not a claim that every official EN 10365:2017 row has been reproduced or that any one mill rolls the full list in S275JR. Historic or additional depths can be reviewed on enquiry; they are not silently added to these tables. Masses are theoretical catalogue figures for identification, estimating and drawing work.
Universal beams (UB)
Swipe horizontally to view all dimensions.
Universal columns (UC)
Swipe horizontally to view all dimensions.
HEM can still be reviewed when it is named on the enquiry; a complete HEM table is not reproduced here. HW/HM/HN belong to GB/T 11263; W-shapes belong to ASTM A36 or ASTM A572 practice, not to these HEA, HEB, IPE, UB or UC rows.
S275JR Chemical Composition (EN 10025-2 Ladle Analysis)
The figures below are ladle-analysis maxima for S275JR long products in EN 10025-2:2019. They are limits, not typical heat results. Carbon is higher than in S235JR, and manganese is limited to 1.50% rather than 1.40%. There is still no general silicon maximum unless a galvanizing agreement is written into the order.
S275JR Carbon Equivalent
The carbon equivalent is calculated from the ladle analysis by CEV = C + Mn/6 + (Cr + Mo + V)/5 + (Cu + Ni)/15. The EN 10025-2:2019 maxima for S275JR long products are:
The third band applies to nominal thicknesses greater than 40 mm and not more than 140 mm. For thicknesses above 140 mm, a carbon-equivalent limit is not tabulated here and must be agreed and verified on the order; no value is invented for that range. Clause 7.2.5 of EN 10025-2:2019 addresses special conditions for S275 and S355. If that clause is to be used, it should be named on the order; this page does not invent a raised CEV figure from it.
S275JR Mechanical Properties: Yield, Tensile and +20 °C Impact
Tensile properties of S275JR are thickness-dependent. The values below are from EN 10025-2:2019 for long products, with elongation based on L0 = 5.65√S0. For sections with nominal thickness greater than 100 mm, the mechanical values shall be agreed and verified on the order; the 100–150 mm row is the published long-product band and is not an invented extension. No mechanical limits beyond 150 mm are given here. Plate elongation and sampling are covered on S275JR steel plate, not by this table.
Quality JR requires 27 J at +20 °C. For long products the Charpy test is normally longitudinal unless the order specifies otherwise. If the project needs 27 J at 0 °C or at −20 °C, the grade to nominate is S275J0 or S275J2, not S275JR.
Use the flange, or the specimen-preparation thickness required by the standard, when selecting the band. HE 240 A, with a 12 mm flange, remains at 275 MPa. HE 300 B, with a 19 mm flange, is 265 MPa.
Delivery Conditions, Inspection and Identification
S275JR sections are commonly supplied as-rolled. The inspection document should show EN 10025-2 and its edition, the grade S275JR (1.0044), the EN 10365 size designation, the EN 10034 edition used for tolerances, the delivery condition, the heat number, ladle analysis, the carbon equivalent, and the tensile and +20 °C impact results. If clause 7.2.5 or a galvanizing chemistry has been agreed, that agreement belongs on the document as well.
An EN 10204 type 3.1 document is the usual export request; type 3.2 or nominated third-party attendance can be added when the specification requires it. Identification follows the mill’s marking practice and the ordered standards. Length is a matter for the rolling programme and the order, often in the region of 6–15 m, not a value fixed by the size table.
Weldability and Surface Condition of S275JR H-Beams
S275JR is a weldable non-alloy structural steel when thickness, joint design and hydrogen control are taken into account. The CEV table above is the starting point; the certificate values, and a procedure suited to the thickness, are the practical controls. This page does not prescribe a procedure or a preheat chart.
The as-rolled surface is mill scale. A blast class, a paint system, or a hot-dip galvanizing chemistry is an order option. If galvanizing is planned, the optional Category B silicon and phosphorus limits, and the processor’s coating specification, should be reviewed before production. Surface quality for sections is commonly specified to EN 10163-3.
Cutting to length, weld-end preparation, forming or coating can be reviewed when the specification is sent with the enquiry. They are not assumed for every size.
EN 10034 Shape Tolerances and Theoretical Mass
Dimensional and mass tolerances for these I and H sections are those of EN 10034, not of EN 10025-2. This article does not reproduce the millimetre tolerance tables; acceptance is against the edition named on the order.
The size tables above are nominal reference dimensions. A delivered HE 240 A will measure close to 230 × 240 × 7.5 × 12 mm within those tolerances, not as a set of exact advertised millimetres. Out-of-square and web off-centre matter for end-plate connections. Settlement on theoretical or weighed mass should follow the contract, not an informal mix of those bases.
Applications and Service Limits
S275JR H-beams are used where a 275 MPa yield class and a +20 °C impact quality are what the specification actually names:
- Building frames and light industrial structures that sit between an S235 and an S355 design.
- General fabrication and platforms that do not require a 0 °C or −20 °C test.
- Mixed-origin packages, provided each line keeps its own material standard and shape system.
It is not specified here for pressure equipment, for nuclear safety-related components, or for structures whose specification requires S355 or a lower test temperature. Durability comes from the coating or fire-protection system, not from the grade name.
S275JR Compared with S235JR, S355JR and A36
S275JR shares the HEA, HEB and IPE system with S355JR and with S235JR, but the yield class, carbon, manganese and carbon-equivalent tables are different. Choosing JR only fixes the +20 °C impact quality; it does not choose 235, 275 or 355 MPa. S275J0 and S275J2 keep the 275 MPa class and move the 27 J test to 0 °C and −20 °C.
ASTM A36 is a 36 ksi [250 MPa] carbon steel on W-shapes, not a 275 MPa European section. Chinese Q235B and Q355B, rolled as HW/HM/HN to GB/T 11263, bracket this yield class rather than matching it. Dual certification is possible only when the delivered piece meets every requirement of each named standard.
Near-Equivalents: Not Automatic Substitutes
The comparisons below are for orientation. They are not a licence to substitute one grade for another on a contract or an inspection certificate.
Sister beam pages in this series (S235JR, S355J0, S355J2) will be linked here once they are published. Until then, use the live category and plate links above, and the published S355JR H-beam page for the 355 MPa JR comparison. The S235JR steel plate page is a plate data sheet, not an S235JR beam page.
Sourcing S275JR H-Beams from SHH STEEL
SHH STEEL supplies S275JR H-beams as an export trading house, coordinating mill production and project procurement. The useful part of that model, for this grade, is to keep the 275 MPa class from being quietly replaced by S235 or S355, to record any clause 7.2.5 or galvanizing agreement, and to align the EN 10365 designation, EN 10034 tolerances and the inspection document before a rolling programme is committed.
Sections can be sourced from mills that SHH STEEL buys from, including Masteel, Rizhao Steel, Laiwu (Shandong Steel Laiwu) and Tung Ho Steel, among others when the programme matches the order. Those mills do not each roll every HEA, HEB or IPE size in S275JR. Mid-range sizes are the usual core; the heaviest HE rows and uncommon IPE variants are confirmed per line.
The same enquiry can also cover Chinese, American or Japanese designations, provided each line states its material standard, shape standard and size. If cutting, weld-end preparation, forming or a coating system is required, include that specification for review. Export packing and container loading can be arranged to the packing list agreed for the shipment.
S275JR H-Beam FAQs
-
How does S275JR differ from S235JR and S355JR?
- All three can be rolled as HEA, HEB or IPE sections, but the yield classes, chemistry and carbon-equivalent tables are different. S275JR has 275 MPa minimum yield up to 16 mm and a CEV maximum of 0.40% through 40 mm. It is not a substitute for S355JR, and S235JR is not a substitute for it, unless the delivered piece is certified to the named grade.
-
Is S275 the same as S275JR?
- S275 is the yield class; JR, J0 and J2 are qualities. JR is tested at +20 °C, J0 at 0 °C and J2 at −20 °C, all at 27 J. An order that says only “S275 H-beam” is incomplete.
-
Why is the minimum yield not always 275 MPa?
- 275 MPa applies only up to 16 mm. The minimum falls through the thickness bands, to 265 MPa between 16 and 40 mm and lower for heavier flanges. HE 300 B has a 19 mm flange, so the minimum yield is 265 MPa. For governing thicknesses greater than 100 mm, the values shall be agreed and verified on the order.
-
Does clause 7.2.5 change the carbon-equivalent limit?
- EN 10025-2:2019 clause 7.2.5 addresses special conditions for S275 and S355. This page quotes the tabulated CEV maxima (0.40 / 0.40 / 0.42 through 140 mm) and does not invent a raised figure from that clause. If the clause is to be used, it should be named on the order and shown on the inspection document.
-
Which standards should appear on the inspection document?
- At least EN 10025-2 and its edition, the grade S275JR (1.0044), the EN 10365 designation, the EN 10034 edition used for tolerances, the delivery condition, ladle analysis, the carbon equivalent, tensile results by thickness, and the +20 °C impact result.
Request a Quotation for EN 10025-2 S275JR H-Beam
EN 10025-2 S275JR H-beam is a non-alloy structural section with 275 MPa minimum yield up to 16 mm and a 27 J impact requirement at +20 °C. Nominate the HEA, HEB or IPE size to EN 10365, the tolerances to EN 10034, and the material to EN 10025-2:2019 (or the edition on the order). The tables are reference dimensions, not a rolling list. Send the size list, edition, certificate type and any processing notes; SHH STEEL will review the package and quote accordingly.