ASTM A269 TP348 Stainless Steel Tube | ASTM A269 Stainless Steel - SHH STEEL

ASTM A269 TP348 Stainless Steel Tube

ASTM A269 TP348 / UNS S34800 nominal-wall seamless and welded Nb-stabilized austenitic tubing with Cr 17.0–19.0%, Ni 9.0–12.0%, C ≤0.08%, Ta ≤0.10% and Co ≤0.20%, solution annealed at ≥1900 °F [1040 °C] with hardness max 192 HBW / 200 HV or 90 HRB. SHH STEEL can produce and supply A269 TP348 tube with EN 10204 3.1 MTCs.
Grade
TP348 / UNS S34800
Standard
ASTM A269 / A269M
Product form
Seamless and welded tube (no filler metal for welded), heat-treated
Size
Typical OD × nominal wall from ~6 mm to 168 mm OD × 0.5–8.0 mm wall; other OD × wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Seamless and Welded
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A269 TP348 Stainless Steel Tube

ASTM A269 / A269M covers nominal-wall seamless and welded austenitic stainless steel tubing for general corrosion-resisting and low- or high-temperature service. Grade TP348 / UNS S34800 is the niobium-stabilized sister of TP347 with explicit tantalum ≤0.10% and cobalt ≤0.20% limits for applications that restrict those residuals. Carbon ≤0.08%, chromium 17.0–19.0%, and nickel 9.0–12.0% sit in the same family window as TP347. Buyers write A269 TP348 when the drawing names S34800 or when Ta/Co limits are contractual — not as a casual nickname for TP347. Name ASTM A269 on the purchase order so nominal-wall rules, hardness, and flaring or flange tests apply to tubing rather than to an A213 or A312 product text.

SHH STEEL can produce and supply ASTM A269 TP348 stainless steel tube as seamless and welded product in the instrument-to-process OD × nominal-wall band, solution annealed, with EN 10204 3.1 certificates reporting Table 1 chemistry (including Ta, Co, and Nb) and Table 2 hardness. Typical sizes run about 6–168 mm OD × 0.5–8.0 mm nominal wall; other sizes by agreement. Compare A269 TP347 and A269 TP321 on the A269/A269M hub. Keep the wall basis nominal. §6.3 high-anneal caution applies to TP348 as it does to TP347 and TP321.

If the duty is actually boiler / heat-exchanger minimum-wall tube or pipe rather than A269 nominal-wall tubing, open A213 TP348, SA213 TP348, A312 TP348 and SA312 TP348 and match the product standard to the drawing.

Chemical Composition of A269 TP348

Heat analysis under A269 Table 1 is mandatory for every TP348 heat; product analysis applies when ordered through ASTM A1016/A1016M and A480/A480M Table A1.1 tolerances. SHH STEEL reports measured ladle values — and product values when ordered — without advertising unpublished tighter catalogue windows.

Public A269 Table 1 excerpts for TP348 / UNS S34800 list Ta ≤0.10% and Co ≤0.20% plus Nb/Cb under Footnote E (ASTM abstract + tubingchina A269 PDF). Confirm Footnote E exact Nb wording in the purchased edition — public excerpt layout makes the footnote letter hard to read beside the TP347 Cb column.

Melting analysis (heat / ladle analysis) — Table 1

Element TP348 / UNS S34800 melting analysis
Carbon (C) ≤ 0.08
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 17.0 – 19.0
Nickel (Ni) 9.0 – 12.0
Tantalum (Ta) ≤ 0.10
Cobalt (Co) ≤ 0.20
Niobium / Columbium (Nb / Cb) per Footnote E (confirm purchased edition — related to TP347 Cb rule)
Molybdenum (Mo) … (no requirement)

Source: ASTM A269/A269M Table 1 for TP348 / UNS S34800 (public excerpts). TP348 is the low-tantalum / low-cobalt Nb-stabilized sister of TP347 for applications that restrict Ta and Co. A269 §6.3 high-anneal IGC caution also applies to TP348.

Mechanical Properties of A269 TP348

ASTM A269 does not publish a tensile-strength, yield, or elongation acceptance table for TP348. Lot acceptance is built on hardness (Table 2), flaring for seamless tube, flange and reverse flattening for welded tube, and hydro or NDE on each length. Do not invent tensile floors from A213 or A312 unless the purchase order adds them as project extras.

Property TP348 requirement (A269 Table 2)
Hardness, max 192 HBW / 200 HV or 90 HRB
Tensile / yield / elongation Not specified as an A269 acceptance table for this grade

Source: ASTM A269/A269M Table 2 for TP348 (public PDF excerpt where verified). Confirm thin-wall superficial Rockwell alternatives in the purchased edition before writing them into a quality plan.

Seamless and Welded Tube

Under A269, TP348 tubing may be seamless or welded, and hot-finished or cold-finished, unless the purchase order locks the route. Welded A269 tube is autogenous — no filler metal in the longitudinal seam — then cold-worked and solution-treated with the tube. That is not A312 WLD/HCW pipe stencil language; A269 simply records seamless or welded on the product and MTC.

Seamless TP348 takes a lot-basis flaring test; welded TP348 takes flange and reverse-flattening tests so the seam is exercised in both opening and reverse-bend modes. Both routes share Table 2 hardness and the mandatory hydrostatic or nondestructive electric test on each length. SHH STEEL can produce and supply both seamless and welded A269 TP348 against the same Table 1 chemistry and Table 2 hardness floors — name the required route on the enquiry.

Dimensions and Tolerances

Order A269 TP348 by outside diameter and nominal wall thickness, not by pipe schedule as the primary size language. Permissible variations come from A269 Table 4 and the general requirements in ASTM A1016/A1016M; thin-wall ovality rules in clause 12.2 apply when wall thickness falls below the thin-wall thresholds listed for each OD group.

OD group (A269 Table 4) Outside diameter tolerance Wall thickness tolerance
Up to ½ in. [13 mm] ±0.005 in. [0.13 mm] ±15%
½ to 1½ in. [13–38 mm], excl. ±0.005 in. [0.13 mm] ±10%
1½ to 3½ in. [38–89 mm], excl. ±0.010 in. [0.25 mm] ±10%
3½ to 5½ in. [89–140 mm], excl. ±0.015 in. [0.38 mm] ±10%
5½ to 8 in. [140–203 mm], excl. ±0.030 in. [0.76 mm] ±10%

Source: ASTM A269/A269M Table 4 (public PDF excerpt). Footnotes allow wider wall variation on heavy wall or low ID/OD ratios and on sub-½ in. ID non-mandrel tube. If a drawing uses A213 minimum-wall language for TP348, say so on the enquiry so SHH STEEL does not build the wrong wall basis.

Equivalent Grades

TP348 / UNS S34800 is the low-Ta/Co Nb-stabilized tubing grade under A269. Related forms may appear under A213/A312/A240 where those standards list S34800. Do not substitute TP347 for TP348 when Ta/Co limits are on the drawing.

Reference Designation Note
ASTM A269 TP348 / UNS S34800 This product standard
UNS S34800 Chemistry identity
ASTM A269 sister TP347 / S34700 Nb-stabilized without Ta/Co ceilings
ASTM A213 / A312 TP348 (where listed) Different product form

Inside A269, step to A269 TP347 when Ta/Co limits are not required, or to A269 TP321 for Ti stabilization.

Same-grade pages under related product standards (different wall basis and mechanical tables — not drop-in substitutes for A269 tubing): A213 TP348, SA213 TP348, A312 TP348 and SA312 TP348. Confirm the product form before treating any of those pages as acceptance text for an A269 order.

Heat Treatment and Delivery Condition

All A269 TP348 tube is furnished solution heat-treated. Table 2 sets austenitizing at ≥1900 °F [1040 °C], followed by water quench or rapid cool by other means. Seamless tube may be quenched immediately after hot forming while still at or above the specified minimum. Ordered final anneals below 1900 °F [1040 °C], when permitted and specified, must be stenciled with the actual temperature after the suffix “HT.” A269 §6.3 high-anneal IGC caution applies to TP348; order Supplementary S3 language explicitly if required.

Item TP348 (A269 Table 2)
Austenitizing temperature ≥1900 °F [1040 °C]
Cooling Water quench or rapid cool
Hardness after heat treatment, max 192 HBW / 200 HV or 90 HRB
Delivery condition Solution heat-treated; pickled or bright-annealed by agreement

Source: ASTM A269/A269M §6 and Table 2 for TP348 (public excerpt where verified). SHH STEEL’s MTC states the heat-treatment condition actually applied to the shipped lengths.

Corrosion Resistance

TP348 provides Nb-stabilized HAZ behaviour similar in intent to TP347, with the added contractual control of tantalum and cobalt residuals. Stabilization protects against sensitization in welded or intermittently heated general-service tubing; it does not add molybdenum for chloride pitting.

A269 publishes no PREN for S34800 — do not invent one. Use TP348 when Ta/Co limits are specified; use TP347 when they are not; use Mo-bearing A269 grades when chlorides drive alloy selection.

Applications of A269 TP348 Tube

A269 TP348 appears where specifications explicitly require low Ta/Co Nb-stabilized tubing — certain nuclear-adjacent, specialty chemical, or OEM lists that name S34800. Bright-annealed cold-finished tube is common on skids; pickled welded tube covers larger runs.

For boiler/HX tube open A213 TP348 where listed; for pipe open A312. SHH STEEL can produce and supply A269 TP348 and will redirect to TP347 when Ta/Co limits are not actually on the drawing.

When a sister enquiry is for boiler tube or pipe of the same grade, use A213 TP348, SA213 TP348, A312 TP348 and SA312 TP348 instead of stretching an A269 tubing page into the wrong product form.

Weldability

Nb stabilization supports as-welded behaviour similar to TP347. GTAW/GMAW with 347/348-type fillers (when filler is used) are typical; mill autogenous A269 welds are already solution-treated with the tube. Shop welds on cut lengths sit outside that mill anneal.

Mind §6.3 when specifying post-fabrication heat treatment. SHH STEEL supplies the mill product and MTC with Ta, Co, and Nb reported as Table 1 requires.

Surface Finishes

Pickled and bright-annealed finishes cover most A269 TP348 orders, and named OD polish grit is quoted as a supplementary finish when the purchase order requires a measured belt polish. Bright anneal is preferred for instrumentation and clean-process ID/OD; pickle is the general-process default when a clean but not bright surface is enough for the duty.

Write any maximum Ra, scrubbed-ID, or electropolish note into the enquiry. SHH STEEL can produce and supply pickled, bright-annealed, and polished A269 TP348 when the mill can measure and report the finish, and we will not claim an unverified polish grade on the certificate.

Inspection and Testing

Lot testing for A269 TP348 covers Table 2 hardness, flaring on seamless tube, and flange plus reverse flattening on welded tube, with lot definitions tied to heat, size, and heat-treatment charge as written in the standard. Each length must also receive a hydrostatic test or a nondestructive electric test; the manufacturer chooses unless the purchase order locks the method, and NDE-tested lengths are marked “NDE” and certified accordingly.

EN 10204 3.1 certificates from SHH STEEL report ladle chemistry including Ta, Co, and niobium, solution-treatment condition, hardness against Table 2, and the hydro or NDE statement. PMI, product analysis, and third-party inspection holds are available when named on the order, and we do not skip mandatory tests to shorten lead time.

Packaging and Shipping

Export and domestic packs for A269 TP348 use end caps, size-sorted bundles or crates, and waterproof wrap for ocean freight so OD finish and ends stay protected in transit. Bright-annealed and polished OD get extra sleeve protection against galling; coiled product, when ordered, follows A269’s continuous-coil rule without circumferential butt welds inside the coil.

Stencil and tags typically carry ASTM A269, TP348 / S34800, size, heat number, seamless or welded identity, and NDE when that route was used. SHH STEEL matches marking to the purchase-order marking clause before dispatch so receiving inspection can verify identity against the MTC.

Why Choose SHH STEEL

SHH STEEL can produce and supply ASTM A269 TP348 as solution-treated seamless or welded tubing with Table 1 chemistry — including Ta, Co, and Nb — Table 2 hardness, and EN 10204 3.1 documentation. We will not ship TP347 and call it TP348 when Ta/Co limits are contractual.

If the drawing does not need Ta/Co ceilings, we point to A269 TP347 rather than overselling residual limits the project never asked for.

Supply Capability

SHH STEEL can produce and supply ASTM A269 TP348 Stainless Steel Tube against the edition, process route, and finish named on your enquiry. Capability and Stock / Available sizes follow.

Item SHH STEEL capability
Standard ASTM A269 / A269M
Grade TP348 / UNS S34800
Product form Seamless and welded tube (no filler metal for welded), hot- or cold-finished
Delivery condition Solution heat-treated (≥1900 °F [1040 °C]); pickled or bright-annealed
Typical size band ~6–168 mm OD × 0.5–8.0 mm nominal wall (others by agreement)
Testing Hardness; flaring (seamless) / flange + reverse flattening (welded); hydro or NDE
Documents EN 10204 3.1 MTC; third-party inspection on request

Stock / Available sizes

Enquiry-oriented supply range — not a frozen warehouse SKU list. Send the OD × nominal-wall list and seamless/welded preference for confirmation against near-term production.

OD (mm) Typical nominal walls (mm) Notes
6 / 8 / 10 / 12 / 14 0.5 / 0.8 / 1.0 / 1.2 / 1.5 Instrument / hydraulic; often BA
12.7 / 15.9 / 19.1 / 25.4 / 31.8 1.0 / 1.2 / 1.5 / 2.0 / 2.5 Inch OD process and utility
38.1 / 48.3 / 60.3 / 76.1 1.5 / 2.0 / 2.5 / 3.0 / 4.0 Utility and light process
88.9 / 114.3 / 141.3 / 168.3 2.0 / 3.0 / 4.0 / 6.0 / 8.0 Larger process tube; lock seamless vs welded

Parallel quotes against A269 TP347 keep the Ta/Co decision visible.

FAQ

What is ASTM A269 TP348 used for?
A269 TP348 is Nb-stabilized nominal-wall tubing with Ta ≤0.10% and Co ≤0.20% for general-service lines that contractually restrict those residuals. It is seamless or welded tubing under ASTM A269 — not boiler tube and not pipe. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
TP348 vs TP347 under A269 — which should I order?
Order TP348 when the drawing names UNS S34800 or requires Ta/Co limits. Order TP347 when standard Nb stabilization without those residual ceilings is enough. They are separate Table 1 grades and must not share one stamp on the MTC. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
Does A269 TP348 include welded tube?
Yes. Seamless and welded routes are both allowed. Welded tube is autogenous, cold-worked, solution-treated with the tube, and flange- plus reverse-flattening-tested. SHH STEEL can produce and supply both routes. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
What hardness limit applies to A269 TP348?
Table 2 caps TP348 at 192 HBW / 200 HV or 90 HRB after ≥1900 °F [1040 °C] solution treatment. A269 does not publish a tensile acceptance table for this grade — do not invent one from A213. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
Why does §6.3 matter for TP348?
Section 6.3 warns that solution annealing above 1950 °F [1065 °C] may impair IGC resistance after subsequent sensitizing exposure in TP321, TP347, and TP348. Order Supplementary S3 stabilization language when the project needs it, and confirm the purchased edition. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
Is A269 TP348 nominal wall or minimum wall?
Nominal wall. Write OD × nominal wall on the enquiry unless you agree another wall basis. Table 4 then governs tolerances. Do not assume A213 minimum-wall practice applies. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
What size range can SHH STEEL produce for TP348?
SHH STEEL can produce and supply about 6–168 mm OD × 0.5–8.0 mm nominal wall in seamless or welded A269 TP348, pickled or bright-annealed, with EN 10204 3.1 MTCs. Other sizes by agreement. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
Must Ta and Co appear on the MTC?
Yes when ordering TP348 / S34800 — Table 1 sets Ta ≤0.10% and Co ≤0.20%, so the ladle analysis should report them with Nb. A certificate that only shows a 347-type nickname is incomplete for TP348. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
What certificate does SHH STEEL provide?
EN 10204 3.1 MTCs report ladle chemistry including Ta, Co, and Nb, solution-treatment condition, hardness, and hydro or NDE. Third-party inspection can be added. Stencil shows ASTM A269, TP348 / S34800, size, heat, and seamless or welded identity. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
How should I enquire for A269 TP348?
List ASTM A269, grade TP348 / UNS S34800, seamless or welded, OD × nominal wall, finish, any S3 language, and any hydro/NDE lock. SHH STEEL can produce and supply to that enquiry or recommend TP347 when Ta/Co limits are not required. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
Does TP348 replace TP321?
Not automatically. TP348 is Nb-stabilized with Ta/Co limits; TP321 is Ti-stabilized. Choose based on the stabilizer and residual limits the material list names, not on a casual shop nickname swap. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.

Conclusion

ASTM A269 TP348 / UNS S34800 is the low-Ta/Co niobium-stabilized austenitic inside the A269 nominal-wall tubing family when residual limits accompany Nb stabilization. SHH STEEL can produce and supply seamless and welded A269 TP348, solution annealed to Table 2, tested, and documented on EN 10204 3.1 certificates. Start from the A269/A269M hub, then send the OD × nominal-wall list. Contact admin@steelspecs.com for a production-backed offer.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X