ASTM A269 UNS S31727 Stainless Steel Tube
What is ASTM A269 UNS S31727 Stainless Steel Tube
ASTM A269 / A269M covers nominal-wall seamless and welded austenitic stainless steel tubing for general corrosion-resisting and low- or high-temperature service. UNS S31727 is a copper-bearing ~4% Mo austenitic with controlled nitrogen under A269, ordered by UNS for chemical duties that want Cu plus Mo rather than plain TP317 or S31730. Name ASTM A269 and UNS S31727 on the purchase order so nominal-wall rules, heat treatment, and hardness apply to tubing — not to an A213 or A312 product text.
SHH STEEL can produce and supply ASTM A269 UNS S31727 stainless steel tube as seamless and welded product in the instrument-to-process OD × nominal-wall band, solution annealed, with EN 10204 3.1 certificates reporting Table 1 chemistry and Table 2 hardness where verified. Typical sizes ~6–168 mm OD × 0.5–8.0 mm nominal wall; other sizes by agreement. Browse the A269/A269M hub. Keep the wall basis nominal.
If the duty is actually boiler / heat-exchanger minimum-wall tube or pipe rather than A269 nominal-wall tubing, open A312 UNS S31727 and SA312 UNS S31727 and match the product standard to the drawing.
Chemical Composition of A269 UNS S31727
Heat analysis under A269 Table 1 is mandatory for every UNS S31727 heat; product analysis applies when ordered through ASTM A1016/A1016M and A480/A480M Table A1.1 tolerances. SHH STEEL reports measured ladle values — and product values when ordered — without advertising unpublished tighter catalogue windows.
Public A269 Table 1 for UNS S31727 — Cu-bearing ~4Mo austenitic with controlled N.
Melting analysis (heat / ladle analysis) — Table 1
| Element | UNS S31727 melting analysis |
|---|---|
| Carbon (C) | ≤ 0.030 |
| Manganese (Mn) | ≤ 1.00 |
| Phosphorus (P) | ≤ 0.030 |
| Sulfur (S) | ≤ 0.030 |
| Silicon (Si) | ≤ 1.00 |
| Chromium (Cr) | 17.5 – 19.0 |
| Nickel (Ni) | 14.5 – 16.5 |
| Molybdenum (Mo) | 3.8 – 4.5 |
| Nitrogen (N) | 0.15 – 0.21 |
| Copper (Cu) | 2.8 – 4.0 |
Source: ASTM A269/A269M Table 1 for UNS S31727. Cu 2.8–4.0%, Mo 3.8–4.5%, N 0.15–0.21% must appear on the MTC. Table 2 austenitizing range 1975–2155 °F [1080–1180 °C]; hardness 192 HBW / 200 HV or 90 HRB.
Mechanical Properties of A269 UNS S31727
ASTM A269 does not publish a tensile-strength, yield, or elongation acceptance table for UNS S31727. Lot acceptance is built on hardness (Table 2), flaring for seamless tube, flange and reverse flattening for welded tube, and hydro or NDE on each length. Do not invent tensile floors from A213 or A312 unless the purchase order adds them as project extras.
| Property | UNS S31727 requirement (A269 Table 2) |
|---|---|
| Hardness, max | 192 HBW / 200 HV or 90 HRB |
| Tensile / yield / elongation | Not specified as an A269 acceptance table for this grade |
Source: ASTM A269/A269M Table 2 for UNS S31727 (public PDF excerpt where verified). Confirm thin-wall superficial Rockwell alternatives in the purchased edition before writing them into a quality plan.
Seamless and Welded Tube
Under A269, UNS S31727 tubing may be seamless or welded, and hot-finished or cold-finished, unless the purchase order locks the route. Welded A269 tube is autogenous — no filler metal in the longitudinal seam — then cold-worked and solution-treated with the tube. That is not A312 WLD/HCW pipe stencil language; A269 simply records seamless or welded on the product and MTC.
Seamless UNS S31727 takes a lot-basis flaring test; welded UNS S31727 takes flange and reverse-flattening tests so the seam is exercised in both opening and reverse-bend modes. Both routes share Table 2 hardness and the mandatory hydrostatic or nondestructive electric test on each length. SHH STEEL can produce and supply both seamless and welded A269 UNS S31727 against the same Table 1 chemistry and Table 2 hardness floors — name the required route on the enquiry.
Dimensions and Tolerances
Order A269 UNS S31727 by outside diameter and nominal wall thickness, not by pipe schedule as the primary size language. Permissible variations come from A269 Table 4 and the general requirements in ASTM A1016/A1016M; thin-wall ovality rules in clause 12.2 apply when wall thickness falls below the thin-wall thresholds listed for each OD group.
| OD group (A269 Table 4) | Outside diameter tolerance | Wall thickness tolerance |
|---|---|---|
| Up to ½ in. [13 mm] | ±0.005 in. [0.13 mm] | ±15% |
| ½ to 1½ in. [13–38 mm], excl. | ±0.005 in. [0.13 mm] | ±10% |
| 1½ to 3½ in. [38–89 mm], excl. | ±0.010 in. [0.25 mm] | ±10% |
| 3½ to 5½ in. [89–140 mm], excl. | ±0.015 in. [0.38 mm] | ±10% |
| 5½ to 8 in. [140–203 mm], excl. | ±0.030 in. [0.76 mm] | ±10% |
Source: ASTM A269/A269M Table 4 (public PDF excerpt). Footnotes allow wider wall variation on heavy wall or low ID/OD ratios and on sub-½ in. ID non-mandrel tube. If a drawing uses A213 minimum-wall language for UNS S31727, say so on the enquiry so SHH STEEL does not build the wrong wall basis.
Equivalent Grades
UNS S31727 is ordered under A269 as listed in Table 1. Related forms may appear under A213/A312/A240 by the same UNS with different wall bases and mechanical tables.
| Reference | Designation | Note |
|---|---|---|
| ASTM A269 | UNS S31727 | This product standard |
| UNS | S31727 | Chemistry identity |
| Other ASTM forms | Same UNS where listed | Confirm product form before substituting |
Compare A269 UNS S31730 when Cu 4–5% and N 0.45 max are named.
Same-grade pages under related product standards (different wall basis and mechanical tables — not drop-in substitutes for A269 tubing): A312 UNS S31727 and SA312 UNS S31727. Confirm the product form before treating any of those pages as acceptance text for an A269 order.
Heat Treatment and Delivery Condition
All A269 UNS S31727 tube is furnished solution heat-treated. Table 2 sets austenitizing at 1975–2155 °F [1080–1180 °C], followed by water quench or rapid cool by other means. Seamless tube may be quenched immediately after hot forming while still at or above the specified minimum. Ordered final anneals below 1900 °F [1040 °C], when permitted and specified, must be stenciled with the actual temperature after the suffix “HT.”
| Item | UNS S31727 (A269 Table 2) |
|---|---|
| Austenitizing temperature | 1975–2155 °F [1080–1180 °C] |
| Cooling | Water quench or rapid cool |
| Hardness after heat treatment, max | 192 HBW / 200 HV or 90 HRB |
| Delivery condition | Solution heat-treated; pickled or bright-annealed by agreement |
Source: ASTM A269/A269M §6 and Table 2 for UNS S31727 (public excerpt where verified). SHH STEEL’s MTC states the heat-treatment condition actually applied to the shipped lengths.
Corrosion Resistance
Copper with Mo and nitrogen targets chemical environments where Cu helps (often reducing-acid related) while Mo supports localised-attack resistance. Medium-specific — not a universal seawater upgrade. A269 publishes no PREN — do not invent one.
Compare A269 UNS S31730 for higher Cu + high N max, or 6Mo grades for seawater chlorides.
Applications of A269 UNS S31727 Tube
A269 UNS S31727 appears on chemical process tubing specs that name S31727 for Cu-Mo-N austenitic. SHH STEEL can produce and supply that product and will redirect when S31730 or 6Mo better matches the medium.
Not boiler tube or pipe unless those standards separately list the UNS.
When a sister enquiry is for boiler tube or pipe of the same grade, use A312 UNS S31727 and SA312 UNS S31727 instead of stretching an A269 tubing page into the wrong product form.
Weldability
Cu-Mo austenitics need filler matched after review. Mill autogenous A269 welds are solution-treated with the tube; shop welds are not. Note the Table 2 anneal is a temperature range, not only a minimum.
SHH STEEL supplies the mill product and MTC with Cu, Mo, and N reported.
Surface Finishes
Pickled and bright-annealed finishes cover most A269 UNS S31727 orders, and named OD polish grit is quoted as a supplementary finish when the purchase order requires a measured belt polish. Bright anneal is preferred for instrumentation and clean-process ID/OD; pickle is the general-process default when a clean but not bright surface is enough for the duty.
Write any maximum Ra, scrubbed-ID, or electropolish note into the enquiry. SHH STEEL can produce and supply pickled, bright-annealed, and polished A269 UNS S31727 when the mill can measure and report the finish, and we will not claim an unverified polish grade on the certificate.
Inspection and Testing
Lot testing for A269 UNS S31727 covers Table 2 hardness, flaring on seamless tube, and flange plus reverse flattening on welded tube, with lot definitions tied to heat, size, and heat-treatment charge as written in the standard. Each length must also receive a hydrostatic test or a nondestructive electric test; the manufacturer chooses unless the purchase order locks the method, and NDE-tested lengths are marked “NDE” and certified accordingly.
EN 10204 3.1 certificates from SHH STEEL report ladle chemistry against Table 1, solution-treatment condition, hardness against Table 2, and the hydro or NDE statement. PMI, product analysis, and third-party inspection holds are available when named on the order, and we do not skip mandatory tests to shorten lead time.
Packaging and Shipping
Export and domestic packs for A269 UNS S31727 use end caps, size-sorted bundles or crates, and waterproof wrap for ocean freight so OD finish and ends stay protected in transit. Bright-annealed and polished OD get extra sleeve protection against galling; coiled product, when ordered, follows A269’s continuous-coil rule without circumferential butt welds inside the coil.
Stencil and tags typically carry ASTM A269, UNS S31727, size, heat number, seamless or welded identity, and NDE when that route was used. SHH STEEL matches marking to the purchase-order marking clause before dispatch so receiving inspection can verify identity against the MTC.
Why Choose SHH STEEL
SHH STEEL can produce and supply ASTM A269 UNS S31727 as solution-treated seamless or welded tubing with Table 1 Cu-Mo-N chemistry, Table 2 hardness, and EN 10204 3.1 documentation.
If higher copper is specified, we also quote A269 UNS S31730.
Supply Capability
SHH STEEL can produce and supply ASTM A269 UNS S31727 Stainless Steel Tube against the edition, process route, and finish named on your enquiry. Capability and Stock / Available sizes follow.
| Item | SHH STEEL capability |
|---|---|
| Standard | ASTM A269 / A269M |
| Grade | UNS S31727 |
| Product form | Seamless and welded tube (no filler metal for welded), hot- or cold-finished |
| Delivery condition | Solution heat-treated (1975–2155 °F [1080–1180 °C]); pickled or bright-annealed |
| Typical size band | ~6–168 mm OD × 0.5–8.0 mm nominal wall (others by agreement) |
| Testing | Hardness; flaring (seamless) / flange + reverse flattening (welded); hydro or NDE |
| Documents | EN 10204 3.1 MTC; third-party inspection on request |
Stock / Available sizes
Enquiry-oriented supply range — not a frozen warehouse SKU list. Send the OD × nominal-wall list and seamless/welded preference for confirmation against near-term production.
| OD (mm) | Typical nominal walls (mm) | Notes |
|---|---|---|
| 6 / 8 / 10 / 12 / 14 | 0.5 / 0.8 / 1.0 / 1.2 / 1.5 | Instrument / hydraulic; often BA |
| 12.7 / 15.9 / 19.1 / 25.4 / 31.8 | 1.0 / 1.2 / 1.5 / 2.0 / 2.5 | Inch OD process and utility |
| 38.1 / 48.3 / 60.3 / 76.1 | 1.5 / 2.0 / 2.5 / 3.0 / 4.0 | Utility and light process |
| 88.9 / 114.3 / 141.3 / 168.3 | 2.0 / 3.0 / 4.0 / 6.0 / 8.0 | Larger process tube; lock seamless vs welded |
Enquiry tip — Compare A269 UNS S31730 when Cu 4–5% and N 0.45 max are named.
FAQ
-
What is ASTM A269 UNS S31727 stainless steel tube used for?
- A269 UNS S31727 is nominal-wall seamless or welded austenitic tubing for general corrosion-resisting and low- or high-temperature service where this UNS chemistry is specified. It is not Code boiler tube (A213) and not pipe (A312). Put A269 on the purchase order so wall basis and tests match.
-
Does ASTM A269 UNS S31727 include welded tube?
- Yes. Seamless and welded routes are both allowed. Welded tube is autogenous, cold-worked, solution-treated with the tube, and flange- plus reverse-flattening-tested. SHH STEEL can produce and supply both routes. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
-
What hardness limit applies to A269 UNS S31727?
- Where verified, Table 2 lists 192 HBW / 200 HV or 90 HRB after the required solution treatment. A269 does not publish a tensile acceptance table for this grade — do not invent tensile floors from A213 or A312 unless the purchase order adds them. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
-
Is A269 UNS S31727 nominal wall or minimum wall?
- Nominal wall. Write OD × nominal wall on the enquiry unless you agree another wall basis with the mill. Table 4 then governs tolerances. Do not assume A213 minimum-wall practice applies. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
-
What size range can SHH STEEL produce for UNS S31727?
- SHH STEEL can produce and supply about 6–168 mm OD × 0.5–8.0 mm nominal wall in seamless or welded A269 UNS S31727, pickled or bright-annealed, with EN 10204 3.1 MTCs. Other sizes by agreement — send the size list for confirmation. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
-
Which tests are mandatory on A269 UNS S31727 tube?
- Hardness to Table 2 where required; flaring for seamless or flange plus reverse flattening for welded; and hydrostatic or nondestructive electric testing on each length. The mill picks hydro or NDE unless the purchase order locks one. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
-
What certificate does SHH STEEL provide for UNS S31727?
- EN 10204 3.1 MTCs report ladle chemistry against Table 1, solution-treatment condition, hardness against Table 2 where verified, and hydro or NDE. Third-party inspection can be added. Stencil shows ASTM A269, UNS S31727, size, heat, and seamless or welded identity. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
-
How should I enquire for A269 UNS S31727 with SHH STEEL?
- List ASTM A269, grade UNS S31727, seamless or welded, OD × nominal wall, finish, and any hydro/NDE lock. Add the service medium if alloy selection is still open. SHH STEEL can produce and supply to that enquiry. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
-
Why is heat treatment a range for S31727?
- Table 2 lists 1975–2155 °F [1080–1180 °C] for UNS S31727 rather than a single minimum like 1900 °F for many 300-series rows. Confirm the purchased edition and report the actual anneal on the MTC. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
-
S31727 vs S31730 under A269?
- S31727 has Mo ~3.8–4.5% with Cu 2.8–4.0% and N 0.15–0.21%; S31730 has Mo 3–4%, Cu 4–5%, and N 0.45 max with different Ni. Choose the UNS the drawing names. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
Conclusion
ASTM A269 UNS S31727 belongs in the A269 nominal-wall tubing family when this chemistry is named for general-service lines. SHH STEEL can produce and supply seamless and welded A269 UNS S31727, heat-treated and tested per the ordered edition, and documented on EN 10204 3.1 certificates. Start from the A269/A269M hub, then send the OD × nominal-wall list. Contact admin@steelspecs.com for a production-backed offer.