ASTM A269 UNS S31730 Stainless Steel Tube | ASTM A269 Stainless Steel - SHH STEEL

ASTM A269 UNS S31730 Stainless Steel Tube

ASTM A269 UNS S31730 nominal-wall seamless and welded austenitic tubing with Cr 17.0–19.0%, Ni 15.0–16.5%, Mo 3.0–4.0%, Cu 4.0–5.0%, N 0.45 max and C ≤0.030%, solution annealed at ≥1900 °F [1040 °C] with hardness max 192 HBW / 200 HV or 90 HRB. SHH STEEL can produce and supply A269 UNS S31730 tube with EN 10204 3.1 MTCs.
Grade
UNS S31730
Standard
ASTM A269 / A269M
Product form
Seamless and welded tube (no filler metal for welded), heat-treated
Size
Typical OD × nominal wall from ~6 mm to 168 mm OD × 0.5–8.0 mm wall; other OD × wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Seamless and Welded
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A269 UNS S31730 Stainless Steel Tube

ASTM A269 / A269M covers nominal-wall seamless and welded austenitic stainless steel tubing for general corrosion-resisting and low- or high-temperature service. UNS S31730 is listed in Table 1 without a TP letter — it is ordered and marked by UNS number — as a copper-bearing, nitrogen-strengthened Mo austenitic with carbon ≤0.030%, chromium 17.0–19.0%, nickel 15.0–16.5%, molybdenum 3.0–4.0%, copper 4.0–5.0%, and nitrogen up to 0.45%. Buyers use A269 UNS S31730 when the duty needs Mo plus copper for sulphuric and similar reducing-acid resistance that plain TP317 does not target. The purchase order must name ASTM A269 and UNS S31730 so nominal-wall rules, hardness, flaring or flange tests, and marking apply to tubing rather than to an A213 or A312 product text.

SHH STEEL can produce and supply ASTM A269 UNS S31730 stainless steel tube as seamless and welded product in the instrument-to-process OD × nominal-wall band, solution annealed, with EN 10204 3.1 mill test certificates reporting Table 1 ladle chemistry and Table 2 hardness. Typical sizes run about 6–168 mm OD × 0.5–8.0 mm nominal wall; other sizes by agreement. Compare on the A269/A269M hub with A269 TP317, A269 TP316L, and 6Mo A269 UNS S31254. Keep the wall basis nominal.

If the duty is actually boiler / heat-exchanger minimum-wall tube or pipe rather than A269 nominal-wall tubing, open A312 UNS S31730 and SA312 UNS S31730 and match the product standard to the drawing.

Chemical Composition of A269 UNS S31730

Heat analysis under Table 1 is mandatory for every UNS S31730 heat; product analysis applies when ordered through A1016/A1016M and A480 Table A1.1. SHH STEEL reports measured ladle and, when ordered, product values — never unpublished tighter catalogue windows.

Melting limits below come from public A269 Table 1 excerpts for UNS S31730 (ASTM abstract cross-checked with the tubingchina A269 PDF). Note the tight sulfur (≤0.010%) and phosphorus (≤0.040%) ceilings beside the Cu and N additions. Confirm the purchased edition.

Melting analysis (heat / ladle analysis) — Table 1

Element UNS S31730 melting analysis
Carbon (C) ≤ 0.030
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.040
Sulfur (S) ≤ 0.010
Silicon (Si) ≤ 1.00
Chromium (Cr) 17.0 – 19.0
Nickel (Ni) 15.0 – 16.5
Molybdenum (Mo) 3.0 – 4.0
Nitrogen (N) 0.45 max
Copper (Cu) 4.0 – 5.0

Source: ASTM A269/A269M Table 1 for UNS S31730 (public excerpts). Read copper and nitrogen with molybdenum: Cu 4.0–5.0% is the acid-service signature that separates this UNS from TP317; N up to 0.45% is a high ceiling that must be reported; Mo 3–4% keeps localised-attack resistance in the higher-Mo austenitic band. Carbon ≤0.030% is already in L-grade territory for as-welded behaviour.

Mechanical Properties of A269 UNS S31730

A269 does not publish a tensile acceptance table for UNS S31730. Lot acceptance rests on Table 2 hardness (192 HBW / 200 HV or 90 HRB), flaring for seamless tube, flange and reverse flattening for welded tube, and hydro or NDE on each length. Do not invent tensile floors from A213 or A312 unless the purchase order adds them.

Property UNS S31730 requirement (A269 Table 2)
Hardness, max 192 HBW / 200 HV or 90 HRB
Tensile / yield / elongation Not specified as an A269 acceptance table for this grade

Source: ASTM A269/A269M Table 2 for UNS S31730 (public PDF excerpt). Confirm thin-wall superficial Rockwell alternatives in the purchased edition before writing them into a quality plan.

Seamless and Welded Tube

UNS S31730 under A269 may be seamless or welded, hot- or cold-finished. Welded A269 tube is autogenous (no filler metal), cold-worked, and solution-treated with the tube — not an A312 WLD/HCW pipe product. Seamless takes flaring; welded takes flange and reverse flattening; both share hardness and hydro/NDE.

Because copper and nitrogen are mandatory Table 1 elements, the MTC must report them for either process route. SHH STEEL can produce and supply both seamless and welded A269 UNS S31730 against the same chemistry and hardness floors — name the required route on the enquiry.

Dimensions and Tolerances

Order by OD and nominal wall thickness. A269 Table 4 sets OD, wall, and cut-length tolerances; clause 12.2 covers thin-wall ovality. Do not use pipe schedule as the primary size language on an A269 tubing order.

OD group (A269 Table 4) Outside diameter tolerance Wall thickness tolerance
Up to ½ in. [13 mm] ±0.005 in. [0.13 mm] ±15%
½ to 1½ in. [13–38 mm], excl. ±0.005 in. [0.13 mm] ±10%
1½ to 3½ in. [38–89 mm], excl. ±0.010 in. [0.25 mm] ±10%
3½ to 5½ in. [89–140 mm], excl. ±0.015 in. [0.38 mm] ±10%
5½ to 8 in. [140–203 mm], excl. ±0.030 in. [0.76 mm] ±10%

Source: ASTM A269/A269M Table 4 (public PDF excerpt). Footnotes allow wider wall variation on heavy wall / low ID/OD and on sub-½ in. ID non-mandrel tube. Flag A213 minimum-wall drawings explicitly on the enquiry.

Equivalent Grades

UNS S31730 is ordered by UNS number under A269 — there is no TP letter in the public Table 1 column for this grade. Related chemistries may appear under other ASTM product standards by the same UNS; plate or pipe cousins are not drop-in substitutes for A269 tubing without checking wall basis and mechanical acceptance.

Reference Designation Note
ASTM A269 UNS S31730 This product standard (no TP letter)
UNS S31730 Chemistry identity
ASTM A269 sister TP317 / S31700 3–4% Mo without Cu / high-N package
Other ASTM forms Same UNS where listed Confirm product form before substituting

Inside A269, step to A269 TP317 when copper is not required, or to a 6Mo grade when chlorides outgrow this chemistry.

Same-grade pages under related product standards (different wall basis and mechanical tables — not drop-in substitutes for A269 tubing): A312 UNS S31730 and SA312 UNS S31730. Confirm the product form before treating any of those pages as acceptance text for an A269 order.

Heat Treatment and Delivery Condition

All A269 UNS S31730 ships solution heat-treated. Table 2 requires ≥1900 °F [1040 °C] austenitizing with water quench or rapid cool. Ordered anneals below 1900 °F must be stenciled with the actual temperature after “HT.”

Item UNS S31730 (A269 Table 2)
Austenitizing temperature, min 1900 °F [1040 °C]
Cooling Water quench or rapid cool
Hardness after heat treatment, max 192 HBW / 200 HV or 90 HRB
Delivery condition Solution heat-treated; pickled or bright-annealed by agreement

Source: ASTM A269/A269M §6 and Table 2 for UNS S31730. SHH STEEL’s MTC states the heat-treatment condition applied to the shipped lengths and will not mark the grade if the anneal falls outside the ordered Table 2 requirement.

Corrosion Resistance

UNS S31730 is aimed at duties where copper helps in reducing-acid and related chemical environments while molybdenum supports localised-attack resistance and low carbon supports as-welded behaviour. It is not a blanket upgrade over TP316L for every chloride duty — copper’s benefit is medium-specific — and it is not a 6Mo seawater alloy.

A269 publishes no PREN table for S31730 — do not invent one. Match the medium with a materials engineer: sulphuric and similar reducing services are the usual reason this UNS appears on a tubing BOM; seawater splash often still needs A269 UNS S31254 or higher.

Applications of A269 UNS S31730 Tube

A269 UNS S31730 shows up on chemical process tubing where copper-bearing Mo austenitic is specified, on acid-plant utility and transfer lines written to A269, and on projects that already standardized on S31730 across product forms. Bright-annealed cold-finished tube is common on skids; pickled welded tube covers larger runs.

Skip it for Code boiler tube (A213) and pipe headers (A312) unless those standards separately list the UNS. SHH STEEL can produce and supply A269 UNS S31730 in the general-service band above and will redirect when the medium needs 6Mo or a different copper-bearing alloy family.

When a sister enquiry is for boiler tube or pipe of the same grade, use A312 UNS S31730 and SA312 UNS S31730 instead of stretching an A269 tubing page into the wrong product form.

Weldability

Low carbon helps as-welded behaviour, but copper-bearing austenitics need filler and procedure choices matched to the alloy — do not assume a generic 316L filler is automatic without engineering review. Mill autogenous A269 welds are already solution-treated with the tube; shop welds on cut lengths sit outside that mill anneal.

Filler selection and procedure qualification remain the fabricator’s scope unless purchased separately. SHH STEEL supplies the mill product and MTC with Cu, Mo, and N reported as Table 1 requires.

Surface Finishes

Pickled and bright-annealed finishes cover most A269 UNS S31730 orders; named OD polish is supplementary when required. Bright anneal suits instrumentation and clean-process ID/OD; pickle is the general-process default.

Write Ra or scrubbed-ID notes into the enquiry. SHH STEEL can produce and supply those finishes when the mill can measure and report them, and we will not claim an unverified polish grade.

Inspection and Testing

Lots are hardness-tested to Table 2, flare-tested when seamless, and flange- plus reverse-flattening-tested when welded. Each length takes hydro or NDE; the mill chooses unless the order locks the method. NDE lengths are marked and certified accordingly.

EN 10204 3.1 certificates from SHH STEEL report ladle chemistry including copper, molybdenum, and nitrogen, heat treatment, hardness, and hydro/NDE. PMI and third-party holds are available when named on the order.

Packaging and Shipping

End caps, bundled sleeves or crates, and waterproof wrap protect UNS S31730 tube in transit. Bright-annealed and polished OD get extra sleeve protection. Coiled product follows A269’s continuous-coil rule without circumferential butt welds inside the coil.

Stencil carries ASTM A269, UNS S31730, size, heat, seamless or welded identity, and NDE when applicable. SHH STEEL matches marking to the purchase-order clause before dispatch.

Why Choose SHH STEEL

SHH STEEL can produce and supply ASTM A269 UNS S31730 as solution-treated seamless or welded tubing with Table 1 chemistry — including copper, molybdenum, and nitrogen — Table 2 hardness, and EN 10204 3.1 documentation. We will not ship TP317 and call it S31730, and we will not omit Cu or N from the certificate when the UNS requires them.

If the medium does not need copper, we point to A269 TP317 or A269 TP316L rather than selling an over-alloyed stamp into the wrong duty.

Supply Capability

SHH STEEL can produce and supply ASTM A269 UNS S31730 to the edition, route, and finish on your enquiry. Capability and Stock / Available sizes follow as an enquiry-oriented map — not a frozen tonnage list.

Item SHH STEEL capability for UNS S31730
Standard ASTM A269 / A269M
Grade UNS S31730
Product form Seamless and welded tube (no filler metal for welded), hot- or cold-finished
Delivery condition Solution heat-treated ≥1900 °F [1040 °C]; pickled or bright-annealed
Typical size band ~6–168 mm OD × 0.5–8.0 mm nominal wall (others by agreement)
Testing Hardness; flaring (seamless) / flange + reverse flattening (welded); hydro or NDE
Documents EN 10204 3.1 MTC; third-party inspection on request

Stock / Available sizes

Send the OD × nominal-wall list and seamless/welded preference for confirmation against near-term production. Peer size catalogues were used only to sanity-check typical instrument and process OD × wall bands.

OD (mm) Typical nominal walls (mm) Notes
6 / 8 / 10 / 12 / 14 0.5 / 0.8 / 1.0 / 1.2 / 1.5 Instrument band; often BA
12.7 / 19.1 / 25.4 / 31.8 1.0 / 1.5 / 2.0 / 2.5 Inch OD process skids
38.1 / 48.3 / 60.3 / 76.1 1.5 / 2.0 / 3.0 / 4.0 Chemical utility / transfer
88.9 / 114.3 / 141.3 / 168.3 2.0 / 3.0 / 4.0 / 6.0 / 8.0 Larger process tube; lock seamless vs welded

Parallel quotes against A269 TP317 keep the copper decision visible on one size list.

FAQ

What is ASTM A269 UNS S31730 used for?
A269 UNS S31730 is a copper-bearing, nitrogen-strengthened Mo austenitic tubing grade for chemical process and related general-service lines where Cu plus 3–4% Mo is specified. It is nominal-wall seamless or welded tubing under ASTM A269 — not boiler tube and not pipe. Order by UNS S31730 because the public Table 1 listing has no TP letter for this grade.
How is UNS S31730 different from TP317 under A269?
TP317 (S31700) is a 3–4% Mo austenitic without the copper and high-nitrogen package. UNS S31730 adds Cu 4.0–5.0%, N up to 0.45%, tighter S/P ceilings, and C ≤0.030%. They are separate Table 1 grades — do not substitute one for the other on the MTC without a materials review of the medium.
Does A269 UNS S31730 include welded tube?
Yes. Seamless and welded routes are both allowed. Welded tube is autogenous, cold-worked, solution-treated with the tube, and flange- plus reverse-flattening-tested. SHH STEEL can produce and supply both routes against the same Table 1 chemistry, including mandatory copper and nitrogen reporting.
What hardness limit applies to A269 UNS S31730?
Table 2 caps UNS S31730 at 192 HBW / 200 HV or 90 HRB after solution treatment at ≥1900 °F [1040 °C]. A269 does not publish a tensile acceptance table for this grade — do not invent tensile floors from A213 or A312 unless the purchase order adds them.
Must copper and nitrogen appear on the MTC?
Yes. Copper 4.0–5.0% and nitrogen (0.45 max) are Table 1 requirements for UNS S31730, so the ladle analysis on an EN 10204 3.1 certificate should report both alongside molybdenum. A certificate that only shows a “317-type” nickname without Cu and N is incomplete for this UNS.
Is A269 UNS S31730 nominal wall or minimum wall?
Nominal wall. Write OD × nominal wall on the enquiry unless you agree another wall basis with the mill. Table 4 then governs tolerances. Do not assume A213 minimum-wall boiler-tube practice applies to an A269 UNS S31730 order.
What size range can SHH STEEL produce for UNS S31730?
SHH STEEL can produce and supply about 6–168 mm OD × 0.5–8.0 mm nominal wall in seamless or welded A269 UNS S31730, pickled or bright-annealed, with EN 10204 3.1 MTCs. Other sizes by agreement — send the size list for confirmation against near-term production.
When should I choose 6Mo instead of UNS S31730?
Choose a 6Mo A269 grade such as UNS S31254 when seawater or aggressive chloride pitting outgrows this copper-bearing Mo austenitic. UNS S31730 is typically selected for copper-aided chemical service, not as a universal seawater substitute. Match the medium with a materials review.
Which tests are mandatory on A269 UNS S31730?
Hardness to Table 2; flaring for seamless or flange plus reverse flattening for welded; and hydrostatic or nondestructive electric testing on each length. The mill picks hydro or NDE unless the purchase order locks one. Product analysis and PMI are supplementary when ordered.
What certificate does SHH STEEL provide?
EN 10204 3.1 MTCs report ladle chemistry including Cu, Mo, and N, solution-treatment condition, hardness, and hydro or NDE. Third-party inspection can be added. Stencil shows ASTM A269, UNS S31730, size, heat, and seamless or welded identity.
How should I enquire for A269 UNS S31730 with SHH STEEL?
List ASTM A269, grade UNS S31730, seamless or welded, OD × nominal wall, finish, and any hydro/NDE lock. Note that Cu and N must appear on the MTC. SHH STEEL can produce and supply to that enquiry or recommend TP317 / TP316L / 6Mo when the medium points that way.

Conclusion

ASTM A269 UNS S31730 is the copper-bearing, nitrogen-strengthened Mo austenitic inside the A269 nominal-wall tubing family when chemical service needs Cu plus 3–4% Mo rather than plain TP317. SHH STEEL can produce and supply seamless and welded A269 UNS S31730, solution annealed to Table 2, tested, and documented on EN 10204 3.1 certificates. Start from the A269/A269M hub, then send the OD × nominal-wall list. Contact admin@steelspecs.com for a production-backed offer.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X