ASTM A269 TP XM-19 Stainless Steel Tube | ASTM A269 Stainless Steel - SHH STEEL

ASTM A269 TP XM-19 Stainless Steel Tube

ASTM A269 TP XM-19 / UNS S20910 nominal-wall seamless and welded nitrogen-strengthened austenitic tubing (Nitronic 50 type) with Cr 20.5–23.5%, Ni 11.5–13.5%, Mo 1.50–3.00%, N 0.20–0.40%, Mn 4.0–6.0%, Cb 0.10–0.30% and V 0.10–0.30%, solution annealed at ≥1900 °F [1040 °C] with hardness max 269 HBW / 285 HV or 25 HRC. SHH STEEL can produce and supply A269 TP XM-19 tube with EN 10204 3.1 MTCs.
Grade
TP XM-19 / UNS S20910
Standard
ASTM A269 / A269M
Product form
Seamless and welded tube (no filler metal for welded), heat-treated
Size
Typical OD × nominal wall from ~6 mm to 168 mm OD × 0.5–8.0 mm wall; other OD × wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Seamless and Welded
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A269 TP XM-19 Stainless Steel Tube

ASTM A269 / A269M covers nominal-wall seamless and welded austenitic stainless steel tubing for general corrosion-resisting and low- or high-temperature service. Grade TP XM-19 / UNS S20910 is the nitrogen-strengthened, molybdenum-bearing austenitic often associated with Nitronic 50-type chemistry: Cr 20.5–23.5%, Ni 11.5–13.5%, Mo 1.50–3.00%, N 0.20–0.40%, Mn 4.0–6.0%, plus Cb and V ranges, with C ≤0.06%. Buyers specify A269 TP XM-19 when the list wants higher strength austenitic with Mo and N rather than commodity 316. Name ASTM A269 on the purchase order so nominal-wall rules and hardness apply to tubing.

SHH STEEL can produce and supply ASTM A269 TP XM-19 stainless steel tube as seamless and welded product, solution annealed, with EN 10204 3.1 certificates. Typical sizes ~6–168 mm OD × 0.5–8.0 mm nominal wall; other sizes by agreement. Compare on the A269/A269M hub with A269 TP316L and A269 TP XM-29. Keep the wall basis nominal.

If the duty is actually boiler / heat-exchanger minimum-wall tube or pipe rather than A269 nominal-wall tubing, open A213 TP XM-19, SA213 TP XM-19, A312 TP XM-19 and SA312 TP XM-19 and match the product standard to the drawing.

Chemical Composition of A269 TP XM-19

Heat analysis under A269 Table 1 is mandatory for every TP XM-19 heat; product analysis applies when ordered through ASTM A1016/A1016M and A480/A480M Table A1.1 tolerances. SHH STEEL reports measured ladle values — and product values when ordered — without advertising unpublished tighter catalogue windows.

Public A269 Table 1 excerpts for TP XM-19 / UNS S20910 (ASTM abstract + tubingchina A269 PDF). Mo + N + Cb + V with elevated Cr/Mn define this Nitronic 50-type chemistry.

Melting analysis (heat / ladle analysis) — Table 1

Element TP XM-19 / UNS S20910 melting analysis
Carbon (C) ≤ 0.06
Manganese (Mn) 4.0 – 6.0
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 20.5 – 23.5
Nickel (Ni) 11.5 – 13.5
Molybdenum (Mo) 1.50 – 3.00
Nitrogen (N) 0.20 – 0.40
Columbium (Cb / Nb) 0.10 – 0.30
Vanadium (V) 0.10 – 0.30

Source: ASTM A269/A269M Table 1 for TP XM-19 / UNS S20910. Nitrogen 0.20–0.40% and Mo 1.50–3.00% must both appear on the MTC with Cb and V. Table 2 hardness ceiling is 269 HBW / 25 HRC — higher than commodity 304/316 rows. (Public PDF layout showed a garbled “269 HBW/25 HV” fragment; Rockwell 25 HRC is the consistent Table 2 companion used for XM-10/11/19 in the same excerpt — confirm purchased edition.)

Mechanical Properties of A269 TP XM-19

ASTM A269 does not publish a tensile-strength, yield, or elongation acceptance table for TP XM-19. Lot acceptance is built on hardness (Table 2), flaring for seamless tube, flange and reverse flattening for welded tube, and hydro or NDE on each length. Do not invent tensile floors from A213 or A312 unless the purchase order adds them as project extras. Hardness Figure 2 for XM-19 is listed with HBW/HV and 25 HRC companions in the public excerpt; confirm the purchased edition if quality plans cite superficial scales.

Property TP XM-19 requirement (A269 Table 2)
Hardness, max 269 HBW / 285 HV or 25 HRC
Tensile / yield / elongation Not specified as an A269 acceptance table for this grade

Source: ASTM A269/A269M Table 2 for TP XM-19 (public PDF excerpt where verified). Confirm thin-wall superficial Rockwell alternatives in the purchased edition before writing them into a quality plan.

Seamless and Welded Tube

Under A269, TP XM-19 tubing may be seamless or welded, and hot-finished or cold-finished, unless the purchase order locks the route. Welded A269 tube is autogenous — no filler metal in the longitudinal seam — then cold-worked and solution-treated with the tube. That is not A312 WLD/HCW pipe stencil language; A269 simply records seamless or welded on the product and MTC.

Seamless TP XM-19 takes a lot-basis flaring test; welded TP XM-19 takes flange and reverse-flattening tests so the seam is exercised in both opening and reverse-bend modes. Both routes share Table 2 hardness and the mandatory hydrostatic or nondestructive electric test on each length. SHH STEEL can produce and supply both seamless and welded A269 TP XM-19 against the same Table 1 chemistry and Table 2 hardness floors — name the required route on the enquiry.

Dimensions and Tolerances

Order A269 TP XM-19 by outside diameter and nominal wall thickness, not by pipe schedule as the primary size language. Permissible variations come from A269 Table 4 and the general requirements in ASTM A1016/A1016M; thin-wall ovality rules in clause 12.2 apply when wall thickness falls below the thin-wall thresholds listed for each OD group.

OD group (A269 Table 4) Outside diameter tolerance Wall thickness tolerance
Up to ½ in. [13 mm] ±0.005 in. [0.13 mm] ±15%
½ to 1½ in. [13–38 mm], excl. ±0.005 in. [0.13 mm] ±10%
1½ to 3½ in. [38–89 mm], excl. ±0.010 in. [0.25 mm] ±10%
3½ to 5½ in. [89–140 mm], excl. ±0.015 in. [0.38 mm] ±10%
5½ to 8 in. [140–203 mm], excl. ±0.030 in. [0.76 mm] ±10%

Source: ASTM A269/A269M Table 4 (public PDF excerpt). Footnotes allow wider wall variation on heavy wall or low ID/OD ratios and on sub-½ in. ID non-mandrel tube. If a drawing uses A213 minimum-wall language for TP XM-19, say so on the enquiry so SHH STEEL does not build the wrong wall basis.

Equivalent Grades

TP XM-19 / UNS S20910 is the ASTM tubing designation for this Nitronic 50-type chemistry. Commercial nicknames do not replace the UNS on the MTC.

Reference Designation Note
ASTM A269 TP XM-19 / UNS S20910 This product standard
UNS S20910 Chemistry identity
Shop name Nitronic 50 type Commercial nickname — confirm UNS

Step to A269 TP316L when standard Mo L-grade is enough, or to 6Mo grades when chlorides outgrow 1.5–3% Mo.

Same-grade pages under related product standards (different wall basis and mechanical tables — not drop-in substitutes for A269 tubing): A213 TP XM-19, SA213 TP XM-19, A312 TP XM-19 and SA312 TP XM-19. Confirm the product form before treating any of those pages as acceptance text for an A269 order.

Heat Treatment and Delivery Condition

All A269 TP XM-19 tube is furnished solution heat-treated. Table 2 sets austenitizing at ≥1900 °F [1040 °C], followed by water quench or rapid cool by other means. Seamless tube may be quenched immediately after hot forming while still at or above the specified minimum. Ordered final anneals below 1900 °F [1040 °C], when permitted and specified, must be stenciled with the actual temperature after the suffix “HT.”

Item TP XM-19 (A269 Table 2)
Austenitizing temperature ≥1900 °F [1040 °C]
Cooling Water quench or rapid cool
Hardness after heat treatment, max 269 HBW / 285 HV or 25 HRC
Delivery condition Solution heat-treated; pickled or bright-annealed by agreement

Source: ASTM A269/A269M §6 and Table 2 for TP XM-19 (public excerpt where verified). SHH STEEL’s MTC states the heat-treatment condition actually applied to the shipped lengths.

Corrosion Resistance

Mo plus elevated Cr and N give XM-19 better localised-attack potential than plain 304 in many chloride-aware general services, while nitrogen strengthens the austenite. It is still not a 6Mo seawater alloy. A269 publishes no PREN for S20910 — do not invent one from marketing sheets.

Match the medium; for seawater splash, compare A269 UNS S31254.

Applications of A269 TP XM-19 Tube

A269 TP XM-19 appears on process and utility tubing specs that call S20910 / XM-19 / Nitronic 50-type chemistry for higher-strength Mo-N austenitic service. SHH STEEL can produce and supply that product and will redirect when 316L or 6Mo is the safer fit.

It is not boiler tube (A213) or pipe (A312) unless those standards separately list the UNS.

When a sister enquiry is for boiler tube or pipe of the same grade, use A213 TP XM-19, SA213 TP XM-19, A312 TP XM-19 and SA312 TP XM-19 instead of stretching an A269 tubing page into the wrong product form.

Weldability

Nitrogen-strengthened Mo austenitics need filler and procedure matched to S20910 — do not assume generic 316L filler without review. Mill autogenous A269 welds are solution-treated with the tube; shop welds are not.

SHH STEEL supplies the mill product and MTC with Mo, N, Cb, and V reported.

Surface Finishes

Pickled and bright-annealed finishes cover most A269 TP XM-19 orders, and named OD polish grit is quoted as a supplementary finish when the purchase order requires a measured belt polish. Bright anneal is preferred for instrumentation and clean-process ID/OD; pickle is the general-process default when a clean but not bright surface is enough for the duty.

Write any maximum Ra, scrubbed-ID, or electropolish note into the enquiry. SHH STEEL can produce and supply pickled, bright-annealed, and polished A269 TP XM-19 when the mill can measure and report the finish, and we will not claim an unverified polish grade on the certificate.

Inspection and Testing

Lot testing for A269 TP XM-19 covers Table 2 hardness, flaring on seamless tube, and flange plus reverse flattening on welded tube, with lot definitions tied to heat, size, and heat-treatment charge as written in the standard. Each length must also receive a hydrostatic test or a nondestructive electric test; the manufacturer chooses unless the purchase order locks the method, and NDE-tested lengths are marked “NDE” and certified accordingly.

EN 10204 3.1 certificates from SHH STEEL report ladle chemistry including Mo, N, Cb, and V, solution-treatment condition, hardness against Table 2, and the hydro or NDE statement. PMI, product analysis, and third-party inspection holds are available when named on the order, and we do not skip mandatory tests to shorten lead time.

Packaging and Shipping

Export and domestic packs for A269 TP XM-19 use end caps, size-sorted bundles or crates, and waterproof wrap for ocean freight so OD finish and ends stay protected in transit. Bright-annealed and polished OD get extra sleeve protection against galling; coiled product, when ordered, follows A269’s continuous-coil rule without circumferential butt welds inside the coil.

Stencil and tags typically carry ASTM A269, TP XM-19 / S20910, size, heat number, seamless or welded identity, and NDE when that route was used. SHH STEEL matches marking to the purchase-order marking clause before dispatch so receiving inspection can verify identity against the MTC.

Why Choose SHH STEEL

SHH STEEL can produce and supply ASTM A269 TP XM-19 as solution-treated seamless or welded tubing with full Table 1 chemistry — including Mo, N, Cb, and V — Table 2 hardness, and EN 10204 3.1 documentation. We will not relabel 316 as XM-19.

If standard 316L is enough, we say so; if 6Mo is needed, we point there.

Supply Capability

SHH STEEL can produce and supply ASTM A269 TP XM-19 Stainless Steel Tube against the edition, process route, and finish named on your enquiry. Capability and Stock / Available sizes follow.

Item SHH STEEL capability
Standard ASTM A269 / A269M
Grade TP XM-19 / UNS S20910
Product form Seamless and welded tube (no filler metal for welded), hot- or cold-finished
Delivery condition Solution heat-treated (≥1900 °F [1040 °C]); pickled or bright-annealed
Typical size band ~6–168 mm OD × 0.5–8.0 mm nominal wall (others by agreement)
Testing Hardness; flaring (seamless) / flange + reverse flattening (welded); hydro or NDE
Documents EN 10204 3.1 MTC; third-party inspection on request

Stock / Available sizes

Enquiry-oriented supply range — not a frozen warehouse SKU list. Send the OD × nominal-wall list and seamless/welded preference for confirmation against near-term production.

OD (mm) Typical nominal walls (mm) Notes
6 / 8 / 10 / 12 / 14 0.5 / 0.8 / 1.0 / 1.2 / 1.5 Instrument / hydraulic; often BA
12.7 / 15.9 / 19.1 / 25.4 / 31.8 1.0 / 1.2 / 1.5 / 2.0 / 2.5 Inch OD process and utility
38.1 / 48.3 / 60.3 / 76.1 1.5 / 2.0 / 2.5 / 3.0 / 4.0 Utility and light process
88.9 / 114.3 / 141.3 / 168.3 2.0 / 3.0 / 4.0 / 6.0 / 8.0 Larger process tube; lock seamless vs welded

Parallel quotes against A269 TP316L keep Mo-N vs L-grade cost visible.

FAQ

What is ASTM A269 TP XM-19 used for?
A269 TP XM-19 / UNS S20910 is nominal-wall seamless or welded austenitic tubing for general corrosion-resisting and low- or high-temperature service where this chemistry is specified. It is not Code boiler tube (A213) and not pipe (A312). Put A269 on the purchase order so wall basis and tests match.
Does A269 TP XM-19 include welded tube?
Yes. Seamless and welded routes are both allowed. Welded tube is autogenous, cold-worked, solution-treated with the tube, and flange- plus reverse-flattening-tested. SHH STEEL can produce and supply both routes. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
What hardness limit applies to A269 TP XM-19?
Table 2 caps TP XM-19 at 269 HBW / 285 HV or 25 HRC after the required solution heat treatment. A269 does not publish a tensile acceptance table for this grade — do not invent tensile floors from A213 or A312 unless the purchase order adds them.
Is A269 TP XM-19 nominal wall or minimum wall?
Nominal wall. Write OD × nominal wall on the enquiry unless you agree another wall basis with the mill. Table 4 then governs tolerances. Do not assume A213 minimum-wall practice applies. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
What size range can SHH STEEL produce for TP XM-19?
SHH STEEL can produce and supply about 6–168 mm OD × 0.5–8.0 mm nominal wall in seamless or welded A269 TP XM-19, pickled or bright-annealed, with EN 10204 3.1 MTCs. Other sizes by agreement — send the size list for confirmation. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
Which tests are mandatory on A269 TP XM-19?
Hardness to Table 2; flaring for seamless or flange plus reverse flattening for welded; and hydrostatic or nondestructive electric testing on each length. The mill picks hydro or NDE unless the purchase order locks one. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
What certificate does SHH STEEL provide?
EN 10204 3.1 MTCs report ladle chemistry against Table 1, solution-treatment condition, hardness against Table 2, and hydro or NDE. Third-party inspection can be added. Stencil shows ASTM A269, TP XM-19 / S20910, size, heat, and seamless or welded identity. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
How should I enquire for A269 TP XM-19?
List ASTM A269, grade TP XM-19 / UNS S20910, seamless or welded, OD × nominal wall, finish, and any hydro/NDE lock. Add the service medium if grade selection is still open. SHH STEEL can produce and supply to that enquiry. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
Is TP XM-19 the same as Nitronic 50?
Nitronic 50 is a commercial name often associated with UNS S20910 chemistry. For an A269 order, the purchase order and MTC must carry ASTM A269 and TP XM-19 / UNS S20910 — a trademark nickname alone is not the product standard. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
Why are Cb and V required on the MTC?
Table 1 sets Cb 0.10–0.30% and V 0.10–0.30% for TP XM-19, so ladle analysis should report both with Mo and N. Omitting them leaves the certificate incomplete for S20910. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.
XM-19 vs TP316L under A269?
TP316L is low-carbon 2–3% Mo 16-10 austenitic with a 192 HBW / 90 HRB ceiling. XM-19 adds higher Cr, Mn, N, Cb, and V with a higher hardness ceiling. Choose based on the UNS and mechanical intent the drawing names. Confirm the purchased A269/A269M edition, OD × nominal wall, and seamless or welded route on the purchase order before treating secondary catalogues as acceptance text.

Conclusion

ASTM A269 TP XM-19 / UNS S20910 is the Mo-N strengthened austenitic (Nitronic 50 type) inside the A269 nominal-wall tubing family when S20910 is named. SHH STEEL can produce and supply seamless and welded A269 TP XM-19, solution annealed to Table 2, tested, and documented on EN 10204 3.1 certificates. Start from the A269/A269M hub, then send the OD × nominal-wall list. Contact admin@steelspecs.com for a production-backed offer.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X