ASTM A269 TP316LN Stainless Steel Tube | ASTM A269 Stainless Steel - SHH STEEL

ASTM A269 TP316LN Stainless Steel Tube

ASTM A269 TP316LN / UNS S31653 nominal-wall seamless and welded austenitic tubing with C ≤0.035%, N 0.10–0.16%, Cr 16.0–18.0%, Ni 10.0–13.0% and Mo 2.00–3.00%, solution annealed at ≥1900 °F [1040 °C] with hardness max 192 HBW / 200 HV or 90 HRB. SHH STEEL can produce and supply A269 TP316LN tube with EN 10204 3.1 MTCs.
Grade
TP316LN / UNS S31653
Standard
ASTM A269 / A269M
Product form
Seamless and welded tube (no filler metal for welded), heat-treated
Size
Typical OD × nominal wall from ~6 mm to 168 mm OD × 0.5–8.0 mm wall; other OD × wall by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Seamless and Welded
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A269 TP316LN Stainless Steel Tube

ASTM A269 / A269M specifies nominal-wall seamless and welded austenitic stainless steel tubing for general corrosion-resisting and low- or high-temperature service. Grade TP316LN is the nitrogen-bearing low-carbon molybdenum grade under UNS S31653: carbon ≤0.035%, nitrogen 0.10–0.16%, chromium 16.0–18.0%, nickel 10.0–13.0%, and molybdenum 2.00–3.00%. Specifiers put LN on the purchase order when they want L-grade as-welded behaviour, Mo for chlorides, and a reported nitrogen range on the MTC — not a heat-treatment nickname on ordinary TP316L. Shop language still says “316LN tube,” but the certificate must carry ASTM A269 Grade TP316LN so nominal-wall tolerances, hardness, and flaring or flange tests apply rather than an A213 or A312 product text.

SHH STEEL can produce and supply ASTM A269 TP316LN stainless steel tube as seamless and welded product in the instrument-to-process OD × nominal-wall band, solution annealed, with EN 10204 3.1 certificates covering Table 1 chemistry and Table 2 hardness. Typical enquiry sizes run about 6–168 mm OD × 0.5–8.0 mm nominal wall; other sizes by agreement. Compare the family on the A269/A269M hub alongside A269 TP316L, A269 TP316, and A269 TP304LN. Keep the wall basis nominal.

If the duty is actually boiler / heat-exchanger minimum-wall tube or pipe rather than A269 nominal-wall tubing, open A312 TP316LN and SA312 TP316LN and match the product standard to the drawing.

Chemical Composition of A269 TP316LN

Heat analysis under Table 1 is mandatory for every TP316LN heat; product analysis applies when ordered through A1016/A1016M and A480 Table A1.1. SHH STEEL reports measured ladle and, when ordered, product values — never unpublished tighter catalogue windows.

Melting limits below come from public A269 Table 1 excerpts for TP316LN / UNS S31653 (ASTM abstract cross-checked with the tubingchina A269 PDF). Footnote B on carbon for small-OD / light-wall drawing practice applies. Confirm the purchased edition.

Melting analysis (heat / ladle analysis) — Table 1

Element TP316LN (UNS S31653) melting analysis
Carbon (C) ≤ 0.035 B
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 16.0 – 18.0
Nickel (Ni) 10.0 – 13.0
Molybdenum (Mo) 2.00 – 3.00
Nitrogen (N) 0.10 – 0.16

Source: ASTM A269/A269M Table 1 for TP316LN / UNS S31653 (public excerpts). Read carbon, molybdenum, and nitrogen together: C ≤0.035% protects as-welded HAZs, Mo 2–3% raises chloride pitting resistance versus 304LN, and N at 0.10–0.16% must appear on the MTC. Nickel stays in a 10–13% band (narrower than TP316L’s 10–15%).

Mechanical Properties of A269 TP316LN

A269 does not publish a tensile acceptance table for TP316LN. Lot acceptance rests on Table 2 hardness (192 HBW / 200 HV or 90 HRB), flaring for seamless tube, flange and reverse flattening for welded tube, and hydro or NDE on each length. Nitrogen strengthens annealed austenite in service, but that effect is not written as an A269 tensile floor — do not invent one from A213 or A312.

Property TP316LN requirement (A269 Table 2)
Hardness, max 192 HBW / 200 HV or 90 HRB
Tensile / yield / elongation Not specified as an A269 acceptance table for this grade

Source: ASTM A269/A269M Table 2 for TP316LN / UNS S31653 (public PDF excerpt). Confirm thin-wall superficial Rockwell alternatives in the purchased edition.

Seamless and Welded Tube

TP316LN may be seamless or welded under A269, hot- or cold-finished. Welded A269 tube is autogenous (no filler metal), cold-worked, and solution-treated with the tube — not an A312 WLD/HCW pipe product. Seamless takes flaring; welded takes flange and reverse flattening; both share hardness and hydro/NDE.

LN chemistry is often chosen because fabrication welds will remain as-welded and the designer wants both Mo and nitrogen on the certificate. The mill anneal still covers only the as-shipped tube. SHH STEEL can produce and supply both seamless and welded A269 TP316LN.

Dimensions and Tolerances

Order A269 TP316LN by outside diameter and nominal wall thickness, not by pipe schedule as the primary size language. Permissible variations in outside diameter, wall thickness, and cut length are given in A269 Table 4 and flow through the general requirements of ASTM A1016/A1016M, while thin-wall ovality rules in clause 12.2 apply when wall thickness falls below the thin-wall thresholds listed for each OD group.

OD group (A269 Table 4) Outside diameter tolerance Wall thickness tolerance
Up to ½ in. [13 mm] ±0.005 in. [0.13 mm] ±15%
½ to 1½ in. [13–38 mm], excl. ±0.005 in. [0.13 mm] ±10%
1½ to 3½ in. [38–89 mm], excl. ±0.010 in. [0.25 mm] ±10%
3½ to 5½ in. [89–140 mm], excl. ±0.015 in. [0.38 mm] ±10%
5½ to 8 in. [140–203 mm], excl. ±0.030 in. [0.76 mm] ±10%

Source: ASTM A269/A269M Table 4 (public PDF excerpt). Footnotes allow ±12.5% wall on heavy wall or low ID/OD ratios and ±15% wall on sub-½ in. ID tube that cannot be mandrel-drawn. If a drawing is written to A213 minimum-wall language, say so on the enquiry — SHH STEEL will not silently convert LN tubing to a min-wall boiler-tube build.

Equivalent Grades

TP316LN / UNS S31653 is the ASTM tubing grade for nitrogen-bearing low-carbon Mo austenitic. Related forms appear under A213 and A312 where listed; plate cousins sit under A240 where listed.

Reference Designation Note
ASTM A269 TP316LN / UNS S31653 This product standard
UNS S31653 Chemistry identity
ASTM A269 sister TP316L / S31603 Low C + Mo without mandatory N range
ASTM A213 / A312 TP316LN (where listed) Different product form / mechanical tables

Step to A269 UNS S31254 when 6Mo is required, or to A269 TP316L when nitrogen is not on the material list.

Same-grade pages under related product standards (different wall basis and mechanical tables — not drop-in substitutes for A269 tubing): A312 TP316LN and SA312 TP316LN. Confirm the product form before treating any of those pages as acceptance text for an A269 order.

Heat Treatment and Delivery Condition

All A269 TP316LN tube is furnished in the solution heat-treated condition. Table 2 sets a minimum austenitizing temperature of 1900 °F [1040 °C], followed by quenching in water or rapid cooling by other means, and seamless tube may alternatively be quenched immediately after hot forming while still at or above that minimum temperature. If a purchaser deliberately orders a final heat treatment below 1900 °F [1040 °C] for controlled structural reasons, each tube must be stenciled with the actual heat-treatment temperature after the suffix “HT” — that is an ordered exception, not default mill practice for TP316LN.

Item TP316LN (A269 Table 2)
Austenitizing temperature, min 1900 °F [1040 °C]
Cooling Water quench or rapid cool
Hardness after heat treatment, max 192 HBW / 200 HV or 90 HRB
Delivery condition Solution heat-treated; pickled or bright-annealed by agreement

Source: ASTM A269/A269M §6 and Table 2 for TP316LN / UNS S31653 (public PDF excerpt). Bright-annealed or pickled surfaces are finish choices on top of the mandatory solution treatment; they do not replace it. SHH STEEL’s MTC states the heat-treatment condition actually applied to the shipped lengths and will not mark a tube as A269 TP316LN if the final anneal falls outside the ordered Table 2 requirement.

Corrosion Resistance

TP316LN combines L-grade carbon control, 2–3% molybdenum, and a mandatory nitrogen window. Low carbon protects welded heat-affected zones against chromium-carbide sensitization; molybdenum raises chloride pitting and crevice resistance relative to TP304LN; nitrogen at 0.10–0.16% supports austenite stability and must appear on the ladle analysis. That combination is why material lists that say “316LN tube” under A269 are usually aiming at as-welded chloride-aware service without jumping yet to a 6Mo alloy.

It is still not a 6Mo grade. Seawater splash zones, strong chlorides, and aggressive chemical media may need A269 UNS S31254 or a similar high-Mo listing under the same product standard. A269 publishes no PREN or CPT table for S31653 — do not invent one from marketing sheets. Use LN when the material list calls out nitrogen with Mo; use A269 TP316L when nitrogen is not required.

Applications of A269 TP316LN Tube

A269 TP316LN shows up on welded chloride-aware instrument and hygienic tubing specifications that explicitly require nitrogen on the MTC, on chemical process skids that will stay as-welded after fabrication, and on projects that standardized on LN chemistry across plate, pipe, and tube. Bright-annealed cold-finished LN is common in panel and skid shops where ID/OD cleanliness matters; pickled welded LN covers larger utility and transfer runs where a bright finish is not mandatory.

It is the wrong first choice for Code boiler or superheater tube — open A213 instead — and for pipe headers — open A312. When seawater or aggressive chlorides outgrow 2–3% Mo, step to a 6Mo A269 grade rather than stretching S31653. SHH STEEL can produce and supply A269 TP316LN in the general-service band above and will redirect the enquiry when the stated medium needs more alloy than this grade can honestly deliver.

When a sister enquiry is for boiler tube or pipe of the same grade, use A312 TP316LN and SA312 TP316LN instead of stretching an A269 tubing page into the wrong product form.

Weldability

Low carbon, molybdenum, and controlled nitrogen make TP316LN a deliberate as-welded Mo-grade choice for chloride-aware fabrications that will not be solution-annealed after welding. GTAW and GMAW with 316L-type filler — when filler is used on fabrication joints — are the usual processes; mill autogenous seams on A269 welded tube are already cold-worked and solution-treated with the tube body before shipment.

Shop or field welds on cut lengths sit outside that mill anneal, so purge quality, filler selection, and procedure qualification remain the fabricator’s scope unless those services are purchased separately. If 6Mo corrosion margin is required by the medium, order A269 UNS S31254 rather than stretching TP316LN past its chloride envelope. SHH STEEL’s A269 scope is the mill tube, chemistry including nitrogen, hardness, and the seamless or welded route named on the purchase order.

Surface Finishes

Pickled and bright-annealed finishes cover most A269 TP316LN orders, and named OD polish grit is quoted as a supplementary finish only when the purchase order requires a measured belt polish. Bright anneal is preferred for instrumentation and hygienic ID/OD work where scale-free surfaces matter; pickle remains the general-process default when a clean but not bright surface is enough for the duty.

Write any maximum Ra, scrubbed-ID, or electropolish note into the enquiry text so the mill can confirm it can measure and report the finish. SHH STEEL can produce and supply pickled, bright-annealed, and polished A269 TP316LN against those agreed surface notes, and we will not claim an unverified polish grade on the certificate or stencil.

Inspection and Testing

Lot testing for A269 TP316LN covers Table 2 hardness, flaring on seamless tube, and flange plus reverse flattening on welded tube, with lot definitions tied to heat, size, and heat-treatment charge as written in the standard. Each length must also receive a hydrostatic test or a nondestructive electric test; the manufacturer chooses unless the purchase order locks the method, and NDE-tested lengths are marked “NDE” and certified accordingly.

EN 10204 3.1 certificates from SHH STEEL report ladle chemistry including the mandatory nitrogen and molybdenum ranges, solution-treatment condition, hardness against Table 2, and the hydro or NDE statement for the shipped lengths. PMI, product analysis, and third-party inspection holds are available when named on the purchase order, and we do not skip mandatory tests to shorten lead time.

Packaging and Shipping

Export and domestic packs for A269 TP316LN use end caps or plugs, size-sorted bundles or crates, and waterproof wrapping for ocean freight so OD finish and ends stay protected in transit. Bright-annealed and polished OD get extra sleeve protection against galling; coiled product, when ordered, follows A269’s continuous-coil rule without circumferential butt welds inside the coil.

Stencil and bundle tags typically carry ASTM A269, TP316LN / S31653, size, heat number, seamless or welded identity, and NDE when that test route was used. SHH STEEL matches marking to the purchase-order marking clause before the tubes leave the mill or finishing shop, so receiving inspection can verify identity against the MTC without guesswork.

Why Choose SHH STEEL

SHH STEEL can produce and supply ASTM A269 TP316LN as solution-treated seamless or welded tubing with Table 1 chemistry — including the mandatory nitrogen range and molybdenum — Table 2 hardness, and EN 10204 3.1 documentation. We will not ship TP316L and call it LN, and we will not omit nitrogen from the certificate when the grade requires it.

If chlorides outgrow 2–3% Mo, we point to a 6Mo A269 grade rather than selling nitrogen as a substitute for higher molybdenum.

Supply Capability

SHH STEEL can produce and supply ASTM A269 TP316LN to the edition, route, and finish on your enquiry. Capability and Stock / Available sizes follow.

Item SHH STEEL capability for TP316LN
Standard ASTM A269 / A269M
Grade TP316LN / UNS S31653
Product form Seamless and welded tube (no filler metal for welded), hot- or cold-finished
Delivery condition Solution heat-treated ≥1900 °F [1040 °C]; pickled or bright-annealed
Typical size band ~6–168 mm OD × 0.5–8.0 mm nominal wall (others by agreement)
Testing Hardness; flaring (seamless) / flange + reverse flattening (welded); hydro or NDE
Documents EN 10204 3.1 MTC; third-party inspection on request

Stock / Available sizes

Enquiry-oriented supply range — not a frozen tonnage list. Confirm against near-term production when you send the OD × wall list.

OD (mm) Typical nominal walls (mm) Notes
6 / 8 / 10 / 12 / 14 0.5 / 0.8 / 1.0 / 1.2 / 1.5 Instrument / hygienic; often BA
12.7 / 15.9 / 19.1 / 25.4 / 31.8 1.0 / 1.2 / 1.5 / 2.0 / 2.5 Inch OD skid tubing
38.1 / 48.3 / 60.3 / 76.1 1.5 / 2.0 / 2.5 / 3.0 / 4.0 Welded process — LN when N is specified
88.9 / 114.3 / 141.3 / 168.3 2.0 / 3.0 / 4.0 / 6.0 / 8.0 Larger process tube; lock seamless vs welded

Parallel quotes against A269 TP316L and A269 UNS S31254 keep nitrogen and 6Mo choices visible.

FAQ

What does LN mean in A269 TP316LN?
LN marks the low-carbon, nitrogen-controlled molybdenum tubing grade under A269. Carbon is ≤0.035% (with Footnote B where it applies), nitrogen is specified at 0.10–0.16%, and molybdenum sits at 2.00–3.00% under UNS S31653. That combination improves as-welded behaviour versus TP316 while putting both Mo and nitrogen on the MTC — it is a separate ASTM grade, not a heat-treatment suffix on TP316L.
TP316L vs TP316LN under A269 — which should I buy?
Buy TP316L when low carbon and molybdenum are enough and nitrogen is not on the material list. Buy TP316LN when the specification explicitly requires nitrogen at 0.10–0.16% along with low carbon and Mo. Nickel bands also differ (TP316L allows up to 15.0% Ni; TP316LN stays 10.0–13.0%). They must not share one grade stamp on the MTC.
Does A269 TP316LN include welded tube?
Yes. Seamless and welded routes are both allowed. Welded tube is autogenous, cold-worked, solution-treated with the tube, and flange- plus reverse-flattening-tested. SHH STEEL can produce and supply both seamless and welded A269 TP316LN against the same Table 1 and Table 2 floors.
What hardness limit applies to A269 TP316LN?
Table 2 caps TP316LN at 192 HBW / 200 HV or 90 HRB after solution treatment at ≥1900 °F [1040 °C]. Nitrogen strengthens service behaviour, but A269 still does not publish a tensile/yield/elongation acceptance table for this grade. Do not invent tensile floors from A213 or A312 unless the purchase order adds them.
Is nitrogen reported on the MTC for TP316LN?
Yes. Nitrogen is a Table 1 requirement with a 0.10–0.16% range for TP316LN / UNS S31653, so the ladle analysis on an EN 10204 3.1 certificate should report nitrogen alongside molybdenum. If a certificate for an “LN” order omits nitrogen, treat that as a documentation problem before accepting the heat.
Is A269 TP316LN nominal wall or minimum wall?
Nominal wall. Write OD × nominal wall on the enquiry unless you agree another wall basis with the mill. Table 4 then governs OD, wall, and cut-length tolerances. Do not assume A213 minimum-wall boiler-tube practice applies to an A269 TP316LN order.
What size range can SHH STEEL produce for TP316LN?
SHH STEEL can produce and supply about 6–168 mm OD × 0.5–8.0 mm nominal wall in seamless or welded A269 TP316LN, pickled or bright-annealed, with EN 10204 3.1 MTCs. Other sizes are quoted by agreement. Send the OD × wall list and process preference for a firm near-term availability answer.
When should I choose 6Mo instead of TP316LN?
Choose a 6Mo A269 grade such as UNS S31254 when seawater, strong chlorides, or aggressive chemical media outgrow the 2–3% Mo band. TP316LN remains appropriate for many chloride-aware as-welded duties where Mo and nitrogen are specified but 6Mo is not yet justified.
Which tests are mandatory on A269 TP316LN?
Hardness to Table 2; flaring for seamless or flange plus reverse flattening for welded; and hydrostatic or nondestructive electric testing on each length. The mill picks hydro or NDE unless the purchase order locks one. Product analysis and PMI are supplementary when ordered.
What certificate does SHH STEEL provide for A269 TP316LN?
EN 10204 3.1 MTCs report ladle chemistry including nitrogen and molybdenum, solution-treatment condition, hardness, and hydro or NDE. Third-party inspection can be added. Stencil shows ASTM A269, TP316LN / S31653, size, heat, and seamless or welded identity.
How should I enquire for A269 TP316LN with SHH STEEL?
List ASTM A269, grade TP316LN / UNS S31653, seamless or welded, OD × nominal wall, finish, and any hydro/NDE lock. Note that nitrogen must appear on the MTC. SHH STEEL can produce and supply to that enquiry or recommend TP316L or a 6Mo sister when the material list points that way.

Conclusion

ASTM A269 TP316LN / UNS S31653 is the nitrogen-bearing low-carbon molybdenum tubing grade for general-service lines that need as-welded corrosion behaviour, chloride-aware Mo, and a reported nitrogen range on the certificate. SHH STEEL can produce and supply seamless and welded A269 TP316LN, solution annealed to Table 2, tested, and documented on EN 10204 3.1 certificates. Start from the A269/A269M hub, then send the OD × nominal-wall list. Contact admin@steelspecs.com for a production-backed offer.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X