LR FH42 Steel Plate | LR/FH42 Marine Steel Plate
What is LR FH42 / LR/FH42 marine steel plate?
LR FH42, often written LR/FH42 on mill certificates and plate markings, is an extra-high-strength hull structural steel under Lloyd’s Register Rules for the Manufacture, Testing and Certification of Materials. IACS Unified Requirement W16 covers this strength band (yield 420 N/mm²); LR implements corresponding requirements in its Materials rules. Minimum yield is 420 N/mm², tensile 530–680 N/mm², elongation 18 % min., with Charpy at −60 °C. It sits above the AH–FH 40 higher-strength family (max yield 390 N/mm² under UR W11). Commercial enquiries use LR FH42 or LR/FH42 marine steel plate.
Equivalent grades: LR FH42 ≈ ASTM A131 (no direct grade at this strength) ≈ ABS FH42 / FQ43 ≈ DNV NV F420 ≈ BV F420 ≈ CCS FH420 ≈ NK KF420 ≈ KR RF43 ≈ RINA F420 ≈ GB 712 Grade FH420 (all class-approved, stamped by the issuing society).
Naming note: Lloyd’s Register titles this strength band as FH42 / LR/FH42 (LR uses AH69, not AH70). DNV often titles the same yield as FH420 / DNV NV F420. ABS often titles FH42 (official ABS FQ43). ASTM A131 has no grade at this strength. Write LR/FH42 on the LR purchase order.
LR/FH42 is almost always produced TM or QT by an LR-approved mill to order rather than taken from open stock. SHH STEEL sources extra-high-strength plate from mills with Lloyd’s Register approval for the grade, under Surveyor attendance, with optional multi-class and EN 10204 3.2.
LR LR/FH42 plate: specification summary
| Item | LR LR/FH42 / FH42 data |
|---|---|
| Rule basis | Lloyd’s Register Rules for Materials (extra-high / high-strength hull steel); IACS UR W16 strength band (see UNCERTAIN for LR paragraph cross-refs without local PDF) |
| Commercial / stamp | LR/FH42 (LR FH42) |
| Yield / tensile / elongation | 420 / 530–680 N/mm² / 18 % min. |
| Impact | −60 °C; ≈ 42 J L or 28 J T average (IACS UR W16 / aligned tables — confirm on mill certificate) |
| Deoxidation | fully killed, fine grain; N-binding elements per manufacturing specification |
| Delivery condition | TM or QT (N/CR routes only where specifically approved) — within mill approval thickness limits |
| Marking | LR FH42 / LR/FH42 (plus delivery-condition / Z / U where ordered) |
| UT | commonly required for thicker EHS plate (e.g. ≥15 mm) — agree standard (EN 10160 / ASTM A578) on PO |
| Thickness tolerance | IACS UR W13 as adopted by LR (confirm class on PO; see UNCERTAIN) |
| Certificate | mill certificate endorsed by the LR Surveyor; includes Ceq/CET/Pcm as applicable; EN 10204 3.1 / 3.2 on request |
Maximum plate thickness depends on delivery condition and the mill’s LR approval sheet — typically TM up to about 100–150 mm and QT higher, but treat the approval limit as governing (UNCERTAIN without local LR PDF). Primary commercial scope we quote is within ~100 mm unless the mill approval and LR survey confirm otherwise.
LR LR/FH42 chemical composition (heat analysis envelope)
| Element | Heat (ladle) analysis, % | Product (check) analysis, % | Note |
|---|---|---|---|
| C (depends on route) | 0.14–0.21 max. by grade/condition (UR W16 / mill approval) | numeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificate | TM/QT and letter routes may tighten C |
| Mn | typically 1.0–1.70 (route-dependent) | numeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificate | as per mill approval |
| Si | typically 0.60 max. (QT may differ) | numeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificate | |
| P / S | tighter than UR W11 HS; often 0.025 max. or lower on EQ/FQ-style routes | numeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificate | confirm on approval sheet |
| Al total min. | fine-grain practice | numeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificate | Al/N control unless other N-binders used |
| Nb / V / Ti | limits per UR W16 / mill approval | numeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificate | combined microalloy caps apply |
| Ni / Cu / Cr / Mo | per approval chemistry | numeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificate | |
| Ceq / CET / Pcm | maxima by category and condition on approval | not applicable (calculated from heat analysis) | report on certificate |
Product (check) analysis column: LR Rules for Materials specify heat (ladle) limits; no numeric product-analysis tolerance is tabulated in the rule text reviewed, so product (check) limits are agreed on the order or taken from the approved mill specification and certificate.
Source: IACS UR W16 chemistry envelope as implemented by Lloyd’s Register for LR/FH42 — exact ladle limits depend on delivery condition (TM vs QT) and toughness letter. Values above are the rule envelope; the purchase order and mill approval sheet govern. Product analysis: as per standard and mill certificate. All intentionally added elements and Ceq (or CET/Pcm) are to be reported. Flagged UNCERTAIN where a local LR Materials PDF was not available to quote paragraph numbers.
LR LR/FH42 tensile and impact properties
| Property | Requirement (IACS UR W16 aligned) |
|---|---|
| Yield strength ReH (or Rp0.2) | 420 N/mm² min. |
| Tensile strength Rm | 530–680 N/mm² |
| Elongation (transverse, 5.65√A) | 18 % min. |
| Impact test temperature | −60 °C |
| Impact energy (indicative) | 42 J L or 28 J T average |
Final acceptance values are as per standard and mill certificate under LR survey. For thick plate, additional mid-thickness tensile/impact positions may apply — confirm at enquiry. Test frequency is typically each heat-treatment batch of same cast/condition/thickness.
Delivery condition and toughness for LR/FH42
Charpy temperature is fixed by the grade letter: FH → −60 °C. Indicative average energy 42 / 28 J (L/T) from IACS UR W16 aligned tables — confirm exact figures on the LR-endorsed certificate. Unlike UR W11 higher-strength tables, EHS energies are usually stated as a single pair rather than rising through many thickness bands; thick-plate mid-thickness rules may still apply.
Allowed delivery conditions are primarily TM and QT within the mill’s approved thickness. Vacuum degassing is commonly required for higher categories and for thicker plate — follow the mill approval. State TM or QT on the PO; do not leave delivery condition blank for FH42.
Thickness tolerance and surface condition
Lloyd’s Register applies IACS UR W13 unless the PO states otherwise (confirm minus class on PO; see UNCERTAIN). Surface repair limits follow the applicable LR / UR rules; state primer/surface class on receipt if needed. For QT plate, avoid notching cut edges; follow mill cutting recommendations.
LR LR/FH42 plate — mill-roll supply in China
| Thickness (mm) | Width (mm) | Length (mm) | Condition | Approx. quantity | Location |
|---|---|---|---|---|---|
| 10 | 2000 / 2200 | 8000 / 12000 | TM / QT | 200+ t | China |
| 12 | 2000 / 2200 / 2500 | 12000 | TM / QT | 200+ t | China |
| 14 | 2000 / 2200 | 12000 | TM / QT | 100+ t | China |
| 16 | 2000 / 2500 | 12000 | TM / QT | 200+ t | China |
| 20 | 2000 / 2500 | 12000 | TM / QT | 100+ t | China |
| 25 | 2200 / 2500 | 12000 | TM / QT | 100+ t | China |
| 30 | 2200 | 10000 / 12000 | TM / QT | 100+ t | China |
| 40 | 2200 | 10000 | TM / QT | 50+ t | China |
| 50 | 2200 | 8000 / 10000 | TM / QT | 50+ t | China |
Extra-high grades such as LR/FH42 are rarely held as open stock; the table shows the size bands we quote against scheduled mill rolls. Quantities are indicative. All plates sold as LR class carry LR/FH42 marking and an LR-endorsed mill certificate. Typical mill lead time including LR survey is about 6–10 weeks (commercial estimate — confirm per quote). Send your size list and we will reply with the next available rolling slot.
Packing. Plates are bundled by size with steel strapping, marked with heat number, grade and LR stamp, and shipped in containers (up to about 11.8 m) or break bulk for longer plates.
LR LR/FH42 equivalents in other rules and standards
| Standard / society | Designation | Comment |
|---|---|---|
| LR (Lloyd’s Register) | LR/FH42 (LR FH42) | this page; LR uses AH69 not AH70 |
| ASTM A131/A131M | ASTM A131/A131M — no direct Grade FH42 | A131 stops at FH40 |
| ABS | ABS FH42 / FQ43 | commercial FH42 / official FQ43 (ABS uses 70 where LR uses 69) |
| DNV | DNV NV F420 | DNV titles FH420 for this yield band |
| BV | BV (per rules) | EHS name not verified from local BV PDF — write per rules |
| CCS | CCS FH420 | CCS follows W16-style naming |
| NK (ClassNK) | NK KF420 | NK KF420 |
| KR | KR RF43 | KR RF43 (KR uses ABS-style category numbers) |
| RINA | RINA (per rules) | EHS name not verified from local RINA PDF |
| GB 712 | GB 712 Grade FH420 | listed in GB 712 EHS band; not class approval alone |
These are comparisons, not substitutions. Always write the LR stamp LR/FH42 on the PO, plus any additional society stamps you need.
LR LR/FH42 vs higher-strength and other EHS grades
Use FH42 when scantlings need yield 420 N/mm². Do not substitute AH40/EH40 (390 N/mm² max under UR W11) without redesign. Within the 42 band, letter choice is toughness: AH 0 °C → DH −20 °C → EH −40 °C → FH −60 °C. Neighbouring strengths are AH–FH 40 / 46 — swapping strength needs class approval of the drawing change.
When LR LR/FH42 is the right choice: typical uses are low-temperature service: Arctic and polar-class hulls, ice belts and offshore units in cold regions where −60 °C toughness is specified at extra-high yield — weight-critical hull girder strakes, polar and ice-class primary structure, and offshore units where 420 N/mm² is specified. See offshore platform steel plates for related offshore grades.
Applications and welding notes for LR LR/FH42
Typical uses: low-temperature service: Arctic and polar-class hulls, ice belts and offshore units in cold regions where −60 °C toughness is specified at ReH 420 N/mm²; strength deck and shell of large container ships and gas carriers where EHS is specified; ice-belt and polar primary structure; selected offshore members. See offshore platform steel plates.
Welding: LR/FH42 is an extra-high-strength steel supplied TM or QT. Welding must follow a procedure qualified for this grade and approved by LR. Ceq/CET/Pcm from the ladle analysis govern hydrogen control, preheat, interpass and heat-input windows. Too much heat input can lower HAZ strength and toughness in QT plate. We send the certificate values before shipment so your welding engineer can confirm the procedure fits. We do not give generic preheat temperatures.
Processing notes: LR/FH42 owes its strength to TM or QT processing. Hot forming or stress relieving above the tempering temperature can lower the properties, so any heat treatment after delivery must be agreed with the mill and LR. Cold forming and bending radii should follow the mill’s data sheet. Thermal cutting parameters follow mill recommendations so the cut edge is not damaged.
Certificates, LR survey and third-party inspection
LR survey at the mill; certificate includes ladle chemistry, Ceq/CET/Pcm as applicable, tensile (ReH ≥ 420, Rm 530–680, A ≥ 18 %), Charpy at −60 °C, delivery condition, UT if ordered, and plate identity. Optional EN 10204 3.2 and multi-class.
On receipt: verify LR/FH42 stamp, −60 °C impact data, energies ≥ ordered/certified minima, thickness within tolerance, Surveyor endorsement, UT report if required.
Charpy acceptance for LR/FH42 (IACS UR W16 aligned; actual results as per standard and mill certificate):
| Thickness t (mm) | Test temperature | Average energy, longitudinal (J min.) | Average energy, transverse (J min.) |
|---|---|---|---|
| as per UR W16 / mill approval (typically t/4 position) | −60 °C | 42 | 28 |
For thickness above ~100 mm, additional mid-thickness rules may apply — confirm at enquiry. If the PO asked for 3.2, the inspector’s report must name the witnessed tests and plate numbers.
Common mistakes when ordering LR FH42 / LR/FH42
- Ordering “LR 42” without the letter (FH) — toughness missing
- Writing ABS FH42 or DNV FH420 on an LR-class PO without arranging that society’s survey (wrong stamp)
- Leaving delivery condition blank (TM vs QT changes price, mill and properties)
- Expecting ASTM A131 dual-cert at this strength (A131 has no EHS grade)
- Skipping UT on thick EHS plate when the yard specification requires it
- Missing LR endorsement / assuming GB 712 Grade FH420 alone is class approval
- Confusing LR AH69 with ABS AH70 — same yield band, different society title
Write grade, TM/QT, impact temperature, UT level and certificate type into the PO.
Sourcing LR LR/FH42: buyer concerns and SHH STEEL solutions
| Concern | How SHH STEEL handles it |
|---|---|
| Fake class plate | LR-approved mills only; traceable LR/FH42 stamp + certificate; 3.2 on request |
| Payment risk | T/T or L/C; inspection before balance |
| Mill minimum / long lead time | combine sizes on one heat where possible; weekly photo updates; clear rolling-slot confirmation before deposit |
| Welding / heat-input risk | send ladle Ceq/CET/Pcm before shipment; support WPS review with mill data |
| Prep before ship | cutting, bevelling, drilling, machining in our workshop (follow mill cutting notes for QT) |
How to order LR LR/FH42 plate
Specify LR FH42 (LR/FH42), delivery condition TM or QT, thickness × width × length × qty, Z/U/UT level, multi-class, certificate type, port. Send to SHH STEEL.
Sample PO line: “Steel plate to Lloyd’s Register Rules for Materials, Grade FH42 (LR/FH42), delivery condition [TM/QT], 30 × 2500 × 12000 mm, 10 pcs, marked LR FH42 / LR/FH42, certificate endorsed by LR Surveyor, EN 10204 3.2 [if required], UT [EN 10160 / ASTM A578 level], CIF [port].”
FAQ
Conclusion
LR FH42 / LR/FH42 is extra-high-strength hull steel (IACS UR W16 band): yield 420 N/mm², tensile 530–680 N/mm², Charpy at −60 °C, marking LR/FH42. Lock on the order: TM or QT, UT level, Ceq/CET/Pcm reporting, multi-class and 3.2.
SHH STEEL supplies LR/FH42 plate rolled by Chinese mills that hold Lloyd’s Register works approval for the grade, so every plate carries the LR/FH42 stamp and a Surveyor-endorsed certificate traceable to its heat. Sizes are scheduled into the mill rolling cycle with LR survey arranged at the mill. On request we add EN 10204 3.2 certificates with third-party witness (TÜV, SGS, BV or another agency) and joint certification with ABS, DNV, BV, CCS, NK, KR or RINA.
We accept T/T or L/C payment, with inspection before the balance is paid. Small quantities in several sizes, or LR/FH42 with neighbouring EHS sizes or higher-strength AH–FH 40 where the drawing allows, can be combined in one container. A dedicated coordinator sends production and shipping updates with photos, and our own workshop cuts to size, bevels, drills and machines plates before shipment so they arrive ready for fabrication.
Request a quotation: send SHH STEEL the grade (LR/FH42 / LR FH42), thickness, width, length, quantity per size and destination port, plus any multi-class, Z/U or 3.2 certificate requirement. We reply with price, available stock and lead time.