Close view of NK KF420 hull structural steel plate, ClassNK (NK) rules

NK KF420 Shipbuilding Steel Plate

NK KF420 extra-high-strength hull plate to ClassNK Part K / IACS UR W16: ReH 420 N/mm², Charpy −60 °C, TM or QT. Mill-rolled at NK-approved Chinese mills via SHH STEEL, with UT, dual class and 3.2 inspection.
Keywords
NK KF420 steel plate, ClassNK KF420, KF420 extra high strength hull steel, NK FH420 plate, Nippon Kaiji Kyokai KF420, UR W16 marine plate
Equivalent Grades:
DNV VL F420; LR FH42; BV F420; CCS FH420; KR RF43; ABS FH42; RINA per rules; GB 712 FH420
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Impact Test and Condition of Supply
Thickness Tolerance
Stock
Equivalent Grades
Grade Selection
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

NK KF420 shipbuilding steel plate — overview

Technical Reviewer: Jack | SHH STEEL Material Solutions Department · Updated: 2026-10-28

NK KF420 is the −60 °C grade of the 420 level, for Arctic and polar service. ClassNK names its extra-high-strength steels with the K prefix, the toughness letter and the yield in N/mm²: KA, KD, KE or KF followed by 420. The 420 level is the entry level of extra-high strength, used on large container ships to keep hatch-coaming and sheer-strake thickness down. It follows IACS UR W16: ReH ≥ 420 N/mm², Rm 530–680 N/mm², A ≥ 18 %.

Equivalent grades: ASTM A131 (no direct grade at this strength) · ABS FH42 / FQ43 · DNV NV F420 · LR FH42 · BV F420 · CCS FH420 · KR RF43 · RINA F420 · GB 712 Grade FH420.

KF420 is made TMCP or quenched and tempered at a mill whose NK approval covers this exact grade and thickness range. It is rolled to order rather than held in stock. SHH STEEL places the order at an NK-approved Chinese mill and arranges the NK survey, with dual class and 3.2 inspection on request.

KF420 key data

ItemNK KF420
Governing rulesClassNK Rules Part K, extra-high-strength rolled steel; IACS UR W16 (Part K numbering UNCERTAIN)
DesignationKF420: K + toughness letter F + yield 420 N/mm²
StrengthReH ≥ 420, Rm 530–680 N/mm², A ≥ 18 %
Charpy V−60 °C; avg. ≥ 42 J L / 28 J T (UR W16-aligned; confirm)
Delivery conditionTM or QT within approved thickness (N only if specially approved)
Steelmakingkilled, fine-grain; vacuum degassing typical
UTusually ordered for this class — agree standard and level
ToleranceIACS UR W13 (confirm class)
DocumentsNK-endorsed certificate incl. Ceq / CET / Pcm; EN 10204 3.2 on request

The maximum thickness depends on the mill’s approval. TM KF420 is often approved to about 50–80 mm and QT thicker, but treat the approval sheet as the limit (UNCERTAIN).

KF420 chemical composition — full alloy list

ElementHeat (ladle) analysis, %Product (check) analysis, %Remark
C0.18 max. (often tighter than AH/DH/EH; TM/QT may further tighten)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Mn1.70 max. (typically 1.00–1.70)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Si0.55 max. (QT may differ — confirm on mill approval)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
P0.020–0.025 max. (FH-route typically tighter — confirm)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
S0.020–0.025 max. (FH-route typically tighter — confirm)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Al0.015 min. acid-soluble / ≈0.020 total Al (fine-grain; Al/N control)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificategrain refiner / N binder
Nb0.05 max. (when used; combined microalloy caps apply)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
V0.10 max. (when used; combined caps apply)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Ti0.05 max. (when used; combined caps apply)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Cu0.50 max. (route-dependent)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Cr0.20–0.25 max. (route-dependent)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Ni2.00 max. or per mill approval (FH often allows higher Ni for toughness)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificatetoughness
Mo0.08–0.50 (route-dependent)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificatehardenability (QT)
B0.005 max. (when intentionally added)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificatehardenability (QT)
N0.012 max. typical with Al present (tighter FH control — confirm)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Nb+V+TiNb+V+Ti typically < 0.26 % for N/TM routes (not QT) — confirm UR W16 / mill approvalnot applicable (calculated from heat analysis)combined
Ceq / CET / PcmCeq / CET / Pcm maxima by category and condition on mill approval — report on certificatenot applicable (calculated from heat analysis)calculated

Product (check) analysis column: ClassNK Part K specify heat (ladle) limits; no numeric product-analysis tolerance is tabulated in the rule text reviewed, so product (check) limits are agreed on the order or taken from the approved mill specification and certificate.

These rows give the UR W16 envelope. ClassNK fixes the exact limits for each mill at approval, so the approval sheet and the order govern (UNCERTAIN vs Part K text). At 420 most mills use a lean C–Mn–Nb–Ti TMCP design with little Ni or Mo. Every intentionally added element must appear on the certificate, along with Ceq, CET or Pcm.

KF420 tensile and impact requirements

PropertyValue
ReH (or Rp0.2)420 N/mm² min.
Rm530–680 N/mm²
A18 % min. (transverse)
Charpy−60 °C, ≥ 42 J L / 28 J T

Tests are taken per heat-treatment batch or rolled length, as the approval requires. Thick plate may need extra mid-thickness tests. Results are as per standard and mill certificate.

KF420: toughness and delivery condition

Charpy specimens are usually taken at quarter thickness and tested at −60 °C. Delivery is TM or QT. The choice changes the mill, price and welding behaviour, so state it on the order. At this toughness level, many owners also ask for CTOD or brittle-crack-arrest data. Those are separate requirements (UNCERTAIN), so specify them.

Thickness tolerance and surface quality

Minus tolerance follows UR W13. Plus tolerance and flatness follow the agreed standard. QT plate is flatter than heavy TM plate but harder to straighten, so agree the flatness class at enquiry.

KF420 mill-roll supply

Thickness (mm)Width (mm)ConditionTypical lot
122000 / 2500TM / QTper heat / rolling
162200 / 2500TM / QTper heat / rolling
202500TM / QTper heat / rolling
252500TM / QTper heat / rolling
302200 / 2500TM / QTper heat / rolling
402200TM / QTper heat / rolling
502200TM / QTper heat / rolling

KF420 is not held as open stock. These are the sizes we normally quote against mill rolling slots. Lead time is about 6–10 weeks including NK survey (commercial estimate).

Packing: bundled by size with steel strapping, painted with grade and heat number, shipped in containers (≤11.8 m) or break bulk.

NK KF420 compared with other societies

Society / standardGradeNote
ClassNKNK KF420this page
DNVDNV VL F420
LRLR FH42LR numbers by yield/10
BVBV F420no H
CCSCCS FH420
KRKR RF43KR yield-class number
ABSABS FH42 / FQ43ABS commercial / official
RINARINA (per rules)not verified
ASTM A131no equivalentstops at FH40
GB 712GB 712 Grade FH420product standard

All sit in the same UR W16 band. The names differ, and only the NK stamp counts for ClassNK.

Where KF420 sits in the ClassNK extra-high-strength series

The neighbours are KF40 (390) below and KF460 above. Within level 420, the letter sets the test temperature: KA 0 °C, KD −20 °C, KE −40 °C, KF −60 °C. Moving to a different level needs ClassNK plan approval. Typical uses: ice-class and polar hulls, Arctic LNG carriers and cold-region offshore units needing −60 °C, at extra-high strength. See NK Steel Plates and offshore platform steel plates.

Fabricating KF420

Welding needs a procedure qualified on KF420 and approved by ClassNK, with low-hydrogen consumables of matching strength and −60 °C toughness. TMCP at this level is generally weldable with modest preheat, but the approved procedure governs. Do not hot form or stress relieve above the tempering temperature without agreement from the mill and ClassNK.

NK survey, certificates and receiving checks

The certificate gives the full alloy analysis, Ceq/CET/Pcm, tensile results, −60 °C Charpy results, delivery condition, UT result and plate numbers, with the NK endorsement. On receipt, check the KF420 stamp, impact temperature and NK endorsement. Dual class with ABS, DNV, LR or BV and 3.2 witness are available.

Ordering errors seen with KF420

  • Writing AH420 or A420 without ClassNK, so the plate gets the wrong stamp
  • Leaving TM vs QT open
  • No UT requirement
  • Ceq/Pcm not requested
  • Ordering from a mill whose NK approval does not cover the thickness
  • Expecting an ASTM A131 dual certificate

Buying KF420 from China: concerns and answers

ConcernAnswer
Is the NK stamp genuine?Only mills with ClassNK approval for KF420; certificate and stamp traceable to the heat; third-party witness on request
Payment safetyT/T with balance after inspection, or L/C at sight
Small or mixed orderssizes grouped onto one heat where possible
Delivery visibilityweekly photos from rolling to loading
Ready-to-fit partscutting, bevelling and drilling in our own workshop

Ordering KF420

State NK KF420, TM or QT, sizes and quantities, UT level, dual class, certificate type and port. Send to SHH STEEL.

Sample line: “Plate to ClassNK Rules Part K, grade KF420, QT, 40 × 2500 × 10000 mm, 8 pcs, UT EN 10160 S1E1, NK-endorsed certificate with Pcm, EN 10204 3.2.”

FAQ

What does the name KF420 mean?
K is the ClassNK prefix, F is the toughness letter (−60 °C), and 420 is the minimum yield in N/mm². It is the IACS UR W16 FH420 grade.
Is KF420 available from stock?
Rarely. It is rolled to order at an NK-approved mill, typically in 6–10 weeks including survey.
TM or QT — which should I order?
TM is usual at this level and gives better weldability. State it on the order.
What impact energy is required?
Indicatively at least 42 J longitudinal or 28 J transverse average at −60 °C (UR W16-aligned; confirm on the certificate).
Which elements appear on the certificate?
C, Mn, Si, P, S, Al, Nb, V, Ti, Cu, Cr, Ni, Mo, B and N where added, plus Ceq, CET or Pcm.
Can KF420 be dual-certified?
Yes, with ABS, DNV, LR or BV, if all the surveyors attend the same tests.
What welding precautions apply?
Use a ClassNK-approved procedure qualified on this grade, low-hydrogen consumables and controlled heat input. Do not apply post-weld heat above the tempering temperature.
What payment terms do you accept?
T/T with a deposit and the balance after inspection, or L/C at sight.

Conclusion

NK KF420 (KF420) is ClassNK extra-high-strength hull steel under Part K of the Rules for the Survey and Construction of Steel Ships: yield 420 N/mm², tensile 530–680 N/mm², Charpy −60 °C. An NK-classed hull accepts it only with the NK stamp and an endorsed certificate.

SHH STEEL supplies KF420 from NK-approved Chinese mills, with cutting, dual class, UT and EN 10204 3.2 on request. Send grade, sizes, quantities and port for a quotation.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *



    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response