RINA Steel Plates

Product Showcase

RINA Steel Plates Carbon Steel Plates

SHH STEEL offers RINA Rules-compliant RINA AH32/DH32/EH36 steel plates. Registro Italiano Navale Rules for Ships specify material approval, testing, and hull requirements for classification. Certified quality, competitive prices, customizable. Trust SHH STEEL!

RINA F500 Shipbuilding Steel Plate

RINA F500 Shipbuilding Steel Plate

RINA F500 extra-high-strength hull plate to RINA Rules Part D / IACS UR W16: ReH 500 N/mm², Charpy −60 °C, TM or QT. Mill-rolled at RINA-approved Chinese mills via SHH STEEL, with UT and 3.2 inspection.
View More
RINA E500 Shipbuilding Steel Plate

RINA E500 Shipbuilding Steel Plate

RINA E500 extra-high-strength hull plate to RINA Rules Part D / IACS UR W16: ReH 500 N/mm², Charpy −40 °C, TM or QT. Mill-rolled at RINA-approved Chinese mills via SHH STEEL, with UT and 3.2 inspection.
View More
RINA D500 Shipbuilding Steel Plate

RINA D500 Shipbuilding Steel Plate

RINA D500 extra-high-strength hull plate to RINA Rules Part D / IACS UR W16: ReH 500 N/mm², Charpy −20 °C, TM or QT. Mill-rolled at RINA-approved Chinese mills via SHH STEEL, with UT and 3.2 inspection.
View More
RINA A500 Shipbuilding Steel Plate

RINA A500 Shipbuilding Steel Plate

RINA A500 extra-high-strength hull plate to RINA Rules Part D / IACS UR W16: ReH 500 N/mm², Charpy 0 °C, TM or QT. Mill-rolled at RINA-approved Chinese mills via SHH STEEL, with UT and 3.2 inspection.
View More
RINA F460 Shipbuilding Steel Plate

RINA F460 Shipbuilding Steel Plate

RINA F460 extra-high-strength hull plate to RINA Rules Part D / IACS UR W16: ReH 460 N/mm², Charpy −60 °C, TM or QT. Mill-rolled at RINA-approved Chinese mills via SHH STEEL, with UT and 3.2 inspection.
View More
RINA E460 Shipbuilding Steel Plate

RINA E460 Shipbuilding Steel Plate

RINA E460 extra-high-strength hull plate to RINA Rules Part D / IACS UR W16: ReH 460 N/mm², Charpy −40 °C, TM or QT. Mill-rolled at RINA-approved Chinese mills via SHH STEEL, with UT and 3.2 inspection.
View More
RINA D460 Shipbuilding Steel Plate

RINA D460 Shipbuilding Steel Plate

RINA D460 extra-high-strength hull plate to RINA Rules Part D / IACS UR W16: ReH 460 N/mm², Charpy −20 °C, TM or QT. Mill-rolled at RINA-approved Chinese mills via SHH STEEL, with UT and 3.2 inspection.
View More
RINA A460 Shipbuilding Steel Plate

RINA A460 Shipbuilding Steel Plate

RINA A460 extra-high-strength hull plate to RINA Rules Part D / IACS UR W16: ReH 460 N/mm², Charpy 0 °C, TM or QT. Mill-rolled at RINA-approved Chinese mills via SHH STEEL, with UT and 3.2 inspection.
View More
RINA F420 Shipbuilding Steel Plate

RINA F420 Shipbuilding Steel Plate

RINA F420 extra-high-strength hull plate to RINA Rules Part D / IACS UR W16: ReH 420 N/mm², Charpy −60 °C, TM or QT. Mill-rolled at RINA-approved Chinese mills via SHH STEEL, with UT and 3.2 inspection.
View More
RINA E420 Shipbuilding Steel Plate

RINA E420 Shipbuilding Steel Plate

RINA E420 extra-high-strength hull plate to RINA Rules Part D / IACS UR W16: ReH 420 N/mm², Charpy −40 °C, TM or QT. Mill-rolled at RINA-approved Chinese mills via SHH STEEL, with UT and 3.2 inspection.
View More
RINA D420 Shipbuilding Steel Plate

RINA D420 Shipbuilding Steel Plate

RINA D420 extra-high-strength hull plate to RINA Rules Part D / IACS UR W16: ReH 420 N/mm², Charpy −20 °C, TM or QT. Mill-rolled at RINA-approved Chinese mills via SHH STEEL, with UT and 3.2 inspection.
View More
RINA A420 Shipbuilding Steel Plate

RINA A420 Shipbuilding Steel Plate

RINA A420 extra-high-strength hull plate to RINA Rules Part D / IACS UR W16: ReH 420 N/mm², Charpy 0 °C, TM or QT. Mill-rolled at RINA-approved Chinese mills via SHH STEEL, with UT and 3.2 inspection.
View More

Shipbuilding Steel Plates

SHH STEEL, a premier Shipbuilding Steel Plates exporter, produces and exports shipbuilding steel plates for marine vessels and offshore structures. Our plates, such as AH36 and DH36, provide high strength, toughness, and corrosion resistance, meeting ABS and BV standards. With a 5,000-ton inventory, we guarantee 3–5 day delivery for in-stock items, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for reliable marine-grade steel plates and custom maritime solutions.

Shipbuilding Steel Plates

SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

    *

    *

    *

    *


    X