RINA FH36 Shipbuilding Steel Plate
RINA FH36 shipbuilding steel plate — overview
RINA FH36 is the −60 °C grade of the 36 level and uses the tighter F-column chemistry: lower C, P and S, a nitrogen limit and more room for Ni. Level 36 is the level most of a modern passenger ship’s hull girder is built from. Cruise and ro-pax designs use 36 plate for strength decks, side shell and bottom, where saved weight buys passenger capacity or stability margin. Minimum yield is 355 N/mm², tensile 490–630 N/mm², elongation 21 %.
Equivalent grades: ASTM A131 Grade FH36 · ABS FH36 · DNV NV F36 · LR FH36 · BV FH36 · CCS F36 / FH36 · NK KF36 · KR RF36 · GB 712 Grade FH36.
In RINA’s high-tensile series the letter sets the Charpy temperature (AH 0 °C, DH −20 °C, EH −40 °C, FH −60 °C) and the number sets the yield (32 → 315, 36 → 355, 40 → 390 N/mm²). FH36 is the F letter at level 36. Typical RINA-classed uses: polar expedition cruise ships, Arctic ice-class tonnage and cold-region offshore units whose design temperature calls for −60 °C.
RINA is the Genoa-based society that classes much of the Italian fleet and a large share of the world’s cruise ships and ferries, many of them built at Fincantieri and other Italian and Mediterranean yards. That background shows in the steel: passenger ships use large areas of thin plate in decks and superstructure, so flatness, weld distortion and consistent supply count as much as the grade letter.
SHH STEEL supplies FH36 from Chinese mills whose RINA approval covers high-tensile hull steel in the ordered condition and thickness, with the RINA survey at the mill. Common 36-level sizes are held in stock; the rest is rolled to order.
How RINA names it. For higher-strength steel RINA uses the IACS form: H for high tensile, the toughness letter in front and the strength level behind, so FH36 = letter F, level 36. Buyers sometimes shorten it to “F36”, but on RINA paperwork the H stays.
Level 36 is the most widely produced high-tensile hull grade in the world, so it has the widest choice of RINA-approved mills, sizes and stock.
RINA FH36: key data at a glance
| Item | RINA FH36 |
|---|---|
| Rule book | RINA Rules for the Classification of Ships, Part D (Materials and Welding), higher-strength hull steel; IACS UR W11 FH36 (RINA numbering not quoted — UNCERTAIN) |
| Designation | FH36: toughness letter FH + strength level 36 |
| Strength | ReH ≥ 355 N/mm², Rm 490–630 N/mm², A ≥ 21 % |
| Charpy V | −60 °C |
| Steelmaking | killed and fine-grain treated (Al, Nb, V or Ti) |
| Condition of supply | AR / CR / N / TM as permitted by thickness and grain refiner; QT where approved |
| TM carbon equivalent | Ceq ≤ 0.38 % (t ≤ 50 mm), ≤ 0.40 % (50–100 mm) — indicative UR W11 practice, confirm on approval |
| Thickness scope | up to 100 mm (UR W11); beyond by agreement with RINA |
| Minus tolerance | IACS UR W13 (confirm class — UNCERTAIN) |
| Certificate | RINA-endorsed mill certificate; EN 10204 3.1 / 3.2 |
Traded FH36 is usually 6–60 mm thick and 2000–3000 mm wide. FH plate above about 50 mm is offered by fewer mills, so check the approval range before you fix the design thickness.
RINA FH36 chemistry — full alloy list
| Element | Ladle (heat) analysis, % | Product (check) analysis, % | Comment |
|---|---|---|---|
| C | 0.16 max. | numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate | FH column |
| Si | 0.10–0.50 | numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate | |
| Mn | 0.90–1.60 | numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate | |
| P | 0.025 max. | numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate | F column tighter |
| S | 0.025 max. | numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate | F column tighter |
| Al (acid-soluble) | 0.015 min. acid-soluble | numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate | grain refiner |
| Nb | 0.02–0.05 when used singly | numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate | grain refiner / strength |
| V | 0.05–0.10 when used singly | numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate | |
| Ti | 0.02 max. | numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate | |
| Cu | 0.35 max. | numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate | |
| Cr | 0.20 max. | numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate | |
| Ni | 0.80 max. | numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate | larger allowance in F column |
| Mo | 0.08 max. | numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate | |
| N | 0.009 max. (0.012 if Al present) | numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate | cap applies to F column |
| Nb+V+Ti | 0.12 max. (combined, when used together) | not applicable (calculated from heat analysis) | combined microalloy cap |
| Ceq (TM plate) | 0.38 / 0.40 max. (calculated) | not applicable (calculated from heat analysis) | t ≤ 50 / 50–100 mm |
Product (check) analysis column: RINA Rules Part D specify heat (ladle) limits; no numeric product-analysis tolerance is tabulated in the rule text reviewed, so product (check) limits are agreed on the order or taken from the approved mill specification and certificate.
Ladle limits are the IACS UR W11 values for higher-strength hull steel, applied by RINA in Part D (not checked against a RINA edition — UNCERTAIN). The F column caps C at 0.16 %, P and S at 0.025 % and N at 0.009 % (0.012 % with Al), and allows Ni up to 0.80 %. Check each of these on the certificate.
For TM plate ask for Ceq on the certificate, and Pcm too if your welding procedure is qualified on it. At level 36, Nb–Ti or Nb–V TM designs are usual. Check-analysis tolerances are agreed case by case.
RINA FH36 tensile requirements
| Property | Requirement |
|---|---|
| ReH | 355 N/mm² min. |
| Rm | 490–630 N/mm² |
| A (5.65√S0) | 21 % min. |
| Charpy test temperature | −60 °C |
Flat 200 mm test pieces — minimum elongation by thickness:
| t (mm) | ≤5 | 5–10 | 10–15 | 15–20 | 20–25 | 25–30 | 30–40 | 40–50 |
|---|---|---|---|---|---|---|---|---|
| A200 min. % | 13 | 15 | 16 | 17 | 18 | 19 | 20 | 21 |
AH36, DH36, EH36 and FH36 share these tensile values; only the Charpy temperature and, for FH, the chemistry differ. Compared with mild steel, FH36 gives 120 N/mm² more yield, which is the margin the designer spends on thinner plate.
Tensile specimens are taken transverse to the rolling direction for plate wider than about 600 mm, as UR W11/W16 practice requires; the certificate should show the specimen orientation. For TM plate, a yield/tensile ratio is often around 0.8–0.9; there is no class limit unless the order adds one (indicative).
RINA FH36: Charpy at −60 °C and condition of supply
| Thickness | Avg. long. (J) | Avg. trans. (J) |
|---|---|---|
| ≤ 50 mm | 34 | 24 |
| 50–70 mm | 41 | 27 |
| 70–100 mm | 50 | 34 |
Required energy rises with thickness: a 70–100 mm FH36 plate must average 50 J longitudinal at −60 °C, against 34 J up to 50 mm. FH plate is almost always TM or N; as-rolled plate rarely meets −60 °C reliably.
Condition of supply sets batch size and test frequency, so it belongs on the order. If the owner’s specification adds strain-aged impact tests or Z-direction properties, those are extra requirements and must be priced and booked in advance.
Thickness tolerance and surface
The minus tolerance follows IACS UR W13 as RINA applies it; plus tolerance, flatness and dimensions follow the agreed standard (EN 10029 or GB/T 709). Weight-optimised high-tensile designs — and passenger ships are among the most weight-sensitive — leave little margin, so measure thickness at several points on receipt. Thin high-tensile deck plate distorts more easily during welding than thicker plate; ordering a tighter flatness class can save fairing work later.
UR W13 also allows local grinding of surface defects and sets how the average thickness of a plate is checked; the measurement points and acceptance method should be agreed at enquiry if the yard has its own procedure. For RINA passenger-ship work we suggest stating both the minus tolerance class and the flatness class on the order for any plate under 10 mm.
RINA FH36 stock and lead time
| Thickness (mm) | Width (mm) | Length (mm) | Condition | Approx. qty |
|---|---|---|---|---|
| 5 | 1500 / 1800 | 6000–12000 | AR / N / TM | 80+ t |
| 6 | 1800 / 2000 | 6000–12000 | AR / N / TM | 100+ t |
| 8 | 2000 | 6000–12000 | AR / N / TM | 150+ t |
| 10 | 2000 / 2200 | 6000–12000 | AR / N / TM | 200+ t |
| 12 | 2000 / 2500 | 6000–12000 | AR / N / TM | 200+ t |
| 16 | 2200 / 2500 | 6000–12000 | AR / N / TM | 150+ t |
| 20 | 2500 | 6000–12000 | AR / N / TM | 120+ t |
| 25 | 2500 | 6000–12000 | AR / N / TM | 100+ t |
| 30 | 2200 / 2500 | 6000–12000 | AR / N / TM | 80+ t |
| 40 | 2200 | 6000–12000 | AR / N / TM | 50+ t |
| 50 | 2200 | 6000–12000 | AR / N / TM | 30+ t |
Quantities change weekly — confirm before booking. Plates are sold as RINA FH36 with the RINA mark and endorsed certificate. Anything outside the stock list goes into the next mill campaign: about 4–6 weeks to certified plate.
Packing: bundled by size with steel strapping, marked with grade and heat number, shipped in containers (≤ 11.8 m) or break bulk to Mediterranean and other ports.
Processing before shipping. We cut FH36 to drawing by plasma or oxy-fuel, bevel edges for welding, shot-blast and prime with shop primer, and mark each piece with grade, heat number and part number so that RINA traceability survives cutting. Cut parts ship with a cutting list that cross-references every piece to its original plate and certificate.
RINA FH36 against other class societies
| Society / standard | Designation | Remark |
|---|---|---|
| RINA | RINA FH36 | this page — Rules for the Classification of Ships, Part D |
| BV | BV FH36 | closest naming habit (A/B/D/E, AH…, A420…) |
| DNV | DNV VL F36 | VL prefix |
| LR | LR FH36 | |
| ABS | ABS FH36 | |
| CCS | CCS F36 / FH36 | |
| KR | KR RF36 | R-prefix |
| NK | NK KF36 | K-prefix |
| ASTM A131 | ASTM A131/A131M Grade FH36 | product standard, no class stamp |
| GB 712 | GB 712 Grade FH36 | Chinese product standard, no class stamp |
All of these share the UR W11 FH36 requirements. Each society accepts only its own mark, so if you need RINA plus a second society, book both surveyors before the plates are tested.
Where FH36 sits in the RINA AH/DH/EH/FH matrix
Think of the series as a grid: moving right (AH36, DH36, EH36, FH36) lowers the test temperature, moving down (FH32, FH36, FH40) raises the yield. The RINA material class table fixes the letter from structural category and thickness; the scantling calculation fixes the number. Substituting a higher letter at the same number is normally accepted; a lower letter is not.
FH36 is chosen for polar and Arctic service. Few designs need it outside ice-class tonnage, so check that the class table really asks for −60 °C before paying for it. Above 390 N/mm², RINA’s extra-high-strength series starts at F420 (IACS UR W16). See RINA Steel Plates.
Level 36 is the default for the main hull girder; designers move to level 40 only where deck or coaming thickness would otherwise become awkward to weld.
Welding and forming RINA FH36
Typical uses: polar expedition cruise ships, Arctic ice-class tonnage and cold-region offshore units whose design temperature calls for −60 °C.
Welding: use RINA-approved high-tensile consumables of grade 5Y or higher (typical UR W17 mapping — confirm in the WPS). Preheat and heat input follow the RINA-approved procedure and the Ceq on the certificate. High-heat-input electrogas or one-side submerged-arc welding of thick FH36 needs a procedure qualified at that heat input.
Forming: TM plate gets part of its strength from controlled rolling and cooling. Keep line heating within the mill’s temperature limit — typically quoted around 650 °C for accelerated-cooled plate (UNCERTAIN, mill-specific).
Why the F letter here. FH36 is tested at −60 °C and is chosen for polar and Arctic service and the coldest design temperatures. FH plate needs the tightest steelmaking control, so certificates should be checked line by line for P, S, N and Ni. When building blocks mix letters, keep FH36 plates physically separated and colour-marked in the yard so that a lower letter is never fitted by mistake.
RINA survey, certificate and receiving checks
The certificate lists ladle chemistry including microalloys, Ceq for TM plate, tensile results, Charpy results at −60 °C, condition of supply and plate numbers, with the RINA surveyor’s endorsement.
On receipt: check the stamp reads FH36 with the RINA mark, the Charpy temperature and thickness band match the plate, and the endorsement is present. We can add EN 10204 3.2 witness, UT to EN 10160 or ASTM A578, Z-direction tests and dual class with another IACS society.
RINA approval of the manufacturer. A mill is approved by RINA for named grades, steelmaking route, delivery condition and maximum thickness, after approval tests and periodic renewal. Before placing an order for FH36, ask to see that the approval scope actually lists this grade and condition up to the thickness you need — this is the single most useful check a buyer can make (approval document format UNCERTAIN).
Mistakes we see on RINA FH36 orders
- Writing only “FH36” without RINA, so the plate arrives with another society’s mark
- Leaving the letter off (“36 grade”), so toughness is undefined
- Accepting a normal-strength A/B/D/E certificate against a high-tensile order
- No Ceq on the certificate for TM plate
- Substituting AH36 without class approval
- F-column limits (N, P, S, Ni) not checked
A clear order line — grade, rule book, condition, certificate — prevents nearly all of them.
With FH36 the expensive errors are mixed letters within a delivery, missing Ceq for TM plate, and plates whose thickness falls into a higher Charpy band than the test covered.
Buying RINA FH36 from China: concerns and answers
| Concern | Answer |
|---|---|
| Is the RINA mark genuine? | Only mills with RINA approval for RINA FH36; certificate and stamp traceable to the heat; third-party witness on request |
| Can the surveyor at our yard verify it? | Yes — the certificate number and heat can be checked against the mill’s RINA records |
| Payment safety | T/T with balance after inspection, or L/C at sight |
| Small or mixed orders | several sizes and RINA grades in one container |
| Delivery visibility | weekly photos from rolling to loading |
| Ready-to-fit parts | cutting, bevelling and drilling in our own workshop |
If your yard has never bought from a Chinese mill under RINA survey, we can arrange a trial lot, share sample certificates in advance, and let your inspector or the RINA surveyor visit the mill during rolling and testing.
Ordering RINA FH36
State: RINA FH36, condition of supply, sizes and quantities, UT / Z-direction, dual class, certificate type and port, and send to SHH STEEL.
Sample line: “Hull plate to RINA Rules for the Classification of Ships, Part D, grade FH36, TM, 12 × 2500 × 12000 mm, 40 pcs, RINA-endorsed certificate with Ceq, EN 10204 3.2, CFR Monfalcone.”
Order checklist:
- Society and rule book: RINA Rules for the Classification of Ships, Part D
- Grade: FH36
- Condition of supply (AR / N / TM as allowed)
- Sizes and quantity per size; flatness class if tighter than standard
- Certificate: RINA-endorsed, EN 10204 3.1 or 3.2
- Extras: UT, Z-direction, dual class, shot-blast/prime, cutting
- Delivery terms and destination port
FAQ
-
Is FH36 the official RINA name?
- FH36 is the IACS UR W11 designation and is the form used on RINA-classed drawings and orders for higher-strength hull steel. Whether a current RINA edition prints any additional prefix has not been verified against the rule text, so always quote “RINA Rules, Part D, grade FH36” on the order to remove any doubt. Its −60 °C test temperature makes it suitable for polar and Arctic service and the coldest design temperatures. Level 36 is the most widely produced high-tensile hull grade in the world, so it has the widest choice of RINA-approved mills, sizes and stock. In practice yards and owners call it FH36, “F36” or “FH-36”; the stamped grade is what the surveyor checks, so make sure the certificate shows the full FH36. Write the society on every document: plates without the RINA mark will be rejected at the yard however good the results are.
-
What strength and toughness does FH36 give?
- ReH ≥ 355 N/mm², Rm 490–620 N/mm², A ≥ 21 %, and Charpy at −60 °C. The required average energy rises with thickness, from 34 J (≤ 50 mm) to 50 J (70–100 mm) longitudinal, so a thick plate has to be tougher than a thin one to pass. FH plate needs the tightest steelmaking control, so certificates should be checked line by line for P, S, N and Ni. For FH36 the impact requirement applies to the thickness delivered, not ordered, so a plate rolled at the top of its tolerance may move into the next band; check the band on the certificate. FH plate is made by fewer mills, so confirm approval scope and lead time before fixing the design.
-
Why do passenger ships use so much FH36?
- Weight. Cruise ships and ferries are among the most weight-sensitive hulls afloat, and every tonne saved in the hull girder goes to stability, payload or fuel. 36-level plate lets the hull be thinner than in mild steel. Where this letter is used: polar expedition cruise ships, Arctic ice-class tonnage and cold-region offshore units whose design temperature calls for −60 °C. At −60 °C, mills usually control sulphur and inclusion shape closely to secure consistent results. At level 36, typical deck and shell thicknesses on passenger ships are 8–20 mm, while tankers and bulk carriers use 15–35 mm (market observation, not a rule). The approved drawing and the RINA material class table decide; the purchase order should simply repeat what the drawing says.
-
Is TM FH36 easier to weld than normalized plate?
- Usually yes. TM plate is made with a lower carbon equivalent — about Ceq 0.38 % up to 50 mm and 0.40 % at 50–100 mm — so it typically needs less preheat and tolerates higher heat input. The RINA-approved WPS still decides, and should be qualified on plate of the same route. FH36 consumables must also meet −60 °C toughness in the weld metal. Low-heat-input FCAW on thin panels and high-heat-input one-side SAW on thick seams behave differently, so a TM plate qualified for one is not automatically qualified for the other. We can send a sample certificate for FH36 before you order so your quality department can check the format.
-
Can FH36 replace another grade, or be replaced?
- A higher letter at the same strength can normally stand in for FH36: nothing at the same number. A lower letter or a lower number cannot. Any change from the approved drawing should be agreed with the RINA surveyor and recorded on the material list. Substitution by a higher letter is a quality upgrade; the cost difference should be agreed before delivery. Substitution within RINA should be documented on the material list the surveyor signs, with the substitute certificate attached. Mixed-grade containers are possible, with each plate clearly stamped.
-
Can one heat be certified as RINA FH36 and to another society?
- Yes, if every surveyor is booked before testing and the plate meets each society’s requirements. It is then stamped with each mark and the certificate shows each endorsement. This is common for ships that may change class later or for stock plate. Marks of other societies are added only if requested at order stage. Dual-stamped plate is popular with stockists because one pile can serve work for several IACS societies; the order must name every society in advance. Your WPS should be qualified on the same grade, thickness range and delivery route.
-
Which thicknesses of FH36 can you supply?
- Typically 6–60 mm from stock or rolling, up to 100 mm within the mill approval. FH plate above about 50 mm is limited to a few mills, so allow extra lead time. Plates for polar and Arctic service and the coldest design temperatures are often specified with Z-direction properties at joints loaded through thickness. Level 36 is the default for the main hull girder; designers move to level 40 only where deck or coaming thickness would otherwise become awkward to weld. For FH36, widths above 3000 mm and lengths above 15 m limit the choice of mills and may add a rolling surcharge. Thickness and width affect price as much as grade, so send the full size list for an accurate quote.
-
What are delivery times and payment terms?
- About 7–15 days from stock and 4–6 weeks for mill rolling plus survey, then shipping. A T/T deposit and balance on passed inspection, or L/C at sight. Trial lots and mixed-size containers are possible. Ask for a pro-forma invoice and inspection plan together, so payment milestones match testing. Prices follow the base plate price plus grade extras for letter and strength level; FH and thick TM plate carry the largest extras. Prices are usually quoted per tonne, with extras for cutting, priming, UT and 3.2 inspection itemised separately.
Conclusion
RINA FH36 is higher-strength hull steel under RINA’s Rules for the Classification of Ships, Part D (Materials and Welding): yield 355 N/mm², tensile 490–630 N/mm², Charpy −60 °C. A RINA-classed ship accepts it only with the RINA mark and an endorsed certificate.
SHH STEEL supplies RINA FH36 from RINA-approved Chinese mills, with cutting, UT and EN 10204 3.2 on request. Send grade, sizes, quantities and port for a quotation.