RINA Grade D Shipbuilding Steel Plate

RINA Grade D Shipbuilding Steel Plate

RINA Grade D normal-strength hull plate to RINA Rules Part D / IACS UR W11: yield 235 N/mm², Charpy at −20 °C. From RINA-approved Chinese mills via SHH STEEL — stock or mill-rolled, with cutting and 3.2 inspection.
Keywords
RINA Grade D steel plate, RINA D shipbuilding steel, Registro Italiano Navale Grade D, RINA D hull plate, normal strength hull structural steel
Equivalent Grades:
BV Grade D; DNV VL D; LR Grade D; ABS D; CCS Grade D; KR Grade D; NK Grade D (KD); ASTM A131 Grade D; GB 712 D
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Impact Test and Condition of Supply
Thickness Tolerance
Stock
Equivalent Grades
Grade Selection
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

RINA Grade D shipbuilding steel plate — overview

Technical Reviewer: Jack | SHH STEEL Material Solutions Department · Updated: 2026-10-28

RINA Grade D is the −20 °C mild hull steel in RINA Part D (Materials and Welding). It is always killed, and above 25 mm it must also be fine-grain treated. Yield (235 N/mm²) and tensile (400–520 N/mm²) are the same as A and B, so the buyer is paying for toughness. In Italian and Mediterranean yard practice it is the usual grade for bilge, sheer and stringer strakes in a mild-steel design.

Equivalent grades: ASTM A131 Grade D · ABS D · DNV NV D · LR Grade D · BV Grade D · CCS Grade D · NK KD · KR RD · GB 712 Grade D.

In the RINA normal-strength series the letter is the toughness: A (no test up to 50 mm), B (0 °C), D (−20 °C), E (−40 °C). Grade D is the standard choice for thick secondary strakes in temperate service. Never accept B in its place.

RINA is the Genoa-based society that classes much of the Italian fleet and a large share of the world’s cruise ships and ferries, many of them built at Fincantieri and other Italian and Mediterranean yards. That background shows in the steel: passenger ships use large areas of thin plate in decks and superstructure, so flatness, weld distortion and consistent supply count as much as the grade letter.

Plates come from a steelworks that holds RINA approval of the manufacturer for this grade, delivery condition and thickness range. Tests are witnessed by, or carried out under the approved scheme of, a RINA surveyor, and each plate is stamped with the RINA mark and grade. SHH STEEL sources RINA Grade D from RINA-approved Chinese plate mills, keeps the common sizes in stock and rolls the rest to order with the RINA survey booked at the mill. The full RINA range is under RINA Grade D.

How RINA names it. For normal-strength steel the RINA designation is just the letter — A, B, D or E — so the plate reads “Grade D” next to the RINA mark. There is no prefix or number to decode, which is why mistakes usually come from leaving the society off the order rather than from the grade name.

RINA Grade D: key data at a glance

Item RINA Grade D
Rule book RINA Rules for the Classification of Ships, Part D (Materials and Welding), normal-strength hull steel; aligned with IACS UR W11 Grade D (RINA chapter/section numbers not quoted — UNCERTAIN)
RINA designation Grade D (same letter as IACS)
Strength class normal strength, ReH ≥ 235 N/mm²
Deoxidation killed ≤25 mm; killed and fine grain >25 mm
Grain refinement required
Condition of supply AR / CR / N / TM as permitted by the UR W11 supply table for the ordered thickness
Charpy V CVN at −20 °C; fine grain above 25 mm
Thickness scope up to 100 mm under UR W11; above by agreement with RINA
Minus tolerance IACS UR W13 as applied by RINA (confirm class on order — UNCERTAIN)
Certificate mill inspection certificate endorsed by the RINA surveyor; EN 10204 3.1 / 3.2 on request

Size window. RINA Grade D is rolled from about 5 mm to 100 mm, 1500–3500 mm wide and up to roughly 18 m long. Passenger-ship work uses a lot of thin plate (5–12 mm) for decks and bulkheads, so flatness matters as much as strength — see the tolerance section. Plate cut from coil is acceptable only when the coil line itself is covered by the RINA approval.

Reading the table. The deoxidation and grain-refinement lines matter more for Grade D than the strength lines, which are the same for all four mild letters. They decide whether a plate from a given heat can be certified as Grade D at the ordered thickness, so check them on the certificate before the strength figures.

RINA Grade D chemistry — every element on the certificate

Element Ladle (heat) analysis, % Product (check) analysis, % Comment
C 0.21 max. numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate plate
Si 0.10–0.35 (min. waived if Al sol. ≥0.015 %) numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate
Mn 0.60 min. numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate
P 0.035 max. numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate
S 0.035 max. numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate
Al (acid-soluble) 0.015 min. where Al is the grain refiner numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate fine-grain practice
Nb may act as grain refiner; report if added numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate
V may act as grain refiner; report if added numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate
Ti report if intentionally added numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate
Cu 0.35 max. (residual) numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate UR W11 residual note
Cr 0.30 max. (residual) numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate residual
Ni 0.40 max. (residual) numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate residual
Mo 0.08 max. (residual) numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate residual
N not specified numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate report on request
Nb+V+Ti not specified for normal strength (calculated if added) not applicable (calculated from heat analysis)
C + Mn/6 0.40 max. (calculated) not applicable (calculated from heat analysis) carbon equivalent cap

Product (check) analysis column: RINA Rules Part D specify heat (ladle) limits; no numeric product-analysis tolerance is tabulated in the rule text reviewed, so product (check) limits are agreed on the order or taken from the approved mill specification and certificate.

The ladle limits are the IACS UR W11 values that RINA applies in Part D. We have not checked them against a current RINA edition, so the RINA text governs (UNCERTAIN). Grade D lowers the Mn minimum to 0.60 % but sets a 0.10–0.35 % Si window, the minimum being waived when acid-soluble Al reaches 0.015 %. Grain-refining elements become mandatory above 25 mm.

Cu, Cr, Ni and Mo are residuals from scrap and should be reported as measured. If the mill adds Al, Nb, V or Ti as grain refiners, the certificate should say so; a blank there on a D or E certificate above 25 mm is a reason to ask questions.

UR W11 gives no numeric check-analysis tolerance. If the yard or owner wants product analysis, fix the tolerance at enquiry and write it on the order.

RINA Grade D tensile requirements

Property Requirement
Yield strength ReH 235 N/mm² min.
Tensile strength Rm 400–520 N/mm²
Elongation A (5.65√S0) 22 % min.
Charpy test temperature −20 °C

Minimum elongation on a flat 200 mm gauge-length specimen depends on thickness:

t (mm) ≤5 5–10 10–15 15–20 20–25 25–30 30–40 40–50
A200 min. % 14 16 17 18 19 20 21 22

A, B, D and E share this tensile band; only toughness and chemistry change. One tensile test is taken per batch, with more for large batches or wide thickness spreads, under the UR W11 batch rules. Thin cruise-ship deck plate (5–8 mm) falls in the lowest elongation bands. That is how the table is built, not a sign of poor ductility.

Tensile specimens are taken transverse to the rolling direction for plate wider than about 600 mm, as UR W11/W16 practice requires; the certificate should show the specimen orientation. For mild steel, yield is reported as ReH; where no clear yield point appears, Rp0.2 is used.

RINA Grade D: Charpy V-notch and delivery condition

Grade D is tested at −20 °C. The batch size depends on the delivery condition, and above 25 mm the plate must also be fine-grain killed.

Thickness Avg. longitudinal (J) Avg. transverse (J)
≤ 50 mm 27 20
50–70 mm 34 24
70–100 mm 41 27

Values are averages of three full-size specimens; one result may fall below the average provided it is at least 70 % of it. Longitudinal specimens are standard unless transverse are ordered. Above 100 mm, agree the requirements with RINA.

Condition of supply matters commercially. AR plate is cheapest; N and TM plate cost more but widen the thickness range in which a lighter test regime applies. State the condition on the order so the mill and the surveyor test to the same plan.

Where the yard specification adds requirements beyond the rules — for example Charpy on Grade A below 50 mm — that is an order extra and should be written on the purchase order.

Thickness tolerance, flatness and surface

RINA applies the IACS UR W13 thickness tolerances to hull plate. UR W13 limits the minus side (commonly quoted as 0.3 mm — confirm on the order) and leaves plus tolerance, flatness, width and length to the agreed dimensional standard, such as EN 10029 or GB/T 709.

For passenger-ship decks in 5–8 mm plate, flatness is often the real issue: wavy thin plate costs the yard hours of straightening and line heating. If your yard works to a tighter flatness class, put it on the order. Surface defects may be ground out as long as the remaining thickness stays inside the minus tolerance; deeper repairs need the surveyor’s agreement.

UR W13 also allows local grinding of surface defects and sets how the average thickness of a plate is checked; the measurement points and acceptance method should be agreed at enquiry if the yard has its own procedure. For RINA passenger-ship work we suggest stating both the minus tolerance class and the flatness class on the order for any plate under 10 mm.

RINA Grade D stock and lead time

Thickness (mm) Width (mm) Length (mm) Condition Approx. qty
5 1500 / 1800 6000–12000 AR / CR / N / TM 80+ t
6 1800 / 2000 6000–12000 AR / CR / N / TM 100+ t
8 2000 6000–12000 AR / CR / N / TM 150+ t
10 2000 / 2200 6000–12000 AR / CR / N / TM 200+ t
12 2000 / 2500 6000–12000 AR / CR / N / TM 200+ t
16 2200 / 2500 6000–12000 AR / CR / N / TM 150+ t
20 2500 6000–12000 AR / CR / N / TM 120+ t
25 2500 6000–12000 AR / CR / N / TM 100+ t
30 2200 / 2500 6000–12000 AR / CR / N / TM 80+ t
40 2200 6000–12000 AR / CR / N / TM 50+ t
50 2200 6000–12000 AR / CR / N / TM 30+ t

Quantities change weekly — confirm before booking. Plates are sold as RINA Grade D with the RINA mark and endorsed certificate. Anything outside the stock list goes into the next mill campaign: about 3–5 weeks to certified plate.

Packing: bundled by size with steel strapping, marked with grade and heat number, shipped in containers (≤ 11.8 m) or break bulk to Mediterranean and other ports.

Processing before shipping. We cut Grade D to drawing by plasma or oxy-fuel, bevel edges for welding, shot-blast and prime with shop primer, and mark each piece with grade, heat number and part number so that RINA traceability survives cutting. Cut parts ship with a cutting list that cross-references every piece to its original plate and certificate.

RINA Grade D against other class societies and standards

Society / standard Designation Remark
RINA RINA Grade D this page — Rules for the Classification of Ships, Part D
BV BV Grade D closest naming habit (A/B/D/E, AH…, A420…)
DNV DNV VL D VL prefix
LR LR Grade D
ABS ABS D
CCS CCS Grade D
KR KR Grade D R-prefix
NK NK Grade D (KD) K-prefix
ASTM A131 ASTM A131/A131M Grade D product standard, no class stamp
GB 712 GB 712 Grade D Chinese product standard, no class stamp

All of these share the IACS chemistry and tensile limits, so one heat can carry several society marks if every surveyor attends the same tests. On paper, though, only the RINA mark satisfies a RINA-classed hull; a GB 712 or A131 mill sheet alone is not acceptable.

Picking the letter: A, B, D or E under RINA

Grade D costs more than B and less than E, and covers most thick mild-steel strakes in temperate service. The RINA material class table picks the letter from the member’s structural category (secondary, primary, special) and its thickness, so the drawing — not the buyer — decides whether a strake is Grade D.

Normal strength stops at 235 N/mm². Passenger ships use a lot of AH32/AH36 in the hull girder and keep mild steel for internal structure; if the design needs more strength, see the AH32–FH40 range under RINA Steel Plates. Typical RINA use for Grade D: bilge, sheer and stringer strakes of mild-steel designs, heavier shell plating of ferries and supply vessels, and the thick end of longitudinal bulkheads.

Using a higher mild letter than needed adds cost without improving the design; using a lower one is a non-conformity the surveyor will raise. Follow the material class table exactly.

Cutting, forming and welding RINA Grade D

Grade D cuts by oxy-fuel, plasma or laser without preheat. It is welded with RINA-approved consumables for normal-strength steel at the matching toughness grade (typically grade 1, 2 or 3 for A, D and E — confirm in the yard WPS), under procedures the RINA surveyor has approved.

Thin passenger-ship panels are welded on automated panel lines with low heat input to limit distortion; the low C + Mn/6 of mild steel makes this straightforward. Thick or highly restrained joints may still need preheat as set by the procedure.

Cold bending, flanging and line heating are routine. Order cold-flanging quality where needed. For offshore primary steel, see offshore platform steel plates.

Where Grade D fits. On ferries and supply vessels, Grade D is a frequent choice for bilge and sheer strakes in mild-steel designs. Grade D is the most common mild letter for strakes that the class table promotes because of thickness. Keep mild-steel and high-tensile plates of similar thickness clearly separated in the yard, because they look identical and differ only in the stamp.

RINA survey, certificate and receiving checks

At the mill the RINA surveyor witnesses or audits tensile and impact tests, checks identification and endorses the inspection certificate. The certificate lists heat number, ladle analysis, tensile results, Charpy results where required, condition of supply and plate numbers.

On receipt: match the stamped grade, heat and plate number to the certificate; check the RINA endorsement; confirm Charpy results are at the right temperature for Grade D; measure thickness at several points. On request we add EN 10204 3.2 third-party witness, ultrasonic testing or dual certification with another IACS society, provided it is booked before testing.

RINA approval of the manufacturer. A mill is approved by RINA for named grades, steelmaking route, delivery condition and maximum thickness, after approval tests and periodic renewal. Before placing an order for Grade D, ask to see that the approval scope actually lists the grade letter up to the thickness you need — this is the single most useful check a buyer can make (approval document format UNCERTAIN).

Mild-steel certificates are often batch certificates covering many plates; check that every plate number you received is listed and that the heat numbers on the plates match the certificate lines.

Mistakes we see on RINA Grade D orders

  • Plate above 25 mm without fine-grain practice
  • Accepting 0 °C results against a −20 °C order
  • Using D where more than 235 N/mm² yield is needed
  • Condition of supply not stated
  • No RINA endorsement

Every one of these is avoidable at enquiry: write the full RINA grade, the condition of supply, the certificate type and any dual-class need on the purchase order.

With normal-strength plate the costly mistakes are rarely about strength; they are about the toughness letter, the class mark and the condition of supply. A rejected certificate at the yard can stop a block for weeks.

Buying RINA Grade D from China: concerns and answers

Concern Answer
Is the RINA mark genuine? Only mills with RINA approval for RINA Grade D; certificate and stamp traceable to the heat; third-party witness on request
Can the surveyor at our yard verify it? Yes — the certificate number and heat can be checked against the mill’s RINA records
Payment safety T/T with balance after inspection, or L/C at sight
Small or mixed orders several sizes and RINA grades in one container
Delivery visibility weekly photos from rolling to loading
Ready-to-fit parts cutting, bevelling and drilling in our own workshop

If your yard has never bought from a Chinese mill under RINA survey, we can arrange a trial lot, share sample certificates in advance, and let your inspector or the RINA surveyor visit the mill during rolling and testing.

Ordering RINA Grade D

Send SHH STEEL: grade (RINA Grade D), sizes and quantity per size, condition of supply, flatness class if tighter than standard, any UT, dual-class or 3.2 requirement, surface finish (shot-blasted and primed or mill finish) and destination port.

Sample line: “Hull plate to RINA Rules for the Classification of Ships, Part D, Grade D, 10 × 2500 × 12000 mm, 60 pcs, RINA-endorsed certificate, EN 10204 3.1, CFR Genoa.”

Order checklist:

  • Society and rule book: RINA Rules for the Classification of Ships, Part D
  • Grade: Grade D
  • Condition of supply (AR / N / TM as allowed)
  • Sizes and quantity per size; flatness class if tighter than standard
  • Certificate: RINA-endorsed, EN 10204 3.1 or 3.2
  • Extras: UT, Z-direction, dual class, shot-blast/prime, cutting
  • Delivery terms and destination port

FAQ

Does RINA really call it Grade D?
Yes. RINA keeps the IACS letters A, B, D and E for normal-strength hull steel in Part D of its Rules for the Classification of Ships, so the plate is stamped Grade D with the RINA mark. “RINA Grade D” is how buyers search for it; on the purchase order write the rule book and grade together so the mill and the surveyor work to the same document. Grade D is the most common mild letter for strakes that the class table promotes because of thickness. On a mill certificate the grade line normally reads “RINA Grade D” or “Grade D” with the RINA reference and the surveyor’s endorsement; whichever wording is used, it must tie to the rule book named on your order. Write the society on every document: plates without the RINA mark will be rejected at the yard however good the results are.
What Charpy toughness does RINA Grade D need?
Cvn at −20 °c; fine grain above 25 mm. Average energies are 27/20 J up to 50 mm, 34/24 J at 50–70 mm and 41/27 J at 70–100 mm (longitudinal/transverse). One value in a set of three may be below the average if it is at least 70 % of it. On ferries and supply vessels, Grade D is a frequent choice for bilge and sheer strakes in mild-steel designs. For thick plate, ask for the test position (normally quarter thickness for plate over 40 mm, practice-based) and whether specimens are longitudinal or transverse, so you can compare results with the right column of the table. Grade D is the letter most often specified for thick mild-steel strakes on ferries and supply vessels in temperate waters.
Will the RINA surveyor accept a GB 712 or ASTM A131 certificate?
No. The chemistry is from the same family, but a RINA-classed hull needs plate from a RINA-approved mill, tested under RINA survey and stamped with the RINA mark. A heat can be certified to RINA and another standard at the same time if the surveyor attends before testing; it cannot be re-certified afterwards from paperwork alone. Results are reported per test unit, so a certificate with fewer results than plates is normal for batch-tested grades. If you hold plate certified only to a product standard, the usual remedy is replacement, not re-certification: RINA cannot endorse tests it did not witness or audit. The approved drawing and the RINA material class table decide; the purchase order should simply repeat what the drawing says.
Where is Grade D used on a passenger ship or ferry?
Typically bilge, sheer and stringer strakes of mild-steel designs, heavier shell plating of ferries and supply vessels, and the thick end of longitudinal bulkheads. The final choice comes from the RINA material class table, which assigns a letter by structural category and thickness, so check the approved drawing before ordering. If the class table requires a tougher letter only for part of a block, the other parts may stay at the lower letter. Mild steel is still a large share of a passenger ship’s tonnage, even though the hull girder is mostly high-tensile, because internal structure is designed for stiffness and minimum thickness rather than strength. We can send a sample certificate for Grade D before you order so your quality department can check the format.
Can Grade D be swapped with another letter?
E may replace D when it also meets the D requirements. B or A may not, because their test temperature is higher or they are untested. Any substitution should be noted on the material list the surveyor checks. Any higher letter supplied must still be stamped with its own grade, not the ordered one. If the substitute plate is thicker or from a different heat, it must still carry its own RINA certificate; a substitution never shares paperwork with the original order. Mixed-grade containers are possible, with each plate clearly stamped.
Does RINA Grade D need preheat for welding?
Usually not in normal thicknesses, because C + Mn/6 is capped at 0.40 and the steel has a low hardening tendency. The yard’s RINA-approved welding procedure sets the rule, especially for thick or restrained joints, damp conditions and cold workshops in winter. Low hydrogen consumables are good practice for thick sections even in mild steel. Cold-workshop welding in winter at northern Adriatic or Baltic yards can call for a modest preheat even on mild steel to drive off moisture; follow the WPS. Your WPS should be qualified on the same grade, thickness range and delivery route.
Which sizes of RINA Grade D are in stock?
Mostly 5–50 mm thick, 1500–2500 mm wide and 6–12 m long, including the thin 5–8 mm gauges used for passenger-ship decks and bulkheads. Other sizes are rolled in about 3–5 weeks with survey, and single plates can be sold from stock for repair work. We can also supply flat bars and sections cut from the same RINA-certified plate. Thin plate under 6 mm is sometimes supplied cut from coil; confirm that the coil processing line is inside the mill’s RINA approval. Thickness and width affect price as much as grade, so send the full size list for an accurate quote.
What are delivery times and payment terms?
About 7–15 days from stock and 3–5 weeks for mill rolling, plus shipping to the Mediterranean or other ports (estimates confirmed per quote). Payment by A T/T deposit and balance on passed inspection, or L/C at sight. EN 10204 3.2 witness, UT and dual class must be booked before testing. Trial orders of a few tonnes are possible from stock. For urgent repair work, a single plate can usually ship within a week from our Chinese stock with the original RINA certificate. Prices are usually quoted per tonne, with extras for cutting, priming, UT and 3.2 inspection itemised separately.

Conclusion

RINA Grade D is normal-strength hull steel under RINA’s Rules for the Classification of Ships, Part D (Materials and Welding): yield 235 N/mm², tensile 400–520 N/mm², Charpy at −20 °C. A RINA-classed ship accepts it only with the RINA mark and an endorsed certificate.

SHH STEEL supplies RINA Grade D from RINA-approved Chinese mills, with cutting, UT and EN 10204 3.2 on request. Send grade, sizes, quantities and port for a quotation.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X