RINA EH32 Shipbuilding Steel Plate

RINA EH32 Shipbuilding Steel Plate

RINA EH32 higher-strength hull plate to RINA Rules Part D / IACS UR W11: ReH 315 N/mm², Rm 440–590 N/mm², Charpy −40 °C. From RINA-approved Chinese mills via SHH STEEL — stock or mill-rolled, with cutting and 3.2 inspection.
Keywords
RINA EH32 steel plate, RINA EH32 shipbuilding steel, Registro Italiano Navale EH32, RINA EH32 hull plate, high tensile marine steel plate
Equivalent Grades:
BV EH32; DNV VL E32; LR EH32; ABS EH32; CCS E32 / EH32; KR RE32; NK KE32; ASTM A131 Grade EH32; GB 712 EH32
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Impact Test and Condition of Supply
Thickness Tolerance
Stock
Equivalent Grades
Grade Selection
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

RINA EH32 shipbuilding steel plate — overview

Technical Reviewer: Jack | SHH STEEL Material Solutions Department · Updated: 2026-10-28

RINA EH32 is the −40 °C grade of the 32 level — the high-tensile plate that RINA plan approval most often assigns to crack-arrest and cold-exposed members. Level 32 is the entry high-tensile level. It is popular on ferries and superyachts, where a modest strength gain over mild steel trims weight high up in the ship without changing welding practice much. Minimum yield is 315 N/mm², tensile 440–590 N/mm², elongation 22 %.

Equivalent grades: ASTM A131 Grade EH32 · ABS EH32 · DNV NV E32 · LR EH32 · BV EH32 · CCS E32 / EH32 · NK KE32 · KR RE32 · GB 712 Grade EH32.

In RINA’s high-tensile series the letter sets the Charpy temperature (AH 0 °C, DH −20 °C, EH −40 °C, FH −60 °C) and the number sets the yield (32 → 315, 36 → 355, 40 → 390 N/mm²). EH32 is the E letter at level 32. Typical RINA-classed uses: crack-arrest strakes on large passenger ships, ice-class Baltic ferries, structure around the fuel tanks of LNG-fuelled ships, and container-ship hatch coamings needing −40 °C.

RINA is the Genoa-based society that classes much of the Italian fleet and a large share of the world’s cruise ships and ferries, many of them built at Fincantieri and other Italian and Mediterranean yards. That background shows in the steel: passenger ships use large areas of thin plate in decks and superstructure, so flatness, weld distortion and consistent supply count as much as the grade letter.

SHH STEEL supplies EH32 from Chinese mills whose RINA approval covers high-tensile hull steel in the ordered condition and thickness, with the RINA survey at the mill. Common 36-level sizes are held in stock; the rest is rolled to order.

How RINA names it. For higher-strength steel RINA uses the IACS form: H for high tensile, the toughness letter in front and the strength level behind, so EH32 = letter E, level 32. Buyers sometimes shorten it to “E32”, but on RINA paperwork the H stays.

Level 32 gives about a third more yield than mild steel at a small price premium, and its weldability is close to mild steel, so it is an easy first step for yards moving superstructure or ferry decks to high-tensile.

RINA EH32: key data at a glance

ItemRINA EH32
Rule bookRINA Rules for the Classification of Ships, Part D (Materials and Welding), higher-strength hull steel; IACS UR W11 EH32 (RINA numbering not quoted — UNCERTAIN)
DesignationEH32: toughness letter EH + strength level 32
StrengthReH ≥ 315 N/mm², Rm 440–590 N/mm², A ≥ 22 %
Charpy V−40 °C
Steelmakingkilled and fine-grain treated (Al, Nb, V or Ti)
Condition of supplyAR / CR / N / TM as permitted by thickness and grain refiner; QT where approved
TM carbon equivalentCeq ≤ 0.36 % (t ≤ 50 mm), ≤ 0.38 % (50–100 mm) — indicative UR W11 practice, confirm on approval
Thickness scopeup to 100 mm (UR W11); beyond by agreement with RINA
Minus toleranceIACS UR W13 (confirm class — UNCERTAIN)
CertificateRINA-endorsed mill certificate; EN 10204 3.1 / 3.2

Traded EH32 is usually 6–60 mm thick and 2000–3000 mm wide. Passenger-ship hulls use a lot of 8–20 mm plate in this grade, which most RINA-approved mills roll routinely.

RINA EH32 chemistry — full alloy list

ElementLadle (heat) analysis, %Product (check) analysis, %Comment
C0.18 max.numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificateAH/DH/EH column
Si0.10–0.50numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate
Mn0.90–1.60 (AH ≤12.5 mm may be 0.70 min.)numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate
P0.035 max.numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate
S0.035 max.numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate
Al (acid-soluble)0.015 min. acid-soluble (or total Al per UR W11 fine-grain practice)numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificategrain refiner
Nb0.02–0.05 when used singlynumeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificategrain refiner / strength
V0.05–0.10 when used singlynumeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate
Ti0.02 max.numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate
Cu0.35 max.numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate
Cr0.20 max.numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate
Ni0.40 max.numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate
Mo0.08 max.numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificate
N—numeric tolerance not tabulated in RINA Rules Part D – agree on order / mill certificateno cap in A/D/E column
Nb+V+Ti0.12 max. (combined, when used together)not applicable (calculated from heat analysis)combined microalloy cap
Ceq (TM plate)0.36 / 0.38 max. (calculated)not applicable (calculated from heat analysis)t ≤ 50 / 50–100 mm

Product (check) analysis column: RINA Rules Part D specify heat (ladle) limits; no numeric product-analysis tolerance is tabulated in the rule text reviewed, so product (check) limits are agreed on the order or taken from the approved mill specification and certificate.

Ladle limits are the IACS UR W11 values for higher-strength hull steel, applied by RINA in Part D (not checked against a RINA edition — UNCERTAIN). For EH grades mills normally add Nb–Ti microalloying and hold sulphur far below the cap to secure −40 °C toughness in thick plate.

For TM plate ask for Ceq on the certificate, and Pcm too if your welding procedure is qualified on it. At level 32, most mills reach the strength with Nb alone. Check-analysis tolerances are agreed case by case.

RINA EH32 tensile requirements

PropertyRequirement
ReH315 N/mm² min.
Rm440–590 N/mm²
A (5.65√S0)22 % min.
Charpy test temperature−40 °C

Flat 200 mm test pieces — minimum elongation by thickness:

t (mm)≤55–1010–1515–2020–2525–3030–4040–50
A200 min. %1416171819202122

AH32, DH32, EH32 and FH32 share these tensile values; only the Charpy temperature and, for FH, the chemistry differ. Compared with mild steel, EH32 gives 80 N/mm² more yield, which is the margin the designer spends on thinner plate.

Tensile specimens are taken transverse to the rolling direction for plate wider than about 600 mm, as UR W11/W16 practice requires; the certificate should show the specimen orientation. For TM plate, a yield/tensile ratio is often around 0.8–0.9; there is no class limit unless the order adds one (indicative).

RINA EH32: Charpy at −40 °C and condition of supply

ThicknessAvg. long. (J)Avg. trans. (J)
≤ 50 mm3122
50–70 mm3826
70–100 mm4631

Required energy rises with thickness: a 70–100 mm EH32 plate must average 46 J longitudinal at −40 °C, against 31 J up to 50 mm. EH plate is supplied N or TM, and impact testing is more frequent than for AH/DH.

Condition of supply sets batch size and test frequency, so it belongs on the order. If the owner’s specification adds strain-aged impact tests or Z-direction properties, those are extra requirements and must be priced and booked in advance.

Thickness tolerance and surface

The minus tolerance follows IACS UR W13 as RINA applies it; plus tolerance, flatness and dimensions follow the agreed standard (EN 10029 or GB/T 709). Weight-optimised high-tensile designs — and passenger ships are among the most weight-sensitive — leave little margin, so measure thickness at several points on receipt. Thin high-tensile deck plate distorts more easily during welding than thicker plate; ordering a tighter flatness class can save fairing work later.

UR W13 also allows local grinding of surface defects and sets how the average thickness of a plate is checked; the measurement points and acceptance method should be agreed at enquiry if the yard has its own procedure. For RINA passenger-ship work we suggest stating both the minus tolerance class and the flatness class on the order for any plate under 10 mm.

RINA EH32 stock and lead time

Thickness (mm)Width (mm)Length (mm)ConditionApprox. qty
51500 / 18006000–12000AR / N / TM80+ t
61800 / 20006000–12000AR / N / TM100+ t
820006000–12000AR / N / TM150+ t
102000 / 22006000–12000AR / N / TM200+ t
122000 / 25006000–12000AR / N / TM200+ t
162200 / 25006000–12000AR / N / TM150+ t
2025006000–12000AR / N / TM120+ t
2525006000–12000AR / N / TM100+ t
302200 / 25006000–12000AR / N / TM80+ t
4022006000–12000AR / N / TM50+ t
5022006000–12000AR / N / TM30+ t

Quantities change weekly — confirm before booking. Plates are sold as RINA EH32 with the RINA mark and endorsed certificate. Anything outside the stock list goes into the next mill campaign: about 4–6 weeks to certified plate.

Packing: bundled by size with steel strapping, marked with grade and heat number, shipped in containers (≤ 11.8 m) or break bulk to Mediterranean and other ports.

Processing before shipping. We cut EH32 to drawing by plasma or oxy-fuel, bevel edges for welding, shot-blast and prime with shop primer, and mark each piece with grade, heat number and part number so that RINA traceability survives cutting. Cut parts ship with a cutting list that cross-references every piece to its original plate and certificate.

RINA EH32 against other class societies

Society / standardDesignationRemark
RINARINA EH32this page — Rules for the Classification of Ships, Part D
BVBV EH32closest naming habit (A/B/D/E, AH…, A420…)
DNVDNV VL E32VL prefix
LRLR EH32
ABSABS EH32
CCSCCS E32 / EH32
KRKR RE32R-prefix
NKNK KE32K-prefix
ASTM A131ASTM A131/A131M Grade EH32product standard, no class stamp
GB 712GB 712 Grade EH32Chinese product standard, no class stamp

All of these share the UR W11 EH32 requirements. Each society accepts only its own mark, so if you need RINA plus a second society, book both surveyors before the plates are tested.

Where EH32 sits in the RINA AH/DH/EH/FH matrix

Think of the series as a grid: moving right (AH32, DH32, EH32, FH32) lowers the test temperature, moving down (EH32, EH36, EH40) raises the yield. The RINA material class table fixes the letter from structural category and thickness; the scantling calculation fixes the number. Substituting a higher letter at the same number is normally accepted; a lower letter is not.

EH32 is where passenger ships put their crack-arrest strakes and where ice-class ferries need cold toughness. Ask whether a TM EH plate also saves preheat compared with an N plate. Above 390 N/mm², RINA’s extra-high-strength series starts at E420 (IACS UR W16). See RINA Steel Plates.

Level 32 is often chosen for thinner upper decks and superstructure fronts where buckling, not yield, governs, so the full 355 N/mm² of level 36 would not be used.

Welding and forming RINA EH32

Typical uses: crack-arrest strakes on large passenger ships, ice-class Baltic ferries, structure around the fuel tanks of LNG-fuelled ships, and container-ship hatch coamings needing −40 °C.

Welding: use RINA-approved high-tensile consumables of grade 4Y or higher (typical UR W17 mapping — confirm in the WPS). Preheat and heat input follow the RINA-approved procedure and the Ceq on the certificate. High-heat-input electrogas or one-side submerged-arc welding of thick EH32 needs a procedure qualified at that heat input.

Forming: TM plate gets part of its strength from controlled rolling and cooling. Keep line heating within the mill’s temperature limit — typically quoted around 650 °C for accelerated-cooled plate (UNCERTAIN, mill-specific).

Why the E letter here. EH32 is tested at −40 °C and is chosen for crack-arrest areas, ice-class ships and cold-region service. Owners of passenger ships often specify EH for sheer strakes and deck stringers regardless of thickness, as an added safety margin. When building blocks mix letters, keep EH32 plates physically separated and colour-marked in the yard so that a lower letter is never fitted by mistake.

RINA survey, certificate and receiving checks

The certificate lists ladle chemistry including microalloys, Ceq for TM plate, tensile results, Charpy results at −40 °C, condition of supply and plate numbers, with the RINA surveyor’s endorsement.

On receipt: check the stamp reads EH32 with the RINA mark, the Charpy temperature and thickness band match the plate, and the endorsement is present. We can add EN 10204 3.2 witness, UT to EN 10160 or ASTM A578, Z-direction tests and dual class with another IACS society.

RINA approval of the manufacturer. A mill is approved by RINA for named grades, steelmaking route, delivery condition and maximum thickness, after approval tests and periodic renewal. Before placing an order for EH32, ask to see that the approval scope actually lists this grade and condition up to the thickness you need — this is the single most useful check a buyer can make (approval document format UNCERTAIN).

Mistakes we see on RINA EH32 orders

  • Writing only “EH32” without RINA, so the plate arrives with another society’s mark
  • Leaving the letter off (“36 grade”), so toughness is undefined
  • Accepting a normal-strength A/B/D/E certificate against a high-tensile order
  • No Ceq on the certificate for TM plate
  • Substituting AH32 without class approval
  • Charpy band for the delivered thickness not checked

A clear order line — grade, rule book, condition, certificate — prevents nearly all of them.

With EH32 the expensive errors are mixed letters within a delivery, missing Ceq for TM plate, and plates whose thickness falls into a higher Charpy band than the test covered.

Buying RINA EH32 from China: concerns and answers

ConcernAnswer
Is the RINA mark genuine?Only mills with RINA approval for RINA EH32; certificate and stamp traceable to the heat; third-party witness on request
Can the surveyor at our yard verify it?Yes — the certificate number and heat can be checked against the mill’s RINA records
Payment safetyT/T with balance after inspection, or L/C at sight
Small or mixed ordersseveral sizes and RINA grades in one container
Delivery visibilityweekly photos from rolling to loading
Ready-to-fit partscutting, bevelling and drilling in our own workshop

If your yard has never bought from a Chinese mill under RINA survey, we can arrange a trial lot, share sample certificates in advance, and let your inspector or the RINA surveyor visit the mill during rolling and testing.

Ordering RINA EH32

State: RINA EH32, condition of supply, sizes and quantities, UT / Z-direction, dual class, certificate type and port, and send to SHH STEEL.

Sample line: “Hull plate to RINA Rules for the Classification of Ships, Part D, grade EH32, TM, 12 × 2500 × 12000 mm, 40 pcs, RINA-endorsed certificate with Ceq, EN 10204 3.2, CFR Monfalcone.”

Order checklist:

  • Society and rule book: RINA Rules for the Classification of Ships, Part D
  • Grade: EH32
  • Condition of supply (AR / N / TM as allowed)
  • Sizes and quantity per size; flatness class if tighter than standard
  • Certificate: RINA-endorsed, EN 10204 3.1 or 3.2
  • Extras: UT, Z-direction, dual class, shot-blast/prime, cutting
  • Delivery terms and destination port

FAQ

Is EH32 the official RINA name?
EH32 is the IACS UR W11 designation and is the form used on RINA-classed drawings and orders for higher-strength hull steel. Whether a current RINA edition prints any additional prefix has not been verified against the rule text, so always quote “RINA Rules, Part D, grade EH32” on the order to remove any doubt. Its −40 °C test temperature makes it suitable for crack-arrest areas, ice-class ships and cold-region service. Level 32 gives about a third more yield than mild steel at a small price premium, and its weldability is close to mild steel, so it is an easy first step for yards moving superstructure or ferry decks to high-tensile. In practice yards and owners call it EH32, “E32” or “EH-32”; the stamped grade is what the surveyor checks, so make sure the certificate shows the full EH32. Write the society on every document: plates without the RINA mark will be rejected at the yard however good the results are.
What strength and toughness does EH32 give?
ReH ≥ 315 N/mm², Rm 440–590 N/mm², A ≥ 22 %, and Charpy at −40 °C. The required average energy rises with thickness, from 31 J (≤ 50 mm) to 46 J (70–100 mm) longitudinal, so a thick plate has to be tougher than a thin one to pass. Owners of passenger ships often specify EH for sheer strakes and deck stringers regardless of thickness, as an added safety margin. For EH32 the impact requirement applies to the thickness delivered, not ordered, so a plate rolled at the top of its tolerance may move into the next band; check the band on the certificate. EH plate is the usual crack-arrest grade, so expect the owner’s specification to ask about it specifically.
Why do passenger ships use so much EH32?
Weight. Cruise ships and ferries are among the most weight-sensitive hulls afloat, and every tonne saved in the hull girder goes to stability, payload or fuel. 32-level plate lets the hull be thinner than in mild steel. Where this letter is used: crack-arrest strakes on large passenger ships, ice-class Baltic ferries, structure around the fuel tanks of LNG-fuelled ships, and container-ship hatch coamings needing −40 °C. At −40 °C, mills usually control sulphur and inclusion shape closely to secure consistent results. At level 32, typical deck and shell thicknesses on passenger ships are 8–20 mm, while tankers and bulk carriers use 15–35 mm (market observation, not a rule). The approved drawing and the RINA material class table decide; the purchase order should simply repeat what the drawing says.
Is TM EH32 easier to weld than normalized plate?
Usually yes. TM plate is made with a lower carbon equivalent — about Ceq 0.36 % up to 50 mm and 0.38 % at 50–100 mm — so it typically needs less preheat and tolerates higher heat input. The RINA-approved WPS still decides, and should be qualified on plate of the same route. EH32 consumables must also meet −40 °C toughness in the weld metal. Low-heat-input FCAW on thin panels and high-heat-input one-side SAW on thick seams behave differently, so a TM plate qualified for one is not automatically qualified for the other. We can send a sample certificate for EH32 before you order so your quality department can check the format.
Can EH32 replace another grade, or be replaced?
A higher letter at the same strength can normally stand in for EH32: FH at the same number. A lower letter or a lower number cannot. Any change from the approved drawing should be agreed with the RINA surveyor and recorded on the material list. Substitution by a higher letter is a quality upgrade; the cost difference should be agreed before delivery. Substitution within RINA should be documented on the material list the surveyor signs, with the substitute certificate attached. Mixed-grade containers are possible, with each plate clearly stamped.
Can one heat be certified as RINA EH32 and to another society?
Yes, if every surveyor is booked before testing and the plate meets each society’s requirements. It is then stamped with each mark and the certificate shows each endorsement. This is common for ships that may change class later or for stock plate. Marks of other societies are added only if requested at order stage. Dual-stamped plate is popular with stockists because one pile can serve work for several IACS societies; the order must name every society in advance. Your WPS should be qualified on the same grade, thickness range and delivery route.
Which thicknesses of EH32 can you supply?
Typically 6–60 mm from stock or rolling, up to 100 mm within the mill approval. Thin 6–12 mm plate for passenger-ship decks is routine; thick plate needs a rolling slot, so plan 4–6 weeks. Plates for crack-arrest areas, ice-class ships and cold-region service are often specified with Z-direction properties at joints loaded through thickness. Level 32 is often chosen for thinner upper decks and superstructure fronts where buckling, not yield, governs, so the full 355 N/mm² of level 36 would not be used. For EH32, widths above 3000 mm and lengths above 15 m limit the choice of mills and may add a rolling surcharge. Thickness and width affect price as much as grade, so send the full size list for an accurate quote.
What are delivery times and payment terms?
About 7–15 days from stock and 4–6 weeks for mill rolling plus survey, then shipping. A T/T deposit and balance on passed inspection, or L/C at sight. Trial lots and mixed-size containers are possible. Ask for a pro-forma invoice and inspection plan together, so payment milestones match testing. Prices follow the base plate price plus grade extras for letter and strength level; FH and thick TM plate carry the largest extras. Prices are usually quoted per tonne, with extras for cutting, priming, UT and 3.2 inspection itemised separately.

Conclusion

RINA EH32 is higher-strength hull steel under RINA’s Rules for the Classification of Ships, Part D (Materials and Welding): yield 315 N/mm², tensile 440–590 N/mm², Charpy −40 °C. A RINA-classed ship accepts it only with the RINA mark and an endorsed certificate.

SHH STEEL supplies RINA EH32 from RINA-approved Chinese mills, with cutting, UT and EN 10204 3.2 on request. Send grade, sizes, quantities and port for a quotation.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *



    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *



      X