JIS G4305 SUS410S Steel Plate | 410S Stainless Steel - SHH STEEL

JIS G4305 SUS410S Steel Plate | 410S Stainless Steel

JIS G4305 SUS410S is a low-carbon 12% chromium stainless steel plate/sheet with improved weldability compared with standard SUS410. It offers moderate corrosion resistance and good formability. SHH STEEL supplies SUS410S as Mill Direct Supply with competitive pricing and full mill certification.
Equivalent Grades:
ASTM A240 410S (S41008) / GB/T 3280 06Cr13 (0Cr13) / EN 10088-2 X6Cr13 (1.4000)
Product form:
Plate, Sheet, Coil, Strip, Foil, Shim, Circle, Ring
Surface:
2B, 2D, BA, No.4, HL, 8K Mirror, Hairline
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Surface Finishes
Delivery Conditions
Key Characteristics
Equivalent Material Grades
Applications
Why Choose SHH STEEL
FAQ
Conclusion

General Description

As a professional stainless steel supplier and China Mill-Direct Exporter, SHH STEEL is pleased to present JIS G4305 SUS410S Steel Plate (also known as 410S stainless steel).

SUS410S is a low-carbon version of the 12% chromium stainless steel under the Japanese standard JIS G4305 for cold-rolled stainless steel plates, sheets and strips. By limiting the carbon content, SUS410S offers significantly better weldability and reduced risk of hardening or cracking after welding compared with standard SUS410. It provides moderate corrosion resistance in mild environments, good formability and is fully magnetic. This grade is widely used as a cost-effective alternative where welding is required and high hardness is not the primary need.

SHH STEEL supplies SUS410S as Mill Direct Supply, sourcing directly from major Chinese stainless steel mills. This ensures competitive mill pricing, consistent quality, shorter lead times and full traceability. We offer thicknesses from 0.4 mm to 6.0 mm, widths up to 1500 mm, in coil or cut-to-length form. All materials are delivered with full Mill Test Certificates.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Primary Standard JIS G4305 Full compliance
Steel Grade SUS410S Confirmed
Product Form Cold-rolled Plate / Sheet / Coil Available
Surface Finish 2B, BA, No.4 (common) Available
Thickness Range 0.4 mm – 6.0 mm Custom sizes available
Width Up to 1500 mm Available
Certification EN 10204 3.1 / Mill Certificate Available

Chemical Composition

Chemical composition according to JIS G4305 (Heat Analysis):

Element Content (%)
Carbon (C) ≤ 0.08
Silicon (Si) ≤ 1.00
Manganese (Mn) ≤ 1.00
Phosphorus (P) ≤ 0.040
Sulfur (S) ≤ 0.030
Chromium (Cr) 11.50 – 13.50
Nickel (Ni) ≤ 0.60

Note: The restricted carbon content is the key difference from standard SUS410, resulting in improved weldability and reduced hardening tendency.

Mechanical Properties

Mechanical properties of JIS G4305 SUS410S (annealed condition):

Property Value
Yield Strength (0.2%) ≥ 205 MPa
Tensile Strength ≥ 410 MPa
Elongation ≥ 20%
Hardness ≤ 183 HB

Density: Approximately 7.75 g/cm³ Magnetic: Yes

Surface Finishes

Finish Description Typical Applications
2B Cold-rolled, annealed, pickled, skin-passed General fabrication
BA Bright Annealed Cleaner surface applications
No.4 Brushed finish Decorative or visible parts

Delivery Conditions

SHH STEEL supplies JIS G4305 SUS410S as Mill Direct Supply in annealed condition.

Additional options available:

  • Coil or cut-to-length sheets/plates
  • Protective film
  • Third-party inspection (SGS, BV, TUV, etc.)

Key Characteristics

  • Improved weldability compared with standard SUS410
  • Lower risk of hardening and cracking after welding
  • Moderate corrosion resistance in mild atmospheres
  • Good formability
  • Fully magnetic
  • Cost-effective 12% chromium stainless steel
  • Suitable for welded structures where high hardness is not required

Equivalent Material Grades

Grade Standard Notes
SUS410S JIS G4305 —
410S ASTM A240 American equivalent
1.4000 / X6Cr13 EN 10088-2 Closest European equivalent
06Cr13 / 0Cr13 GB/T 3280 Chinese equivalents
UNS S41008 — Unified Numbering System

Applications

JIS G4305 SUS410S is used in applications requiring moderate corrosion resistance and good weldability. Typical applications include:

Application Area Typical Components / Uses (Keywords)
Automotive Exhaust components, structural parts – 410S Automotive
Industrial Equipment Containers, ducts, welded parts – 410S Industrial
Petrochemical Columns, vessels (mild service) – 410S Petrochemical
General Fabrication Welded structures – 410S Fabrication
Heat-Resistant Parts Moderate temperature service – 410S Heat Resistant
Construction Architectural and structural components – 410S Construction

Why Choose SHH STEEL

SHH STEEL provides SUS410S as Mill Direct Supply. We maintain long-term strategic cooperation with major Chinese stainless steel mills and act as a first-level agent. This direct mill supply model allows us to offer competitive mill-direct pricing, faster delivery times, consistent quality, and full Mill Test Certificates for JIS G4305 SUS410S Steel Plate.

Customers benefit from reliable supply, short lead times and cost-effective solutions for low-carbon 12% chromium stainless steel projects. Our professional export team provides technical support on material selection and processing.

FAQ

What is the main difference between SUS410 and SUS410S?
SUS410S has lower carbon content, which significantly improves weldability and reduces the tendency to harden during cooling after welding. Standard SUS410 can be hardened by heat treatment.

Conclusion

JIS G4305 SUS410S Steel Plate (410S Stainless Steel) from SHH STEEL is a low-carbon 12% chromium stainless steel offering improved weldability and moderate corrosion resistance. As Mill Direct Supply, we provide competitive pricing, consistent quality and full technical support. Trust SHH STEEL for your SUS410S stainless steel requirements.

Contact SHH STEEL today for stock availability, pricing and technical support. JIS G4305 SUS410S Steel Plate, SUS410S, 410S stainless steel, 410S stainless steel plate, SUS410S supplier

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X