JIS G4305 SUS316TI Steel Plate | 316TI Stainless Steel - SHH STEEL

JIS G4305 SUS316TI Steel Plate | 316TI Stainless Steel

JIS G4305 SUS316TI is a titanium-stabilized molybdenum-bearing austenitic stainless steel plate/sheet offering excellent resistance to intergranular corrosion, good high-temperature performance and superior pitting resistance. SHH STEEL supplies SUS316TI as Mill Direct Supply with competitive pricing and full mill certification.
Equivalent material:
ASTM A240 316Ti (S31635) / GB/T 3280 06Cr17Ni12Mo2Ti (0Cr18Ni12Mo3Ti) / EN 10088-2 X6CrNiMoTi17-12-2 (1.4571)
Surface:
2B, 2D, BA, No.4, HL, 8K Mirror, Hairline
Product form:
Plate, Sheet, Coil, Strip, Foil, Shim, Circle, Ring
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Surface Finishes
Delivery Conditions
Key Characteristics
Equivalent Material Grades
Applications
Why Choose SHH STEEL
FAQ
Conclusion

What is JIS G4305 SUS316TI Steel Plate?

As a professional stainless steel supplier and China Mill-Direct Exporter, SHH STEEL is pleased to present JIS G4305 SUS316TI Steel Plate, also known as 316TI stainless steel.

JIS G4305 SUS316TI is a titanium-stabilized version of the molybdenum-bearing austenitic stainless steel under the Japanese standard for cold-rolled stainless steel plates, sheets and strips. The addition of titanium stabilizes the carbon, providing excellent resistance to intergranular corrosion even after welding or exposure to high temperatures. Combined with molybdenum, SUS316TI stainless steel offers superior pitting resistance in chloride environments and reliable performance in chemical, petrochemical and high-temperature applications. SHH STEEL supplies high-quality JIS G4305 SUS316TI as Mill Direct Supply from leading Chinese stainless steel mills.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Primary Standard JIS G4305 Full compliance
Steel Grade SUS316TI Confirmed
Product Form Cold-rolled Plate / Sheet / Coil Available
Surface Finish 2B, BA, No.4, HL, polished Available
Thickness Range 0.3 mm – 6.0 mm (standard) Custom sizes available
Width Up to 1500 mm or wider Available
Certification EN 10204 3.1 / Mill Certificate Available

JIS G4305 SUS316TI steel plate is available in various thicknesses and finishes to meet the requirements of demanding 316TI stainless steel applications.

Chemical Composition

Chemical composition of JIS G4305 SUS316TI (Heat Analysis):

Element Content (%)
Carbon (C) ≤ 0.08
Silicon (Si) ≤ 1.00
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Chromium (Cr) 16.00 – 18.00
Nickel (Ni) 10.00 – 14.00
Molybdenum (Mo) 2.00 – 3.00
Titanium (Ti) ≥ 5 × C%

The titanium addition in SUS316TI stainless steel effectively stabilizes carbon and prevents chromium carbide precipitation, giving JIS G4305 SUS316TI excellent resistance to intergranular corrosion.

Mechanical Properties

Mechanical properties of JIS G4305 SUS316TI (annealed condition):

Property Value
Yield Strength (0.2%) ≥ 205 MPa
Tensile Strength ≥ 520 MPa
Elongation ≥ 40%
Hardness ≤ 187 HB

JIS G4305 SUS316TI stainless steel maintains good strength and excellent toughness, making 316TI stainless steel plate suitable for both fabrication and high-temperature service.

Density: Approximately 7.98 g/cm³ Magnetic: Non-magnetic in annealed condition.

Surface Finishes

Finish Description Typical Applications
2B Cold-rolled, annealed, pickled, skin-passed General industrial use of SUS316TI
BA Bright Annealed Clean and decorative 316TI applications
No.4 Brushed finish Architectural 316TI stainless steel
HL Hairline finish Decorative panels
Polished Mirror or custom polish High-end 316TI stainless steel products

SHH STEEL provides JIS G4305 SUS316TI steel plate in multiple surface finishes to suit both functional and aesthetic requirements of 316TI stainless steel projects.

Delivery Conditions

SHH STEEL supplies JIS G4305 SUS316TI as Mill Direct Supply in annealed condition with various surface finishes.

Additional options available for SUS316TI stainless steel:

  • Coil or cut-to-length sheets/plates
  • Protective film
  • Third-party inspection (SGS, BV, TUV, etc.)

Key Characteristics

  • Excellent resistance to intergranular corrosion due to titanium stabilization in SUS316TI
  • Superior pitting and crevice corrosion resistance from molybdenum addition
  • Good high-temperature performance of 316TI stainless steel
  • Reliable weldability of JIS G4305 SUS316TI without risk of sensitization
  • Non-magnetic in annealed condition
  • Suitable for continuous service at elevated temperatures
  • Preferred grade for chemical and petrochemical welded equipment

Equivalent Material Grades

Grade Standard Notes
SUS316TI JIS G4305 —
316Ti ASTM A240 American equivalent
1.4571 / X6CrNiMoTi17-12-2 EN 10088-2 European equivalent
06Cr17Ni12Mo2Ti GB/T 3280 Chinese equivalent
UNS S31635 — Unified Numbering System

JIS G4305 SUS316TI is fully equivalent to international 316Ti stainless steel grades and is widely accepted in global projects.

Applications

JIS G4305 SUS316TI (316TI Stainless Steel) is widely used in corrosive and high-temperature welded applications. Typical uses include:

Application Area Typical Components / Uses (Keywords)
Chemical & Petrochemical Reactors, heat exchangers, pipelines – SUS316TI Chemical
High-Temperature Equipment Furnace parts, thermal components – 316TI High Temperature
Food & Pharmaceutical Processing equipment – 316TI Food Grade
Marine & Coastal Corrosive environment structures – 316TI Marine
Heat Exchangers Tubesheets and shells – 316TI Heat Exchanger
General Fabrication Welded corrosive-service parts – 316TI Fabrication

Why Choose SHH STEEL

SHH STEEL provides JIS G4305 SUS316TI as Mill Direct Supply. We maintain long-term strategic cooperation with major Chinese stainless steel mills and act as a first-level agent. This direct mill supply model allows us to offer competitive mill-direct pricing, faster delivery times, consistent quality, and full Mill Test Certificates for JIS G4305 SUS316TI Steel Plate.

Customers benefit from reliable supply of high-quality 316TI stainless steel, short lead times and professional technical support for SUS316TI projects worldwide.

FAQ

What is the main advantage of SUS316TI over SUS316L?
JIS G4305 SUS316TI is titanium-stabilized, providing excellent resistance to intergranular corrosion and better performance in high-temperature service, while SUS316L relies on ultra-low carbon content.
Is SUS316TI suitable for high-temperature applications?
Yes. 316TI stainless steel offers good oxidation resistance and strength at elevated temperatures, making it suitable for many continuous high-temperature services.
Is SUS316TI magnetic?
316TI stainless steel is non-magnetic in the annealed condition. It may become slightly magnetic after heavy cold working.
What is the density of SUS316TI?
Approximately 7.98 g/cm³ for JIS G4305 SUS316TI stainless steel.

Conclusion

JIS G4305 SUS316TI Steel Plate (316TI Stainless Steel) from SHH STEEL is a titanium-stabilized molybdenum-bearing austenitic stainless steel offering excellent intergranular corrosion resistance, superior pitting resistance and reliable high-temperature performance. As Mill Direct Supply, we provide competitive pricing, consistent quality and full technical support. Trust SHH STEEL for your SUS316TI stainless steel requirements.

Contact SHH STEEL today for stock availability, pricing and technical support. JIS G4305 SUS316TI Steel Plate, SUS316TI, 316TI stainless steel, 316TI stainless steel plate, SUS316TI supplier

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *