JIS G4305 SUS301 Steel Plate | 301 Stainless Steel - SHH STEEL

JIS G4305 SUS301 Steel Plate | 301 Stainless Steel

JIS G4305 SUS301 is an austenitic stainless steel plate/sheet with high work-hardening rate, offering high strength after cold working and good corrosion resistance. SHH STEEL supplies SUS301 as Mill Direct Supply with competitive pricing and full mill certification.
Equivalent Grades:
ASTM A240 301 (S30100) / GB/T 3280 12Cr17Ni7 (1Cr17Ni7) / EN 10088-2 X5CrNi17-7 (1.4319)
Surface:
2B, 2D, BA, No.4, HL, 8K Mirror, Hairline
Product form:
Plate, Sheet, Coil, Strip, Foil, Shim, Circle, Ring
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Surface Finishes
Delivery Conditions
Key Characteristics
Equivalent Material Grades
Applications
Why Choose SHH STEEL
FAQ
Conclusion

What is JIS G4305 SUS301 Steel Plate?

As a professional stainless steel supplier and China Mill-Direct Exporter, SHH STEEL is pleased to present JIS G4305 SUS301 Steel Plate (also known as 301 stainless steel).

SUS301 is an austenitic stainless steel under the Japanese standard JIS G4305 for cold-rolled stainless steel plates, sheets and strips. It contains higher carbon and slightly lower nickel than SUS304, resulting in a significantly higher work-hardening rate. This allows SUS301 to achieve high strength and hardness through cold working while maintaining good corrosion resistance and formability in the annealed condition. It is widely used for applications requiring high strength-to-weight ratio, such as springs, railway components, fasteners and structural parts.

SHH STEEL supplies SUS301 as Mill Direct Supply, sourcing directly from major Chinese stainless steel mills. This ensures competitive mill pricing, consistent quality, shorter lead times and full traceability. We offer thicknesses from 0.3 mm to 3.0 mm (thicker plates available on request), widths up to 1500 mm, in coil or cut-to-length form. All materials are delivered with full Mill Test Certificates.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Primary Standard JIS G4305 Full compliance
Steel Grade SUS301 Confirmed
Product Form Cold-rolled Plate / Sheet / Coil Available
Surface Finish 2B, BA, No.4, polished (common) Available
Thickness Range 0.3 mm – 3.0 mm (standard) Custom sizes available
Width Up to 1500 mm Available
Certification EN 10204 3.1 / Mill Certificate Available

Chemical Composition

Chemical composition according to JIS G4305 (Heat Analysis):

Element Content (%)
Carbon (C) ≤ 0.15
Silicon (Si) ≤ 1.00
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Chromium (Cr) 16.00 – 18.00
Nickel (Ni) 6.00 – 8.00
Nitrogen (N) ≤ 0.10

Note: Higher carbon and lower nickel compared with SUS304 give SUS301 its characteristic high work-hardening rate.

Mechanical Properties

Mechanical properties of JIS G4305 SUS301 (annealed condition):

Property Value
Yield Strength (0.2%) ≥ 205 MPa
Tensile Strength ≥ 520 MPa
Elongation ≥ 40%
Hardness ≤ 207 HB

After cold working, strength and hardness can be significantly increased (¼ Hard, ½ Hard, ¾ Hard, Full Hard tempers available).

Density: Approximately 7.93 g/cm³ Magnetic: Generally non-magnetic in annealed condition; becomes slightly magnetic after cold working.

Surface Finishes

Finish Description Typical Applications
2B Cold-rolled, annealed, pickled, skin-passed General fabrication
BA Bright Annealed Cleaner and decorative applications
No.4 Brushed finish Architectural and visible parts
Polished Mirror or custom polish Decorative and high-end uses

SHH STEEL supplies JIS G4305 SUS301 as Mill Direct Supply in annealed or various cold-worked tempers (¼H, ½H, ¾H, Full Hard) according to customer requirements.

Additional options available:

  • Coil or cut-to-length sheets/plates
  • Protective film
  • Third-party inspection (SGS, BV, TUV, etc.)

Key Characteristics

  • High work-hardening rate → excellent strength after cold working
  • Good corrosion resistance in mild to moderate environments
  • Excellent formability in annealed condition
  • High strength-to-weight ratio
  • Can be supplied in multiple hardness tempers
  • Good fatigue resistance
  • Cost-effective alternative to higher-nickel austenitic grades for strength-critical applications

Equivalent Material Grades

Grade Standard Notes
SUS301 JIS G4305 —
301 ASTM A240 American equivalent
1.4310 / X10CrNi18-8 EN 10088-2 European equivalent
12Cr17Ni7 / 1Cr17Ni7 GB/T 3280 Chinese equivalent
UNS S30100 — Unified Numbering System

Applications

JIS G4305 SUS301 is widely used where high strength after cold working is required. Typical applications include:

Application Area Typical Components / Uses (Keywords)
Springs & Fasteners Springs, clips, fasteners – 301 Spring
Railway & Transportation Railway cars, structural components – 301 Railway
Automotive Structural parts, trim – 301 Automotive
Architectural & Construction Structural panels, supports – 301 Construction
Industrial Equipment High-strength formed parts – 301 Industrial
General Fabrication Cold-worked components – 301 Fabrication

Why Choose SHH STEEL

SHH STEEL provides SUS301 as Mill Direct Supply. We maintain long-term strategic cooperation with major Chinese stainless steel mills and act as a first-level agent. This direct mill supply model allows us to offer competitive mill-direct pricing, faster delivery times, consistent quality, and full Mill Test Certificates for JIS G4305 SUS301 Steel Plate.

Customers benefit from reliable supply, short lead times and cost-effective solutions for high work-hardening austenitic stainless steel projects. Our professional export team provides technical support on temper selection, material properties and processing.

FAQ

What is the main difference between SUS301 and SUS304?
SUS301 has higher carbon and lower nickel content, resulting in a much higher work-hardening rate. It can achieve significantly higher strength through cold working compared with SUS304.
Is SUS301 magnetic?
In the annealed condition it is generally non-magnetic. After cold working it becomes slightly magnetic.
What tempers are available for SUS301?
Annealed, ¼ Hard, ½ Hard, ¾ Hard and Full Hard tempers are commonly available.

Conclusion

JIS G4305 SUS301 Steel Plate (301 Stainless Steel) from SHH STEEL is a high work-hardening austenitic stainless steel offering excellent strength after cold working, good corrosion resistance and formability. As Mill Direct Supply, we provide competitive pricing, consistent quality and full technical support. Trust SHH STEEL for your SUS301 stainless steel requirements.

Contact SHH STEEL today for stock availability, pricing and technical support. JIS G4305 SUS301 Steel Plate, SUS301, 301 stainless steel, 301 stainless steel plate, SUS301 supplier

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X