JIS G4305 SUS304 Steel Plate | 304 Stainless Steel - SHH STEEL

JIS G4305 SUS304 Steel Plate | 304 Stainless Steel

JIS G4305 SUS304 is the most widely used austenitic stainless steel plate/sheet, offering excellent corrosion resistance, outstanding formability and good weldability. SHH STEEL supplies SUS304 as Mill Direct Supply with competitive pricing and full mill certification.
Equivalent Grades:
ASTM A240 304 (S30400) / GB/T 3280 06Cr19Ni10 (0Cr18Ni9) / EN 10088-2 X5CrNi18-10 (1.4301)
Surface:
2B, 2D, BA, No.4, HL, 8K Mirror, Hairline
Product form:
Plate, Sheet, Coil, Strip, Foil, Shim, Circle, Ring
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Surface Finishes
Delivery Conditions
Key Characteristics
Equivalent Material Grades
Applications
Why Choose SHH STEEL
FAQ
Conclusion

What is JIS G4305 SUS304 Steel Plate?

As a professional stainless steel supplier and China Mill-Direct Exporter, SHH STEEL is pleased to present JIS G4305 SUS304 Steel Plate (also known as 304 stainless steel).

SUS304 is the most widely used austenitic stainless steel under the Japanese standard JIS G4305 for cold-rolled stainless steel plates, sheets and strips. It contains 18% chromium and 8% nickel, providing excellent corrosion resistance in a wide range of environments, outstanding formability, good weldability and attractive surface appearance. SUS304 is non-magnetic in the annealed condition and is the first choice for countless industrial, architectural, food and household applications.

SHH STEEL supplies SUS304 as Mill Direct Supply, sourcing directly from major Chinese stainless steel mills. This ensures competitive mill pricing, consistent quality, shorter lead times and full traceability. We offer thicknesses from 0.3 mm to 6.0 mm (thicker plates available on request), widths up to 1500 mm or more, in coil or cut-to-length form. All materials are delivered with full Mill Test Certificates.

Material Specification

Specification Element Requirement SHH STEEL Compliance
Primary Standard JIS G4305 Full compliance
Steel Grade SUS304 Confirmed
Product Form Cold-rolled Plate / Sheet / Coil Available
Surface Finish 2B, BA, No.4, HL, polished (common) Available
Thickness Range 0.3 mm – 6.0 mm (standard) Custom sizes available
Width Up to 1500 mm or wider Available
Certification EN 10204 3.1 / Mill Certificate Available

Chemical Composition

Chemical composition according to JIS G4305 (Heat Analysis):

Element Content (%)
Carbon (C) ≤ 0.08
Silicon (Si) ≤ 1.00
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Chromium (Cr) 18.00 – 20.00
Nickel (Ni) 8.00 – 10.50
Nitrogen (N) ≤ 0.10

Note: The classic 18-8 composition (18% Cr + 8% Ni) provides the best balance of corrosion resistance, formability and cost among austenitic stainless steels.

Mechanical Properties

Mechanical properties of JIS G4305 SUS304 (annealed condition):

Property Value
Yield Strength (0.2%) ≥ 205 MPa
Tensile Strength ≥ 520 MPa
Elongation ≥ 40%
Hardness ≤ 187 HB / ≤ 90 HRB

Density: Approximately 7.93 g/cm³ Magnetic: Non-magnetic in annealed condition; may become slightly magnetic after heavy cold working.

Surface Finishes

Finish Description Typical Applications
2B Cold-rolled, annealed, pickled, skin-passed General fabrication, industrial
BA Bright Annealed – high reflectivity Kitchen, decorative, clean rooms
No.4 Brushed finish Architectural, elevators, kitchen
HL Hairline finish Decorative panels
Polished Mirror or custom polish High-end decorative and food equipment

Delivery Conditions

SHH STEEL supplies JIS G4305 SUS304 as Mill Direct Supply in annealed condition with various surface finishes.

Additional options available:

  • Coil or cut-to-length sheets/plates
  • Protective film
  • Third-party inspection (SGS, BV, TUV, etc.)

Key Characteristics

  • Excellent corrosion resistance in a wide range of environments
  • Outstanding formability and deep-drawing capability
  • Good weldability
  • Attractive surface appearance with multiple finish options
  • Non-magnetic in annealed condition
  • Excellent toughness even at low temperatures
  • The most versatile and widely used stainless steel grade

Equivalent Material Grades

Grade Standard Notes
SUS304 JIS G4305 —
304 ASTM A240 American equivalent
1.4301 / X5CrNi18-10 EN 10088-2 European equivalent
06Cr19Ni10 GB/T 3280 Chinese equivalent
UNS S30400 — Unified Numbering System

Applications

IS G4305 SUS304 is used across almost every industry. Typical applications include:

Application Area Typical Components / Uses (Keywords)
Kitchen & Food Equipment Sinks, countertops, cookware, food machinery – 304 Kitchen
Architectural & Construction Cladding, elevators, handrails, panels – 304 Architectural
Chemical & Pharmaceutical Tanks, pipes, equipment – 304 Chemical
Automotive & Transportation Trim, exhaust components, structural parts – 304 Automotive
Home Appliances Washing machines, refrigerators, panels – 304 Appliances
General Fabrication Tanks, vessels, formed parts – 304 Fabrication

Why Choose SHH STEEL

SHH STEEL provides SUS304 as Mill Direct Supply. We maintain long-term strategic cooperation with major Chinese stainless steel mills and act as a first-level agent. This direct mill supply model allows us to offer competitive mill-direct pricing, faster delivery times, consistent quality, and full Mill Test Certificates for JIS G4305 SUS304 Steel Plate.

Customers benefit from reliable supply, short lead times and cost-effective solutions for the world’s most popular stainless steel grade. Our professional export team provides technical support on surface selection, processing and packaging.

FAQ

What is the difference between SUS304 and SUS304L?
SUS304L has lower carbon content (≤0.030%), which provides better resistance to intergranular corrosion after welding. SUS304 is suitable for most general applications, while 304L is preferred for heavy welded structures.
Is SUS304 magnetic?
Is SUS304 magnetic?
What is the most common surface finish for SUS304?
2B is the most widely used industrial finish. BA and No.4 are very popular for decorative and kitchen applications.

Conclusion

JIS G4305 SUS304 Steel Plate (304 Stainless Steel) from SHH STEEL is the most versatile austenitic stainless steel, offering excellent corrosion resistance, outstanding formability and good weldability. As Mill Direct Supply, we provide competitive pricing, consistent quality and full technical support. Trust SHH STEEL for your SUS304 stainless steel requirements.

Contact SHH STEEL today for stock availability, pricing and technical support. JIS G4305 SUS304 Steel Plate, SUS304, 304 stainless steel, 304 stainless steel plate, SUS304 supplier

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X