ISO 4957 Carbon Steel Plates
SHH STEEL offers ISO 4957-compliant non-alloy and alloy tool steels. ISO 4957 specifies grades for cold/hot work and plastic molds with defined hardness and toughness requirements. Global standard, certified quality, competitive prices, customizable. Trust SHH STEEL!
-
ISO 4957 70MnMoCr8 Tool Steel Plate
ISO 4957 70MnMoCr8 is a manganese-molybdenum-chromium cold-work tool steel for cold punches, die inserts and tooling blanks. Its carbon range is 0.65–0.75 %, with the delivery condition and alloy balance defining the appropriate tooling route. Plate and flat blanks are selected by chemistry, surface quality, machining allowance and the actual section rather than by an unqualified foreign-grade nickname. Finished tooling still requires a qualified treatment and inspection basis. SHH STEEL produces and exports 70MnMoCr8 plate to the specified edition, dimensions and inspection requirements.View More -
ISO 4957 60WCrV8 Tool Steel Plate
ISO 4957 60WCrV8 is a tungsten-chromium-vanadium cold-work tool steel for wear-loaded punches, chisels and supported cold-tool inserts. Its carbon range is 0.55–0.65 %, with the delivery condition and alloy balance defining the appropriate tooling route. Plate and flat blanks are selected by chemistry, surface quality, machining allowance and the actual section rather than by an unqualified foreign-grade nickname. Finished tooling still requires a qualified treatment and inspection basis. SHH STEEL produces and exports 60WCrV8 plate to the specified edition, dimensions and inspection requirements.View More -
ISO 4957 21MnCr5 Tool Steel Plate
ISO 4957 21MnCr5 is a low-carbon manganese-chromium carburizing tool steel for case-hardened tool components and cold-tool blanks. Its carbon range is 0.18–0.24 %, with the delivery condition and alloy balance defining the appropriate tooling route. Plate and flat blanks are selected by chemistry, surface quality, machining allowance and the actual section rather than by an unqualified foreign-grade nickname. Finished tooling still requires a qualified treatment and inspection basis. SHH STEEL produces and exports 21MnCr5 plate to the specified edition, dimensions and inspection requirements.View More -
ISO 4957 102Cr6 Tool Steel Plate
ISO 4957 102Cr6 is a high-carbon chromium cold-work tool steel for cold-tool blanks, gauges and precision cutting inserts. Its carbon range is 0.95–1.10 %, with the delivery condition and alloy balance defining the appropriate tooling route. Plate and flat blanks are selected by chemistry, surface quality, machining allowance and the actual section rather than by an unqualified foreign-grade nickname. Finished tooling still requires a qualified treatment and inspection basis. SHH STEEL produces and exports 102Cr6 plate to the specified edition, dimensions and inspection requirements.View More -
ISO 4957 C90U Tool Steel Plate
ISO 4957 C90U is a non-alloy high-carbon cold-work tool steel for cold dies, gauges and cutting-tool blanks. Its carbon range is 0.85–0.95 %, with the delivery condition and alloy balance defining the appropriate tooling route. Plate and flat blanks are selected by chemistry, surface quality, machining allowance and the actual section rather than by an unqualified foreign-grade nickname. Finished tooling still requires a qualified treatment and inspection basis. SHH STEEL produces and exports C90U plate to the specified edition, dimensions and inspection requirements.View More -
ISO 4957 C80U Tool Steel Plate
ISO 4957 C80U is a non-alloy carbon cold-work tool steel for cold punches, small cutters and tool blanks. Its carbon range is 0.75–0.85 %, with the delivery condition and alloy balance defining the appropriate tooling route. Plate and flat blanks are selected by chemistry, surface quality, machining allowance and the actual section rather than by an unqualified foreign-grade nickname. Finished tooling still requires a qualified treatment and inspection basis. SHH STEEL produces and exports C80U plate to the specified edition, dimensions and inspection requirements.View More -
ISO 4957 C70U Tool Steel Plate
ISO 4957 C70U is a non-alloy carbon cold-work tool steel for cold-tool blanks, punches and supported cutting tools. Its carbon range is 0.65–0.75 %, with the delivery condition and alloy balance defining the appropriate tooling route. Plate and flat blanks are selected by chemistry, surface quality, machining allowance and the actual section rather than by an unqualified foreign-grade nickname. Finished tooling still requires a qualified treatment and inspection basis. SHH STEEL produces and exports C70U plate to the specified edition, dimensions and inspection requirements.View More -
ISO 4957 C45U Tool Steel Plate
ISO 4957 C45U is a non-alloy medium-carbon cold-work tool steel for general-purpose tool blanks, fixtures and tooling supports. Its carbon range is 0.42–0.50 %, with the delivery condition and alloy balance defining the appropriate tooling route. Plate and flat blanks are selected by chemistry, surface quality, machining allowance and the actual section rather than by an unqualified foreign-grade nickname. Finished tooling still requires a qualified treatment and inspection basis. SHH STEEL produces and exports C45U plate to the specified edition, dimensions and inspection requirements.View More -
ISO 4957 C120U Tool Steel Plate
ISO 4957 C120U is a non-alloy very-high-carbon cold-work tool steel for wear-loaded cutting tools and supported tool edges. Its carbon range is 1.15–1.25 %, with the delivery condition and alloy balance defining the appropriate tooling route. Plate and flat blanks are selected by chemistry, surface quality, machining allowance and the actual section rather than by an unqualified foreign-grade nickname. Finished tooling still requires a qualified treatment and inspection basis. SHH STEEL produces and exports C120U plate to the specified edition, dimensions and inspection requirements.View More -
ISO 4957 C105U Tool Steel Plate
ISO 4957 C105U is a non-alloy high-carbon cold-work tool steel for fine-edge cutters, gauges and cold-tool blanks. Its carbon range is 1.00–1.10 %, with the delivery condition and alloy balance defining the appropriate tooling route. Plate and flat blanks are selected by chemistry, surface quality, machining allowance and the actual section rather than by an unqualified foreign-grade nickname. Finished tooling still requires a qualified treatment and inspection basis. SHH STEEL produces and exports C105U plate to the specified edition, dimensions and inspection requirements.View More -
ISO 4957 50WCrV8 Tool Steel Plate
ISO 4957 50WCrV8 is a tungsten-chromium-vanadium cold-work tool steel for impact-loaded punches, chisels and cold-tool inserts. Its carbon range is 0.45–0.55 %, with the delivery condition and alloy balance defining the appropriate tooling route. Plate and flat blanks are selected by chemistry, surface quality, machining allowance and the actual section rather than by an unqualified foreign-grade nickname. Finished tooling still requires a qualified treatment and inspection basis. SHH STEEL produces and exports 50WCrV8 plate to the specified edition, dimensions and inspection requirements.View More -
ISO 4957 105V Tool Steel Plate
ISO 4957 105V is a vanadium-alloyed cold-work tool steel for cold punches, fine-edge tools and precision tool blanks. Its carbon range is 1.00–1.10 %, with the delivery condition and alloy balance defining the appropriate tooling route. Plate and flat blanks are selected by chemistry, surface quality, machining allowance and the actual section rather than by an unqualified foreign-grade nickname. Finished tooling still requires a qualified treatment and inspection basis. SHH STEEL produces and exports 105V plate to the specified edition, dimensions and inspection requirements.View More
ISO 4957 Carbon Steel Plates
Tool and Die Steel Plates
SHH STEEL, a leading Tool and Die Steel Plates exporter, produces and exports tool and die steel plates for mold-making, tooling, and automotive applications. Our plates, such as D2 and P20, ensure durability and machinability, meeting global standards. With a 5,000-ton inventory, we provide 3–5 day delivery for in-stock items, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for tool steel plates and custom precision manufacturing solutions.