ISO 4957 X40Cr14 Tool Steel Plate | ISO 4957 Tool Steel - SHH STEEL

ISO 4957 X40Cr14 Tool Steel Plate

ISO 4957 X40Cr14 is a high-chromium cold-work tool steel for mould-related inserts and machined tooling blanks. Its carbon range is 0.36–0.42 %, with the delivery condition and alloy balance defining the appropriate tooling route. Plate and flat blanks are selected by chemistry, surface quality, machining allowance and the actual section rather than by an unqualified foreign-grade nickname. Finished tooling still requires a qualified treatment and inspection basis. SHH STEEL produces and exports X40Cr14 plate to the specified edition, dimensions and inspection requirements.
Equivalent Grades:
Foreign grades require review; substitution requires review.
Heat Treatment
Annealed; alternative delivery condition by agreement.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is ISO 4957 X40Cr14 plate?

ISO 4957 X40Cr14 Tool Steel Plate is a high-chromium cold-work tool steel, associated with steel number 1.2083 in informative Annex C of ISO 4957:1999. Chromium 12.50–14.50 % accompanies an annealed maximum and a separate oil-quenched specimen test; note h mentions an alternative delivery condition.

The numerical basis here is the finalized 1999 edition. Its broad wrought-product scope includes hot-rolled, forged, cold-drawn and cold-rolled products and permits powder metallurgy; plate and flat enquiries must identify the actual form and finish. This dated reference is not a statement that a later edition has identical requirements.

Chromium content alone does not establish corrosion performance, polishability or final tool hardness; clarify the alternative condition before ordering.

SHH STEEL produces and exports X40Cr14 plate against the agreed specification and inspection basis. The standard hub is ISO 4957 within Tool and Die Steel Plates.

Material specification for X40Cr14

Parameter Reference / scope
Standard / symbol ISO 4957:1999; X40Cr14
Steel number 1.2083; informative Annex C, EN 10027-2:1992 designation
Family Alloy cold-work tool steel
Product form Broad wrought-product scope; state plate/flat, manufacture, dimensions and finish
Delivery condition Annealed (+A) unless otherwise specified
Condition hardness 241 HB maximum when supplied annealed (+A), Table 4
Hardening-test minimum 52 HRC on the prescribed test basis; not as-delivered plate HRC
Dimensions Agreement under clause 4.4; flat-bar references not automatic plate tolerances
Inspection Agreed document and test scope; ISO 10474 references as cited by the 1999 edition

Cast-analysis composition of X40Cr14

Table 4 values below are cast-analysis requirements, mass percent. They are not product-analysis limits with an arbitrary extra allowance already included.

Element Cast-analysis requirement (wt. %)
Carbon (C) 0.36–0.42
Silicon (Si) 1.00 max
Manganese (Mn) 1.00 max
Phosphorus (P) 0.030 max
Sulfur (S) 0.030 max
Chromium (Cr) 12.50–14.50

For product analysis use the applicable Table 5 deviations and sampling conditions. Elements not quoted must not be intentionally added without purchaser agreement except to finish the heat; precautions against additions from scrap/materials are required. A dash is not a zero-residual guarantee.

Table 5 product-analysis deviations are a separate acceptance basis, not a relaxation of the cast-analysis windows above.

Element Permissible product-analysis deviation (wt. %)
Carbon (C) ±0.03
Silicon (Si) ±0.05
Manganese (Mn) ±0.04
Chromium (Cr) ±0.15
Phosphorus (P) +0.005
Sulfur (S) +0.005

Table 5 direction/sampling note allows deviation either above or below the range, but not both for the same element from different sample products of the same cast. Maxima-only deviations are positive only. Values require ISO 14284 samples representing the average composition of the product cross-section.

Where only a cast-analysis maximum is specified, the product-analysis deviation is positive only under the table note; do not create a negative lower-bound requirement from the printed ± entries for silicon, manganese or the maximum-only nickel entry.

Delivery hardness and hardening-test response for X40Cr14

241 HB maximum when supplied annealed (+A), Table 4. The condition-specific Brinell maximum is different from the minimum HRC after the reference hardening test.

Property / regime Value / meaning
Delivery-condition Brinell basis 241 HB maximum when supplied annealed (+A), Table 4
Hardening-test minimum 52 HRC after the stipulated test treatment
Cold-drawn stock The applicable table note permits annealed plus cold-drawn (+A+C) hardness up to 20 HB higher than annealed (+A); do not transfer this allowance to annealed plate or an untreated C45U basis
Final tool hardness Specified separately for the real section and production treatment

Table 1 note c adds the minimum-hardness hardening-test requirements. Supplementary verification is defined by normative Annex B.3, with Annex B.1 requiring supplementary/special items to be specified at enquiry and order. These numerical minima are not an informative tempering-curve estimate or a blanket finished-tool guarantee.

The approximately 300 HB alternative in note h is not the annealed maximum or the minimum HRC specimen response. Specify the exact alternative treatment and acceptance if required.

Delivery condition and test treatment for X40Cr14

Specify Annealed (+A) unless otherwise specified. Clause 4.1.2.1 gives annealed delivery unless otherwise specified. A separate production heat treatment must be qualified for the actual tool.

Table 4 / Annex B.3 hardening-test item Reference
Hardening temperature 1010 °C (±10 °C)
Quench medium Oil
Tempering temperature 180 °C (±10 °C)
Minimum test hardness 52 HRC
Salt-bath total heating, Table B.1 25 ± 1 min for hardening; 60 min for tempering
Other heating methods Extend the heating time accordingly; no universal production holding time assigned

B.3 requires the Figure 1 test-piece location, conditions avoiding decarburization, and hardness measurement on the prepared cut surface to ISO 6508. Untreated samples may be annealed before the test at the manufacturer’s discretion. No preheat temperature is specified by these rows, so none is inferred. These are specimen-test conditions, not guaranteed production recipes for every plate section. Annex A hardness-tempering curves are informative guidance, not identical acceptance limits.

Table 4 note h also mentions an alternative condition at approximately 300 HB, using the wording “pre-heated”. Confirm the intended delivery treatment and acceptance in the order; this wording is not used to invent a heat-treatment recipe or replace the annealed 241 HB maximum.

Welding, cutting and finishing X40Cr14

X40Cr14 tool steel requires a qualified repair-welding procedure matched to chemistry, supplied condition, restraint and final treatment; it is not a generic readily weldable fabrication plate. No unsourced welding temperature is prescribed.

Thermal cutting, EDM and grinding can change the surface layer and introduce damage. Review cleanup allowance, inspect critical edges and avoid representing an unaffected core analysis as proof of sound tool surfaces. Chromium content alone does not establish corrosion performance, polishability or final tool hardness; clarify the alternative condition before ordering.

Plate/flat dimensions and surface acceptance

Clause 4.4 requires shape, dimensions and tolerances agreed at enquiry and order, preferably using corresponding international or suitable national standards. ISO 1035-1/-3/-4 are cited for rolled round and flat bars; their bar tolerances must not simply be relabelled as plate tolerances. No invented plate capacity range, thickness deviation or flatness number is supplied here.

Clause 4.3 requires a workmanlike surface. Ground, polished or finished-machined products are to be free of surface imperfections and surface decarburization. Hot-rolled, forged, cold-drawn or rough-machined stock requires sufficient cleanup material; machining allowance is agreed under the 1999 provisions. Do not transfer round-product hardenability or surface limits to plate without the appropriate basis.

Applications and selection limits for X40Cr14

Qualitative engineering applications for X40Cr14 include mould-related inserts and machined tooling blanks. Chromium 12.50–14.50 % accompanies an annealed maximum and a separate oil-quenched specimen test; note h mentions an alternative delivery condition. The actual finished tool, duty and edge support must be reviewed rather than assumed from a grade nickname.

Chromium content alone does not establish corrosion performance, polishability or final tool hardness; clarify the alternative condition before ordering.

The standard’s condition hardness and hardening-test response do not provide a numerical impact property, corrosion rating or guaranteed tool life. High carbon or alloy content alone is not a substitute for a drawing and final acceptance requirements.

Compare X40Cr14 with three published own plates

These own product pages are already live. The following comparisons are material-selection contrasts, not automatic substitution approvals.

Material Family / chemistry Condition Property basis Substitution limit
X40Cr14 (this plate) high-chromium cold-work tool steel 241 HB maximum when supplied annealed (+A), Table 4 Minimum specimen-test 52 HRC, not as-delivered plate hardness Condition/form/test basis must match
JIS G4401 SK105 Tool Steel Plate Carbon tool steel; published C 1.00–1.10 % JIS G4401:2009 plate/strip condition basis; as-hot-rolled unless otherwise specified Not the ISO 4957:1999 Table 4 specimen-test acceptance Compare actual carbon, Si/Mn limits, condition and plate rules
JIS G4401 SK120 Tool Steel Plate Carbon tool steel; published C 1.15–1.25 % JIS G4401:2009 plate/strip condition basis; as-hot-rolled unless otherwise specified Not the ISO 4957:1999 Table 4 specimen-test acceptance Compare actual carbon, Si/Mn limits, condition and plate rules
ASTM A829 4140 Alloy Steel Plate Engineering Cr-Mo plate; separate chemistry-ordered specification Ordered condition on the own live page Chemistry-ordered engineering plate, not this tool-test acceptance Not a direct tool-grade substitute

Country comparisons and substitution limits for X40Cr14

The country comparison uses actual cited editions, not an unrestricted trade-name list. The steel number is the informative Annex C designation association, not proof that foreign delivery and test requirements are identical.

System Grade / number Actual chemistry / form difference Condition / substitution limit
ISO / international X40Cr14 Cast-analysis Table 4; this grade and edition Delivery condition, specimen response and plate/flat requirements must be specified
Europe / designation number 1.2083 Informative Annex C associates the EN 10027-2:1992 number; it is not an independently verified later DIN specification No automatic national-edition or product-condition certification inferred
United States ASTM A681-08 P20 — contrast only ASTM Cr 1.40–2.00 versus ISO Cr 12.50–14.50; ASTM C 0.28–0.40 versus ISO C 0.36–0.42. A shared mould-related application does not establish an A681 counterpart, corrosion rating or equivalent delivery condition.

Where printed, ISO hardening-test HRC is a genuine specimen-response basis, not supplied-condition hardness; no missing minimum is inferred. It must not be confused with JIS G4404 practical-decarburization HV criteria, JIS plate delivery hardness or an informative tempering curve. Verify the complete foreign standard, form and ordered condition before substitution.

Why choose SHH STEEL for X40Cr14

SHH STEEL produces and exports X40Cr14 plate against the stated standard, supplied condition and agreed inspection plan. We keep cast analysis, delivery hardness and final tooling acceptance distinct.

  • Confirm the required edition and correct material designation.
  • Use plate/flat tolerances and cleanup allowance appropriate to the actual form.
  • Agree supplementary verification and required reports before acceptance.
  • Maintain heat identification and review any proposed foreign substitution.

Enquiry and inspection planning for X40Cr14

Enquiry item What to specify
Grade / edition X40Cr14; ISO edition and any associated drawing requirement
Form / dimensions Plate or flat, thickness × width × length, quantity, finish and machining allowance
Condition Annealed (+A) unless otherwise specified
Hardness basis 241 HB maximum when supplied annealed (+A), Table 4
Verification State whether Annex B.3 hardening verification, product analysis or other supplementary tests are required
Final tooling Actual tool duty, final property acceptance and production-treatment responsibility
Reports / logistics Inspection-document type, heat traceability, packing, destination and target timing

Dimensions, manufacturing route and any additional NDT or quality requirement are reviewed for feasibility. This page is not an unconditional stock, capacity or finished-tool performance commitment.

FAQ

What distinguishes X40Cr14?
Chromium 12.50–14.50 % accompanies an annealed maximum and a separate oil-quenched specimen test; note h mentions an alternative delivery condition. Chromium content alone does not establish corrosion performance, polishability or final tool hardness; clarify the alternative condition before ordering.
Does the HRC value describe supplied plate?
No. The reference hardening test gives 52 HRC minimum on its stipulated specimen basis. The delivery-condition entry is 241 HB maximum when supplied annealed (+A), Table 4. Final tool properties require a separate qualified basis.
Are these temperatures a production heat-treatment guarantee?
No. The table/B.3 regime is a specimen test. Table 1 note c provides the minimum-response requirement, while Annex B.1 makes supplementary verification an enquiry/order item. Annex A curves are informative; actual tool treatment depends on section and application.
Can round hardenability or bar tolerances be used directly for plate?
No. Follow the actual product-form agreement under clause 4.4 and Figure 1 sample rules. Any Table 2 round-diameter hardenability statements are not plate-thickness guarantees.
Is the foreign grade or steel number an automatic equivalent?
No. Use the explicit country-table differences, complete source edition, actual form, delivery condition and test acceptance. Historical JIS names and informative steel-number associations do not establish unconditional substitution.

Request a quotation

Request a quotation for ISO 4957 X40Cr14 tool steel plate or flat stock. Send the required edition, quantity, dimensions, finish, machining allowance and drawing. State the supplied condition explicitly: Annealed (+A) unless otherwise specified. Identify the intended tooling duty and whether dimensions describe raw blanks or finished pieces.

Include the delivery-hardness acceptance, required inspection document and heat-traceability needs. Specify any supplementary product analysis, Annex B.3 hardening-test verification, surface/decarburization evaluation or additional NDT, with the agreed method and acceptance criteria. Do not treat a specimen-response HRC or round-diameter hardenability note as an arbitrary-section plate guarantee.

Provide the final tool properties and production-treatment responsibility separately. For a proposed foreign grade, attach its governing specification and drawing so chemistry, form and condition differences can be reviewed. Include cutting details, edge preparation, inspection stages, destination, packing and target timing; requested processes and dimensions are reviewed for feasibility before confirmation.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X