ISO 4957 35CrMo7 Tool Steel Plate | ISO 4957 Tool Steel - SHH STEEL

ISO 4957 35CrMo7 Tool Steel Plate

ISO 4957 35CrMo7 is a chromium-molybdenum cold-work tool steel for machined mould-related tooling and support inserts. Its carbon range is 0.30–0.40 %, with the delivery condition and alloy balance defining the appropriate tooling route. Plate and flat blanks are selected by chemistry, surface quality, machining allowance and the actual section rather than by an unqualified foreign-grade nickname. Finished tooling still requires a qualified treatment and inspection basis. SHH STEEL produces and exports 35CrMo7 plate to the specified edition, dimensions and inspection requirements.
Equivalent Grades:
P20 contrast; substitution requires review.
Heat Treatment
Quenched and tempered.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is ISO 4957 35CrMo7 plate?

ISO 4957 35CrMo7 Tool Steel Plate is a chromium-molybdenum cold-work tool steel, associated with steel number 1.2302 in informative Annex C of ISO 4957:1999. Table 4 note f describes usual quenched-and-tempered supply at approximately 300 HB rather than a numerical annealed maximum or ordinary hardening-test cycle.

The numerical basis here is the finalized 1999 edition. Its broad wrought-product scope includes hot-rolled, forged, cold-drawn and cold-rolled products and permits powder metallurgy; plate and flat enquiries must identify the actual form and finish. This dated reference is not a statement that a later edition has identical requirements.

The approximate usual-condition hardness is not a guaranteed acceptance band; agree the supplied condition and measured acceptance before machining.

SHH STEEL produces and exports 35CrMo7 plate against the agreed specification and inspection basis. The standard hub is ISO 4957 within Tool and Die Steel Plates.

Material specification for 35CrMo7

Parameter Reference / scope
Standard / symbol ISO 4957:1999; 35CrMo7
Steel number 1.2302; informative Annex C, EN 10027-2:1992 designation
Family Alloy cold-work tool steel
Product form Broad wrought-product scope; state plate/flat, manufacture, dimensions and finish
Delivery condition Quenched and tempered normally; agree delivery acceptance (Table 4 note f)
Condition hardness Approximately 300 HB in usual quenched-and-tempered supply, Table 4 note f; no annealed maximum printed
Response / usual condition No ordinary numerical hardening-test cycle or HRC minimum printed; Table 4 note f describes usual QT supply
Dimensions Agreement under clause 4.4; flat-bar references not automatic plate tolerances
Inspection Agreed document and test scope; ISO 10474 references as cited by the 1999 edition

Cast-analysis composition of 35CrMo7

Table 4 values below are cast-analysis requirements, mass percent. They are not product-analysis limits with an arbitrary extra allowance already included.

Element Cast-analysis requirement (wt. %)
Carbon (C) 0.30–0.40
Silicon (Si) 0.30–0.70
Manganese (Mn) 0.60–1.00
Phosphorus (P) 0.030 max
Sulfur (S) 0.030 max
Chromium (Cr) 1.50–2.00
Molybdenum (Mo) 0.35–0.55

For product analysis use the applicable Table 5 deviations and sampling conditions. Elements not quoted must not be intentionally added without purchaser agreement except to finish the heat; precautions against additions from scrap/materials are required. A dash is not a zero-residual guarantee.

Table 5 product-analysis deviations are a separate acceptance basis, not a relaxation of the cast-analysis windows above.

Element Permissible product-analysis deviation (wt. %)
Carbon (C) ±0.03
Silicon (Si) ±0.03
Manganese (Mn) ±0.04
Chromium (Cr) ±0.07
Molybdenum (Mo) ±0.05
Phosphorus (P) +0.005
Sulfur (S) +0.005

Table 5 direction/sampling note allows deviation either above or below the range, but not both for the same element from different sample products of the same cast. Maxima-only deviations are positive only. Values require ISO 14284 samples representing the average composition of the product cross-section.

Delivery hardness and hardening-test response for 35CrMo7

Approximately 300 HB in usual quenched-and-tempered supply, Table 4 note f; no annealed maximum printed. This is approximate usual-condition information, not an annealed maximum, a guaranteed hardness range or a minimum specimen-response HRC.

Table 4 uses footnote f in place of a numerical annealed maximum and ordinary hardening-test treatment/response. No hardening temperature, quench medium, tempering temperature, preheat or HRC minimum is inferred from a neighboring row.

Table 1 note c and normative Annex B.3 verification selected under Annex B.1 do not create missing grade-specific numerical criteria. Agree the applicable source and order acceptance. Annex A curves are informative. The cold-drawn allowance does not create an unprinted annealed maximum or add a margin to the approximate quenched-and-tempered value.

Delivery condition and test treatment for 35CrMo7

Quenched and tempered normally; agree delivery acceptance (Table 4 note f). Clause 4.1.2.1 specifically excepts this grade from the ordinary annealed default.

Table 4 note f states that the steel is normally supplied quenched and tempered at approximately 300 HB. Agree an actual acceptance basis rather than treating this approximate description as a maximum, minimum or guaranteed band.

No numerical reference cycle or HRC minimum is printed for this row. Annex B.3 and general Table B.1 specimen heating do not supply the absent grade-specific cycle. Do not copy a cycle from a foreign alias or another ISO row. Annex A is informative; these source provisions are not guaranteed production recipes for arbitrary plate sections.

Welding, cutting and finishing 35CrMo7

35CrMo7 tool steel requires a qualified repair-welding procedure matched to chemistry, supplied condition, restraint and final treatment; it is not a generic readily weldable fabrication plate. No unsourced welding temperature is prescribed.

Thermal cutting, EDM and grinding can change the surface layer and introduce damage. Review cleanup allowance, inspect critical edges and avoid representing an unaffected core analysis as proof of sound tool surfaces. The approximate usual-condition hardness is not a guaranteed acceptance band; agree the supplied condition and measured acceptance before machining.

Plate/flat dimensions and surface acceptance

Clause 4.4 requires shape, dimensions and tolerances agreed at enquiry and order, preferably using corresponding international or suitable national standards. ISO 1035-1/-3/-4 are cited for rolled round and flat bars; their bar tolerances must not simply be relabelled as plate tolerances. No invented plate capacity range, thickness deviation or flatness number is supplied here.

Clause 4.3 requires a workmanlike surface. Ground, polished or finished-machined products are to be free of surface imperfections and surface decarburization. Hot-rolled, forged, cold-drawn or rough-machined stock requires sufficient cleanup material; machining allowance is agreed under the 1999 provisions. Do not transfer round-product hardenability or surface limits to plate without the appropriate basis.

Applications and selection limits for 35CrMo7

Qualitative engineering applications for 35CrMo7 include machined mould-related tooling and support inserts. Table 4 note f describes usual quenched-and-tempered supply at approximately 300 HB rather than a numerical annealed maximum or ordinary hardening-test cycle. The actual finished tool, duty and edge support must be reviewed rather than assumed from a grade nickname.

The approximate usual-condition hardness is not a guaranteed acceptance band; agree the supplied condition and measured acceptance before machining.

The standard’s condition hardness and hardening-test response do not provide a numerical impact property, corrosion rating or guaranteed tool life. High carbon or alloy content alone is not a substitute for a drawing and final acceptance requirements.

Compare 35CrMo7 with three published own plates

These own product pages are already live. The following comparisons are material-selection contrasts, not automatic substitution approvals.

Material Family / chemistry Condition Property basis Substitution limit
35CrMo7 (this plate) chromium-molybdenum cold-work tool steel Approximately 300 HB in usual quenched-and-tempered supply, Table 4 note f; no annealed maximum printed No ordinary numerical hardening-test cycle or HRC minimum printed; Table 4 note f describes usual QT supply Condition/form/test basis must match
JIS G4401 SK105 Tool Steel Plate Carbon tool steel; published C 1.00–1.10 % JIS G4401:2009 plate/strip condition basis; as-hot-rolled unless otherwise specified Not the ISO 4957:1999 Table 4 specimen-test acceptance Compare actual carbon, Si/Mn limits, condition and plate rules
JIS G4401 SK120 Tool Steel Plate Carbon tool steel; published C 1.15–1.25 % JIS G4401:2009 plate/strip condition basis; as-hot-rolled unless otherwise specified Not the ISO 4957:1999 Table 4 specimen-test acceptance Compare actual carbon, Si/Mn limits, condition and plate rules
ASTM A829 4140 Alloy Steel Plate Engineering Cr-Mo plate; separate chemistry-ordered specification Ordered condition on the own live page Chemistry-ordered engineering plate, not this tool-test acceptance Not a direct tool-grade substitute

Country comparisons and substitution limi

The country comparison uses actual cited editions, not an unrestricted trade-name list. The steel number is the informative Annex C designation association, not proof that foreign delivery and test requirements are identical.

System Grade / number Actual chemistry / form difference Condition / substitution limit
ISO / international 35CrMo7 Cast-analysis Table 4; this grade and edition Delivery condition, specimen response and plate/flat requirements must be specified
Europe / designation number 1.2302 Informative Annex C associates the EN 10027-2:1992 number; it is not an independently verified later DIN specification No automatic national-edition or product-condition certification inferred
United States ASTM A681-08 P20 ASTM C 0.28–0.40, Si 0.20–0.80, Cr 1.40–2.00 and Mo 0.30–0.55 versus ISO C 0.30–0.40, Si 0.30–0.70, Cr 1.50–2.00 and Mo 0.35–0.55. Mould-related tool contrast only; overlap is not full acceptance or equivalent delivery hardness.

Where printed, ISO hardening-test HRC is a genuine specimen-response basis, not supplied-condition hardness; no missing minimum is inferred. It must not be confused with JIS G4404 practical-decarburization HV criteria, JIS plate delivery hardness or an informative tempering curve. Verify the complete foreign standard, form and ordered condition before substitution.

Why choose SHH STEEL for 35CrMo7

SHH STEEL produces and exports 35CrMo7 plate against the stated standard, supplied condition and agreed inspection plan. We keep cast analysis, delivery hardness and final tooling acceptance distinct.

  • Confirm the required edition and correct material designation.
  • Use plate/flat tolerances and cleanup allowance appropriate to the actual form.
  • Agree supplementary verification and required reports before acceptance.
  • Maintain heat identification and review any proposed foreign substitution.

Enquiry and inspection planning for 35CrMo7

Enquiry item What to specify
Grade / edition 35CrMo7; ISO edition and any associated drawing requirement
Form / dimensions Plate or flat, thickness × width × length, quantity, finish and machining allowance
Condition Quenched and tempered normally; agree delivery acceptance (Table 4 note f)
Hardness basis Approximately 300 HB in usual quenched-and-tempered supply, Table 4 note f; no annealed maximum printed
Verification State whether Annex B.3 hardening verification, product analysis or other supplementary tests are required
Final tooling Actual tool duty, final property acceptance and production-treatment responsibility
Reports / logistics Inspection-document type, heat traceability, packing, destination and target timing

Dimensions, manufacturing route and any additional NDT or quality requirement are reviewed for feasibility. This page is not an unconditional stock, capacity or finished-tool performance commitment.

FAQ

What distinguishes 35CrMo7?
Table 4 note f describes usual quenched-and-tempered supply at approximately 300 HB rather than a numerical annealed maximum or ordinary hardening-test cycle. The approximate usual-condition hardness is not a guaranteed acceptance band; agree the supplied condition and measured acceptance before machining.
What does the usual hardness describe?
Approximately 300 HB in usual quenched-and-tempered supply, Table 4 note f; no annealed maximum printed. It is not an annealed maximum or guaranteed acceptance band. No ordinary numerical hardening-test cycle or HRC minimum is printed for this row; agree the applicable acceptance source and order.
Can a neighboring heat-treatment cycle fill the missing test row?
No. Table 4 note f describes usual quenched-and-tempered delivery, not a numerical hardening response. Agree the applicable source/order criteria; Annex B.1/B.3 verification and informative Annex A curves do not create unprinted treatment values.
Can round hardenability or bar tolerances be used directly for plate?
No. Follow the actual product-form agreement under clause 4.4 and Figure 1 sample rules. Any Table 2 round-diameter hardenability statements are not plate-thickness guarantees.
Is the foreign grade or steel number an automatic equivalent?
No. Use the explicit country-table differences, complete source edition, actual form, delivery condition and test acceptance. Historical JIS names and informative steel-number associations do not establish unconditional substitution.

Request a quotation

Request a quotation for ISO 4957 35CrMo7 tool steel plate or flat stock. Send the required edition, quantity, dimensions, finish, machining allowance and drawing. State the supplied condition explicitly: Quenched and tempered normally; agree delivery acceptance (Table 4 note f). Identify the intended tooling duty and whether dimensions describe raw blanks or finished pieces.

Include the delivery-hardness acceptance, required inspection document and heat-traceability needs. Specify any supplementary product analysis, Annex B.3 hardening-test verification, surface/decarburization evaluation or additional NDT, with the agreed method and acceptance criteria. Do not treat a specimen-response HRC or round-diameter hardenability note as an arbitrary-section plate guarantee.

Provide the final tool properties and production-treatment responsibility separately. For a proposed foreign grade, attach its governing specification and drawing so chemistry, form and condition differences can be reviewed. Include cutting details, edge preparation, inspection stages, destination, packing and target timing; requested processes and dimensions are reviewed for feasibility before confirmation.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X