Product Showcase
GOST 1435 Carbon Steel Plates
SHH STEEL offers GOST 1435-compliant non-alloy tool steels like U8/U10. GOST 1435 specifies forged and hot-rolled bars, strips and coils for hammers, chisels and files with high hardness after hardening. Traditional reliability, certified quality, competitive prices, customizable. Trust SHH STEEL!
-
GOST 1435 U12A Tool Steel Plate | U12A Carbon Tool Steel
U12A tool steel plate is supplied as high-quality (A) unalloyed (carbon) tool steel under GOST 1435-99, whose official English title is Bars, strips and reels of tool unalloyed steel. General specifications. The official grade designation is U12A (У12А). GOST 1435-99 applies to forged bars and strips and to hot-rolled, calibrated and special-surface-finish bars, strips and coils; its chemical-composition limits also apply to ingots, billets, sheet, tape, wire and other metal products. The standard product forms are bars, strips and coils; plate or flat is supplied cut from strip or by agreement, against the composition and hardness requirements of this edition. This page is written to GOST 1435-99; confirm that this is the edition on the order.View More -
GOST 1435 U12 Tool Steel Plate | U12 Carbon Tool Steel
U12 tool steel plate is supplied as quality unalloyed (carbon) tool steel under GOST 1435-99, whose official English title is Bars, strips and reels of tool unalloyed steel. General specifications. The official grade designation is U12 (У12). GOST 1435-99 applies to forged bars and strips and to hot-rolled, calibrated and special-surface-finish bars, strips and coils; its chemical-composition limits also apply to ingots, billets, sheet, tape, wire and other metal products. The standard product forms are bars, strips and coils; plate or flat is supplied cut from strip or by agreement, against the composition and hardness requirements of this edition. This page is written to GOST 1435-99; confirm that this is the edition on the order.View More -
GOST 1435 U10A Tool Steel Plate | U10A Carbon Tool Steel
U10A tool steel plate is supplied as high-quality (A) unalloyed (carbon) tool steel under GOST 1435-99, whose official English title is Bars, strips and reels of tool unalloyed steel. General specifications. The official grade designation is U10A (У10А). GOST 1435-99 applies to forged bars and strips and to hot-rolled, calibrated and special-surface-finish bars, strips and coils; its chemical-composition limits also apply to ingots, billets, sheet, tape, wire and other metal products. The standard product forms are bars, strips and coils; plate or flat is supplied cut from strip or by agreement, against the composition and hardness requirements of this edition. This page is written to GOST 1435-99; confirm that this is the edition on the order.View More -
GOST 1435 U10 Tool Steel Plate | U10 Carbon Tool Steel
U10 tool steel plate is supplied as quality unalloyed (carbon) tool steel under GOST 1435-99, whose official English title is Bars, strips and reels of tool unalloyed steel. General specifications. The official grade designation is U10 (У10). GOST 1435-99 applies to forged bars and strips and to hot-rolled, calibrated and special-surface-finish bars, strips and coils; its chemical-composition limits also apply to ingots, billets, sheet, tape, wire and other metal products. The standard product forms are bars, strips and coils; plate or flat is supplied cut from strip or by agreement, against the composition and hardness requirements of this edition. This page is written to GOST 1435-99; confirm that this is the edition on the order.View More -
GOST 1435 U9A Tool Steel Plate | U9A Carbon Tool Steel
U9A tool steel plate is supplied as high-quality (A) unalloyed (carbon) tool steel under GOST 1435-99, whose official English title is Bars, strips and reels of tool unalloyed steel. General specifications. The official grade designation is U9A (У9А). GOST 1435-99 applies to forged bars and strips and to hot-rolled, calibrated and special-surface-finish bars, strips and coils; its chemical-composition limits also apply to ingots, billets, sheet, tape, wire and other metal products. The standard product forms are bars, strips and coils; plate or flat is supplied cut from strip or by agreement, against the composition and hardness requirements of this edition. This page is written to GOST 1435-99; confirm that this is the edition on the order.View More -
GOST 1435 U9 Tool Steel Plate | U9 Carbon Tool Steel
U9 tool steel plate is supplied as quality unalloyed (carbon) tool steel under GOST 1435-99, whose official English title is Bars, strips and reels of tool unalloyed steel. General specifications. The official grade designation is U9 (У9). GOST 1435-99 applies to forged bars and strips and to hot-rolled, calibrated and special-surface-finish bars, strips and coils; its chemical-composition limits also apply to ingots, billets, sheet, tape, wire and other metal products. The standard product forms are bars, strips and coils; plate or flat is supplied cut from strip or by agreement, against the composition and hardness requirements of this edition. This page is written to GOST 1435-99; confirm that this is the edition on the order.View More -
GOST 1435 U8GA Tool Steel Plate | U8GA Carbon Tool Steel
U8GA tool steel plate is supplied as high-quality (A) unalloyed (carbon) tool steel under GOST 1435-99, whose official English title is Bars, strips and reels of tool unalloyed steel. General specifications. The official grade designation is U8GA (У8ГА). GOST 1435-99 applies to forged bars and strips and to hot-rolled, calibrated and special-surface-finish bars, strips and coils; its chemical-composition limits also apply to ingots, billets, sheet, tape, wire and other metal products. The standard product forms are bars, strips and coils; plate or flat is supplied cut from strip or by agreement, against the composition and hardness requirements of this edition. This page is written to GOST 1435-99; confirm that this is the edition on the order.View More -
GOST 1435 U8G Tool Steel Plate | U8G Carbon Tool Steel
U8G tool steel plate is supplied as quality unalloyed (carbon) tool steel under GOST 1435-99, whose official English title is Bars, strips and reels of tool unalloyed steel. General specifications. The official grade designation is U8G (У8Г). GOST 1435-99 applies to forged bars and strips and to hot-rolled, calibrated and special-surface-finish bars, strips and coils; its chemical-composition limits also apply to ingots, billets, sheet, tape, wire and other metal products. The standard product forms are bars, strips and coils; plate or flat is supplied cut from strip or by agreement, against the composition and hardness requirements of this edition. This page is written to GOST 1435-99; confirm that this is the edition on the order.View More -
GOST 1435 U8A Tool Steel Plate | U8A Carbon Tool Steel
U8A tool steel plate is supplied as high-quality (A) unalloyed (carbon) tool steel under GOST 1435-99, whose official English title is Bars, strips and reels of tool unalloyed steel. General specifications. The official grade designation is U8A (У8А). GOST 1435-99 applies to forged bars and strips and to hot-rolled, calibrated and special-surface-finish bars, strips and coils; its chemical-composition limits also apply to ingots, billets, sheet, tape, wire and other metal products. The standard product forms are bars, strips and coils; plate or flat is supplied cut from strip or by agreement, against the composition and hardness requirements of this edition. This page is written to GOST 1435-99; confirm that this is the edition on the order.View More -
GOST 1435 U8 Tool Steel Plate | U8 Carbon Tool Steel
U8 tool steel plate is supplied as quality unalloyed (carbon) tool steel under GOST 1435-99, whose official English title is Bars, strips and reels of tool unalloyed steel. General specifications. The official grade designation is U8 (У8). GOST 1435-99 applies to forged bars and strips and to hot-rolled, calibrated and special-surface-finish bars, strips and coils; its chemical-composition limits also apply to ingots, billets, sheet, tape, wire and other metal products. The standard product forms are bars, strips and coils; plate or flat is supplied cut from strip or by agreement, against the composition and hardness requirements of this edition. This page is written to GOST 1435-99; confirm that this is the edition on the order.View More -
GOST 1435 U7A Tool Steel Plate | U7A Carbon Tool Steel
U7A tool steel plate is supplied as high-quality (A) unalloyed (carbon) tool steel under GOST 1435-99, whose official English title is Bars, strips and reels of tool unalloyed steel. General specifications. The official grade designation is U7A (У7А). GOST 1435-99 applies to forged bars and strips and to hot-rolled, calibrated and special-surface-finish bars, strips and coils; its chemical-composition limits also apply to ingots, billets, sheet, tape, wire and other metal products. The standard product forms are bars, strips and coils; plate or flat is supplied cut from strip or by agreement, against the composition and hardness requirements of this edition. This page is written to GOST 1435-99; confirm that this is the edition on the order.View More -
GOST 1435 U7 Tool Steel Plate | U7 Carbon Tool Steel
U7 tool steel plate is supplied as quality unalloyed (carbon) tool steel under GOST 1435-99, whose official English title is Bars, strips and reels of tool unalloyed steel. General specifications. The official grade designation is U7 (У7). GOST 1435-99 applies to forged bars and strips and to hot-rolled, calibrated and special-surface-finish bars, strips and coils; its chemical-composition limits also apply to ingots, billets, sheet, tape, wire and other metal products. The standard product forms are bars, strips and coils; plate or flat is supplied cut from strip or by agreement, against the composition and hardness requirements of this edition. This page is written to GOST 1435-99; confirm that this is the edition on the order.View More
GOST 1435 Carbon Steel Plates
Tool and Die Steel Plates
SHH STEEL, a leading Tool and Die Steel Plates exporter, produces and exports tool and die steel plates for mold-making, tooling, and automotive applications. Our plates, such as D2 and P20, ensure durability and machinability, meeting global standards. With a 5,000-ton inventory, we provide 3–5 day delivery for in-stock items, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for tool steel plates and custom precision manufacturing solutions.
Tool and Die Steel Plates
X