ASTM A681 Carbon Steel Plates
SHH STEEL offers ASTM A681-compliant alloy tool steels like O1/D2/H13. ASTM A681 specifies carbon and alloy tool steels for cold/hot work dies, punches, and shear blades. High hardness, wear-resistant, certified quality, competitive prices, customizable. Trust SHH STEEL!
-
ASTM A681 P6 Tool Steel Plate
ASTM A681 P6 is a low-carbon nickel-chromium mould steel for carburized mould blocks and inserts. Its carbon requirement is 0.05–0.15 %, distinguishing this mould route from higher-carbon cutting-tool steels. Plate and flat blanks need a defined delivery condition, surface quality and inspection basis. The reference does not assign this type a Table 3 hardening-response HRC; final mould properties require the applicable source and order. SHH STEEL produces and exports P6 plate to the specified edition, dimensions and inspection requirements.View More -
ASTM A681 P5 Tool Steel Plate
ASTM A681 P5 is a low-carbon chromium-alloyed mould steel for carburized mould inserts and cavity stock. Its carbon requirement is 0.06–0.10 %, distinguishing this mould route from higher-carbon cutting-tool steels. Plate and flat blanks need a defined delivery condition, surface quality and inspection basis. The reference does not assign this type a Table 3 hardening-response HRC; final mould properties require the applicable source and order. SHH STEEL produces and exports P5 plate to the specified edition, dimensions and inspection requirements.View More -
ASTM A681 P4 Tool Steel Plate
ASTM A681 P4 is a low-carbon chromium-molybdenum mould steel for carburized mould cavities and tooling inserts. Its carbon requirement is 0.12 max %, distinguishing this mould route from higher-carbon cutting-tool steels. Plate and flat blanks need a defined delivery condition, surface quality and inspection basis. The reference does not assign this type a Table 3 hardening-response HRC; final mould properties require the applicable source and order. SHH STEEL produces and exports P4 plate to the specified edition, dimensions and inspection requirements.View More -
ASTM A681 P3 Tool Steel Plate
ASTM A681 P3 is a low-carbon nickel-chromium mould steel for carburized mould inserts and cavity blanks. Its carbon requirement is 0.10 max %, distinguishing this mould route from higher-carbon cutting-tool steels. Plate and flat blanks need a defined delivery condition, surface quality and inspection basis. The reference does not assign this type a Table 3 hardening-response HRC; final mould properties require the applicable source and order. SHH STEEL produces and exports P3 plate to the specified edition, dimensions and inspection requirements.View More -
ASTM A681 P21 Tool Steel Plate
ASTM A681 P21 is a nickel-aluminium-bearing mould steel for preconditioned mould inserts and blocks. Its carbon requirement is 0.18–0.22 %, distinguishing this mould route from higher-carbon cutting-tool steels. Plate and flat blanks need a defined delivery condition, surface quality and inspection basis. The reference does not assign this type a Table 3 hardening-response HRC; final mould properties require the applicable source and order. SHH STEEL produces and exports P21 plate to the specified edition, dimensions and inspection requirements.View More -
ASTM A681 P20 Tool Steel Plate
ASTM A681 P20 is a chromium-molybdenum mould steel for preconditioned mould blocks and inserts. Its carbon requirement is 0.28–0.40 %, distinguishing this mould route from higher-carbon cutting-tool steels. Plate and flat blanks need a defined delivery condition, surface quality and inspection basis. The reference does not assign this type a Table 3 hardening-response HRC; final mould properties require the applicable source and order. SHH STEEL produces and exports P20 plate to the specified edition, dimensions and inspection requirements.View More -
ASTM A681 P2 Tool Steel Plate
ASTM A681 P2 is a low-carbon chromium-molybdenum mould steel for carburized mould cavities and inserts. Its carbon requirement is 0.10 max %, distinguishing this mould route from higher-carbon cutting-tool steels. Plate and flat blanks need a defined delivery condition, surface quality and inspection basis. The reference does not assign this type a Table 3 hardening-response HRC; final mould properties require the applicable source and order. SHH STEEL produces and exports P2 plate to the specified edition, dimensions and inspection requirements.View More -
ASTM A681 L6 Tool Steel Plate
ASTM A681 L6 is a nickel-chromium special-purpose tool steel for tool inserts and short-run tooling blanks. Its carbon range is 0.65–0.75 %, with alloy limits that distinguish it from neighboring die steels. Plate and flat blanks are selected by chemistry, delivery condition, surface quality and heat-treatment response rather than by a generic tool-steel nickname. Final tooling performance also depends on section, cooling and the qualified temper. SHH STEEL produces and exports L6 plate to the specified edition, dimensions and inspection requirements.View More -
ASTM A681 L3 Tool Steel Plate
ASTM A681 L3 is a high-carbon chromium-vanadium special-purpose tool steel for short-run tools and cold-tool blanks. Its carbon range is 0.95–1.10 %, with alloy limits that distinguish it from neighboring die steels. Plate and flat blanks are selected by chemistry, delivery condition, surface quality and heat-treatment response rather than by a generic tool-steel nickname. Final tooling performance also depends on section, cooling and the qualified temper. SHH STEEL produces and exports L3 plate to the specified edition, dimensions and inspection requirements.View More -
ASTM A681 F2 Tool Steel Plate
ASTM A681 F2 is a high-carbon higher-tungsten special-purpose tool steel for short-run fine-edge cutters and tool blanks. Its carbon range is 1.20–1.40 %, with alloy limits that distinguish it from neighboring die steels. Plate and flat blanks are selected by chemistry, delivery condition, surface quality and heat-treatment response rather than by a generic tool-steel nickname. Final tooling performance also depends on section, cooling and the qualified temper. SHH STEEL produces and exports F2 plate to the specified edition, dimensions and inspection requirements.View More -
ASTM A681 F1 Tool Steel Plate
ASTM A681 F1 is a high-carbon tungsten special-purpose tool steel for short-run fine-edge cutting-tool blanks. Its carbon range is 0.95–1.25 %, with alloy limits that distinguish it from neighboring die steels. Plate and flat blanks are selected by chemistry, delivery condition, surface quality and heat-treatment response rather than by a generic tool-steel nickname. Final tooling performance also depends on section, cooling and the qualified temper. SHH STEEL produces and exports F1 plate to the specified edition, dimensions and inspection requirements.View More -
ASTM A681 S7 Tool Steel Plate
ASTM A681 S7 is a chromium-molybdenum shock-resisting tool steel for impact-loaded punches, shear tooling and cold-work inserts. Its carbon range is 0.45–0.55 %, with alloy limits that distinguish it from neighboring die steels. Plate and flat blanks are selected by chemistry, delivery condition, surface quality and heat-treatment response rather than by a generic tool-steel nickname. Final tooling performance also depends on section, cooling and the qualified temper. SHH STEEL produces and exports S7 plate to the specified edition, dimensions and inspection requirements.View More
ASTM A681 Carbon Steel Plates
Tool and Die Steel Plates
SHH STEEL, a leading Tool and Die Steel Plates exporter, produces and exports tool and die steel plates for mold-making, tooling, and automotive applications. Our plates, such as D2 and P20, ensure durability and machinability, meeting global standards. With a 5,000-ton inventory, we provide 3–5 day delivery for in-stock items, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for tool steel plates and custom precision manufacturing solutions.