ISO 4957 55NiCrMoV7 Tool Steel Plate
What is ISO 4957 55NiCrMoV7 plate?
ISO 4957 55NiCrMoV7 Tool Steel Plate is a nickel-chromium-molybdenum-vanadium hot-work tool steel, associated with steel number 1.2714 in informative Annex C of ISO 4957:1999. This is formally a Table 6 hot-work row; its minimum specimen response is qualified for smaller dimensions by note g.
The numerical basis here is the finalized 1999 edition. Its broad wrought-product scope includes hot-rolled, forged, cold-drawn and cold-rolled products and permits powder metallurgy; plate and flat enquiries must identify the actual form and finish. This dated reference is not a statement that a later edition has identical requirements.
Greater dimensions are normally supplied quenched and tempered at approximately 380 HB under note f; no numerical size boundary or through-hardness guarantee is supplied.
SHH STEEL produces and exports 55NiCrMoV7 plate against the agreed specification and inspection basis. The standard hub is ISO 4957 within Tool and Die Steel Plates.
Material specification for 55NiCrMoV7
| Parameter | Reference / scope |
|---|---|
| Standard / symbol | ISO 4957:1999; 55NiCrMoV7 |
| Steel number | 1.2714; informative Annex C, EN 10027-2:1992 designation |
| Family | Hot-work tool steel |
| Product form | Broad wrought-product scope; state plate/flat, manufacture, dimensions and finish |
| Delivery condition | Annealed or quenched-and-tempered condition as ordered; Table 6 note f governs usual greater-dimension supply |
| Condition hardness | 248 HB maximum when supplied annealed (+A), Table 6 |
| Hardening-test minimum | 42 HRC minimum on the Table 6 specimen basis, for smaller dimensions only under note g; not supplied-plate HRC |
| Dimensions | Agreement under clause 4.4; flat-bar references not automatic plate tolerances |
| Inspection | Agreed document and test scope; ISO 10474 references as cited by the 1999 edition |
Cast-analysis composition of 55NiCrMoV7
Table 6 values below are cast-analysis requirements, mass percent. They are not product-analysis limits with an arbitrary extra allowance already included.
| Element | Cast-analysis requirement (wt. %) |
|---|---|
| Carbon (C) | 0.50–0.60 |
| Silicon (Si) | 0.10–0.40 |
| Manganese (Mn) | 0.60–0.90 |
| Phosphorus (P) | 0.030 max |
| Sulfur (S) | 0.030 max |
| Chromium (Cr) | 0.80–1.20 |
| Molybdenum (Mo) | 0.35–0.55 |
| Vanadium (V) | 0.05–0.15 |
| Nickel (Ni) | 1.50–1.80 |
For product analysis use the applicable Table 7 deviations and sampling conditions. Elements not quoted must not be intentionally added without purchaser agreement except to finish the heat; precautions against additions from scrap/materials are required. A dash is not a zero-residual guarantee.
Table 7 product-analysis deviations are a separate acceptance basis, not a relaxation of the cast-analysis windows above.
| Element | Permissible product-analysis deviation (wt. %) |
|---|---|
| Carbon (C) | ±0.02 |
| Silicon (Si) | ±0.03 |
| Manganese (Mn) | ±0.04 |
| Chromium (Cr) | ±0.05 |
| Molybdenum (Mo) | ±0.04 |
| Nickel (Ni) | ±0.07 |
| Vanadium (V) | ±0.02 |
| Phosphorus (P) | +0.005 |
| Sulfur (S) | +0.005 |
Table 7 direction/sampling note allows deviation either above or below the range, but not both for the same element from different sample products of the same cast. Maxima-only deviations are positive only. Values require ISO 14284 samples representing the average composition of the product cross-section.
Table 6 note b normally limits sulfur to 0.020 %, but the grade-specific note e for 55NiCrMoV7 explicitly permits sulfur up to 0.030 %. The grade-specific limit is used here.
Delivery hardness and hardening-test response for 55NiCrMoV7
248 HB maximum when supplied annealed (+A), Table 6. The condition-specific Brinell maximum is different from the minimum HRC after the reference hardening test.
| Property / regime | Value / meaning |
|---|---|
| Delivery-condition Brinell basis | 248 HB maximum when supplied annealed (+A), Table 6 |
| Hardening-test minimum | 42 HRC after the stipulated test treatment; smaller dimensions only, note g |
| Cold-drawn stock | The applicable table note permits annealed plus cold-drawn (+A+C) hardness up to 20 HB higher than annealed (+A); do not transfer this allowance to annealed plate or an untreated C45U basis |
| Final tool hardness | Specified separately for the real section and production treatment |
Table 1 note c adds the minimum-hardness hardening-test requirements. Supplementary verification is defined by normative Annex B.3, with Annex B.1 requiring supplementary/special items to be specified at enquiry and order. These numerical minima are not an informative tempering-curve estimate or a blanket finished-tool guarantee.
Table 6 note g limits the 42 HRC test value to smaller dimensions only. Note f says greater dimensions are normally supplied quenched and tempered at approximately 380 HB; the 248 HB maximum applies to annealed condition. Clause 4.1.2.1 excepts this grade from automatic annealed default. No numerical boundary between smaller and greater dimensions is supplied here, so none is invented.
Delivery condition and test treatment for 55NiCrMoV7
Specify Annealed or quenched-and-tempered condition as ordered; Table 6 note f governs usual greater-dimension supply. Clause 4.1.2.1 excepts this grade from automatic annealed default. A separate production heat treatment must be qualified for the actual tool.
| Table 6 / Annex B.3 hardening-test item | Reference |
|---|---|
| Hardening temperature | 850 °C (±10 °C) |
| Quench medium | Oil |
| Tempering temperature | 500 °C (±10 °C) |
| Minimum test hardness | 42 HRC; smaller dimensions only, note g |
| Salt-bath total heating, Table B.1 | 25 ± 1 min for hardening; 60 min for tempering |
| Other heating methods | Extend the heating time accordingly; no universal production holding time assigned |
B.3 requires the Figure 1 test-piece location, conditions avoiding decarburization, and hardness measurement on the prepared cut surface to ISO 6508. Untreated samples may be annealed before the test at the manufacturer’s discretion. No preheat temperature is specified by these rows, so none is inferred. These are specimen-test conditions, not guaranteed production recipes for every plate section. Annex A hardness-tempering curves are informative guidance, not identical acceptance limits.
For greater dimensions, Table 6 note f describes usual quenched-and-tempered delivery at approximately 380 HB, not an unconditional acceptance maximum or a conversion from the specimen HRC value. Agree the dimension/condition basis; no size cutoff is inferred.
Welding, cutting and finishing 40CrMnNiMo8-6
55NiCrMoV7 tool steel requires a qualified repair-welding procedure matched to chemistry, supplied condition, restraint and final treatment; it is not a generic readily weldable fabrication plate. No unsourced welding temperature is prescribed.
Thermal cutting, EDM and grinding can change the surface layer and introduce damage. Review cleanup allowance, inspect critical edges and avoid representing an unaffected core analysis as proof of sound tool surfaces. Greater dimensions are normally supplied quenched and tempered at approximately 380 HB under note f; no numerical size boundary or through-hardness guarantee is supplied.
Plate/flat dimensions and surface acceptance
Clause 4.4 requires shape, dimensions and tolerances agreed at enquiry and order, preferably using corresponding international or suitable national standards. ISO 1035-1/-3/-4 are cited for rolled round and flat bars; their bar tolerances must not simply be relabelled as plate tolerances. No invented plate capacity range, thickness deviation or flatness number is supplied here.
Clause 4.3 requires a workmanlike surface. Ground, polished or finished-machined products are to be free of surface imperfections and surface decarburization. Hot-rolled, forged, cold-drawn or rough-machined stock requires sufficient cleanup material; machining allowance is agreed under the 1999 provisions. Do not transfer round-product hardenability or surface limits to plate without the appropriate basis.
Applications and selection limits for 55NiCrMoV7
Qualitative engineering applications for 55NiCrMoV7 include forging-die blanks, hot-tool inserts and supported tooling. This is formally a Table 6 hot-work row; its minimum specimen response is qualified for smaller dimensions by note g. The actual finished tool, duty and edge support must be reviewed rather than assumed from a grade nickname.
Greater dimensions are normally supplied quenched and tempered at approximately 380 HB under note f; no numerical size boundary or through-hardness guarantee is supplied.
The standard’s condition hardness and hardening-test response do not provide a numerical impact property, corrosion rating or guaranteed tool life. High carbon or alloy content alone is not a substitute for a drawing and final acceptance requirements.
Compare 55NiCrMoV7 with three published own plates
These own product pages are already live. The following comparisons are material-selection contrasts, not automatic substitution approvals.
| Material | Family / chemistry | Condition | Property basis | Substitution limit |
|---|---|---|---|---|
| 55NiCrMoV7 (this plate) | nickel-chromium-molybdenum-vanadium hot-work tool steel | 248 HB maximum when supplied annealed (+A), Table 6 | Minimum specimen-test 42 HRC for smaller dimensions only; not supplied-plate HRC | Condition/form/test basis must match |
| JIS G4401 SK105 Tool Steel Plate | Carbon tool steel; published C 1.00–1.10 % | JIS G4401:2009 plate/strip condition basis; as-hot-rolled unless otherwise specified | Not the ISO 4957:1999 Table 6 specimen-test acceptance | Compare actual carbon, Si/Mn limits, condition and plate rules |
| JIS G4401 SK120 Tool Steel Plate | Carbon tool steel; published C 1.15–1.25 % | JIS G4401:2009 plate/strip condition basis; as-hot-rolled unless otherwise specified | Not the ISO 4957:1999 Table 6 specimen-test acceptance | Compare actual carbon, Si/Mn limits, condition and plate rules |
| ASTM A829 4140 Alloy Steel Plate | Engineering Cr-Mo plate; separate chemistry-ordered specification | Ordered condition on the own live page | Chemistry-ordered engineering plate, not this tool-test acceptance | Not a direct tool-grade substitute |
Country comparisons and substitution limi
The country comparison uses actual cited editions, not an unrestricted trade-name list. The steel number is the informative Annex C designation association, not proof that foreign delivery and test requirements are identical.
| System | Grade / number | Actual chemistry / form difference | Condition / substitution limit |
|---|---|---|---|
| ISO / international | 55NiCrMoV7 | Cast-analysis Table 6; this grade and edition | Delivery condition, specimen response and plate/flat requirements must be specified |
| Europe / designation number | 1.2714 | Informative Annex C associates the EN 10027-2:1992 number; it is not an independently verified later DIN specification | No automatic national-edition or product-condition certification inferred |
| Japan | JIS G4404:2015 SKT4 | C 0.50–0.60, Si 0.10–0.40, Mn 0.60–0.90, Ni 1.50–1.80, Cr 0.80–1.20, Mo 0.35–0.55 and V 0.05–0.15 match these rows, but JIS S is 0.020 maximum versus ISO grade-specific 0.030. | Annex JA.1 association, not blanket substitution. Preserve the ISO smaller-dimensions test qualification and greater-dimensions usual QT condition. |
Where printed, ISO hardening-test HRC is a genuine specimen-response basis, not supplied-condition hardness; no missing minimum is inferred. It must not be confused with JIS G4404 practical-decarburization HV criteria, JIS plate delivery hardness or an informative tempering curve. Verify the complete foreign standard, form and ordered condition before substitution.
Why choose SHH STEEL for 55NiCrMoV7
SHH STEEL produces and exports 55NiCrMoV7 plate against the stated standard, supplied condition and agreed inspection plan. We keep cast analysis, delivery hardness and final tooling acceptance distinct.
- Confirm the required edition and correct material designation.
- Use plate/flat tolerances and cleanup allowance appropriate to the actual form.
- Agree supplementary verification and required reports before acceptance.
- Maintain heat identification and review any proposed foreign substitution.
Enquiry and inspection planning for 55NiCrMoV7
| Enquiry item | What to specify |
|---|---|
| Grade / edition | 55NiCrMoV7; ISO edition and any associated drawing requirement |
| Form / dimensions | Plate or flat, thickness × width × length, quantity, finish and machining allowance |
| Condition | Annealed or quenched-and-tempered condition as ordered; Table 6 note f governs usual greater-dimension supply |
| Hardness basis | 248 HB maximum when supplied annealed (+A), Table 6 |
| Verification | State whether Annex B.3 hardening verification, product analysis or other supplementary tests are required |
| Final tooling | Actual tool duty, final property acceptance and production-treatment responsibility |
| Reports / logistics | Inspection-document type, heat traceability, packing, destination and target timing |
Dimensions, manufacturing route and any additional NDT or quality requirement are reviewed for feasibility. This page is not an unconditional stock, capacity or finished-tool performance commitment.
FAQ
-
Is 55NiCrMoV7 formally a hot-work grade?
- This is formally a Table 6 hot-work row; its minimum specimen response is qualified for smaller dimensions by note g. The Table 6 assignment is verified from the primary standard, not inferred from sequence or a trade name. Greater dimensions are normally supplied quenched and tempered at approximately 380 HB under note f; no numerical size boundary or through-hardness guarantee is supplied.
-
How do the three hardness references differ?
- 248 HB is the annealed maximum. The 42 HRC minimum test response at 850 °C oil quenching and 500 °C tempering applies to smaller dimensions only. Greater dimensions are normally supplied quenched and tempered at approximately 380 HB. These are not interchangeable acceptance regimes; no numerical dimension boundary is printed.
-
Are these temperatures a production heat-treatment guarantee?
- No. The table/B.3 regime is a specimen test. Table 1 note c provides the minimum-response requirement, while Annex B.1 makes supplementary verification an enquiry/order item. Annex A curves are informative; actual tool treatment depends on section and application.
-
Can round hardenability or bar tolerances be used directly for plate?
- No. Follow the actual product-form agreement under clause 4.4 and Figure 1 sample rules. Any Table 2 round-diameter hardenability statements are not plate-thickness guarantees.
-
Is the foreign grade or steel number an automatic equivalent?
- No. Use the explicit country-table differences, complete source edition, actual form, delivery condition and test acceptance. Historical JIS names and informative steel-number associations do not establish unconditional substitution.
Request a quotation
Request a quotation for ISO 4957 55NiCrMoV7 tool steel plate or flat stock. Send the required edition, quantity, dimensions, finish, machining allowance and drawing. State the supplied condition explicitly: Annealed or quenched-and-tempered condition as ordered; Table 6 note f governs usual greater-dimension supply. Identify the intended tooling duty and whether dimensions describe raw blanks or finished pieces.
Include the delivery-hardness acceptance, required inspection document and heat-traceability needs. Specify any supplementary product analysis, Annex B.3 hardening-test verification, surface/decarburization evaluation or additional NDT, with the agreed method and acceptance criteria. Do not treat a specimen-response HRC or round-diameter hardenability note as an arbitrary-section plate guarantee.
Provide the final tool properties and production-treatment responsibility separately. For a proposed foreign grade, attach its governing specification and drawing so chemistry, form and condition differences can be reviewed. Include cutting details, edge preparation, inspection stages, destination, packing and target timing; requested processes and dimensions are reviewed for feasibility before confirmation.
Contact: admin@steelspecs.com