Product Showcase
ISO 4957 Carbon Steel Plates
SHH STEEL offers ISO 4957-compliant non-alloy and alloy tool steels. ISO 4957 specifies grades for cold/hot work and plastic molds with defined hardness and toughness requirements. Global standard, certified quality, competitive prices, customizable. Trust SHH STEEL!
-
ISO 4957 HS2-9-2 Tool Steel Plate
ISO 4957 HS2-9-2 is a alloy high-speed tool steel for cutting-tool blanks, supported cutting inserts and tooling components. Its carbon range is 0.95–1.05 %, with the delivery condition and alloy balance defining the appropriate tooling route. Plate and flat blanks are selected by chemistry, surface quality, machining allowance and the actual section rather than by an unqualified foreign-grade nickname. Finished tooling still requires a qualified treatment and inspection basis. SHH STEEL produces and exports HS2-9-2 plate to the specified edition, dimensions and inspection requirements.View More -
ISO 4957 HS18-0-1 Tool Steel Plate
ISO 4957 HS18-0-1 is a alloy high-speed tool steel for cutting-tool blanks, supported cutting inserts and tooling components. Its carbon range is 0.73–0.83 %, with the delivery condition and alloy balance defining the appropriate tooling route. Plate and flat blanks are selected by chemistry, surface quality, machining allowance and the actual section rather than by an unqualified foreign-grade nickname. Finished tooling still requires a qualified treatment and inspection basis. SHH STEEL produces and exports HS18-0-1 plate to the specified edition, dimensions and inspection requirements.View More -
ISO 4957 HS1-8-1 Tool Steel Plate
ISO 4957 HS1-8-1 is a alloy high-speed tool steel for cutting-tool blanks, supported cutting inserts and tooling components. Its carbon range is 0.77–0.87 %, with the delivery condition and alloy balance defining the appropriate tooling route. Plate and flat blanks are selected by chemistry, surface quality, machining allowance and the actual section rather than by an unqualified foreign-grade nickname. Finished tooling still requires a qualified treatment and inspection basis. SHH STEEL produces and exports HS1-8-1 plate to the specified edition, dimensions and inspection requirements.View More -
ISO 4957 HS1-4-2 Tool Steel Plate
ISO 4957 HS1-4-2 is a alloy high-speed tool steel for cutting-tool blanks, supported cutting inserts and tooling components. Its carbon range is 0.85–0.95 %, with the delivery condition and alloy balance defining the appropriate tooling route. Plate and flat blanks are selected by chemistry, surface quality, machining allowance and the actual section rather than by an unqualified foreign-grade nickname. Finished tooling still requires a qualified treatment and inspection basis. SHH STEEL produces and exports HS1-4-2 plate to the specified edition, dimensions and inspection requirements.View More -
ISO 4957 HS0-4-1 Tool Steel Plate
ISO 4957 HS0-4-1 is a alloy high-speed tool steel for cutting-tool blanks, supported cutting inserts and tooling components. Its carbon range is 0.77–0.85 %, with the delivery condition and alloy balance defining the appropriate tooling route. Plate and flat blanks are selected by chemistry, surface quality, machining allowance and the actual section rather than by an unqualified foreign-grade nickname. Finished tooling still requires a qualified treatment and inspection basis. SHH STEEL produces and exports HS0-4-1 plate to the specified edition, dimensions and inspection requirements.View More -
ISO 4957 X40CrMoV5-1 Tool Steel Plate
ISO 4957 X40CrMoV5-1 is a chromium-molybdenum-vanadium hot-work tool steel for hot dies, tooling inserts and supported forming tools. Its carbon range is 0.35–0.42 %, with the delivery condition and alloy balance defining the appropriate tooling route. Plate and flat blanks are selected by chemistry, surface quality, machining allowance and the actual section rather than by an unqualified foreign-grade nickname. Finished tooling still requires a qualified treatment and inspection basis. SHH STEEL produces and exports X40CrMoV5-1 plate to the specified edition, dimensions and inspection requirements.View More -
ISO 4957 X38CrMoV5-3 Tool Steel Plate
ISO 4957 X38CrMoV5-3 is a molybdenum-rich chromium-vanadium hot-work tool steel for hot-tool inserts, dies and supported forming tools. Its carbon range is 0.35–0.40 %, with the delivery condition and alloy balance defining the appropriate tooling route. Plate and flat blanks are selected by chemistry, surface quality, machining allowance and the actual section rather than by an unqualified foreign-grade nickname. Finished tooling still requires a qualified treatment and inspection basis. SHH STEEL produces and exports X38CrMoV5-3 plate to the specified edition, dimensions and inspection requirements.View More -
ISO 4957 X37CrMoV5-1 Tool Steel Plate
ISO 4957 X37CrMoV5-1 is a chromium-molybdenum-vanadium hot-work tool steel for hot dies, die inserts and supported tooling blanks. Its carbon range is 0.33–0.41 %, with the delivery condition and alloy balance defining the appropriate tooling route. Plate and flat blanks are selected by chemistry, surface quality, machining allowance and the actual section rather than by an unqualified foreign-grade nickname. Finished tooling still requires a qualified treatment and inspection basis. SHH STEEL produces and exports X37CrMoV5-1 plate to the specified edition, dimensions and inspection requirements.View More -
ISO 4957 X35CrWMoV5 Tool Steel Plate
ISO 4957 X35CrWMoV5 is a chromium-tungsten-molybdenum-vanadium hot-work tool steel for hot dies, tool inserts and supported tooling blanks. Its carbon range is 0.32–0.40 %, with the delivery condition and alloy balance defining the appropriate tooling route. Plate and flat blanks are selected by chemistry, surface quality, machining allowance and the actual section rather than by an unqualified foreign-grade nickname. Finished tooling still requires a qualified treatment and inspection basis. SHH STEEL produces and exports X35CrWMoV5 plate to the specified edition, dimensions and inspection requirements.View More -
ISO 4957 X30WCrV9-3 Tool Steel Plate
ISO 4957 X30WCrV9-3 is a tungsten-chromium-vanadium hot-work tool steel for hot-tool inserts, extrusion-related tools and supported dies. Its carbon range is 0.25–0.35 %, with the delivery condition and alloy balance defining the appropriate tooling route. Plate and flat blanks are selected by chemistry, surface quality, machining allowance and the actual section rather than by an unqualified foreign-grade nickname. Finished tooling still requires a qualified treatment and inspection basis. SHH STEEL produces and exports X30WCrV9-3 plate to the specified edition, dimensions and inspection requirements.View More -
ISO 4957 50CrMoV13-15 Tool Steel Plate
ISO 4957 50CrMoV13-15 is a chromium-molybdenum-vanadium hot-work tool steel for hot-tool blanks, supported die inserts and tooling components. Its carbon range is 0.45–0.55 %, with the delivery condition and alloy balance defining the appropriate tooling route. Plate and flat blanks are selected by chemistry, surface quality, machining allowance and the actual section rather than by an unqualified foreign-grade nickname. Finished tooling still requires a qualified treatment and inspection basis. SHH STEEL produces and exports 50CrMoV13-15 plate to the specified edition, dimensions and inspection requirements.View More -
ISO 4957 38CrCoWV18-17-17 Tool Steel Plate
ISO 4957 38CrCoWV18-17-17 is a cobalt-tungsten-vanadium alloy hot-work tool steel for hot-tool inserts, specialized dies and supported tooling. Its carbon range is 0.35–0.45 %, with the delivery condition and alloy balance defining the appropriate tooling route. Plate and flat blanks are selected by chemistry, surface quality, machining allowance and the actual section rather than by an unqualified foreign-grade nickname. Finished tooling still requires a qualified treatment and inspection basis. SHH STEEL produces and exports 38CrCoWV18-17-17 plate to the specified edition, dimensions and inspection requirements.View More
ISO 4957 Carbon Steel Plates
Tool and Die Steel Plates
SHH STEEL, a leading Tool and Die Steel Plates exporter, produces and exports tool and die steel plates for mold-making, tooling, and automotive applications. Our plates, such as D2 and P20, ensure durability and machinability, meeting global standards. With a 5,000-ton inventory, we provide 3–5 day delivery for in-stock items, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for tool steel plates and custom precision manufacturing solutions.
Tool and Die Steel Plates
X