EN 10028-7 Carbon Steel Plates
SHH STEEL offers EN 10028-7-compliant X2CrNiMo17-12-2 stainless steel plates. EN 10028-7 specifies flat stainless steel products for pressure purposes, including austenitic creep-resisting steels. Corrosion-resistant, certified quality, competitive prices, customizable. Trust SHH STEEL!
-
EN 10028-7 X2CrNiN23-4 1.4362 Pressure Vessel Stainless Plate
EN 10028-7 X2CrNiN23-4 (1.4362) is an austenitic-ferritic (duplex) stainless steel for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 400 MPa and Rm 600 – 800 MPa (Table 10). SHH STEEL supplies it up to 50 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X1NiCrMoCu31-27-4 1.4563 Pressure Vessel Stainless Plate
EN 10028-7 X1NiCrMoCu31-27-4 (1.4563) is a highly alloyed (super-austenitic) stainless steel for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 220 MPa and Rm 500 – 700 MPa (Table 9). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X1CrNiMoCuN20-18-7 1.4547 Pressure Vessel Stainless Plate
EN 10028-7 X1CrNiMoCuN20-18-7 (1.4547) is a highly alloyed (super-austenitic) stainless steel for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 300 MPa and Rm 650 – 850 MPa (Table 9). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X1NiCrMoCuN25-20-7 1.4529 Pressure Vessel Stainless Plate
EN 10028-7 X1NiCrMoCuN25-20-7 (1.4529) is a highly alloyed (super-austenitic) stainless steel for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 300 MPa and Rm 650 – 850 MPa (Table 9). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X1CrNiMoCuN25-25-5 1.4537 Pressure Vessel Stainless Plate
EN 10028-7 X1CrNiMoCuN25-25-5 (1.4537) is a highly alloyed (super-austenitic) stainless steel for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 290 MPa and Rm 600 – 800 MPa (Table 9). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X1NiCrMoCu25-20-5 1.4539 Pressure Vessel Stainless Plate
EN 10028-7 X1NiCrMoCu25-20-5 (1.4539) is a highly alloyed (super-austenitic) stainless steel for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 220 MPa and Rm 520 – 720 MPa (Table 9). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X6CrNiMoNb17-12-2 1.4580 Pressure Vessel Stainless Plate
EN 10028-7 X6CrNiMoNb17-12-2 (1.4580) is a stabilized austenitic stainless steel for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 220 MPa and Rm 520 – 720 MPa (Table 9). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X6CrNiMoTi17-12-2 1.4571 Pressure Vessel Stainless Plate
EN 10028-7 X6CrNiMoTi17-12-2 (1.4571) is a stabilized austenitic stainless steel for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 220 MPa and Rm 520 – 670 MPa (Table 9). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X1CrNiMoN25-22-2 1.4466 Pressure Vessel Stainless Plate
EN 10028-7 X1CrNiMoN25-22-2 (1.4466) is a high-chromium, high-nickel austenitic stainless steel for special corrosive duties for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 250 MPa and Rm 540 – 740 MPa (Table 9). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X2CrNiMoN17-13-5 1.4439 Pressure Vessel Stainless Plate
EN 10028-7 X2CrNiMoN17-13-5 (1.4439) is a molybdenum-alloyed austenitic stainless steel for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 270 MPa and Rm 580 – 780 MPa (Table 9). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X2CrNiMo18-15-4 1.4438 Pressure Vessel Stainless Plate
EN 10028-7 X2CrNiMo18-15-4 (1.4438) is a molybdenum-alloyed austenitic stainless steel for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 220 MPa and Rm 520 – 720 MPa (Table 9). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More -
EN 10028-7 X3CrNiMo17-13-3 1.4436 Pressure Vessel Stainless Plate
EN 10028-7 X3CrNiMo17-13-3 (1.4436) is a molybdenum-alloyed austenitic stainless steel for pressure equipment. Plate delivered solution annealed (+AT) has Rp0.2 ≥ 220 MPa and Rm 530 – 730 MPa (Table 9). SHH STEEL supplies it up to 75 mm, cut to size, with EN 10204 3.1 or 3.2 certificates.View More
EN 10028-7 Carbon Steel Plates
Nuclear-Grade Steel Plates
SHH STEEL, a trusted Nuclear-Grade Steel Plates exporter, produces and exports nuclear-grade steel plates for nuclear power plants and energy applications. Our plates, like SA533, offer exceptional toughness and safety, meeting ASME standards. With a 5,000-ton inventory, we ensure 3–5 day delivery for in-stock items, supported by SGS/TUV inspections and mill certificates. Rely on SHH STEEL for nuclear power steel plates and custom high-safety solutions.
Nuclear-Grade Steel Plates
ASME SA542/SA542M
ASME SA543/SA543M
ASME SA612/SA612M
ASME SA662/SA662M
ASME SA737/SA737M
ASME SA202/SA202M
ASTM A202/A202M
ASTM A1017/A1017M
SA-1017/SA-1017M
ASTM A662/A662M
ASME SA724/SA724M
ASME SA736/SA736M
ASME SA832/SA832M
ASME SA533/SA533M
ASTM A533
ASME SA508/SA508M
ASTM A508
ASME SA387/SA387M
ASTM A387/A387M
ASME SA-738/SA-738M
ASTM A738
ASME SA-203/SA-203M
ASTM A203
EN 10028-7
RCC-M M3307
JIS G3118
GB/T 3531
GOST 10859
X