ASTM A681 A9 Tool Steel Plate | ASTM A681 Tool Steel - SHH STEEL

ASTM A681 A9 Tool Steel Plate

ASTM A681 A9 is a nickel-bearing chromium-molybdenum-vanadium cold-work tool steel for toughness-oriented cold dies, punches and inserts. Its carbon range is 0.45–0.55 %, with alloy limits that distinguish it from neighboring die steels. Plate and flat blanks are selected by chemistry, delivery condition, surface quality and heat-treatment response rather than by a generic tool-steel nickname. Final tooling performance also depends on section, cooling and the qualified temper. SHH STEEL produces and exports A9 plate to the specified edition, dimensions and inspection requirements.
Equivalent Grades:
SKD12: cold-work contrast, not an established counterpart; chemistry and condition require review.
Heat Treatment
Annealed; hardened and tempered as specified.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is ASTM A681 A9 plate?

ASTM A681 A9 Tool Steel Plate is nickel-bearing chromium-molybdenum-vanadium cold-work tool steel. Nickel 1.25–1.75 % and silicon 0.95–1.15 % accompany carbon 0.45–0.55 %; tungsten has no listed range. A distinct low-carbon nickel-bearing air-hardening route rather than an H13 or A2 substitute.

Numerical requirements here follow the finalized ASTM A681-08 (2008) text, approved 1 October 2008. This is a dated published-standard reference, not a claim that a later edition has identical tables. Plate, sheet, strip, bars and forgings are expressly within the wrought-product scope.

Greater toughness within the A-type comparison is not a quantitative impact guarantee; wear, section response and the final temper still need review.

SHH STEEL produces and exports A9 plate against the agreed grade, condition and inspection basis. See ASTM A681 within Tool and Die Steel Plates.

Material specification for A9

Parameter Requirement / scope
Standard / type ASTM A681-08; A9, UNS T30109; cold-work tool steel
Product scope Available wrought products including hot/cold finished bar, plate, sheet, strip, rod, wire and forgings
Manufacture Electric melting unless otherwise specified; ingot/slab reduction sufficient to refine solidification structure, clause 5.1
Condition State annealed, hardened and tempered, or other specified condition under ordering clause 4.1.6
Chemistry Table 1 heat analysis; listed limits already include product-analysis tolerances
Annealed hardness Table 2: 248 BHN maximum
Cold-drawn hardness Table 2: 262 BHN maximum for that condition; not an annealed plate limit
Hardening response Table 3: minimum 56 HRC on the prescribed test specimen and treatment
Lot Each shipment of a heat by type, size and shape is a lot, clause 12.1
Unit basis Inch-pound values govern; parenthetical SI values are informational conversions, clause 1.3

Chemical composition of A9

Table 1 values below are mass percent. Listed limits already include product-analysis tolerances; do not add a separate allowance. An ellipsis means no listed limit for that element here, not a zero-content guarantee.

Element A681-08 Table 1 chemical requirement (wt. %)
Carbon (C) 0.45–0.55
Manganese (Mn) 0.20–0.50
Phosphorus (P) 0.030 max
Sulfur (S) 0.030 max
Silicon (Si) 0.95–1.15
Chromium (Cr) 4.75–5.50
Vanadium (V) 0.80–1.40
Tungsten (W) Not specified in Table 1
Molybdenum (Mo) 1.30–1.80
Nickel (Ni) 1.25–1.75

Unless otherwise specified, nickel plus copper shall not exceed 0.75 % (Table 1 note A). Where specified, sulfur may be 0.06–0.15 % to improve machinability (note D); this optional resulfurized route is distinct from the normal 0.030 % sulfur maximum. Heat analysis is required under clause 6.1. Clause 6.2 purchaser analysis is specifically described for finished bars/forgings; it is not a substitute plate sampling method or permission to widen the limits.

Table 1 explicitly specifies nickel for this type. Do not use the default Ni+Cu cap to override that mandatory nickel range; confirm any additional copper requirement against the applicable order.

Hardness and minimum hardening response for A9

Table 2 gives A9 maximum annealed hardness of 248 BHN and a separate cold-drawn maximum of 262 BHN. Clause 7.1 refers to ASTM A370 and equivalent Rockwell values. The condition matters: a cold-drawn-flat limit is not automatically the limit for annealed plate.

Property / regime Value Meaning
Annealed acceptance 248 BHN max Specified annealed condition, Table 2
Cold-drawn acceptance 262 BHN max Only that delivery condition, Table 2
Minimum response to hardening 56 HRC Table 3 specimen response after stipulated treatment, not an as-delivered annealed hardness
Production tool properties Defined by the tool specification A test response does not guarantee arbitrary plate-section or finished-die properties

Clause 7.2 uses 1/4-in. (6.4-mm) thick disks representing the full cross section or the position midway between center and outer surface. Where form/size is unsuitable, longitudinal specimens may be used; these are at least 3 in. (76 mm) long with parallel flats ground on the original mill surfaces. Clause 7.2.1 uses the average of at least five hardness readings in the stated location, with light-load tests agreed where needed for thin pieces.

Delivery condition and response-test treatment for A9

Specify the delivery condition. An enquiry for annealed machining stock is different from one for hardened-and-tempered material. Table 2 calls the condition annealed; this edition does not impose a blanket spheroidizing temperature or a universal spheroidized-carbide rating. Specify any additional carbide-morphology requirement separately.

A681-08 Table 3 response-test item Reference
Preheat 1450 °F (788 °C)
Salt-bath austenitizing 1825 °F (996 °C)
Controlled-atmosphere austenitizing 1850 °F (1010 °C)
Listed austenitizing time 5–15 min; apply Table 3 note 2 for furnace/salt method
Quench medium Air
Temper 950 °F (510 °C); double temper, 2 h each cycle
Minimum test response 56 HRC

Table 3 note 1 restricts these austenitizing temperatures to the response-to-hardening test; other combinations may be used for particular applications. Note 2 permits preheat ±25 °F (14 °C), but austenitizing/tempering ±10 °F (5.6 °C). Controlled-atmosphere specimens are held 5–15 min after reaching temperature; salt treatment follows the minimum time indicated. These are test-piece parameters, not a guaranteed production cycle for every plate thickness.

Welding, cutting and grinding A9

A9 is an alloy tool steel, not a readily weldable general fabrication plate. Tool repair welding requires a procedure matched to chemistry, prior condition, section, restraint and the intended final heat treatment. No generic preheat or post-weld temperature is prescribed here.

Thermal cutting, electrical discharge machining and grinding can leave altered layers or local cracking at the tool surface. Allow for finishing and inspect critical edges before final service. Grinding burn and tensile surface stresses can defeat an otherwise suitable die chemistry. Greater toughness within the A-type comparison is not a quantitative impact guarantee; wear, section response and the final temper still need review.

Plate/flat dimensions, surface quality and inspection

Clause 10.1 invokes the applicable dimensional tables. Hot-rolled sheet/plate has its own Table 24 thickness tolerances and machining allowances, Table 25 trimmed width/length tolerances, Table 26 flatness and Table 27 camber. Flat bar or machined stock must use its applicable form-specific table rather than a round-bar diameter tolerance.

As a Table 24 example, hot-rolled plate over 0.500 through 1.000 in. (12.7–25.4 mm) has a 0.100-in. (2.54-mm) thickness tolerance, all over the specified thickness, and a 0.063-in. (1.60-mm) machining allowance. The table notes relate maximum decarburization to 80 % of the machining allowance per side and permit additional cleanup for flatness. This example is a tolerance reference, not a stock or capacity range.

Under clause 9.2, ground/polished, ground-finished or machine-finished material must be free of scale and decarburization. For other finishes, apply the appropriate size/shape limits and agree any tighter acceptance. Macrostructure is examined under clause 8/ASTM A561 for harmful porosity, segregation, inclusions, pipe and cracks; apply the appropriate composition/size rating, not an invented universal plate class.

Applications and selection limits for A9

Engineering applications considered for A9 include toughness-oriented cold dies, punches and inserts. A distinct low-carbon nickel-bearing air-hardening route rather than an H13 or A2 substitute. The standard classifies composition; the exact finished die, duty cycle and heat treatment still require engineering qualification.

Nickel 1.25–1.75 % and silicon 0.95–1.15 % accompany carbon 0.45–0.55 %; tungsten has no listed range.

Greater toughness within the A-type comparison is not a quantitative impact guarantee; wear, section response and the final temper still need review. Corrosion protection and thermal management are separate design matters; cold-work tool steel is not a pressure-vessel or stainless-service specification.

Compare A9 with published tool and engineering plates

The following own pages are already published. These are material-selection contrasts, not substitutes; tool performance cannot be inferred from carbon content or a shared plate form.

Material Type / chemistry Condition Property basis Typical route Substitution limit
A9 (this plate) nickel-bearing chromium-molybdenum-vanadium cold-work tool steel Annealed 248 BHN max; other condition specified Minimum response 56 HRC on Table 3 specimen Cold-work dies/punches Not a carbon cutting-tool or machinery-alloy substitute
JIS G4401 SK140 Tool Steel Plate Carbon tool steel; published C 1.30–1.50 % As-hot-rolled unless otherwise specified; annealed/cold-rolled by agreement JIS G4401:2009 plate/strip hardness basis; not A681 Table 3 Cutting/file or edge-tool blanks as appropriate High-carbon cutting-tool route; lacks this specified tool-steel alloy balance
JIS G4401 SK120 Tool Steel Plate Carbon tool steel; published C 1.15–1.25 % As-hot-rolled unless otherwise specified; annealed/cold-rolled by agreement JIS G4401:2009 plate/strip hardness basis; not A681 Table 3 Cutting/file or edge-tool blanks as appropriate High-carbon cutting-tool route; lacks this specified tool-steel alloy balance
ASTM A829 4140 Alloy Steel Plate Cr-Mo engineering plate; published reference C 0.36–0.44 % Ordered condition on existing page Chemistry-ordered plate; no automatic A681 tool-hardness/response package Machinery parts and later heat-treated components Structural-quality engineering alloy, not an A681 matching tool-steel specification

International comparisons and substitution limits for A9

The JIS comparison below uses finalized JIS G 4404:2015 Table 4. Values in each pair are JIS first, ASTM second; all are wt. %. The ISO name, where present, is the JIS informational Annex JA.1 association, not a direct ASTM-certified equivalent.

Country / system Designation Actual differences / form Condition and substitution limit
United States ASTM A681-08 A9, UNS T30109 This wrought tool-steel specification, including plate Table 2 condition-specific hardness and Table 3 test response apply
Japan JIS G 4404:2015 SKD12 JIS SKD12 C 0.95–1.05 and Si 0.10–0.40 versus A9 C 0.45–0.55 and Si 0.95–1.15; A9 explicitly specifies Ni 1.25–1.75. Different low-carbon/nickel-bearing route; full chemistry and form review required. JIS annealed delivery, plate/flat acceptance and test regimes differ. The cited JIS sulfur limit is not automatically the ASTM limit.
International / European ISO route X100CrMoV5 JIS Annex JA.1 informational comparison only; no complete ISO chemical window is asserted identical Confirm actual ISO edition, product form, heat-treatment and acceptance requirements; no direct DIN/ASTM alias is inferred

A681 Table 3 measures minimum response to hardening; JIS G4404 Table 10 and G4403 Table 7 HV values instead define practical-decarburization depth. Those regimes are not interchangeable. Similar principal chemistry does not establish equal manufacturing, cleanliness, carbide distribution or finished-tool performance.

Why choose SHH STEEL for A9

SHH STEEL produces and exports A9 plate to a stated specification rather than an unqualified trade-name cross-reference. We review the product form, condition, machining allowance and inspection requirements before confirming the enquiry.

  • Keep chemical limits and optional resulfurized variants explicit.
  • Separate annealed acceptance from prescribed hardening response and final tool properties.
  • Use plate/flat dimensional rules appropriate to the actual finish.
  • Maintain heat identification and the required inspection reports.

Enquiry and inspection planning for A9

Enquiry item What to specify
Type / edition A9 and the required ASTM edition
Form and dimensions Plate or flat; thickness × width × length, quantity and finish
Condition Annealed (248 BHN max on the reference basis) or separately specified treated state
Chemistry variant Normal chemistry or explicitly specified resulfurized variant; required analysis reporting
Toolmaking Intended die duty, final tool condition and any additional carbide/microstructure requirement
Inspection Chemistry, hardness, test response, surface/decarburization and macrostructure acceptance
Documentation Required test reports, heat identification and purchaser-witness provisions
Logistics Destination, timing, packing and machining allowance

Additional NDT or stricter quality requirements need agreed methods and acceptance criteria. A requested dimension or process is reviewed for feasibility; this page is not an unconditional stock or capacity commitment.

FAQ

What distinguishes A9 from other hot-work steels?
Nickel 1.25–1.75 % and silicon 0.95–1.15 % accompany carbon 0.45–0.55 %; tungsten has no listed range. Greater toughness within the A-type comparison is not a quantitative impact guarantee; wear, section response and the final temper still need review.
Does the Table 3 HRC value describe annealed plate?
No. Annealed acceptance is 248 BHN maximum in Table 2. The 56 HRC value is minimum hardening response on the prescribed specimen after the Table 3 treatment; it is not a universal final-die or as-delivered hardness.
Are the Table 3 temperatures a production heat-treatment guarantee?
No. They are stipulated for the response test. The specified preheat, salt/furnace temperatures, quench medium and tempering duration define that test regime; the actual values are listed in the delivery section. Actual tool treatment depends on section and application.
Do these chemical limits allow an extra product-analysis tolerance?
No. Table 1 note A says its limits include product-analysis tolerances. Normal P/S maxima and the Ni+Cu rule must be respected; optional sulfur or resulfurized H13 manganese rules require an explicitly specified variant.
Is the cited JIS or ISO name automatically equivalent?
Different low-carbon/nickel-bearing route; full chemistry and form review required. JIS SKD12 C 0.95–1.05 and Si 0.10–0.40 versus A9 C 0.45–0.55 and Si 0.95–1.15; A9 explicitly specifies Ni 1.25–1.75. Match product form, full chemistry, hardness/test regime and inspection before any substitution.

Request a quotation

Request a quotation for ASTM A681 A9 tool steel plate or flat stock. Send the required edition, quantity, thickness, width and length, finish and machining allowance. Describe the die or tooling duty and identify whether the requirement is annealed machining stock or a separately specified hardened-and-tempered condition.

Include the hardness acceptance basis, hardening-response requirement and any additional macrostructure, carbide-quality, decarburization or NDT criteria. If a resulfurized variant is required, state that explicitly with the chemical and machining requirements. Provide the intended final tool properties separately rather than treating a specimen test as a production guarantee.

Send the inspection-report and heat-traceability requirements, destination, target delivery timing and packing needs. For a proposed foreign substitute, attach the governing specification and drawing so chemical, form and test differences can be reviewed before confirming the quotation.

For cut pieces, include the cutting drawing, grain-orientation needs, edge preparation and inspection stage. Confirm whether supplied dimensions are raw blanks or finished dimensions before order acceptance.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X