ASTM A681 A5 Tool Steel Plate | ASTM A681 Tool Steel - SHH STEEL

ASTM A681 A5 Tool Steel Plate

ASTM A681 A5 is a high-manganese chromium-molybdenum cold-work tool steel for cold-work die, punch and tooling blanks. Its carbon range is 0.95–1.05 %, with alloy limits that distinguish it from neighboring die steels. Plate and flat blanks are selected by chemistry, delivery condition, surface quality and heat-treatment response rather than by a generic tool-steel nickname. Final tooling performance also depends on section, cooling and the qualified temper. SHH STEEL produces and exports A5 plate to the specified edition, dimensions and inspection requirements.
Equivalent Grades:
SKS3: cold-work contrast, not an established counterpart; chemistry and condition require review.
Heat Treatment
Annealed; hardened and tempered as specified.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is ASTM A681 A5 plate?

ASTM A681 A5 Tool Steel Plate is high-manganese chromium-molybdenum cold-work tool steel. Table 1 lists manganese 2.80–3.20 %, above A4, with carbon 0.95–1.05 % and molybdenum 0.90–1.40 %. A specifically identified historical A5 chemistry requirement rather than a substitute chosen from neighboring type numbers.

Numerical requirements here follow the finalized ASTM A681-08 (2008) text, approved 1 October 2008. This is a dated published-standard reference, not a claim that a later edition has identical tables. Plate, sheet, strip, bars and forgings are expressly within the wrought-product scope.

The reference includes the chemistry row but no A5 Table 2 or Table 3 row; hardness and heat-treatment acceptance must be agreed against an applicable source and order.

SHH STEEL produces and exports A5 plate against the agreed grade, condition and inspection basis. See ASTM A681 within Tool and Die Steel Plates.

Material specification for A5

Item A5 requirement / scope
Standard / identity ASTM A681-08 Table 1; A5, UNS T30105
Form Wrought products including plate, sheet, strip and flat bar
Chemistry Verified Table 1 analysis; product-analysis tolerances already included
Delivery condition Specify annealed or other agreed condition
Hardness / treatment acceptance Agree against the applicable source and order; no A5 Table 2/3 row in this reference
Manufacture Electric melting unless otherwise specified; refinement under clause 5.1
Lot Shipment of heat by type, size and shape
Dimensional basis Use the applicable plate/flat form and finish tables; inch-pound values govern

Chemical composition of A5

Table 1 values below are mass percent. Listed limits already include product-analysis tolerances; do not add a separate allowance. An ellipsis means no listed limit for that element here, not a zero-content guarantee.

Element A681-08 Table 1 chemical requirement (wt. %)
Carbon (C) 0.95–1.05
Manganese (Mn) 2.80–3.20
Phosphorus (P) 0.030 max
Sulfur (S) 0.030 max
Silicon (Si) 0.10–0.70
Chromium (Cr) 0.90–1.40
Vanadium (V) Not specified in Table 1
Tungsten (W) Not specified in Table 1
Molybdenum (Mo) 0.90–1.40

Unless otherwise specified, nickel plus copper shall not exceed 0.75 % (Table 1 note A). Where specified, sulfur may be 0.06–0.15 % to improve machinability (note D); this optional resulfurized route is distinct from the normal 0.030 % sulfur maximum. Heat analysis is required under clause 6.1. Clause 6.2 purchaser analysis is specifically described for finished bars/forgings; it is not a substitute plate sampling method or permission to widen the limits.

Hardness acceptance basis for A5

A5 is a formal Table 1 chemistry type in ASTM A681-08. That edition contains no A5 row in Table 2 or Table 3. Accordingly, no numerical annealed/cold-drawn maximum or minimum hardening-response HRC is assigned here.

Acceptance item Basis for A5
Annealed or other delivery hardness Agree against the applicable source and order
Hardening-response acceptance Agree the governing source, specimen regime and value before purchase
Final tool properties Specified separately for the actual tool
Neighboring type data A2, A4 and A6 numbers are not A5 requirements

This omission must not be filled with a producer typical value presented as an ASTM limit. The general specification sampling and inspection provisions remain relevant; define the additional property acceptance and reporting in the enquiry.

Delivery condition and response-test treatment for A5

Specify the A5 delivery condition and the agreed hardness/heat-treatment acceptance against an applicable source and order. The verified 2008 reference gives A5 chemistry but no Table 2 maximum or Table 3 response-treatment row.

A5 annealing, hardening, quenching and tempering parameters require a separately agreed applicable basis. A production heat treatment must be qualified for its actual composition, section and tool requirements. Neighboring A-type cycles do not become A5 acceptance requirements.

Welding, cutting and grinding A5

A5 is an alloy tool steel, not a readily weldable general fabrication plate. Tool repair welding requires a procedure matched to chemistry, prior condition, section, restraint and the intended final heat treatment. No generic preheat or post-weld temperature is prescribed here.

Thermal cutting, electrical discharge machining and grinding can leave altered layers or local cracking at the tool surface. Allow for finishing and inspect critical edges before final service. Grinding burn and tensile surface stresses can defeat an otherwise suitable die chemistry. The reference includes the chemistry row but no A5 Table 2 or Table 3 row; hardness and heat-treatment acceptance must be agreed against an applicable source and order.

Plate/flat dimensions, surface quality and inspection

Clause 10.1 invokes the applicable dimensional tables. Hot-rolled sheet/plate has its own Table 24 thickness tolerances and machining allowances, Table 25 trimmed width/length tolerances, Table 26 flatness and Table 27 camber. Flat bar or machined stock must use its applicable form-specific table rather than a round-bar diameter tolerance.

As a Table 24 example, hot-rolled plate over 0.500 through 1.000 in. (12.7–25.4 mm) has a 0.100-in. (2.54-mm) thickness tolerance, all over the specified thickness, and a 0.063-in. (1.60-mm) machining allowance. The table notes relate maximum decarburization to 80 % of the machining allowance per side and permit additional cleanup for flatness. This example is a tolerance reference, not a stock or capacity range.

Under clause 9.2, ground/polished, ground-finished or machine-finished material must be free of scale and decarburization. For other finishes, apply the appropriate size/shape limits and agree any tighter acceptance. Macrostructure is examined under clause 8/ASTM A561 for harmful porosity, segregation, inclusions, pipe and cracks; apply the appropriate composition/size rating, not an invented universal plate class.

Applications and selection limits for A5

Engineering applications considered for A5 include cold-work die, punch and tooling blanks. A specifically identified historical A5 chemistry requirement rather than a substitute chosen from neighboring type numbers. The standard classifies composition; the exact finished die, duty cycle and heat treatment still require engineering qualification.

Table 1 lists manganese 2.80–3.20 %, above A4, with carbon 0.95–1.05 % and molybdenum 0.90–1.40 %.

The reference includes the chemistry row but no A5 Table 2 or Table 3 row; hardness and heat-treatment acceptance must be agreed against an applicable source and order. Corrosion protection and thermal management are separate design matters; cold-work tool steel is not a pressure-vessel or stainless-service specification.

Compare A5 with published tool and engineering plates

The following own pages are already published. These are material-selection contrasts, not substitutes; tool performance cannot be inferred from carbon content or a shared plate form.

Material Type / chemistry Condition Property basis Typical route Substitution limit
A5 (this plate) high-manganese chromium-molybdenum cold-work tool steel Agreed delivery condition and hardness No A5 Table 3 row; acceptance by agreed applicable basis Cold-work dies/punches Not a carbon cutting-tool or machinery-alloy substitute
JIS G4401 SK140 Tool Steel Plate Carbon tool steel; published C 1.30–1.50 % As-hot-rolled unless otherwise specified; annealed/cold-rolled by agreement JIS G4401:2009 plate/strip hardness basis; not A681 Table 3 Cutting/file or edge-tool blanks as appropriate High-carbon cutting-tool route; lacks this specified tool-steel alloy balance
JIS G4401 SK120 Tool Steel Plate Carbon tool steel; published C 1.15–1.25 % As-hot-rolled unless otherwise specified; annealed/cold-rolled by agreement JIS G4401:2009 plate/strip hardness basis; not A681 Table 3 Cutting/file or edge-tool blanks as appropriate High-carbon cutting-tool route; lacks this specified tool-steel alloy balance
ASTM A829 4140 Alloy Steel Plate Cr-Mo engineering plate; published reference C 0.36–0.44 % Ordered condition on existing page Chemistry-ordered plate; no automatic A681 tool-hardness/response package Machinery parts and later heat-treated components Structural-quality engineering alloy, not an A681 matching tool-steel specification

International comparisons and substitution limits for A5

The JIS comparison below uses finalized JIS G 4404:2015 Table 4. Values in each pair are JIS first, ASTM second; all are wt. %. The ISO name, where present, is the JIS informational Annex JA.1 association, not a direct ASTM-certified equivalent.

Country / system Designation Actual differences / form Condition and substitution limit
United States ASTM A681-08 A5, UNS T30105 This wrought tool-steel specification, including plate Formal Table 1 chemistry; no A5 Table 2/3 row; agree hardness/treatment acceptance
Japan JIS G 4404:2015 SKS3 JIS SKS3 Mn 0.90–1.20 versus A5 Mn 2.80–3.20; SKS3 specifies W 0.50–1.00 and prohibits intentional Mo, while A5 specifies Mo 0.90–1.40. Not an A5 equivalent; chemistry and property acceptance cannot be borrowed from this contrast. JIS annealed delivery, plate/flat acceptance and test regimes differ. The cited JIS sulfur limit is not automatically the ASTM limit.
International / European ISO route No ISO symbol assigned to the cited JIS grade JIS Annex JA.1 informational comparison only; no complete ISO chemical window is asserted identical Confirm actual ISO edition, product form, heat-treatment and acceptance requirements; no direct DIN/ASTM alias is inferred

A681 Table 3 measures minimum response to hardening; JIS G4404 Table 10 and G4403 Table 7 HV values instead define practical-decarburization depth. Those regimes are not interchangeable. Similar principal chemistry does not establish equal manufacturing, cleanliness, carbide distribution or finished-tool performance.

Why choose SHH STEEL for A5

SHH STEEL produces and exports A5 plate to a stated specification rather than an unqualified trade-name cross-reference. We review the product form, condition, machining allowance and inspection requirements before confirming the enquiry.

  • Keep chemical limits and optional resulfurized variants explicit.
  • Separate annealed acceptance from prescribed hardening response and final tool properties.
  • Use plate/flat dimensional rules appropriate to the actual finish.
  • Maintain heat identification and the required inspection reports.

Enquiry and inspection planning for A5

Enquiry item What to specify
Type / edition A5 and the required ASTM edition
Form and dimensions Plate or flat; thickness × width × length, quantity and finish
Condition Specify condition and agreed hardness/heat-treatment acceptance; no number assumed
Chemistry variant Normal chemistry or explicitly specified resulfurized variant; required analysis reporting
Toolmaking Intended die duty, final tool condition and any additional carbide/microstructure requirement
Inspection Chemistry, hardness, test response, surface/decarburization and macrostructure acceptance
Documentation Required test reports, heat identification and purchaser-witness provisions
Logistics Destination, timing, packing and machining allowance

Additional NDT or stricter quality requirements need agreed methods and acceptance criteria. A requested dimension or process is reviewed for feasibility; this page is not an unconditional stock or capacity commitment.

FAQ

Is A5 formally listed in the reference?
Yes. Table 1 of ASTM A681-08 lists A5, UNS T30105, including the verified high-manganese chromium-molybdenum chemistry.
What annealed hardness does this page guarantee?
No numerical A5 hardness is assigned from this reference: Table 2 has no A5 row. Agree hardness against the applicable source and order rather than borrowing A4 or A6 limits.
What is the A5 minimum response-to-hardening HRC?
No A5 row occurs in Table 3 of the verified edition. Agree the governing source, specimen regime and acceptance before purchase; no neighboring-type HRC is used.
Does A681 include A5 plate or only bars?
The general wrought-product scope includes plate, sheet, strip and bars. State the actual product form, finish, dimensions and inspection requirements; bar tolerances are not automatically plate tolerances.
Can SKS3 or another cold-work steel replace A5?
Not automatically. The comparison shows major manganese and molybdenum differences. Match complete chemistry, product form and the separately agreed property/treatment basis before substitution.

Request a quotation

Request a quotation for ASTM A681 A5 tool steel plate or flat stock. Send the required edition, quantity, thickness, width and length, finish and machining allowance. Describe the die or tooling duty and identify whether the requirement is annealed machining stock or a separately specified hardened-and-tempered condition.

Include the hardness acceptance basis, hardening-response requirement and any additional macrostructure, carbide-quality, decarburization or NDT criteria. If a resulfurized variant is required, state that explicitly with the chemical and machining requirements. Provide the intended final tool properties separately rather than treating a specimen test as a production guarantee.

Send the inspection-report and heat-traceability requirements, destination, target delivery timing and packing needs. For a proposed foreign substitute, attach the governing specification and drawing so chemical, form and test differences can be reviewed before confirming the quotation.

For cut pieces, include the cutting drawing, grain-orientation needs, edge preparation and inspection stage. Confirm whether supplied dimensions are raw blanks or finished dimensions before order acceptance.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X