ASTM A681 P2 is a low-carbon chromium-molybdenum mould steel for carburized mould cavities and inserts. Its carbon requirement is 0.10 max %, distinguishing this mould route from higher-carbon cutting-tool steels. Plate and flat blanks need a defined delivery condition, surface quality and inspection basis. The reference does not assign this type a Table 3 hardening-response HRC; final mould properties require the applicable source and order. SHH STEEL produces and exports P2 plate to the specified edition, dimensions and inspection requirements.
Equivalent Grades:
SKS3 contrast; substitution requires review.
Heat Treatment
Annealed; carburized and hardened final condition.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is ASTM A681 P2 plate?

ASTM A681 P2 Tool Steel Plate is a low-carbon chromium-molybdenum mould steel. Table 1 specifies carbon 0.10 % maximum, chromium 0.75–1.25 %, molybdenum 0.15–0.40 % and nickel 0.10–0.50 %. Carburizing mould stock where low core carbon and the specified chromium-molybdenum balance are required.

Numerical requirements here follow the finalized ASTM A681-08 (2008) text, approved 1 October 2008. This is a dated published-standard reference, not a claim that a later edition has identical tables. Plate, sheet, strip, bars and forgings are expressly within the wrought-product scope.

The standard identifies P2–P6 as used in the carburized condition; neither case depth nor final case/core hardness is assigned by a Table 3 response row.

SHH STEEL produces and exports P2 plate against the agreed grade, condition and inspection basis. See ASTM A681 within Tool and Die Steel Plates.

Material specification for P2

Parameter Requirement / scope
Standard / identity ASTM A681-08; P2, UNS T51602; mould steel
Product scope Wrought plate, sheet, strip, bar and other forms within clause 1.2
Manufacture Electric melting unless otherwise specified; refinement under clause 5.1
Chemistry Verified Table 1 analysis and applicable footnotes; product-analysis tolerances already included
Delivery / hardness Annealed: 100 BHN maximum, Table 2; final carburized condition separately specified
Cold-drawn maximum No numerical value listed in Table 2 for this type
Response-to-hardening Table 3 note 4 excludes P-type response testing; no type-specific specimen-response HRC row
Lot Shipment by heat, type, size and shape, clause 12.1
Units Inch-pound values govern; SI conversions informational

Chemical composition of P2

Table 1 values below are mass percent. Listed limits already include product-analysis tolerances; do not add a separate allowance. An ellipsis means no listed limit for that element here, not a zero-content guarantee.

Element A681-08 Table 1 chemical requirement (wt. %)
Carbon (C) 0.10 max
Manganese (Mn) 0.10–0.40
Phosphorus (P) 0.030 max
Sulfur (S) 0.030 max
Silicon (Si) 0.10–0.40
Chromium (Cr) 0.75–1.25
Vanadium (V) Not specified in Table 1
Tungsten (W) Not specified in Table 1
Molybdenum (Mo) 0.15–0.40
Nickel (Ni) 0.10–0.50

Unless otherwise specified, nickel plus copper shall not exceed 0.75 % (Table 1 note A). Where specified, sulfur may be 0.06–0.15 % to improve machinability (note D); this optional resulfurized route is distinct from the normal 0.030 % sulfur maximum. Heat analysis is required under clause 6.1. Clause 6.2 purchaser analysis is specifically described for finished bars/forgings; it is not a substitute plate sampling method or permission to widen the limits.

The explicit nickel requirement is part of this type row and must be read with Table 1 note A. Do not replace a specified nickel range with a generic residual limit; confirm any supplementary copper requirement on the applicable order.

Delivery hardness and final mould acceptance for P2

The P2 Table 2 basis is: Annealed: 100 BHN maximum, Table 2; final carburized condition separately specified. A numerical cold-drawn maximum is not supplied by the printed row. It must not be filled from a nearby tool-steel type.

Acceptance item Basis
Supply condition Annealed: 100 BHN maximum, Table 2; final carburized condition separately specified
Hardening-response specimen Table 3 note 4 excludes P-type response testing; no type-specific specimen-response HRC row
Final mould properties Agreed against the applicable source and order; not an inherited tool-family HRC
Case/core requirements Specify applicable depth, hardness and inspection if required; no numbers inferred

Clause 3.1.8.1 identifies P2–P6 as carburizing mould steels: after machining or hubbing they require carburizing to obtain the intended hard surface. The annealed maximum is not final case hardness, core strength or case depth.

Delivery condition and response-test treatment for P2

Specify the actual supplied condition for P2: Annealed: 100 BHN maximum, Table 2; final carburized condition separately specified. The ordered dimensions, finish and final mould requirements remain separate acceptance items.

Table 3 note 4 states that P-types shall not be tested for response to heat treatment. Its explanation identifies P2–P6 as used in the carburized condition and P20 as normally prehardened. P21 likewise has no Table 3 treatment row; its normally prehardened basis is supplied by clause 3.1.8.2 and Table 2 footnote A.

No preheat, austenitizing temperature, holding time, quench medium, tempering or ageing recipe is assigned from an absent response-test row. Use the applicable source and order for any subsequent treatment. A producer typical range is not an ASTM limit unless separately adopted in the order.

Welding, cutting and grinding P2

P2 is an alloy tool steel, not a readily weldable general fabrication plate. Tool repair welding requires a procedure matched to chemistry, prior condition, section, restraint and the intended final heat treatment. No generic preheat or post-weld temperature is prescribed here.

Thermal cutting, electrical discharge machining and grinding can leave altered layers or local cracking at the tool surface. Allow for finishing and inspect critical edges before final service. Grinding burn and tensile surface stresses can defeat an otherwise suitable die chemistry. The standard identifies P2–P6 as used in the carburized condition; neither case depth nor final case/core hardness is assigned by a Table 3 response row.

Plate/flat dimensions, surface quality and inspection

Clause 10.1 invokes the applicable dimensional tables. Hot-rolled sheet/plate has its own Table 24 thickness tolerances and machining allowances, Table 25 trimmed width/length tolerances, Table 26 flatness and Table 27 camber. Flat bar or machined stock must use its applicable form-specific table rather than a round-bar diameter tolerance.

As a Table 24 example, hot-rolled plate over 0.500 through 1.000 in. (12.7–25.4 mm) has a 0.100-in. (2.54-mm) thickness tolerance, all over the specified thickness, and a 0.063-in. (1.60-mm) machining allowance. The table notes relate maximum decarburization to 80 % of the machining allowance per side and permit additional cleanup for flatness. This example is a tolerance reference, not a stock or capacity range.

Under clause 9.2, ground/polished, ground-finished or machine-finished material must be free of scale and decarburization. For other finishes, apply the appropriate size/shape limits and agree any tighter acceptance. Macrostructure is examined under clause 8/ASTM A561 for harmful porosity, segregation, inclusions, pipe and cracks; apply the appropriate composition/size rating, not an invented universal plate class.

Applications and selection limits for P2

Engineering applications considered for P2 include carburized mould cavities and inserts. Carburizing mould stock where low core carbon and the specified chromium-molybdenum balance are required. The standard classifies composition; the exact finished die, duty cycle and heat treatment still require engineering qualification.

Table 1 specifies carbon 0.10 % maximum, chromium 0.75–1.25 %, molybdenum 0.15–0.40 % and nickel 0.10–0.50 %.

The standard identifies P2–P6 as used in the carburized condition; neither case depth nor final case/core hardness is assigned by a Table 3 response row. Corrosion protection and thermal management are separate design matters; mould steel is not a pressure-vessel or stainless-service specification.

Compare P2 with published tool and engineering plates

The following own pages are already published. These are material-selection contrasts, not substitutes; tool performance cannot be inferred from carbon content or a shared plate form.

Material Type / chemistry Condition Property basis Typical route Substitution limit
P2 (this plate) low-carbon chromium-molybdenum mould steel Annealed: 100 BHN maximum, Table 2; final carburized condition separately specified P-type response testing excluded; no specimen-response HRC assigned Mould tooling; condition-specific route Not a carbon cutting-tool or machinery-alloy substitute
JIS G4401 SK140 Tool Steel Plate Carbon tool steel; published C 1.30–1.50 % As-hot-rolled unless otherwise specified; annealed/cold-rolled by agreement JIS G4401:2009 plate/strip hardness basis; not A681 Table 3 Cutting/file or edge-tool blanks as appropriate High-carbon cutting-tool route; lacks this specified tool-steel alloy balance
JIS G4401 SK120 Tool Steel Plate Carbon tool steel; published C 1.15–1.25 % As-hot-rolled unless otherwise specified; annealed/cold-rolled by agreement JIS G4401:2009 plate/strip hardness basis; not A681 Table 3 Cutting/file or edge-tool blanks as appropriate High-carbon cutting-tool route; lacks this specified tool-steel alloy balance
ASTM A829 4140 Alloy Steel Plate Cr-Mo engineering plate; published reference C 0.36–0.44 % Ordered condition on existing page Chemistry-ordered plate; no automatic A681 tool-hardness/response package Machinery parts and later heat-treated components Structural-quality engineering alloy, not an A681 matching tool-steel specification

International comparisons and substitution limits for P2

The JIS comparison below uses finalized JIS G 4404:2015 Table 4. Values in each pair are JIS first, ASTM second; all are wt. %. The ISO name, where present, is the JIS informational Annex JA.1 association, not a direct ASTM-certified equivalent.

Country / system Designation Actual differences / form Condition and substitution limit
United States ASTM A681-08 P2, UNS T51602 This wrought tool-steel specification, including plate Table 2 condition basis; P-type Table 3 response testing excluded
Japan JIS G 4404:2015 SKS3 JIS SKS3 C 0.90–1.00 versus P2 C 0.10 maximum. P2 requires Mo 0.15–0.40; SKS3 prohibits intentional Mo and requires W 0.50–1.00. Different cold-tool versus carburizing-mould routes; not a near counterpart. JIS annealed delivery, plate/flat acceptance and test regimes differ. The cited JIS sulfur limit is not automatically the ASTM limit.
International / European ISO route No ISO symbol assigned to the cited JIS grade JIS Annex JA.1 informational comparison only; no complete ISO chemical window is asserted identical Confirm actual ISO edition, product form, heat-treatment and acceptance requirements; no direct DIN/ASTM alias is inferred

A681 Table 3 measures minimum response to hardening; JIS G4404 Table 10 and G4403 Table 7 HV values instead define practical-decarburization depth. Those regimes are not interchangeable. Similar principal chemistry does not establish equal manufacturing, cleanliness, carbide distribution or finished-tool performance.

Why choose SHH STEEL for P2

SHH STEEL produces and exports P2 plate against the specified chemistry, delivery condition and inspection plan. We distinguish the supplied mould-stock condition from separately agreed final case/core or treated properties.

  • Identify the correct ASTM edition and chemical footnotes.
  • Keep plate dimensions, finish and machining allowance explicit.
  • Agree hardness acceptance without inventing an excluded specimen test.
  • Maintain heat traceability and inspection documentation.

Enquiry and inspection planning for P2

Enquiry item What to specify
Type / edition P2, ASTM edition and any additional drawing specification
Dimensions Plate/flat, thickness × width × length, quantity, finish and machining allowance
Supply / acceptance Annealed: 100 BHN maximum, Table 2; final carburized condition separately specified
Final mould basis Intended duty and applicable source for final properties or subsequent treatment
Inspection Heat analysis, agreed supply hardness, dimensions, surface/decarburization and additional NDT if specified
Reporting / delivery Required reports, heat identification, destination, packing and target timing

No numerical finished-mould property, stock size or process capability is guaranteed without enquiry review.

FAQ

What distinguishes P2?
Table 1 specifies carbon 0.10 % maximum, chromium 0.75–1.25 %, molybdenum 0.15–0.40 % and nickel 0.10–0.50 %. The standard identifies P2–P6 as used in the carburized condition; neither case depth nor final case/core hardness is assigned by a Table 3 response row.
What supplied hardness does the reference specify?
Annealed: 100 BHN maximum, Table 2; final carburized condition separately specified. This is not a final-mould performance guarantee.
What is the minimum Table 3 response HRC?
P-type response testing is excluded by Table 3 note 4; no type-specific test cycle or minimum HRC is assigned here. Use the type-specific condition and agreed final acceptance rather than importing another tool family test.
Does the reference include mould plate or only bars?
Clause 1.2 includes wrought plate. Use the applicable plate/flat dimensional and finish rules; do not transfer bar tolerances or another type specimen requirement to the plate.
Is the foreign comparison a direct substitute?
Different cold-tool versus carburizing-mould routes; not a near counterpart. JIS SKS3 C 0.90–1.00 versus P2 C 0.10 maximum. P2 requires Mo 0.15–0.40; SKS3 prohibits intentional Mo and requires W 0.50–1.00. Compare chemistry, product form, delivery condition and final acceptance before substitution.

Request a quotation

Request a quotation for ASTM A681 P2 mould steel plate or flat stock. Send the required edition, dimensions, quantity, finish and machining allowance, together with the drawing and intended mould duty. Identify the supplied condition explicitly: Annealed: 100 BHN maximum, Table 2; final carburized condition separately specified.

Specify the governing hardness acceptance and reporting basis rather than copying a generic tool-steel HRC range. P-type response testing is excluded in the reference; no absent specimen cycle is assumed. For final carburized or otherwise treated mould requirements, identify the applicable source and agree case/core properties, treatment responsibility and inspection stages separately.

Include the full chemical requirements and any supplementary quality criteria, heat-traceability needs, surface or decarburization acceptance and any NDT method with its acceptance criteria. For a proposed foreign substitute, provide the complete governing specification and drawing for review of chemistry, form and condition differences.

State whether dimensions are raw blanks or finished sizes; include cutting details, inspection reports, destination, packing and target timing. Any requested process or dimension is reviewed for feasibility before confirmation.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X