Product Showcase
ASTM A681 Carbon Steel Plates
SHH STEEL offers ASTM A681-compliant alloy tool steels like O1/D2/H13. ASTM A681 specifies carbon and alloy tool steels for cold/hot work dies, punches, and shear blades. High hardness, wear-resistant, certified quality, competitive prices, customizable. Trust SHH STEEL!
-
ASTM A681 H42 Tool Steel Plate
ASTM A681 H42 is tungsten-molybdenum hot-work tool steel for high-alloy hot-work die inserts. Its carbon range is 0.55–0.70 %, with alloy limits that distinguish it from neighboring die steels. Plate and flat blanks are selected by chemistry, delivery condition, surface quality and heat-treatment response rather than by a generic tool-steel nickname. Final tooling performance also depends on section, cooling and the qualified temper. SHH STEEL produces and exports H42 plate to the specified edition, dimensions and inspection requirements.View More -
ASTM A681 H41 Tool Steel Plate
ASTM A681 H41 is molybdenum-rich hot-work tool steel for hot-work inserts requiring the low-carbon HSS-derived alloy balance. Its carbon range is 0.60–0.75 %, with alloy limits that distinguish it from neighboring die steels. Plate and flat blanks are selected by chemistry, delivery condition, surface quality and heat-treatment response rather than by a generic tool-steel nickname. Final tooling performance also depends on section, cooling and the qualified temper. SHH STEEL produces and exports H41 plate to the specified edition, dimensions and inspection requirements.View More -
ASTM A681 H26 Tool Steel Plate
ASTM A681 H26 is very-high-tungsten hot-work tool steel for thermal wear-loaded hot-work dies. Its carbon range is 0.45–0.55 %, with alloy limits that distinguish it from neighboring die steels. Plate and flat blanks are selected by chemistry, delivery condition, surface quality and heat-treatment response rather than by a generic tool-steel nickname. Final tooling performance also depends on section, cooling and the qualified temper. SHH STEEL produces and exports H26 plate to the specified edition, dimensions and inspection requirements.View More -
ASTM A681 H25 Tool Steel Plate
ASTM A681 H25 is lower-carbon high-tungsten hot-work tool steel for hot extrusion and press-tool inserts. Its carbon range is 0.22–0.32 %, with alloy limits that distinguish it from neighboring die steels. Plate and flat blanks are selected by chemistry, delivery condition, surface quality and heat-treatment response rather than by a generic tool-steel nickname. Final tooling performance also depends on section, cooling and the qualified temper. SHH STEEL produces and exports H25 plate to the specified edition, dimensions and inspection requirements.View More -
ASTM A681 H24 Tool Steel Plate
ASTM A681 H24 is high-tungsten hot-work tool steel for hot press and extrusion tooling. Its carbon range is 0.42–0.53 %, with alloy limits that distinguish it from neighboring die steels. Plate and flat blanks are selected by chemistry, delivery condition, surface quality and heat-treatment response rather than by a generic tool-steel nickname. Final tooling performance also depends on section, cooling and the qualified temper. SHH STEEL produces and exports H24 plate to the specified edition, dimensions and inspection requirements.View More -
ASTM A681 H23 Tool Steel Plate
ASTM A681 H23 is high-chromium high-tungsten hot-work tool steel for hot extrusion inserts and thermal wear-loaded tooling. Its carbon range is 0.25–0.35 %, with alloy limits that distinguish it from neighboring die steels. Plate and flat blanks are selected by chemistry, delivery condition, surface quality and heat-treatment response rather than by a generic tool-steel nickname. Final tooling performance also depends on section, cooling and the qualified temper. SHH STEEL produces and exports H23 plate to the specified edition, dimensions and inspection requirements.View More -
ASTM A681 A2 Tool Steel Plate
ASTM A681 A2 is air-hardening chromium-molybdenum cold-work tool steel for cold blanking dies, punches, gauges and shear blades. Its carbon range is 0.95–1.05 %, with alloy limits that distinguish it from neighboring die steels. Plate and flat blanks are selected by chemistry, delivery condition, surface quality and heat-treatment response rather than by a generic tool-steel nickname. Final tooling performance also depends on section, cooling and the qualified temper. SHH STEEL produces and exports A2 plate to the specified edition, dimensions and inspection requirements.View More -
ASTM A681 H22 Tool Steel Plate
ASTM A681 H22 is high-tungsten hot-work tool steel for hot extrusion and thermal wear-loaded die inserts. Its carbon range is 0.30–0.40 %, with alloy limits that distinguish it from neighboring die steels. Plate and flat blanks are selected by chemistry, delivery condition, surface quality and heat-treatment response rather than by a generic tool-steel nickname. Final tooling performance also depends on section, cooling and the qualified temper. SHH STEEL produces and exports H22 plate to the specified edition, dimensions and inspection requirements.View More -
ASTM A681 H21 Tool Steel Plate
ASTM A681 H21 is tungsten-rich hot-work tool steel for hot press dies and extrusion tools. Its carbon range is 0.26–0.36 %, with alloy limits that distinguish it from neighboring die steels. Plate and flat blanks are selected by chemistry, delivery condition, surface quality and heat-treatment response rather than by a generic tool-steel nickname. Final tooling performance also depends on section, cooling and the qualified temper. SHH STEEL produces and exports H21 plate to the specified edition, dimensions and inspection requirements.View More -
ASTM A681 H19 Tool Steel Plate
ASTM A681 H19 is cobalt-tungsten-vanadium hot-work tool steel for hot-work dies and highly alloyed extrusion inserts. Its carbon range is 0.32–0.45 %, with alloy limits that distinguish it from neighboring die steels. Plate and flat blanks are selected by chemistry, delivery condition, surface quality and heat-treatment response rather than by a generic tool-steel nickname. Final tooling performance also depends on section, cooling and the qualified temper. SHH STEEL produces and exports H19 plate to the specified edition, dimensions and inspection requirements.View More -
ASTM A681 H14 Tool Steel Plate
ASTM A681 H14 is tungsten-bearing chromium hot-work tool steel for hot-work inserts and thermal wear-loaded tooling. Its carbon range is 0.35–0.45 %, with alloy limits that distinguish it from neighboring die steels. Plate and flat blanks are selected by chemistry, delivery condition, surface quality and heat-treatment response rather than by a generic tool-steel nickname. Final tooling performance also depends on section, cooling and the qualified temper. SHH STEEL produces and exports H14 plate to the specified edition, dimensions and inspection requirements.View More -
ASTM A681 H13 Tool Steel Plate
ASTM A681 H13 is chromium-molybdenum-vanadium hot-work tool steel for die-casting dies, extrusion inserts and hot press tools. Its carbon range is 0.32–0.45 %, with alloy limits that distinguish it from neighboring die steels. Plate and flat blanks are selected by chemistry, delivery condition, surface quality and heat-treatment response rather than by a generic tool-steel nickname. Final tooling performance also depends on section, cooling and the qualified temper. SHH STEEL produces and exports H13 plate to the specified edition, dimensions and inspection requirements.View More
ASTM A681 Carbon Steel Plates
Tool and Die Steel Plates
SHH STEEL, a leading Tool and Die Steel Plates exporter, produces and exports tool and die steel plates for mold-making, tooling, and automotive applications. Our plates, such as D2 and P20, ensure durability and machinability, meeting global standards. With a 5,000-ton inventory, we provide 3–5 day delivery for in-stock items, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for tool steel plates and custom precision manufacturing solutions.
Tool and Die Steel Plates