ASTM A533 Type C Class 3 Steel Plate | A533 Gr.C Cl.3 Mn-Mo-Ni Vessel Plate | ASTM A533 Steel - SHH STEEL

ASTM A533 Type C Class 3 Steel Plate | A533 Gr.C Cl.3 Mn-Mo-Ni Vessel Plate

ASTM A533 Type C Class 3 is a quenched and tempered Mn-Mo-Ni alloy steel plate for welded pressure vessels to ASTM A533/A533M-24. Type C carries 0.70–1.00 % nickel. Class 3 requires 100 to 125 ksi [690 to 860 MPa] tensile strength. SHH STEEL produces and exports this plate to the ordered thickness, tests and inspection document.
Equivalent Grades:
Code companion: ASME SA-533 Type C Class 3. Not automatic substitutes.
Heat Treatment
Water quenched from 845–980 °C and tempered at 595 °C minimum; Class 3 690 to 860 MPa.
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is ASTM A533 Type C Class 3 steel plate?

ASTM A533 Type C Class 3 is a quenched and tempered Mn-Mo-Ni alloy steel plate to ASTM A533/A533M-24, Standard Specification for Pressure Vessel Plates, Alloy Steel, Quenched and Tempered, Manganese-Molybdenum and Manganese-Molybdenum-Nickel. The specification is written for the construction of welded pressure vessels. Type C is one of the four Mn-Mo-Ni types; its nickel range is 0.70–1.00 % by heat analysis.

A533/A533M-24 was approved on 1 March 2024 and published in March 2024, replacing A533/A533M-16. It covers five types, A, B, C, D and E, each available in three strength classes. The type fixes the chemistry; the class fixes the tensile strength window. Class 3 requires a tensile strength of 100 to 125 ksi [690 to 860 MPa].

For ASME Boiler and Pressure Vessel Code construction, ASTM refers users to SA-533/SA-533M in Section II of the Code. The related Code page is ASME SA533 Type C Class 3. The two designations are closely related, but a certificate to one does not automatically satisfy an order written to the other.

SHH STEEL produces and exports ASTM A533 Type C Class 3 plate as a producer, exporter and mill agent, to the type, class, thickness, supplementary requirements and inspection document written on the enquiry. The grade sits in our ASTM A533 range under Nuclear-Grade Steel Plates. Other classes of the same type are ASTM A533 Type C Class 1, ASTM A533 Type C Class 2.

Material specification for ASTM A533 Type C Class 3

The table summarises the specification items that apply to this type and class. Plate dimensions are agreed per order; no stock range is implied.

Parameter Detail
Specification ASTM A533/A533M-24
Type and class Type C (Mn-Mo-Ni), Class 3
Product form Alloy steel plates for welded pressure vessels
General requirements ASTM A20/A20M (testing, retesting, dimensional variations, quality and repair of defects, marking, loading, ordering)
Steelmaking Killed steel meeting the fine austenitic grain size requirement of A20/A20M
Heat treatment Heated to 1550 °F to 1800 °F [845 °C to 980 °C], water quenched, tempered at not less than 1100 °F [595 °C]
Tensile strength (Class 3) 100 to 125 ksi [690 to 860 MPa]
Thickness (scope) For Type C Class 3, the maximum thickness is 2 1/2 in. [65 mm]; minimum nominal thickness 0.25 in. [6.5 mm] for all classes
Units Inch-pound (A533) or SI (A533M), used independently
Our supply We produce and export ASTM A533 Type C Class 3 plate to the thickness and tests written on the order

Chemical composition of ASTM A533 Type C Class 3

Heat analysis and product analysis shall meet Table 1 of A533/A533M-24 for Type C. The class does not change the chemistry, except for the manganese allowance described below.

Element Type C heat analysis, % Type C product analysis, %
Carbon, max 0.25 0.25
Manganese 1.15–1.50 1.07–1.62
Phosphorus, max 0.025 0.025
Sulfur, max 0.025 0.025
Silicon 0.15–0.40 0.13–0.45
Molybdenum 0.45–0.60 0.41–0.64
Nickel 0.70–1.00 0.67–1.03
Chromium No requirement No requirement

Carbon, phosphorus and sulfur limits apply to both heat and product analyses. For Types A, B, C and D, the maximum manganese may be increased to 1.60 % on heat analysis and 1.65 % on product analysis when Class 2 or Class 3 properties are specified and Supplementary Requirement S3 of A20/A20M is specified with a total holding time of more than 1 h/in. [2.4 min/mm] of thickness. It applies only when the order invokes it.

Mechanical properties of ASTM A533 Type C Class 3

Tension tests follow A20/A20M. The Class 3 tensile strength window is stated in the scope of A533/A533M-24 and is shown below. Minimum yield strength and elongation are taken from Table 2 of A533/A533M-93 (reapproved 2004), which lists the same class requirements used in ASME SA-533. Elongation is subject to the A20/A20M adjustment in that table’s footnote. Confirm the figures against Table 2 of the 2024 edition cited on the purchase order.

Property Class 3 requirement
Tensile strength 100 to 125 ksi [690 to 860 MPa]
Yield strength, min 83 ksi [570 MPa]
Elongation in 2 in. [50 mm], min 16%, subject to A20/A20M adjustments
Charpy V-notch impact Not a base requirement; ordered as a supplementary requirement with temperature, energy, orientation and location
Drop-weight test Only when ordered as a supplementary requirement

For comparison, Table 2 of A533/A533M-93(2004) requires Class 1: 80 to 100 ksi [550 to 690 MPa], 50 ksi [345 MPa] min yield, 18% min elongation; Class 2: 90 to 115 ksi [620 to 795 MPa], 70 ksi [485 MPa] min yield, 16% min elongation; Class 3: 100 to 125 ksi [690 to 860 MPa], 83 ksi [570 MPa] min yield, 16% min elongation. A plate tested to one class should not be re-stamped to a higher class.

Heat treatment and delivery condition of ASTM A533 Type C Class 3

All A533 plates are delivered heat treated. The specification requires heating to a suitable temperature in the range 1550 °F to 1800 °F [845 °C to 980 °C], holding to obtain uniform temperature through the thickness, quenching in water, and tempering at a temperature that develops the specified properties but not less than 1100 °F [595 °C], held for at least 1/2 h/in. [1.2 min/mm] of thickness and not less than 1/2 h.

  • Condition: quenched and tempered, Type C Class 3
  • Heat treatment by the fabricator is possible under the specification’s own clause and must be agreed and stated on the order
  • In the as-rolled condition these alloy plates are sensitive to cracking during transit and handling, particularly above 1 in. [25 mm]; as-rolled shipment only by mutual agreement of manufacturer and purchaser
  • Supplementary requirements such as simulated post-weld heat treatment of test coupons, ultrasonic examination, Charpy V-notch or drop-weight testing and vacuum treatment apply only when ordered

Welding ASTM A533 Type C Class 3 plate

A533 plates are intended for welded pressure vessels. ASTM A533 Type C Class 3 is a quenched and tempered Mn-Mo-Ni steel, so the welding procedure should be qualified on the actual type, class and thickness, with controlled preheat, interpass temperature and heat input to avoid degrading the quenched and tempered properties and to limit hydrogen cracking risk in heavy sections.

Post-weld heat treatment should stay below the tempering temperature used for the plate. Where the vessel will be stress relieved, order simulated post-weld heat treatment of the mechanical test coupons so the certificate reflects the fabricated condition. Higher classes and thicker sections need closer control.

Dimensions, thickness limits and examination

Permitted variations in dimensions and mass, quality and repair of defects, and marking follow ASTM A20/A20M, as A533 refers to it for these requirements.

Item Requirement
Thickness, width, length, flatness ASTM A20/A20M permitted variations for the ordered size
Thickness limit (this type and class) 2 1/2 in. [65 mm] (specification maximum, Class 3)
Minimum nominal thickness 0.25 in. [6.5 mm]
Ultrasonic examination A435/A435M, A577/A577M or A578/A578M only when ordered as a supplementary requirement
Repair of defects Per A20/A20M

Applications and specification limits

ASTM A533 Type C Class 3 plate is used for shells, heads and other pressure parts of welded pressure vessels that call for quenched and tempered Mn-Mo-Ni strength in heavy sections. The specification notes that A533 plates are often used in the beltline region of nuclear reactor vessels, where material properties may be affected by high levels of radiation, and its Appendix X1 gives information pertinent to that usage.

Listing this specification in our ASTM A533 range under the Nuclear-Grade Steel Plates family is a catalogue grouping only. It is not a nuclear qualification, an RCC-M qualification or an ASME Section III certification of SHH STEEL, of the mill or of any heat. Where plate is intended for nuclear construction, the Code edition, material organisation and quality-system rules, fracture-toughness testing and project chemistry limits must be written on the purchase order and confirmed before acceptance.

  • Thickness: 2 1/2 in. [65 mm] (specification maximum) for Type C Class 3
  • Design stresses come from the construction code named on the order, not from this page
  • Impact, drop-weight or radiation-related chemistry controls must be ordered explicitly

Compare ASTM A533 Type C Class 3 with related vessel plates

Within A533, the type and class must both match the drawing. A Type C heat cannot be certified as another type, and a Class 3 test result cannot be re-stamped to another class. Related specifications may look similar on one property but differ in chemistry, heat treatment or test basis, so none is an automatic substitute.

Grade Route and chemistry Tensile strength Relation
ASTM A533 Type C Class 3 QT Mn-Mo-Ni 100 to 125 ksi This page
ASTM A533 Type C Class 1 QT Mn-Mo-Ni 80 to 100 ksi Same chemistry, different class
ASTM A533 Type C Class 2 QT Mn-Mo-Ni 90 to 115 ksi Same chemistry, different class
ASTM A533 Type A Class 3 QT Mn-Mo, no Ni requirement 100 to 125 ksi Same class, different chemistry
ASTM A533 Type B Class 3 QT Mn-Mo-Ni, Ni 0.40–0.70 100 to 125 ksi Same class, different chemistry
ASTM A533 Type D Class 3 QT Mn-Mo-Ni, Ni 0.20–0.40 100 to 125 ksi Same class, different chemistry
ASTM A533 Type E Class 3 QT Mn-Mo-Ni, Ni 0.60–1.00 100 to 125 ksi Same class, different chemistry
ASTM A302 Grade B Mn-Mo plate under its own specification Different specification Not a substitute
ASTM A302 Grade C Mn-Mo-Ni plate under its own specification Different specification Not a substitute
ASTM A537 Class 2 QT C-Mn-Si plate Different specification Not a substitute

For forged components of similar Mn-Mo-Ni vessels, see ASTM A508/A508M Pressure Vessel Forgings; forgings are a different product form and are not interchangeable with plate.

Equivalent and related grades for ASTM A533 Type C Class 3

Equivalents below are engineering judgement only and are not automatic substitutes. Each has its own chemistry, heat treatment, test and certification rules; an equivalence must be approved by the designer or the code authority for the project. Where no live page exists, the grade is given as plain text.

Region Grade Note
USA (ASME) ASME SA533 Type C Class 3 Code companion, closely related
France (nuclear) Mn-Ni-Mo grades such as 18MND5 procured to their own RCC-M procurement specifications (plain text) Different code and requirements; not a substitute

Why choose SHH STEEL for ASTM A533 Type C Class 3

  • SHH STEEL produces and exports ASTM A533 Type C Class 3 quenched and tempered plate as a producer, exporter and mill agent
  • We keep ASTM A533 and ASME SA-533 designations distinct and quote dual certification only when confirmed
  • We check type chemistry and class tensile windows against A533/A533M-24 before quoting
  • We do not present the Nuclear-Grade Steel Plates listing as a nuclear qualification
  • We match the inspection document and supplementary tests to the purchase order

How to enquire for ASTM A533 Type C Class 3

Send the following with your enquiry so the plate can be reviewed before production.

Item What to state
Specification ASTM A533/A533M-24, Type C, Class 3
Size Thickness, width, length and quantity
Supplementary requirements For example simulated PWHT of coupons, Charpy V-notch, drop-weight, ultrasonic examination, vacuum treatment, S3 manganese allowance where applicable
Code and project rules Any ASME, nuclear or project requirements, written on the order
Documentation Inspection document required, for example EN 10204 3.1 or 3.2

We also process plate by cutting, bevelling and other services when they are written on the order.

FAQ

What is ASTM A533 Type C Class 3?
A quenched and tempered Mn-Mo-Ni alloy steel plate for welded pressure vessels to A533/A533M-24. Type C sets the chemistry and Class 3 sets the 100 to 125 ksi [690 to 860 MPa] tensile strength window.
Is Type C a nickel-bearing type?
Yes. Type C requires 0.70–1.00 % nickel by heat analysis.
What thickness does the specification allow?
For Type C Class 3, the maximum thickness is 2 1/2 in. [65 mm]. The minimum nominal thickness for all classes is 0.25 in. [6.5 mm]. Actual sizes are agreed per order.
Is ASTM A533 the same as ASME SA-533?
They are closely related; ASTM refers Code users to SA-533/SA-533M in Section II. A dual certificate must be confirmed on the order.
Does an A533 plate qualify for nuclear service?
No plate qualifies just by its specification. A533 plates are often used in reactor vessel beltline regions, but nuclear construction requirements, testing and quality-system rules must be written on the order.

Request a quotation

Contact SHH STEEL for a quotation for ASTM A533 Type C Class 3 quenched and tempered pressure vessel plate. Please send the specification and edition, grade, thickness, width, length, quantity, delivery destination and preferred delivery schedule so we can review your production and export requirements.

If your design also names ASME SA533 Type C Class 3 or a related grade, send the specification set with your enquiry so dual certification and differences can be reviewed.

State any supplementary requirements, simulated post-weld heat treatment, impact testing, ultrasonic examination and the inspection document required, so they are agreed before the order is placed.

For a detailed quotation, email your material specification, drawing, quantity and delivery requirements to our team.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X