Q500ME TMCP Steel Plate GB/T 1591 Supplier
What is Q500ME TMCP Steel Plate GB/T 1591?
Q500ME, also searched as GB/T 1591 Q500ME, Q500ME steel plate, Q500ME TMCP plate and Q500 ME, is the 500 MPa quality-grade-E grade delivered by thermomechanical controlled process in GB/T 1591-2018. Q is the yield symbol, 500 is the thin-plate minimum yield in MPa, M is the delivery letter, and E is the quality letter for Charpy impact at −40°C.
The M is the point of this page. A quenched-and-tempered certificate cannot be stamped ME. That route is GB/T 16270 Q500E. Grade C on the TMCP route is GB/T 1591 Q500MC. Grade D is GB/T 1591 Q500MD. The 460 MPa TMCP sister at the same temperature is GB/T 1591 Q460ME. The full family sits on GB/T 1591. Do not drop a 500 MPa drawing onto a 460 MPa plate, and do not upgrade it to GB/T 16270 Q550E without a price check.
EN 10025-4 stops at S460M and S460ML. There is no S500M. The usual European comparison is EN 10025-6 S500QL, which is quenched and tempered, not TMCP, and is tested at −40°C. EN 10025-6 S500Q is only −20°C. EN 10025-4 S460ML is one yield step lower. EN 10025-6 is the QT book. On the US side, ASTM A572 Grade 70 is 70 ksi / 485 MPa, one step lower, and it is not an ME twin. ASTM A572 Gr.55 is 55 ksi. Dual mark only when both books are fully met. See high strength low alloy plates.
SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. We source Q500ME from first-line structural mills that can actually run the TMCP schedule at 500 MPa and hold −40°C impact, print heat analysis and product analysis when ordered, and ship plate to fabricators in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Related pages include structural steel plates and the products index.
Material Specification
| Specification Element | Requirement | SHH STEEL Compliance |
|---|---|---|
| Plate book | GB/T 1591-2018 Q500ME | Confirmed |
| Other search names | Q500ME steel plate, Q500 ME, Q500ME TMCP | Covered |
| Delivery condition | Thermomechanical controlled process | Confirmed |
| Yield, ≤ 16 mm | 500 MPa min | Confirmed |
| Quality grade | E, impact at −40°C | Confirmed |
| Not this page | GB/T 16270 Q500E | QT, different book |
| Warmer TMCP sister | GB/T 1591 Q500MD | −20°C |
| EN comparison | EN 10025-6 S500QL is QT | Not a swap |
| US comparison | ASTM A572 Gr.70 is 485 MPa | Not a twin |
| Product analysis | GB/T 222 column when ordered | Confirmed |
| Supply role | Global steel mill sourcing partner | SHH STEEL |
| Certification | EN 10204 3.1 or 3.2 | As ordered |
Nearby pages that buyers compare, but must not swap blindly, include GB/T 1591 Q460ME, GB/T 16270 Q500C and ASTM A572 Gr.55.
Chemical Composition
Heat analysis is the mill ladle table in GB/T 1591-2018 for TMCP Q500. Product analysis, when ordered, follows GB/T 222. Q500ME is a microalloyed HSLA plate. Grade E is the tightest cleanliness letter on this TMCP family, because the impact test is at −40°C. Mills may add Nb, V or Ti, and some heats use nickel, chromium or molybdenum to hold the 500 MPa window. The certificate shows the elements actually used. TMCP chemistry is often leaner than a QT heat of the same yield, because the rolling schedule does part of the strengthening.
Heat Analysis and Product Analysis — GB/T 1591 Q500ME, TMCP
| Element | Heat analysis (%) | Product analysis (%) |
|---|---|---|
| Carbon (C), max | 0.18 | 0.20 |
| Silicon (Si), max | 0.60 | 0.65 |
| Manganese (Mn), max | 1.80 | 1.90 |
| Phosphorus (P), max | 0.020 | 0.025 |
| Sulfur (S), max | 0.015 | 0.020 |
| Niobium (Nb), max | 0.11 | 0.12 |
| Vanadium (V), max | 0.12 | 0.13 |
| Titanium (Ti), max | 0.20 | 0.21 |
| Chromium (Cr), max | 0.60 | 0.65 |
| Nickel (Ni), max | 0.80 | 0.85 |
| Copper (Cu), max | 0.55 | 0.60 |
| Molybdenum (Mo), max | 0.20 | 0.21 |
| Nitrogen (N), max | 0.015 | 0.017 |
| Aluminium (Als), min when used | 0.015 | 0.010 |
Carbon equivalent is limited by thickness in the standard. The M route often has a lower CEV window than quenched-and-tempered GB/T 16270 Q500E. If the purchase order writes product analysis, SHH STEEL prints both columns and the thickness band used for the tensile test. A 460 MPa file is GB/T 1591 Q460ME, not this grade.
Mechanical Properties
Buyers search Q500ME mechanical properties, Q500ME yield strength, GB/T 1591 Q500ME tensile and Q500ME impact −40°C.
Tensile and impact — GB/T 1591 Q500ME, TMCP
| Thickness | Yield min | Tensile | Elongation min | Impact |
|---|---|---|---|---|
| ≤ 16 mm | 500 MPa | 610–770 MPa | 17% | −40°C, grade E |
| > 16–40 mm | 480 MPa | 600–760 MPa | 17% | −40°C, grade E |
| > 40–63 mm | 470 MPa | 590–750 MPa | 16% | −40°C, grade E |
| > 63–80 mm | 450 MPa | 570–730 MPa | 16% | −40°C, grade E |
| > 80–100 mm | 440 MPa | 560–720 MPa | 16% | −40°C, grade E |
Impact energy is the average of three longitudinal Charpy V-notch specimens, commonly 27 J to 34 J minimum at −40°C, depending on the ordered edition and thickness. One value may fall below the table, but not below 70% of that value. Write a higher energy on the order if the owner requires it. Not every TMCP heat will hold E on thick plate. SHH STEEL confirms the thickness before promising the letter.
Yield steps down with thickness. A 500 MPa name on 12 mm plate is not the minimum on a 40 mm flange. 500 MPa is about 72.5 ksi. ASTM A572 Grade 70 is 70 ksi and is not this book. Density is 7.85 g/cm³. Hardness is not a design value for this grade. Z15, Z25 or Z35 through-thickness tensile is an extra, not part of the E letter.
Material Comparison
| Grade | Book | Delivery | Yield, thin plate | Impact | Swap? |
|---|---|---|---|---|---|
| GB/T 16270 Q500E | GB/T 16270 | QT | 500 MPa | −40°C | Different process |
| GB/T 1591 Q500MD | GB/T 1591-2018 | TMCP | 500 MPa | −20°C | Warmer M sister |
| Q500ME | GB/T 1591-2018 | TMCP | 500 MPa | −40°C | This page |
| GB/T 1591 Q460ME | GB/T 1591-2018 | TMCP | 460 MPa | −40°C | Lower yield |
| GB/T 16270 Q550E | GB/T 16270 | QT | 550 MPa | −40°C | Higher yield |
| EN 10025-6 S500QL | EN 10025-6 | QT | 500 MPa | −40°C | Different process |
| EN 10025-4 S460ML | EN 10025-4 | TMCP | 460 MPa | −50°C | Lower yield |
| ASTM A572 Gr.55 | ASTM A572 | As rolled | 380 MPa | Different | Lower yield |
A warmer TMCP file is GB/T 1591 Q500MC. A 420 MPa file is GB/T 1591 Q420ME.
Equivalent Material Grades
There is no official one-to-one substitute for Q500ME. What buyers compare is a 500 MPa TMCP plate tested at −40°C.
EN 10025-4 has no S500M. EN 10025-6 S500QL is the strength comparison at the same impact temperature, but it is quenched and tempered. EN 10025-6 S500Q is only −20°C. EN 10025-4 S460ML is the nearest TMCP book grade and is one step lower. EN 10025-2 S355JR is +20°C and only 355 MPa. In the United States, ASTM A572 Grade 70 is 70 ksi / 485 MPa. ASTM A572 Gr.55 is 55 ksi. ASTM A36 is 36 ksi and is well below this yield. SHH STEEL will not stamp EN 10025-6 S500QL or ASTM A572 Gr.70 on a Q500ME certificate unless the purchase order names both books and both tables are met.
| Designation | Country / region | Standard | Notes |
|---|---|---|---|
| Q500ME | China | GB/T 1591-2018 | Name on this page |
| GB/T 16270 Q500E | China | GB/T 16270 | QT, not this page |
| GB/T 1591 Q500MD | China | GB/T 1591-2018 | TMCP, −20°C |
| GB/T 1591 Q460ME | China | GB/T 1591-2018 | 460 MPa, TMCP |
| EN 10025-6 S500QL | Europe | EN 10025-6 | QT, −40°C |
| EN 10025-4 S460ML | Europe | EN 10025-4 | TMCP, lower yield |
| ASTM A572 Gr.70 | USA | ASTM A572 | 70 ksi, lower yield |
| JIS G3106 SM570 | Japan | JIS G3106 | Lower yield comparison |
Structural Service
Buyers pick Q500ME when a bridge, building member or welded fabrication wants about 500 MPa yield, a TMCP condition, and impact at −40°C. Search phrases such as Q500ME steel plate and GB/T 1591 Q500ME all point here. The family index is GB/T 1591.
It is the wrong plate when the drawing says quenched and tempered. That work is GB/T 16270 Q500E. It is the wrong plate for a −20°C file. That work is GB/T 1591 Q500MD, and the QT sister is GB/T 16270 Q500D. It is the wrong plate for a 0°C file. That work is GB/T 1591 Q500MC. It is the wrong plate for a 460 MPa file. That work is GB/T 1591 Q460ME or GB/T 1591 Q460NE. It is the wrong plate for a 550 MPa file. That work is GB/T 16270 Q550E. It is the wrong plate for a pressure vessel. That work sits on ASTM A516 or pressure vessel steel plates.
SHH STEEL supplies this plate when the drawing names GB/T 1591, quality grade E, and the M condition at 500 MPa.
Weldability
Q500ME is a weldable TMCP HSLA structural plate. Carbon is controlled, and many heats use Nb, V or Ti. A procedure written for ASTM A36 is not a finished WPS for thick Q500ME. Carbon equivalent on the M route is often lower than quenched-and-tempered GB/T 16270 Q500E, which helps the root pass, but the TMCP microstructure still needs a qualified procedure. A procedure qualified only at −20°C may miss the −40°C coupon.
Typical consumables are matching 80 ksi low-hydrogen electrodes or wires. E7018-class electrodes are under-matched if the joint must develop full plate strength. A procedure written for ASTM A572 Gr.55 does not cover 500 MPa. Preheat follows thickness, hydrogen and the approved WPS. Heat input should stay inside the mill window. A very high heat input can soften the TMCP zone next to the weld.
The fabricator owns the WPS. SHH STEEL can share mill heat data, product analysis and carbon equivalent for that review. Do not use a Q500ME procedure on GB/T 1591 Q420MB without checking the lower-yield carbon equivalent. Do not use it on GB/T 1591 Q460MC either if the joint must develop 500 MPa.
Heat Treatment and Delivery Condition
Usual delivery from SHH STEEL for Q500ME is thermomechanical controlled process. The plate is not quenched and tempered as GB/T 16270 Q500E.
TMCP combines controlled rolling and accelerated cooling. Finish rolling is held in the non-recrystallization range, then the plate is cooled on the run-out table to a finish temperature the mill records. Do not order Q500ME as quenched and tempered. That route belongs to GB/T 16270. Stress relief after fabrication, if used, should be agreed before cutting, because a high temper can move the TMCP properties.
The certificate lists GB/T 1591 Q500ME, heat number, delivery condition, heat analysis, product analysis when ordered, tensile by thickness band, and −40°C impact. Certificates may be EN 10204 3.1 or EN 10204 3.2. Dual marking to EN 10025-6 S500QL is available only when both books are fully met. S500QL is not a TMCP grade.
Dimensions
Usual supply range from SHH STEEL for Q500ME steel plate:
- Thickness: commonly 8 mm – 40 mm, heavier plate to 50 mm by mill confirmation
- Width: 1500 mm – 3000 mm, wider by enquiry
- Length: 3000 mm – 12000 mm
Cut-to-size webs, flanges, base plates and gussets are available. Browse more sizes on structural steel plates.
Tolerances
Dimensional limits for Q500ME follow GB/T 709 unless the purchase order names EN 10029 or another table.
Typical thickness tolerance idea for Q500ME plate
| Nominal thickness (mm) | Usual minus (mm) | Usual plus (mm) |
|---|---|---|
| 8 – 15 | −0.3 | +0.8 |
| 15 – 25 | −0.4 | +0.9 |
| 25 – 40 | −0.5 | +1.1 |
| 40 – 50 | −0.6 | +1.3 |
Width on 1500–3000 mm plate is commonly held to about +20 / 0 mm or ±25 mm unless a tighter extra is named. Length on 3000–12000 mm plate is commonly held to about +50 / 0 mm. Flatness follows the agreed class. SHH STEEL will not assume a zero-minus extra on Q500ME unless the order says so.
Supplementary Requirements
Q500ME already defines 500 MPa yield, TMCP delivery and −40°C impact. Extra items still have to be written on the purchase order.
Book name. Write GB/T 1591 Q500ME. Do not write only Q500, and do not write GB/T 16270 if the mill must stamp M. The family page is GB/T 1591.
Impact. Grade E is −40°C. Write a higher energy if the owner requires it. Do not expect this result from GB/T 1591 Q500MD.
Delivery condition. Write thermomechanical controlled process. Write GB/T 16270 Q500E if quenched and tempered is required.
EN or US comparison. Write EN 10025-6 S500QL or ASTM A572 Gr.70 only if dual mark is required and both tables are met. S500QL is QT, not TMCP. Do not treat S500Q as a −40°C grade.
Product analysis. Write it if the file needs the second chemistry column.
Through-thickness. Z15, Z25 or Z35 when the joint is loaded through the thickness.
NDE. UT to GB/T 2970 or the named class.
Identification. Heat number, Q500ME, thickness and mill logo.
Third-party witness. EN 10204 3.2 with SGS, TÜV, BV, ABS or the inspector named.
Applications
| Industry | Typical components |
|---|---|
| Cold-region bridges | Q500ME webs and flanges from SHH STEEL |
| Outdoor structures | Q500ME columns and base plates tested at −40°C |
| Construction machinery | Q500ME frames where the drawing names M and −40°C |
| General fabrication | Q500ME gussets and connection plates |
| Comparison vs EN 10025-4 | Q500ME next to EN 10025-4 S460ML |
| Comparison vs ASTM A572 | Q500ME next to ASTM A572 Gr.55 |
| Lower yield option | GB/T 1591 Q460MF when 460 MPa and −60°C are the file |
Q500ME is the plate for a 500 MPa TMCP file tested at −40°C. It is the wrong plate for a painted weathering facade that needs corten. It is the wrong plate for a 690 MPa QT boom under GB/T 16270. A warmer QT file is GB/T 16270 Q500D.
Supply Capability
SHH STEEL sources Q500ME from first-line Chinese structural mills and ships it on worldwide terms. Partner mills include Wuyang (Wugang), Angang, Shougang, Hanye, Anyang Iron and Steel, Baosteel, Xinyu, Xingcheng and other qualified mills when the size requires it.
Mill test certificates are issued to EN 10204 3.1 as standard. EN 10204 3.2 is arranged when the order names a third-party hold point.
Usual rolling thickness: 8 mm, 10 mm, 12 mm, 16 mm, 20 mm, 25 mm, 30 mm, 40 mm. Heavier plate is confirmed before order.
Processing: CNC or flame cutting, bevel, flattening, shot blast, UT to the named class.
Trade terms: FOB Shanghai main, CIF destination available. Payment: TT, LC, or TT + LC.
Ocean time from Shanghai: US West 14–18 days; US Gulf 28–35 days; Rotterdam / Antwerp 28–35 days; Jebel Ali 18–25 days; Singapore 7–12 days; other ports quoted.
Third-party: SGS, TÜV, BV, ABS, CCS, GL, VL, DNV, RINA, NK, KR, or the inspector named.
Global Delivery and Markets
SHH STEEL is a global steel mill sourcing partner with mill partnerships in China. We supply GB, ASTM, ASME, EN, DIN and JIS steel to buyers in the United States, Europe, the Middle East, Southeast Asia, Africa and South America. Origin is mill-direct, China origin.
SHH STEEL has supplied steel plates to the USA, Mexico, Argentina, Peru, El Salvador, Spain, Netherlands, Germany, UAE, Saudi Arabia, South Africa, India, Thailand, Singapore, Vietnam, the Philippines, Japan and Korea.
Typical lead time: ex-stock 5–7 days when an E heat is in yard; standard TMCP with −40°C test about 35–50 days; 3.2 inspection about 45–55 days.
Why Choose SHH STEEL
SHH STEEL is a global steel mill sourcing partner and steel manufacturer and exporter, mill-direct, China origin. For Q500ME that means mill-direct structural price, not a multi-layer stockist mark-up. We buy from mills that can actually run the TMCP schedule at 500 MPa and test at −40°C, so the M and the E are both on the certificate.
Delivery is short when the size is in rolling range: ex-stock 5–7 days, standard ME heat about 35–50 days, 3.2 inspection about 45–55 days. Cutting, bevel and UT can run in the same window. FOB Shanghai is the main term. CIF to US West, US Gulf, Rotterdam, Jebel Ali and Singapore is quoted on the same file.
Experience on this grade is simple: print GB/T 1591 Q500ME, keep the TMCP route, and do not ship GB/T 16270 Q500E or GB/T 1591 Q500MD as ME. We will not drop the M to save a cooling cycle, and we will not change E to D to save a cold test. If the drawing needs quenched and tempered plate, we will move the inquiry to Q500E under GB/T 16270. If the drawing needs 460 MPa, we will move it to GB/T 1591 Q460MF or GB/T 1591 Q460NC.
FAQ
-
What is Q500ME steel plate?
- Q500ME in GB/T 1591-2018 is thermomechanical controlled process high-strength low-alloy plate with 500 MPa minimum yield on thin plate and Charpy impact at −40°C. SHH STEEL supplies this plate worldwide as a global steel mill sourcing partner.
-
Is Q500ME the same as GB/T 16270 Q500E?
- No. Both can yield at 500 MPa and both can be tested at −40°C. GB/T 16270 Q500E is quenched and tempered. Q500ME is TMCP.
-
Is Q500ME the same as Q500MD?
- No. Both are TMCP. Q500MD is tested at −20°C. Q500ME is tested at −40°C.
-
Is Q500ME the same as Q460ME?
- No. Both are TMCP and both are tested at −40°C. Q460ME is 460 MPa. Q500ME is 500 MPa.
-
What is the European equivalent of Q500ME?
- There is no S500M in EN 10025-4. The strength comparison is EN 10025-6 S500QL, which is quenched and tempered and tested at −40°C. Dual mark only when both books are fully met.
-
What is the US equivalent of Q500ME?
- There is no official ASTM twin. ASTM A572 Grade 70 is 70 ksi / 485 MPa, slightly lower, and it does not carry an ME letter. SHH STEEL does not dual-mark ASTM A572 unless both books are met.
Conclusion
Q500ME steel plate to GB/T 1591 is 500 MPa TMCP structural plate with impact at −40°C. It is not quenched-and-tempered GB/T 16270 Q500E. EN 10025-4 has no S500M. EN 10025-6 S500QL is the strength comparison and is QT. ASTM A572 Grade 70 is 485 MPa and is not a substitute. Whether the inquiry says Q500ME, GB/T 1591 Q500ME or Q500ME TMCP plate, SHH STEEL as a global steel mill sourcing partner supplies plate with Q500ME chemistry, heat and product analysis as ordered, GB/T 709 tolerances and EN 10204 3.1 or 3.2 certification.
SHH STEEL supplies Q500ME Steel Plate to the United States, Europe, the Middle East, Africa, Asia and the Americas for work that actually names the M condition. The grade family is listed on GB/T 1591.
Contact SHH STEEL for mill rolling, −40°C impact, cutting, UT, 3.2 inspection or a worldwide quotation.