LR FH40 marine steel plate per Lloyd's Register (LR) rules at SHH STEEL warehouse

LR FH40 Steel Plate | LR/FH40 Marine Steel Plate

LR LR/FH40 (FH40) higher-strength hull structural steel plate, yield 390 N/mm², tensile 510–650 N/mm², Charpy at −60 °C, stamped LR FH40 / LR/FH40 with Lloyd’s Register–endorsed certificates. SHH STEEL supplies stock and mill-roll plate in China with cutting, multi-class and 3.2 inspection.
Keywords
LR FH40 steel plate, LR/FH40 marine steel plate, LR FH40 shipbuilding plate, FH40 hull steel, Lloyd's Register FH40 plate, AH/DH/EH/FH 40 marine plate
Equivalent Grades:
ASTM A131 Grade FH40; ABS FH40; DNV NV F40; BV Grade FH40; CCS FH40; NK KF40; KR RF40; RINA Grade FH40; GB 712 Grade FH40
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Impact Test and Condition of Supply
Thickness Tolerance
Stock
Equivalent Grades
Grade Selection
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

What is LR FH40 / LR/FH40 marine steel plate?

Technical Reviewer: Jack | SHH STEEL Material Solutions Department · Updated: 2026-10-27

LR FH40, often written LR/FH40 on mill certificates and plate markings, is a higher-strength hull structural steel under Lloyd’s Register Rules for the Manufacture, Testing and Certification of Materials, which implement IACS UR W11 for the AH–FH 32/36/40 family. Strength level 40 means minimum yield 390 N/mm², tensile 510–650 N/mm² and elongation 20 % min. (A5). The letter FH fixes Charpy V-notch testing at −60 °C. In commercial enquiries it is called LR FH40 or LR/FH40 marine steel plate.

Equivalent grades: LR FH40 ≈ ASTM A131 Grade FH40 ≈ ABS FH40 ≈ DNV NV F40 ≈ BV FH40 ≈ CCS F40 / FH40 ≈ NK KF40 ≈ KR RF40 ≈ RINA FH40 ≈ GB 712 Grade FH40 (all class-approved, stamped by the issuing society).

LR/FH40 is selected when scantlings need the higher yield of the 40 band and the material class assigns −60 °C toughness. Ordinary-strength LR Grade A–E stay at 235 N/mm² yield and cannot replace FH40 without a drawing change. Within the 40 band, letter choice is toughness: AH 0 °C → DH −20 °C → EH −40 °C → FH −60 °C; within the FH letter, strength steps 32 → 36 → 40 raise yield from 315 to 355 to 390 N/mm².

Plates that pass mill tests under Lloyd’s Register survey are die-stamped or stencilled LR FH40 or LR/FH40 (plus Z or U where through-thickness or ultrasonic requirements apply) and are supplied with a mill certificate the LR Surveyor endorses. SHH STEEL supplies LR/FH40 from Chinese mills that hold Lloyd’s Register works approval for the grade, from stock in common sizes or from a mill rolling cycle, with LR survey arranged at the mill.

LR LR/FH40 plate: specification summary

ItemLR LR/FH40 / FH40 data
Rule basisLloyd’s Register Rules for Materials; IACS UR W11 higher-strength Grade FH40
Strength levelhigher strength 40, yield 390 N/mm² min., tensile 510–650 N/mm²
Toughness classFH → Charpy at −60 °C
Plate thickness primarily coveredup to 100 mm under IACS UR W11 scope for plates; greater thickness by special consideration (see UNCERTAIN)
Deoxidationkilled, fine grain practice (UR W11)
Impact testCharpy V at −60 °C; frequency and supply condition per UR W11 tables
MarkingLR FH40 / LR/FH40; plus Z / U / TM where ordered and qualified
TMCP Ceq (indicative UR W11 / industry practice)≤ 0.40 % for t ≤ 50 mm; ≤ 0.42 % for 50 < t ≤ 100 mm (TM steels) — confirm on mill approval / PO
Thickness toleranceIACS UR W13 as adopted by LR (minus tolerance commonly 0.3 mm class — confirm on PO; see UNCERTAIN)
Certificatemill certificate endorsed by the LR Surveyor; EN 10204 3.1 / 3.2 on request

Size range. Common market thicknesses for FH40 are about 6–80 mm (heavier plates available as per mill approval), widths 1500–3500 mm. Exact maximum thickness for a given delivery condition is as per standard and mill certificate / LR works approval. Ask for confirmation above 100 mm.

LR FH40 / LR/FH40 chemical composition (heat and product analysis)

ElementHeat (ladle) analysis, %Product (check) analysis, %Note
C0.16 max.numeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificateFH group
Mn0.90–1.60numeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificate
Si0.10–0.50numeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificatemin. waived if acid-soluble Al ≥ 0.015 %
P0.025 max.numeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificatetighter for FH
S0.025 max.numeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificatetighter for FH
Al (acid soluble) min.0.015 min. acid-solublenumeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificategrain refining
Nb0.02–0.05 when used singlynumeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificatewhen used singly; combined minima in UR W11
V0.05–0.10 when used singlynumeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificatewhen used singly
Ti0.02 max.numeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificateneed not be reported unless intentionally added
Cu0.35 max.numeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificate
Cr0.20 max.numeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificate
Ni0.80 max.numeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificateFH allows higher Ni than AH/DH/EH
Mo0.08 max.numeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificate
N0.009 max. (0.012 if Al present)numeric tolerance not tabulated in LR Rules for Materials – agree on order / mill certificateFH specifies N max.

Product (check) analysis column: LR Rules for Materials specify heat (ladle) limits; no numeric product-analysis tolerance is tabulated in the rule text reviewed, so product (check) limits are agreed on the order or taken from the approved mill specification and certificate.

Source: IACS UR W11 higher-strength chemistry tables (ladle samples) — the chemistry Lloyd’s Register applies to LR/FH40. AH/DH/EH share one chemistry column; FH is tighter on C, P, S and adds N control with higher Ni allowance. Toughness is differentiated by impact temperature and supply routes, not by separate C/Mn caps within AH/DH/EH. Product (check) analysis numeric tolerances are not tabulated in UR W11; when required, agree tolerances at enquiry. TMCP steels must also meet the applicable Ceq / Pcm limits on the mill approval — ask for Ceq on the certificate.

LR LR/FH40 tensile properties

PropertyRequirement (IACS UR W11)
Tensile strength Rm510–650 N/mm²
Yield strength ReH390 N/mm² min.
Elongation A520 % min.
Impact test temperature−60 °C

Alternative flat-specimen elongations by thickness (indicative UR W11 / industry table for strength 40):

Thickness (mm)≤5>5–10>10–15>15–20>20–25>25–30>30–40>40–50
Elongation min. %1214151617181920

Same tensile band applies to AH/DH/EH/FH 40; only impact temperature and chemistry group (FH vs AH/DH/EH) change across the letter.

LR LR/FH40: Charpy at −60 °C and supply condition

ThicknessLong. avg. at −60 °CTrans. avg. at −60 °C
t ≤ 50 mm39 J26 J
50 < t ≤ 70 mm46 J31 J
70 < t ≤ 100 mm55 J37 J

Source: IACS UR W11 impact table for higher-strength Grade FH40 (full-size; either direction acceptable unless specified). Energies rise with thickness — a 60 mm plate must meet higher values than a 20 mm plate at the same −60 °C. Condition of supply and impact lot size depend on grain-refining practice and thickness (AR/CR/N/TM/QT as permitted). For TMCP FH40, respect Ceq caps ≈ 0.40 % (t≤50) / 0.42 % (50

Thickness tolerance and surface condition

Lloyd’s Register applies IACS UR W13 thickness tolerances unless the PO states otherwise (often 0.3 mm minus class — confirm on PO; see UNCERTAIN). Plus/flatness/width/length per agreed standard (ASTM A6 or EN 10029). Surface quality per EN 10163 or equivalent accepted by LR; state primer/surface class on receipt if needed.

LR LR/FH40 plate stock in China

Thickness (mm)Width (mm)Length (mm)ConditionApprox. quantityLocation
61800 / 20006000 / 8000AR / CR / N / TM100+ tChina
81800 / 20008000 / 12000AR / CR / N / TM200+ tChina
102000 / 22008000 / 12000AR / CR / N / TM200+ tChina
122000 / 2200 / 250012000AR / CR / N / TM200+ tChina
142000 / 220012000AR / CR / N / TM100+ tChina
162000 / 250012000AR / CR / N / TM200+ tChina
202000 / 250012000AR / CR / N / TM100+ tChina
252200 / 250012000AR / CR / N / TM100+ tChina
30220010000 / 12000AR / CR / N / TM100+ tChina
40220010000AR / CR / N / TM50+ tChina
5022008000 / 10000AR / CR / N / TM50+ tChina

Quantities are approximate and change daily (indicative — confirm before booking); all stock plates carry LR/FH40 marking and LR-endorsed mill certificates when sold as LR class plate. Sizes outside the table (for example 3000 mm width, 60–100 mm thickness, or fixed lengths for a cutting plan) are produced in the next mill rolling cycle, typically 3–6 weeks including LR survey. Send your size list and we will reply with what is in stock and what must be rolled.

Packing. Plates are bundled by size with steel strapping, marked with heat number, grade and LR stamp, and shipped in containers (up to about 11.8 m) or break bulk for longer plates.

LR LR/FH40 equivalents in other rules and standards

Standard / societyDesignationComment
LR (Lloyd’s Register)LR/FH40 (LR FH40)this page; stamped under LR survey
ASTM A131/A131MASTM A131/A131M Grade FH40A131 lists AH–FH 32/36/40; product standard only
ABSABS FH40IACS UR W11 higher-strength; live product page
DNVDNV NV F40IACS UR W11; live product page
BVBV Grade FH40IACS UR W11; category link only
CCSCCS FH40IACS UR W11; category link only
NK (ClassNK)NK KF40ClassNK KF40
KRKR RF40KR RF40
RINARINA Grade FH40confirm exact designation per RINA rules
GB 712GB 712 Grade FH40not class approval by itself
Structural (indicative)EN 10025-2 S355JR / S355J2land structural; no class marking

These are comparisons, not substitutions. Multi-class stamps require joint survey before rolling.

LR LR/FH40 vs other LR hull grades

Pick FH40 when the drawing specifies higher-strength grade FH40 (or the society equivalent). Do not substitute ordinary Grade A/B unless the designer recalculates scantlings — yield differs (390 vs 235). Within the 40 band, letter choice is toughness: AH 0 °C → DH −20 °C → EH −40 °C → FH −60 °C. Within the FH letter, strength steps 32 → 36 → 40 raise yield from 315 to 355 to 390 N/mm².

For yields above 390 N/mm² Lloyd’s Register / IACS move to extra-high strength (UR W16 naming — LR uses AH42…AH69, not AH420 / AH70).

When LR LR/FH40 is the right choice: typical uses are low-temperature service: Arctic and polar-class hulls, ice belts and offshore units in cold regions where −60 °C toughness is specified. The Charpy temperature (−60 °C) is fixed by the letter, and the strength by the number (ReH 390 N/mm²). Pick the strength from the scantling calculation and the letter from the material class and design temperature on the approved drawing.

Applications, cutting and welding of LR LR/FH40

Typical uses: low-temperature service: Arctic and polar-class hulls, ice belts and offshore units in cold regions where −60 °C toughness is specified; weight-saving vs ordinary-strength plate in large tankers, bulkers and container ships. See offshore platform steel plates when primary offshore grades apply.

Welding: higher-strength hull steels need approved higher-strength consumables matched to −60 °C weld-metal toughness; preheat and heat input follow the approved WPS and often track Ceq/Pcm from the mill certificate. TMCP FH40 must respect the Ceq caps noted above. Cutting by oxy-fuel/plasma/laser is routine; thick FH plate may need hydrogen control — follow mill recommendations.

Processing notes for LR/FH40: cold forming is routine within normal shipyard radii. Line heating and fairing of TMCP plate should stay within the temperature limits recommended by the mill, because overheating can reduce the strength gained in controlled rolling. Check the delivery condition on the certificate before planning hot forming.

Certificates, LR survey and third-party inspection

Every plate is tested and marked at the mill under Lloyd’s Register survey; the mill certificate lists heat number, ladle chemistry, Ceq where applicable, tensile results (ReH ≥ 390 N/mm², Rm 510–650 N/mm², A ≥ 20 %), Charpy at −60 °C, delivery condition and plate numbers, endorsed by the Surveyor. Optional EN 10204 3.2, UT (U), Z-direction, multi-class.

On receipt: verify LR/FH40 stamp, −60 °C impact data, energies for the delivered thickness band, thickness within UR W13 / PO tolerance, LR endorsement present.

Charpy acceptance for LR/FH40 by thickness (IACS UR W11; actual results as per standard and mill certificate):

Thickness t (mm)Test temperatureAverage energy, longitudinal (J min.)Average energy, transverse (J min.)
t ≤ 50−60 °C3926
50 < t ≤ 70−60 °C4631
70 < t ≤ 100−60 °C5537

If UT or 3.2 was ordered, check the UT report and inspector’s plate list as well.

Common mistakes when ordering LR FH40 / LR/FH40

  • Ordering “LR 40” without the letter (FH/…) — toughness class missing
  • Accepting ordinary-strength Grade A/B certificates for a FH40 PO
  • Ignoring TMCP Ceq caps on TM plate
  • FH chemistry (tighter P/S, N) not checked when the PO says FH
  • Coil-cut plate without coil approval
  • Missing LR endorsement on the MTC

Write grade, delivery condition, impact temperature and certificate type into the PO.

Sourcing LR LR/FH40: buyer concerns and SHH STEEL solutions

ConcernHow SHH STEEL handles it
Fake class plateLR-approved mills only; traceable LR/FH40 stamp + certificate; 3.2 on request
Payment riskT/T or L/C; inspection before balance
Mixed sizes / gradesFH40 combined with LR Grade A/B/D/E or other AH–FH sizes in one container
Lead time visibilityweekly photo updates from dedicated coordinator
Prep before shipcutting, bevelling, drilling, machining in our workshop

How to order LR LR/FH40 plate

Specify LR FH40 (LR/FH40), delivery condition (AR/CR/N/TM/QT as applicable), thickness × width × length × qty, Z/U, multi-class, certificate type, port. Send to SHH STEEL.

Sample PO line: “Steel plate to Lloyd’s Register Rules for Materials, Grade FH40 (LR/FH40), delivery condition [AR/CR/N/TM/QT], 20 × 2500 × 12000 mm, 30 pcs, marked LR FH40 / LR/FH40, certificate endorsed by LR Surveyor, EN 10204 3.2 [if required], UT [if required], CIF [port].”

FAQ

What sizes and minimum order quantity can you supply for LR FH40 / LR/FH40 plate?
IACS UR W11 lists FH40 plate primarily up to 100 mm; thicker plate needs special LR consideration. Most enquiries we receive for FH40 are 8–60 mm thick, 1800–3000 mm wide and 6000–12000 mm long. Popular sizes can come from China stock carrying the LR/FH40 marking, with no fixed minimum. A mill rolling for a special width, thickness above roughly 60 mm or a Z-grade normally needs a minimum quantity per size, which we confirm per order. We can combine several sizes, or FH40 with other hull grades, to reach a rolling or container quantity.
How is LR LR/FH40 certified, and can you arrange EN 10204 3.2 witness inspection?
Every plate is made by an LR-approved mill under Lloyd’s Register survey. It is die-stamped or stencilled LR FH40 / LR/FH40 with the heat or plate number, and the mill test certificate is endorsed by the LR Surveyor. The certificate gives the ladle chemistry, the tensile results (ReH ≥ 390 N/mm², Rm 510–650 N/mm², A ≥ 20 %), the Charpy results at −60 °C, the delivery condition and the plate identity. If your contract asks for EN 10204 3.2, we arrange it before rolling. The witness can be the LR Surveyor, a second class society (dual or multi-class stamping, e.g. LR + ABS or DNV), or a third-party inspector such as SGS or BV. 3.2 cannot be added after testing, so please state it on the enquiry.
What is the impact test temperature and energy for LR FH40 / LR/FH40, and do thickness limits apply?
LR/FH40 is tested at −60 °C. Required average energies (longitudinal/transverse, J min.) under IACS UR W11 rise with thickness: ≤50 mm 39/26; 50–70 mm 46/31; 70–100 mm 55/37. This matters when you order thick FH40: a 60 mm plate must meet higher values than a 20 mm plate at the same −60 °C. The test lot size and the permitted delivery condition (AR, CR, N, TM or QT) follow the UR W11 supply table. Above 100 mm, agree data positions and energies with LR. Results are as per standard and mill certificate.
What welding and preheat guidance applies to LR LR/FH40?
LR/FH40 needs higher-strength welding consumables approved for −60 °C weld-metal toughness. For TMCP plate, Ceq is commonly capped near 0.40 % (t ≤ 50 mm) and 0.42 % (50 < t ≤ 100 mm) under UR W11 practice; above 100 mm it is agreed at mill approval. N or AR plate of the same grade may have a higher actual Ceq, so the delivery condition affects how easy the plate is to weld. Preheat, interpass temperature and heat input must follow your LR-approved WPS. We send the mill certificate’s ladle analysis and Ceq before shipment so the welding engineer can confirm the procedure qualifies. We do not give generic preheat temperatures.
What is the delivery time for LR LR/FH40 plate?
Stock sizes of LR/FH40 can usually be cut, inspected and loaded in about 7–15 days. Mill-rolled orders typically take about 3–6 weeks plus inspection, depending on thickness, delivery condition and the mill schedule. These are commercial estimates, confirmed with each quote. If 3.2 witness or multi-class survey is required, we book the inspector when we place the mill order so testing is not delayed. A dedicated coordinator sends weekly progress photos until the bill of lading is issued.
Which payment terms do you accept for LR FH40, and how is my deposit protected?
We accept T/T or L/C at sight. With T/T, the usual terms are a 30 % deposit and the balance against the documents or after inspection. You or your inspector can check the LR/FH40 stamping, the dimensions and the Surveyor-endorsed certificate before you pay the balance. With L/C, payment is tied to the presented documents. For first orders we can start with a smaller trial lot. The proforma invoice shows the grade (LR/FH40 / LR FH40), sizes and certificate type.
What are the equivalent grades of LR LR/FH40 among class societies and GB 712?
LR/FH40 corresponds to ASTM A131/A131M Grade FH40, ABS FH40, DNV NV F40, BV Grade FH40, CCS FH40, NK KF40, KR RF40, RINA Grade FH40 (confirm RINA designation per rules), and GB 712 Grade FH40. All share yield 390 N/mm², tensile 510–650 N/mm² and a Charpy test at −60 °C under IACS UR W11. Even so, a plate is only accepted by the society whose stamp and certificate it carries. Order LR FH40 for LR class, or ask for multi-class when one stock must serve several projects. GB 712 or A131 certificates alone do not replace the LR/FH40 stamp.
Can you cut, bevel or machine LR LR/FH40 plates, and how are they packed for export?
Yes. In our workshop we can flame, plasma or laser cut FH40 to drawings, bevel weld edges (V, X or K preparation to your angle and land), drill and machine. Every cut piece keeps traceability: we transfer the LR/FH40 marking and heat number before cutting, and the cutting list is tied to the mill certificate. For export, plates are bundled with steel straps and timber spacers, marked with grade, size and heat number, and loaded in containers or as break-bulk. Shot blasting and shop primer are available on request. See SHH STEEL for our processing capabilities.

Conclusion

LR FH40 / LR/FH40 is higher-strength hull steel under Lloyd’s Register Materials rules and IACS UR W11: yield 390 N/mm², tensile 510–650 N/mm², Charpy at −60 °C, marking LR/FH40. Lock on the order: delivery condition, impact lot size, TMCP Ceq if TM, product analysis if needed, multi-class and 3.2.

SHH STEEL supplies LR/FH40 plate rolled by Chinese mills that hold Lloyd’s Register works approval for the grade, so every plate carries the LR/FH40 stamp and a Surveyor-endorsed certificate traceable to its heat. Common thicknesses are available from stock; other sizes are scheduled into the mill rolling cycle with LR survey arranged at the mill. On request we add EN 10204 3.2 certificates with third-party witness (TÜV, SGS, BV or another agency) and joint certification with ABS, DNV, BV, CCS, NK, KR or RINA.

We accept T/T or L/C payment, with inspection before the balance is paid. Small quantities in several sizes, or LR/FH40 mixed with LR Grade A/B/D/E or other AH–FH sizes, can be combined in one container. A dedicated coordinator sends production and shipping updates with photos, and our own workshop cuts to size, bevels, drills and machines plates before shipment so they arrive ready for fabrication.

Request a quotation: send SHH STEEL the grade (LR/FH40 / LR FH40), thickness, width, length, quantity per size and destination port, plus any multi-class, Z/U or 3.2 certificate requirement. We reply with price, available stock and lead time.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *



    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *



      X