NK F40 FH40 shipbuilding steel plate to ClassNK (NK) rules, stacked hull plates

NK F40/FH40 Shipbuilding Steel Plate

NK F40/FH40 (KF40) high-tensile hull structural steel plate to ClassNK Part K: ReH 390 N/mm², Rm 510–650 N/mm², Charpy −60 °C. From NK-approved Chinese mills via SHH STEEL, from stock or mill-rolled, with cutting, dual-class and 3.2 inspection.
Keywords
NK F40/FH40 steel plate, KF40 steel plate, ClassNK KF40, NK FH40 shipbuilding plate, NK F40 marine steel, Nippon Kaiji Kyokai FH40, high tensile hull steel
Equivalent Grades:
DNV VL F40; LR FH40; BV FH40; CCS F40/FH40; KR RF40; ABS FH40; RINA FH40; ASTM A131 FH40; GB 712 FH40
Share:
Overview
Specification
Chemical Composition
Mechanical Properties
Impact Test and Condition of Supply
Thickness Tolerance
Stock
Equivalent Grades
Grade Selection
Applications and Fabrication
Testing and Inspection
Specification Mistakes
Buyer Concerns
How to Order
FAQ
Conclusion

NK F40/FH40 (KF40) shipbuilding steel plate — overview

Technical Reviewer: Jack | SHH STEEL Material Solutions Department · Updated: 2026-10-28

NK F40/FH40 is the −60 °C plate of the 40 level, called KF40 in ClassNK documents. It uses the tighter F chemistry, with lower C, P and S and a nitrogen limit. Level 40 is the top of the UR W11 high-tensile range, chosen for thick deck and hatch-coaming plating where 355 N/mm² is not enough. It gives ReH ≥ 390 N/mm², Rm 510–650 N/mm² and A ≥ 20 %. The title uses the dual trade name (F40/FH40) because Japanese and Chinese buyers search for both forms, but the plate itself is stamped KF40.

Equivalent grades: ASTM A131 Grade FH40 · ABS FH40 · DNV NV F40 · LR FH40 · BV FH40 · CCS F40 / FH40 · KR RF40 · RINA FH40 · GB 712 Grade FH40.

In the ClassNK series the letter sets the test temperature (KA 0 °C, KD −20 °C, KE −40 °C, KF −60 °C) and the number sets the yield (32 → 315, 36 → 355, 40 → 390 N/mm²). KF40 is the F letter at level 40. Typical NK uses: ice-class and polar hulls, Arctic LNG carriers and cold-region offshore units needing −60 °C.

SHH STEEL sources KF40 from Chinese mills that hold NK approval for high-tensile hull steel, with the NK survey at the mill. Stock is held in the common 36-level sizes and other sizes are rolled to order.

KF40 (F40/FH40) key data

ItemNK F40/FH40 / KF40
Governing rulesClassNK Rules for the Survey and Construction of Steel Ships, Part K; IACS UR W11 high-tensile grade FH40 (Part K numbering UNCERTAIN)
NamesNK designation KF40; trade dual F40/FH40; IACS FH40
StrengthReH ≥ 390 N/mm², Rm 510–650 N/mm², A ≥ 20 %
Charpy V−60 °C
Steelmakingkilled, fine-grain treated (Al, Nb, V or Ti)
Delivery conditionAR / CR / N / TM as permitted by thickness and grain refiner (QT where approved)
TMCP carbon equivalentCeq ≤ 0.40 % (t ≤ 50 mm), ≤ 0.42 % (50–100 mm), indicative UR W11 practice — confirm at mill approval
Thicknessup to 100 mm (UR W11 scope); beyond by agreement with ClassNK
ToleranceIACS UR W13 as applied by ClassNK (UNCERTAIN class)
DocumentsNK-endorsed mill certificate; EN 10204 3.1/3.2

Commonly traded KF40 runs 8–60 mm thick in 2000–3000 mm widths. Heavier plate depends on the mill’s NK approval range for the delivery condition.

KF40 chemical composition — heat and product analysis

ElementHeat (ladle) analysis, %Product (check) analysis, %Remark
C0.16 max.numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificateFH column
Mn0.90–1.60numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Si0.10–0.50numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
P0.025 max.numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificateF column tighter
S0.025 max.numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificateF column tighter
Al (acid-soluble)0.015 min. acid-solublenumeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificategrain refiner
Nb0.02–0.05 when used singlynumeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificategrain refiner / strengthening
V0.05–0.10 when used singlynumeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Ti0.02 max.numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Cu0.35 max.numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Cr0.20 max.numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
Ni0.80 max.numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificatehigher allowance in F column
Mo0.08 max.numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificate
N0.009 max. (0.012 if Al present)numeric tolerance not tabulated in ClassNK Part K – agree on order / mill certificateN cap applies to F only
Nb+V+Ti0.12 max. (combined, when used together)not applicable (calculated from heat analysis)combined microalloy cap
Ceq (TM plate)0.40 / 0.42 max. (calculated)not applicable (calculated from heat analysis)for t ≤ 50 / 50–100 mm

Product (check) analysis column: ClassNK Part K specify heat (ladle) limits; no numeric product-analysis tolerance is tabulated in the rule text reviewed, so product (check) limits are agreed on the order or taken from the approved mill specification and certificate.

The ladle values follow IACS UR W11 for high-tensile hull steel, which ClassNK adopts in Part K (not checked against a Part K edition — UNCERTAIN). The F column caps C at 0.16 %, P and S at 0.025 % and N at 0.009 %, and allows Ni up to 0.80 %. Check every one of these on the certificate. For TMCP plate, ask for Ceq (and Pcm if your welding procedure uses it) on the certificate. Product analysis tolerances are agreed case by case.

KF40 tensile requirements

PropertyValue
ReH390 N/mm² min.
Rm510–650 N/mm²
A (5.65√S0)20 % min.
Charpy temperature−60 °C

Flat 200 mm test pieces: minimum elongation by thickness

t (mm)≤55–1010–1515–2020–2525–3030–4040–50
A200 min. %1214151617181920

KA40, KD40, KE40 and KF40 share these values. Only the Charpy temperature and, for KF, the chemistry differ.

KF40: Charpy at −60 °C and delivery condition

ThicknessAvg. long. (J)Avg. trans. (J)
≤ 50 mm3926
50–70 mm4631
70–100 mm5537

Required energy rises with thickness. A 70 mm KF40 plate must reach 55 J longitudinal at −60 °C, against 39 J for plate up to 50 mm. The delivery condition (AR, CR, N or TM) affects batch size and test frequency. For KF plate, mills generally supply TM or N, since as-rolled plate rarely meets −60 °C reliably.

Thickness tolerance and surface quality

Minus tolerance follows IACS UR W13 as ClassNK applies it. Plus tolerance, flatness and dimensions follow the agreed standard (JIS G3193, EN 10029 or GB/T 709). Weight-optimised high-tensile designs leave less margin, so check thickness at several points on receipt.

KF40 stock and lead time

Thickness (mm)Width (mm)Length (mm)ConditionApprox. qty
61800 / 20006000–12000AR / N / TM100+ t
820006000–12000AR / N / TM150+ t
102000 / 22006000–12000AR / N / TM200+ t
122000 / 25006000–12000AR / N / TM200+ t
162200 / 25006000–12000AR / N / TM150+ t
2025006000–12000AR / N / TM120+ t
2525006000–12000AR / N / TM100+ t
302200 / 25006000–12000AR / N / TM80+ t
4022006000–12000AR / N / TM50+ t
5022006000–12000AR / N / TM30+ t

Stock quantities change every week, so confirm before you book. Plates are sold as KF40 with the NK stamp and endorsed certificate. Sizes not in stock are rolled in about 4–6 weeks including survey.

Packing: bundled by size with steel strapping, painted with grade and heat number, shipped in containers (≤11.8 m) or break bulk.

NK F40/FH40 (KF40) compared with other societies

Society / standardGradeNote
ClassNKNK F40/FH40 / KF40this page
DNVDNV VL F40
LRLR FH40
BVBV FH40
CCSCCS F40 / FH40
KRKR RF40
ABSABS FH40
RINARINA FH40 (designation per RINA rules)no product page yet
ASTM A131ASTM A131/A131M Grade FH40product standard only
GB 712GB 712 Grade FH40product standard only

All share the UR W11 FH40 requirements. Each society accepts only its own stamp, so dual certification must be booked before the plates are tested.

Choosing KF40 within the ClassNK high-tensile series

Read across for toughness (KA40 → KD40 → KE40 → KF40) and down for strength (KF32 → KF36 → KF40). ClassNK’s material-grade table fixes the letter from member category and thickness. The designer fixes the number from the scantlings. Substituting a higher letter of the same number is normally accepted; a lower letter is not.

Above 390 N/mm², ClassNK’s extra-high-strength grades start at KA420 (IACS UR W16). See NK Steel Plates for the full series.

Using KF40 in the yard

Uses: ice-class and polar hulls, Arctic LNG carriers and cold-region offshore units needing −60 °C. Welding: use high-tensile consumables approved by ClassNK for −60 °C toughness (grade 5Y or higher, typical — confirm in the WPS). Preheat and heat input come from the NK-approved procedure and the certificate Ceq. Large-heat-input electrogas or one-side SAW on thick KF40 needs a procedure qualified for that heat input.

Forming: TMCP plate gets part of its strength from controlled rolling. Keep line heating within the mill’s temperature limits, typically below about 650 °C for water cooling (UNCERTAIN, mill-specific).

NK survey, certificates and receiving checks

The certificate lists ladle chemistry including microalloys, Ceq for TM plate, tensile results, Charpy results at −60 °C, delivery condition and plate numbers, with the NK endorsement. We can add EN 10204 3.2 third-party witness, UT to EN 10160 or ASTM A578, Z-direction testing, and dual class with ABS, DNV, LR or BV.

On receipt: check the stamp reads KF40, Charpy results are at −60 °C for the right thickness band, and the NK endorsement is present.

Ordering errors seen with KF40

  • Writing only “AH40” or “A40” without stating ClassNK, so the plate arrives with another society’s stamp
  • Omitting the letter, so toughness is undefined
  • Accepting mild-steel KA–KE certificates against a high-tensile order
  • No Ceq on the certificate for TM plate
  • Substituting KA40 without approval
  • F column limits (N, P, S) not checked

Buying KF40 from China: concerns and answers

ConcernAnswer
Is the NK stamp genuine?Only mills with ClassNK approval for KF40; certificate and stamp traceable to the heat; third-party witness on request
Payment safetyT/T with balance after inspection, or L/C at sight
Small or mixed ordersseveral sizes and NK grades in one container
Delivery visibilityweekly photos from rolling to loading
Ready-to-fit partscutting, bevelling and drilling in our own workshop

Ordering KF40

State: NK F40/FH40 (KF40), delivery condition, sizes and quantities, UT/Z, dual-class, certificate type and port. Send to SHH STEEL.

Sample line: “Hull plate to ClassNK Rules Part K, grade KF40 (NK F40/FH40), TM, 25 × 2500 × 12000 mm, 20 pcs, NK-endorsed certificate with Ceq, EN 10204 3.2, CFR Busan/Imabari.”

FAQ

Why is the plate titled F40/FH40 but stamped KF40?
Buyers search for both A/AH-style names, but ClassNK writes its high-tensile grades with a K prefix. The plate and certificate show KF40, which equals IACS FH40.
What are the strength and toughness of KF40?
ReH ≥ 390 N/mm², Rm 510–650 N/mm², A ≥ 20 %. Charpy at −60 °C, from 39 J (≤50 mm) up to 55 J (70–100 mm) longitudinal average.
Is a TMCP KF40 plate easier to weld?
Usually. TM plate carries a Ceq limit of about 0.40 % (≤50 mm) and 0.42 % (50–100 mm), so it needs less preheat. Your NK-approved procedure still decides.
Can one heat be certified as KF40 and as ABS/DNV/LR/BV FH40?
Yes, if all the surveyors are booked before testing and the plate meets every society’s requirements. It is then stamped with each mark.
Which thicknesses of KF40 do you supply?
Typically 8–60 mm from stock or rolling, up to 100 mm by mill approval. KF plate over about 50 mm is limited to a few mills.
What changes between KF32, KF36 and KF40?
Only strength: 315, 355 and 390 N/mm² yield. The Charpy temperature stays the same because the letter is the same.
How long is delivery for KF40?
About 7–15 days from stock, and 4–6 weeks for mill rolling plus survey. Confirmed per quote.
What payment terms do you accept?
T/T with the balance after inspection, or L/C at sight. Trial lots are possible.

Conclusion

NK F40/FH40 (KF40) is ClassNK high-tensile hull steel under Part K of the Rules for the Survey and Construction of Steel Ships: yield 390 N/mm², tensile 510–650 N/mm², Charpy −60 °C. An NK-classed hull accepts it only with the NK stamp and an endorsed certificate.

SHH STEEL supplies KF40 from NK-approved Chinese mills, with cutting, dual class, UT and EN 10204 3.2 on request. Send grade, sizes, quantities and port for a quotation.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *



    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *



      X