ISO 5832-2 Grade 4B Titanium Plate | Cold-Worked Implant Grade 4

ISO 5832-2 Grade 4B titanium plate is cold-worked implant Grade 4 titanium supplied cold worked. It is specified for 680 MPa minimum tensile strength, 520 MPa yield and 10% minimum elongation. Typical uses include craniomaxillofacial and trauma plates. SHH STEEL reviews size, finish and certificate requirements before quoting.
Keywords
ISO 5832-2 Grade 4B titanium plate, Grade 4B titanium plate, cold-worked implant Grade 4 titanium plate, ISO 5832-2 titanium sheet, ISO 5832-2 Grade 4B titanium sheet
Equivalent Grades:
UNS R50700, ASTM B265 Gr.4, ASME SB-265 Gr.4, JIS Class 4 (TP550), GB/T TA4G, ISO 5832-2 Gr.4A, 3.7065
Share:
General Description
Material Specification
Chemical Composition
Mechanical Properties
Delivery Conditions
Weldability
Tolerances
Applications and service limits
Compare
Equivalent Material Grade
Why choose Us
Our Service
FAQ
Conclusion

What is ISO 5832-2 Grade 4B titanium plate?

ISO 5832-2 Grade 4B titanium plate is made to ISO 5832-2, the international standard for unalloyed titanium used to manufacture surgical implants. Grade 4B is the cold-worked condition of Grade 4, with 680 MPa minimum tensile strength. It is used where the highest strength of unalloyed titanium is needed, typically in bar for dental implants, and is less common in plate.

Unalloyed titanium for implants is commercially pure titanium with tightly controlled interstitials. Strength rises with oxygen and iron content, and the material cannot be hardened by heat treatment, so higher strength grades rely on higher interstitials or, for Grade 4B, cold work. Biocompatibility rests on the stable oxide film formed on the surface.

Its typical density of about 4.51 g/cm³ is a little over half that of carbon steel, which is one reason titanium plate is chosen where weight matters.

The ISO 5832 series covers metallic materials for surgical implants; Part 2 covers unalloyed titanium and Part 3 covers Ti-6Al-4V. Grades are defined by oxygen and iron limits and the resulting tensile strength, with Grade 4 available annealed (4A) or cold worked (4B).

SHH STEEL handles Grade 4B plate enquiries within its range of titanium alloy plates and sheets, checking the ordered ISO 5832-2 edition, product form and certificate type before confirming supply. Related designations covered on this site include ASTM B265 Grade 4, ASME SB-265 Grade 4, JIS H4600 Class 4 TP550.

Material specification for ISO 5832-2 Grade 4B

ISO 5832-2 specifies the characteristics of, and test methods for, unalloyed titanium for use in the manufacture of surgical implants. It is a raw-material standard: it covers chemistry, microstructure and mechanical properties, not the finished device. The 2025 edition lists six grades defined by tensile strength.

Ordering item ISO 5832-2 basis
Standard ISO 5832-2; state the edition (2018 or 2025) required by the device file
Grade Grade 4B
Condition Cold worked
Product form Plate or sheet cut to the device maker’s size; bar and wire are also covered by the standard
Microstructure Uniform, grain size not coarser than the specified limit, free of continuous alpha case
Certificate Inspection certificate with chemistry, hydrogen after final processing and mechanical results

Except for hydrogen, chemical requirements may be met by the ingot analysis; hydrogen is determined on the product after the final heat treatment and pickling. Device makers normally add their own requirements for surface condition, traceability and cleanliness on the purchase order.

Device files often cite both ISO 5832-2 and ASTM F67, the ASTM specification for unalloyed titanium for surgical implants. The two are close but not identical in grade limits and test details, so material certified to one standard is not automatically acceptable under the other. If both are named, the certificate must show compliance with each, and the edition of each standard should be fixed in the device technical file.

Chemical composition of ISO 5832-2 Grade 4B

Single values are maximums. Titanium is the balance, and no other elements are intentionally added.

Element Limit, % (mass fraction)
Nitrogen (N) 0.05 max
Carbon (C) 0.08 max
Hydrogen (H) 0.0125 max
Iron (Fe) 0.50 max
Oxygen (O) 0.40 max
Titanium (Ti) Balance

Except for hydrogen, chemical requirements may be met by the ingot analysis. Hydrogen is determined on the product after the final heat treatment and pickling, because surface treatments can raise it.

Mechanical properties of ISO 5832-2 Grade 4B

The values below are the requirements for Grade 4B plate in the cold worked condition.

Property Requirement
Condition Cold worked
Tensile strength Rm, min 680 MPa
0.2% proof strength Rp0.2, min 520 MPa
Elongation after fracture A, min 10%
Reduction of area Z, min —

Tensile tests follow ISO 6892-1 at room temperature. Values are for the cold worked condition. The microstructure must be uniform, with a grain size not coarser than the limit in the standard and no continuous alpha case.

Fatigue and device-level properties are not set by the material standard and must be validated by the device manufacturer.

Delivery condition, finish and marking

Implant-grade plate is supplied in the condition stated for the grade, with a surface agreed with the device manufacturer. Surface contamination, embedded particles and alpha case are not acceptable.

  • Condition: Cold worked
  • Surface: pickled, ground or machined, as agreed
  • Traceability: heat and lot identification on every piece and on the certificate
  • Packing: clean, protected packing that prevents contamination and damage

Material is supplied annealed, except Grade 4B, which is supplied cold worked. Device makers often specify extra cleanliness, inclusion or ultrasonic requirements; include them on the order.

Welding and fabrication of Grade 4B titanium plate

Implant manufacturers rarely weld Grade 4B plate, but where joining is used the same rules as for industrial CP titanium apply: full inert-gas shielding until the metal is below about 400 °C, and no contamination of the surface.

  • Cut and machine with clean, sharp tools and controlled heat
  • Avoid iron pick-up and embedded abrasive; agree pickling or passivation after machining
  • Keep material traceability to heat and lot through every processing step
  • Qualify any welding or forming route as part of the device validation

Forming of plate for craniofacial and trauma parts is normally done on annealed material, with bend radii and springback set by the device maker’s process qualification.

Machining for implants uses sharp tools, controlled speeds and clean coolant that is compatible with the later cleaning process. Surface layers affected by machining or grinding are removed or controlled by the device maker’s validated finishing route.

These are general practices, not a qualified procedure. The fabricator must qualify the welding procedure, filler metal and inspection to the applicable code.

Dimensional tolerances and flatness

ISO 5832-2 does not set plate dimensional tolerances; these are agreed between the device manufacturer and the supplier, often by drawing or by reference to an industrial plate standard.

State thickness, width, length, flatness, surface roughness and any cut-to-size drawing on the order. No stock sizes are implied by this page.

Titanium plate can be cut by waterjet, abrasive saw, plasma or machining. Thermal cutting leaves an oxygen-enriched edge that should be removed by machining or grinding before welding or forming, so agree the cut-edge condition and any machining allowance on the order.

Applications and service limits of Grade 4B titanium plate

Typical uses of Grade 4B plate include:

  • Craniomaxillofacial and trauma plates
  • Bone plates, mesh and reconstruction plates
  • Dental implant and abutment blanks
  • Instrument and device components to the device maker’s drawing

Cold-worked Grade 4B and annealed Grade 4A are not interchangeable. ISO 5832-2 covers the raw material only. Fitness for a medical device depends on the design, processing, cleaning, sterilisation and regulatory approval, which are the device manufacturer’s responsibility. The material should not be bought to this standard for industrial process equipment, where ASTM B265 or similar industrial specifications apply.

When selecting Grade 4B, compare it with Grade 1 ELI, Grade 1, Grade 2. The choice usually turns on the balance of strength, formability, corrosion behaviour in the actual medium and cost, and on which standard the drawing or design code names.

Compare Grade 4B with other ISO 5832-2 grades

The grades below are the closest neighbours of Grade 4B in ISO 5832-2. Values are tensile strength, 0.2% yield or proof strength and minimum elongation, as set by the standard.

Grade Tensile strength Yield / proof strength Elongation, min Typical role
Grade 1 ELI 200 MPa 140 MPa min 30% Lowest-interstitial implant grade
Grade 1 240 MPa 170 MPa min 24% Most ductile standard implant grade
Grade 2 345 MPa 275 MPa min 20% Common orthopaedic CP grade
Grade 3 450 MPa 380 MPa min 18% Higher-strength implant CP grade
Grade 4A 550 MPa 483 MPa min 15% Annealed Grade 4
Grade 4B 680 MPa 520 MPa min 10% Cold-worked Grade 4

Higher-oxygen grades give more strength but less ductility. Grade 4A and Grade 4B differ in condition, not in chemistry, and must not be interchanged without device-level review.

ISO 5832-2 Grade 4B equivalent grades

The designations below are commonly compared with ISO 5832-2 Grade 4B. They are close in composition and role, but limits, tests and product forms are set by each standard, so they are not automatically interchangeable.

Standard / system Designation Relationship to ISO 5832-2 Grade 4B
ASTM B265 Grade 4 Close equivalent; ASTM limits and tests apply
ASME SB-265 Grade 4 ASME Code version of the ASTM grade; ordered for pressure equipment
JIS H4600 Class 4 (TP550) Close equivalent; JIS strength range and tests differ
GB/T 3621 TA4G Close equivalent; confirm grade name and limits in the ordered edition
ISO 5832-2 Grade 4A Implant-grade counterpart; medical scope and tighter controls
UNS R50700 Same unified number as ASTM Grade 4
DIN / EN material number 3.7065 (Ti 4) Close CP equivalent

Where a drawing names one designation and the supplier offers another, agree in writing which standard governs chemistry, tensile values, testing and marking. Dual or multiple certification is possible only when the material meets every cited standard in full, and the certificate must show the results against each one.

Why choose SHH STEEL for Grade 4B titanium plate

SHH STEEL supports specification-led purchasing of titanium plate and sheet.

  • We quote to the ISO 5832-2 edition required by your device file
  • Certificates are checked against the Grade 4B chemistry, hydrogen, tensile and microstructure requirements
  • Sizes, quantities, testing and delivery are confirmed in the quotation, not assumed
  • Finish, marking and packing are agreed before production

Questions on equivalents, dual certification or edition changes are answered before an order is placed.

How to enquire for ISO 5832-2 Grade 4B plate

Send the material schedule with the details below. We review the enquiry and raise any open points before confirming the supply route.

Enquiry item Information required
Material ISO 5832-2 Grade 4B, edition
Product form Plate or sheet; device drawing if cut to size
Dimensions Thickness, width, length, quantity and any cutting drawing
Finish Descaled, sandblasted, ground or other agreed surface
Testing Hydrogen after final processing, microstructure and any device-specific tests
Documents Certificate type and any third-party inspection
Destination Delivery place and packing requirements

FAQ

Can ISO 5832-2 Grade 4B be used for industrial equipment?
It can be supplied, but ISO 5832-2 is a raw-material standard for surgical implants and costs more to certify. Industrial process equipment is normally ordered to ASTM B265 or a similar industrial plate standard.
What is the tensile strength of ISO 5832-2 Grade 4B titanium plate?
The requirement is 680 MPa minimum. The 0.2% proof or yield strength is 520 MPa minimum. Minimum elongation is 10%. Values apply to the condition and thickness range stated in the standard.
What is Grade 4B mainly used for?
Typical uses include craniomaxillofacial and trauma plates, bone plates, mesh and reconstruction plates and dental implant and abutment blanks. Cold-worked Grade 4B and annealed Grade 4A are not interchangeable.
Does ISO 5832-2 set plate dimensions?
No. It sets chemistry, microstructure and mechanical properties. Dimensions, tolerances and surface condition are agreed between the device maker and the supplier, usually by drawing.
What should I send for a quotation?
Send ISO 5832-2 Grade 4B, the edition, product form, thickness, width, length and quantity, the finish, any special testing, the certificate type and the destination.

Request a quotation for ISO 5832-2 Grade 4B titanium plate

ISO 5832-2 Grade 4B is cold-worked implant Grade 4 titanium specified for 680 MPa minimum tensile strength, 520 MPa minimum yield or proof strength and 10% minimum elongation in the cold worked condition. Typical uses include craniomaxillofacial and trauma plates and bone plates, mesh and reconstruction plates.

Send the product form, sizes, quantity, finish, certificate type and destination to SHH STEEL. Compare other grades on the ISO 5832-2 page or browse all titanium alloy plates and sheets. Availability, testing and delivery are confirmed against each enquiry.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X